CN104470256B - A kind of ink for screen printing technique of flexible circuitry edge connector - Google Patents

A kind of ink for screen printing technique of flexible circuitry edge connector Download PDF

Info

Publication number
CN104470256B
CN104470256B CN201410709888.6A CN201410709888A CN104470256B CN 104470256 B CN104470256 B CN 104470256B CN 201410709888 A CN201410709888 A CN 201410709888A CN 104470256 B CN104470256 B CN 104470256B
Authority
CN
China
Prior art keywords
ink
green oil
wiring board
half tone
screen printing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410709888.6A
Other languages
Chinese (zh)
Other versions
CN104470256A (en
Inventor
张美林
赵虎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Xinyu Tengyue Electronics Co Ltd
Original Assignee
Shenzhen Xinyu Tengyue Electronics Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Xinyu Tengyue Electronics Co Ltd filed Critical Shenzhen Xinyu Tengyue Electronics Co Ltd
Priority to CN201410709888.6A priority Critical patent/CN104470256B/en
Publication of CN104470256A publication Critical patent/CN104470256A/en
Application granted granted Critical
Publication of CN104470256B publication Critical patent/CN104470256B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of ink for screen printing technique of flexible circuitry edge connector, including:Line film modification is carried out, width is respectively etched at the two ends for covering each single-piece of copper face of base material and is 0.1mm contraposition tag line, and carries out green oil half tone data modification;The photoresists for choosing 120T mesh numbers, 18N/cm tension force and 45 degree of polyester net and 10um thickness carry out preparation before printing down, then go out to shine the green oil film according to the test harmomegathus value for treating golden finger wiring board on ink for screen printing and shine green oil half tone;On the premise of without profit is opened, using hat product L45LG20 thermosetting green oils, according to L45LG20:H43a=94:6 ratios carry out ink formulation;Contraposition printing is carried out using screen printer;Preliminary drying and solidification are carried out to the wiring board printed.The present invention has the advantages that aligning accuracy is high, technique is simple, flexibility is good and is easily controlled, in the manufacture that can be widely applied to wiring board.

