CN104445873A - 能够延龄的玻璃熔窑池壁砖 - Google Patents

能够延龄的玻璃熔窑池壁砖 Download PDF

Info

Publication number
CN104445873A
CN104445873A CN201410753473.9A CN201410753473A CN104445873A CN 104445873 A CN104445873 A CN 104445873A CN 201410753473 A CN201410753473 A CN 201410753473A CN 104445873 A CN104445873 A CN 104445873A
Authority
CN
China
Prior art keywords
wall brick
hole
pipeline
side wall
service life
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201410753473.9A
Other languages
English (en)
Inventor
赵迎珂
李道云
刘清
梅红锦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China Triumph International Engineering Co Ltd
Original Assignee
China Triumph International Engineering Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China Triumph International Engineering Co Ltd filed Critical China Triumph International Engineering Co Ltd
Priority to CN201410753473.9A priority Critical patent/CN104445873A/zh
Publication of CN104445873A publication Critical patent/CN104445873A/zh
Withdrawn legal-status Critical Current

Abstract

一种能够延龄的玻璃熔窑池壁砖,所述砖体内部形成有贯通的孔洞,以供管道穿过此孔洞。根据本发明的能够延龄的玻璃熔窑池壁砖,具有冷却效果好、冷却效率高、耐侵蚀性能强的优点,从而达到延长池壁砖使用寿命的效果。

Description

能够延龄的玻璃熔窑池壁砖
技术领域
本发明涉及能够延龄的玻璃熔窑池壁砖结构。
背景技术
在玻璃生产过程中,玻璃熔窑熔化部池壁砖与玻璃液面的三相界面处因高温极端环境及高温玻璃液的持续冲刷等原因,池壁砖上部侵蚀严重,影响了玻璃熔窑的使用寿命。为了减缓熔化部池壁砖的侵蚀,现行的手段主要有在池壁砖的外侧吹风冷却和贴冷却水包,但这两种冷却手段效率较低,能耗较高,对池壁砖的保护效果一般。
发明内容
本发明旨在解决玻璃熔窑熔化部池壁砖局部侵蚀严重、寿命短的问题,而提供的一种能够延龄的玻璃熔窑池壁砖结构。
为了达成上述目的,提供了一种能够延龄的玻璃熔窑池壁砖,所述砖体内部形成有贯通的孔洞,以供管道穿过此孔洞。
一些实施例中,所述孔洞在制造玻璃熔窑池壁砖时被预制在砖体内部。
一些实施例中,所述孔洞可为矩形或者圆形。
一些实施例中,所述管道与熔窑池壁砖冷却系统管路连接。
一些实施例中,所述熔窑池壁砖冷却系统向所述管道供应冷却介质。
一些实施例中,所述冷却介质为空气或水。
根据本发明的能够延龄的玻璃熔窑池壁砖,具有冷却效果好、冷却效率高、耐侵蚀性能强的优点,从而达到延长池壁砖使用寿命的效果。
以下结合附图,通过示例说明本发明主旨的描述,以清楚本发明的其他方面和优点。
附图说明
结合附图,通过下文的详细说明,可更清楚地理解本发明的上述及其他特征和优点,其中:
图1为根据本发明实施例的壁砖的侧视图;
图2为沿图1中的1-1线的剖视图;
图3为根据本发明另一实施例的壁砖的侧视图;
图4为沿图1中的2-2线的剖视图。
具体实施方式
参见本发明具体实施例的附图,下文将更详细地描述本发明。然而,本发明可以以许多不同形式实现,并且不应解释为受在此提出之实施例的限制。相反,提出这些实施例是为了达成充分及完整公开,并且使本技术领域的技术人员完全了解本发明的范围。
现参考附图,详细说明根据本发明实施例的一种能够延龄的玻璃熔窑池壁砖,所述砖体内部形成有贯通的孔洞,以供管道穿过此孔洞。
如图1和2所示,池壁砖砖体1中形成有贯穿孔洞,管道2通过所述贯穿孔洞。所述孔洞在制造玻璃熔窑池壁砖时被预制在砖体内部。所述孔洞可为矩形或者圆形。所述管道与熔窑池壁砖冷却系统管路连接。所述熔窑池壁砖冷却系统向所述管道供应冷却介质。所述冷却介质为空气或水。
制造玻璃熔窑池壁砖时,砖体内部预制贯通的孔洞,安装池壁砖时,用管道穿过此孔洞,并与熔窑池壁砖冷却系统管路连接。如图1和2所示,预制的孔洞可为矩形,或者如图2和3所示,预制的孔洞可为圆形,只要便于管道的选材即可。应理解,所述预制的孔洞的形状不限于圆形或矩形,而是可为任何容易加工的形状。
在玻璃熔窑生产时,熔窑池壁砖冷却系统供应的冷却介质(空气或水)在贯通池壁砖的管道中流动,从而迅速带走砖体热量,大幅度降低砖体温度。另一方面由于内部冷却强度高,可实现与高温玻璃液接触的池壁砖表层保持在较低温度,从而使接触池壁砖表层区域的玻璃液温度降低并凝固附着在池壁砖表面形成保护层。这两方面均可减缓池壁砖的侵蚀,延长砖体的寿命。
根据本发明的能够延龄的玻璃熔窑池壁砖,具有冷却效果好、冷却效率高、耐侵蚀性能强的优点,从而达到延长池壁砖使用寿命的效果。
以上详细描述了本发明的较佳具体实施例。应当理解,本领域的普通技术人员无需创造性劳动就可以根据本发明的构思做出诸多修改和变化。凡本技术领域中技术人员依本发明的构思在现有技术的基础上通过逻辑分析、推理或者有限的实验可以得到的技术方案,皆应在由权利要求书所确定的保护范围内。

Claims (6)

1.一种能够延龄的玻璃熔窑池壁砖,其特征在于,所述砖体内部形成有贯通的孔洞,以供管道穿过此孔洞。
2.根据权利要求1所述的壁砖,其特征在于,所述孔洞在制造玻璃熔窑池壁砖时被预制在砖体内部。
3.根据权利要求2所述的壁砖,其特征在于,所述孔洞可为矩形或者圆形。
4.根据权利要求3所述的壁砖,其特征在于,所述管道与熔窑池壁砖冷却系统管路连接。
5.根据权利要求4所述的壁砖,其特征在于,所述熔窑池壁砖冷却系统向所述管道供应冷却介质。
6.根据权利要求5所述的壁砖,其特征在于,所述冷却介质为空气或水。
CN201410753473.9A 2014-12-10 2014-12-10 能够延龄的玻璃熔窑池壁砖 Withdrawn CN104445873A (zh)