Description

A kind of ink for screen printing technique of flexible circuitry edge connector
Technical field
The present invention relates to the manufacturing process of wiring board, especially a kind of ink for screen printing technique of flexible circuitry edge connector.
Background technology
Develop as electronic product is intended to " light, thin, convenient " change, FPC is widely used in each electronic product In, play a part of being electrically connected electronic component, become the widely used important accessory of electronics industry.The gold of FPC Finger, is being commonly called as the edge connector that FPC is connected with each other, itself is a part for FPC, by flexible circuitry Copper foil layer one end extension of plate is formed.
The bending protection of current FPC, especially printed circuit board is mainly by printing-ink covering come real Existing, it is designed with wide 1mm cover layer bridge to stop that green oil permeates in golden finger and bent area.With communication electronic device Develop rapidly, to the cabling requirement more and more higher of wiring board, it is desirable to which inner bending effect in bent area is consistent, and wiring board is bent Area's inner width 1mm cover layer bridges have had a strong impact on bending performance, therefore remove wide 1mm cover layer bridge and directly print golden on ink Finger is into new developing direction.
However, current golden finger printing-ink technique has following shortcoming or deficiency:
(1), existing technique is typically using the contraposition of 4 jiaos of crosses, it is impossible to clearly examine the printing effect of single-piece, it is right Position precision is low, it is impossible to ensure the length of golden finger in the range of customer requirement.
(2), using green oil bar replace PI in existing green oil bent area(Polyimides)Bar can also realize that golden finger prints Brush ink, it needs increase photosensitive-ink to be covered in golden finger area, first passes through exposure imaging and go out one and PI bar said functions Ink strip, then ink for screen printing is in bent area, and weak point is that it needs multiple printing-ink, and technique is more complicated and easily causes The bending effect of ink overlapping is harder, and flexibility is poor.
(3), prior art typically printed using 120T, 0 degree of polyester net, the green oil pattern edge printed out is sawed Dentation, it is impossible to control the length of golden finger.
The content of the invention
In order to solve the above-mentioned technical problem, the purpose of the present invention is:There is provided a kind of aligning accuracy height, technique simple, soft Property it is good and be easily controlled, the ink for screen printing technique of flexible circuitry edge connector.
The technical solution adopted for the present invention to solve the technical problems is:
A kind of ink for screen printing technique of flexible circuitry edge connector, including:
S1, progress line film modification, it is 0.1mm's that width is respectively etched at the two ends for covering each single-piece of copper face of base material Tag line is aligned, and carries out green oil half tone data modification, pair that the contraposition tag line and substrate location for making green oil half tone are etched Bit identification line is completely superposed;
S2, the photoresists for choosing 120T mesh numbers, 18N/cm tension force and 45 degree of polyester net and 10um thickness are shone Preparation before version, then goes out to shine the green oil film according to the test harmomegathus value for treating golden finger wiring board on ink for screen printing and shines green oil Half tone;
S3, on the premise of without profit is opened, using hat product L45LG20 thermosetting green oils, according to L45LG20:H43a= 94:6 ratios carry out ink formulation;
S4, the contraposition tag line of single-piece and the wide contraposition marks of the 0.1mm of wiring board single-piece etching on green oil half tone is ensured On the premise of line is overlapped, contraposition printing is carried out to wiring board using screen printer;
S5, preliminary drying and solidification are carried out to the wiring board that prints, so that ink and wiring board are combined closely.
Further, the step S1 will also be met when carrying out green oil half tone data modification:The print of green oil half tone after modification Map brushing shape inside contracts 0.2mm with respect to client's green oil tag line.
Further, the step S1 will also be met when carrying out green oil half tone data modification:Green oil half tone opens after modification Window position press against golden finger at least 0.2mm, if length not enough if need the extension of golden finger to 0.2mm.
Further, the technological parameter of screen printer is in the step S4:Continuous precision is 0.05mm, and silk-screen speed is less than 5 Lattice, scraper angle is 15 degree, nets a width of 1-5mm.
Further, the step S5, it includes:
S51, by the green oil wiring board printed stand 15-30 minutes;
S52, the preliminary drying under 70 degrees Celsius of temperature conditionss to the progress 20 minutes of green oil wiring board;
S53, under 150 degrees Celsius of temperature conditionss, the ink solidification of 60 minutes is carried out to pre-baked green oil wiring board.
The beneficial effects of the invention are as follows:Employ single-piece technique of counterpoint, flexible printed circuit board base material to cover copper face every The two ends of individual single-piece respectively etch width 0.1mm to bit line, can clearly examine the printing effect of single-piece, and aligning accuracy is high, It can guarantee that the length of golden finger in the range of customer requirement;Golden finger silk-screen is same green by hat product L45LG20 thermosettings The ink of oil allotment, no to need multiple printing-ink, technique is simple and better softness;Using 120T, 45 degree of polyester net Instead of traditional 120T, 0 degree of polyester net, green oil edge relatively smooth straight line can be printed out, so as to form shape The green oil covering golden finger of specification, it is easy to control the length of golden finger.Further, the printed pattern of green oil half tone is relative after modification Client's green oil tag line inside contracts 0.2mm, it is ensured that green oil oil spillage, relatively reliable.Further, after modification green oil half tone windowing Position press against golden finger at least 0.2mm, prevent from causing green oil along the oil spillage between finger because the finger for the position that opens a window is too short It is different, it is relatively reliable.
Brief description of the drawings
The invention will be further described with reference to the accompanying drawings and examples.
Fig. 1 is a kind of flow chart of the ink for screen printing technique of flexible circuitry edge connector of the invention;
Fig. 2 is step S5 of the present invention flow chart;
Fig. 3 is the process chart of the embodiment of the present invention one;
Fig. 4 is the schematic diagram that base material copper of the present invention etches silk-screen contraposition;
Fig. 5 is the schematic diagram that green oil half tone of the present invention aligns tag line.
Reference:1st, client's green oil tag line;2nd, the contraposition tag line that substrate location is etched;3rd, pair of green oil half tone Bit identification line.
Embodiment
Reference picture 1, a kind of ink for screen printing technique of flexible circuitry edge connector, including:
S1, progress line film modification, it is 0.1mm's that width is respectively etched at the two ends for covering each single-piece of copper face of base material Tag line is aligned, and carries out green oil half tone data modification, pair that the contraposition tag line and substrate location for making green oil half tone are etched Bit identification line is completely superposed;
S2, the photoresists for choosing 120T mesh numbers, 18N/cm tension force and 45 degree of polyester net and 10um thickness are shone Preparation before version, then goes out to shine the green oil film according to the test harmomegathus value for treating golden finger wiring board on ink for screen printing and shines green oil Half tone;
S3, on the premise of without profit is opened, using hat product L45LG20 thermosetting green oils, according to L45LG20:H43a= 94:6 ratios carry out ink formulation;
S4, the contraposition tag line of single-piece and the wide contraposition marks of the 0.1mm of wiring board single-piece etching on green oil half tone is ensured On the premise of line is overlapped, contraposition printing is carried out to wiring board using screen printer;
S5, preliminary drying and solidification are carried out to the wiring board that prints, so that ink and wiring board are combined closely.
Wherein, L45LG20, H43a and the allotment ratio between them are provided by ink manufacturer.L45LG20 is ink Host, H43a is ink solidification agent.
It is further used as preferred embodiment, the step S1 will also be met when carrying out green oil half tone data modification: The printed pattern of green oil half tone inside contracts 0.2mm with respect to client's green oil tag line after modification.
Further, the step S1 will also be met when carrying out green oil half tone data modification:Green oil half tone opens after modification Window position press against golden finger at least 0.2mm, if length not enough if need the extension of golden finger to 0.2mm.
It is further used as preferred embodiment, the technological parameter of screen printer is in the step S4:Continuously precision is 0.05mm, silk-screen speed is less than 5 lattice, and scraper angle is 15 degree, nets a width of 1-5mm.
Reference picture 2, is further used as preferred embodiment, the step S5, and it includes:
S51, by the green oil wiring board printed stand 15-30 minutes;
S52, the preliminary drying under 70 degrees Celsius of temperature conditionss to the progress 20 minutes of green oil wiring board;
S53, under 150 degrees Celsius of temperature conditionss, the ink solidification of 60 minutes is carried out to pre-baked green oil wiring board.
The present invention is described in further detail with reference to specific embodiment.
Embodiment one
As shown in figure 3, the ink for screen printing technique of the flexible printed circuit board golden finger of the present invention, including data modification, net Version prepares, contraposition printing and preliminary drying are with solidifying this five processes.This five processes are introduced one by one separately below:
(One)Data modification
The data modification process of the present invention includes:
(1)Line film change, base material cover copper face etch each single-piece two ends etch width be 0.1mm pair Bit identification line(The contraposition tag line 2 that i.e. Fig. 4 substrate location is etched);
(2)Green oil half tone data modification, ink tag line of the printed pattern with respect to customer requirement of green oil half tone(That is Fig. 4 Client's green oil tag line 1)0.2mm is inside contracted as green oil oil spillage, green oil half tone windowing position ensures to press against golden finger 0.2mm More than, needed when not enough finger extension to 0.2mm, prevent that the finger of windowing position is too short, and because ditch effect causes Green oil is different along the oil spillage between finger.
Moreover, it is noted that the contraposition tag line of green oil half tone during modification(As shown in Figure 5)Etch what is come with substrate location Bit line must be overlapped.
(Two)Half tone prepares
The tension force of polyester net of the present invention is 18N/cm and mesh number is 120T, it is therefore an objective to ensure that green oil thickness is requiring 10- In the range of 18um;The thickness control of photoresists is 10um, it is intended that reduce oil spillage of the ink between finger;Polyester net is adopted With 45 degree of inclined wires, it is therefore an objective to allow the green oil pattern edge printed out to form uniform straight line, it is easy to the length progress to golden finger Control.
After the completion of polyester net and photoresists are chosen, it is possible to according to the harmomegathus for treating that finger wiring board is tested on ink for screen printing It is worth the solarization green oil film and shines half tone, this process must also ensures that the contraposition tag line of half tone and wiring board is completely superposed.
(Three)Ink formulation
The present invention uses hat product L45LG20 thermosetting green oils, without profit is opened, according to L45LG20:H43a=94:6 ratios Carry out ink formulation.100g ink is such as allocated, first can be placed in weighed using electronic scale 94 grams of L45LG20 ink hosts once Property cup in, then 6 grams of H43a curing agent are added to sanitary cup, and host is well mixed with curing agent by stirring, Just can normally it be used after standing 10 minutes.
(Four)Contraposition printing
The present invention must etch the contraposition tag line of single-piece on green oil half tone and wiring board single-piece when carrying out contraposition printing Out 0.1mm width contraposition tag line overlap, therefore require screen printer continuous precision be 0.05mm, silk-screen speed be 5 lattice with Under, scraper angle is 15 degree, and net is away from for 1-5mm, so that the pattern printed out is smooth.
(Five)Preliminary drying and solidification
The green oil wiring board printed first stands 15-30 minutes, is then solidified by the way of segmentation baking:First 70 degrees Celsius, 20 minutes of stage preliminary drying;Second stage solidifies 150 degrees Celsius, 60 minutes.
The bubble produced when 15-30 minutes being and printing to allow is stood to overflow;The purpose of preliminary drying is slowly to drive away in green oil The solvent in face, prevents that golden finger length is different caused by solvent volatilization is too fast;Ink solidification is carried out again after 20 minutes preliminary dryings, is made Ink is closely linked with wiring board.
The flexible printed circuit board golden finger ink for screen printing technique of the present invention, can obtain the golden finger silk-screen of ideal form Ink, and this technique is simple, is easily controlled, cost is low.
Above is the preferable implementation to the present invention is illustrated, but the invention is not limited to the implementation Example, those skilled in the art can also make a variety of equivalent variations or replace on the premise of without prejudice to spirit of the invention Change, these equivalent deformations or replacement are all contained in the application claim limited range.

Claims (5)

1. a kind of ink for screen printing technique of flexible circuitry edge connector, it is characterised in that:Including:
Step S1, progress line film modification, it is 0.1mm's that width is respectively etched at the two ends for covering each single-piece of copper face of base material Tag line is aligned, and carries out green oil half tone data modification, pair that the contraposition tag line and substrate location for making green oil half tone are etched Bit identification line is completely superposed;
Step S2, the photoresists for choosing 120T mesh numbers, 18N/cm tension force and 45 degree of polyester net and 10um thickness are shone Preparation before version, then goes out to shine the green oil film according to the test harmomegathus value for treating golden finger wiring board on ink for screen printing and shines green oil Half tone;
Step S3, on the premise of without profit is opened, using hat product L45LG20 thermosetting green oils, according to L45LG20:H43a= 94:6 mass ratio carries out ink formulation, and the H43a is ink solidification agent;
Step S4, the contraposition tag line of single-piece and the wide contraposition marks of the 0.1mm of wiring board single-piece etching on green oil half tone is ensured On the premise of line is overlapped, contraposition printing is carried out using screen printer;
Step S5, preliminary drying and solidification are carried out to the wiring board that prints, so that ink and wiring board are combined closely.
2. a kind of ink for screen printing technique of flexible circuitry edge connector according to claim 1, it is characterised in that:The step Rapid S1 will also be met when carrying out green oil half tone data modification:The printed pattern of green oil half tone is identified with respect to client's green oil after modification Line inside contracts 0.2mm.
3. a kind of ink for screen printing technique of flexible circuitry edge connector according to claim 2, it is characterised in that:The step Rapid S1 will also be met when carrying out green oil half tone data modification:The windowing position of green oil half tone press against golden finger at least after modification 0.2mm, if length not enough if need the extension of golden finger to 0.2mm.
4. a kind of ink for screen printing technique of flexible circuitry edge connector according to claim 2, it is characterised in that:
The technological parameter of screen printer is in the step S4:Continuous precision is 0.05mm, and silk-screen speed is less than 5 lattice, scraper angle For 15 degree, a width of 1-5mm is netted.
5. a kind of ink for screen printing technique of flexible circuitry edge connector according to claim 1, it is characterised in that:The step Rapid S5, it includes:
S51, by the green oil wiring board printed stand 15-30 minutes;
S52, the preliminary drying under 70 degrees Celsius of temperature conditionss to the progress 20 minutes of green oil wiring board;
S53, under 150 degrees Celsius of temperature conditionss, the ink solidification of 60 minutes is carried out to pre-baked green oil wiring board.
CN201410709888.6A 2014-11-28 2014-11-28 A kind of ink for screen printing technique of flexible circuitry edge connector Active CN104470256B (en)