CN104131301B - 一种添加杀菌防腐剂的适用于钢铁的抛光液及其制备方法 - Google Patents

一种添加杀菌防腐剂的适用于钢铁的抛光液及其制备方法 Download PDF

Info

Publication number
CN104131301B
CN104131301B CN201410308848.0A CN201410308848A CN104131301B CN 104131301 B CN104131301 B CN 104131301B CN 201410308848 A CN201410308848 A CN 201410308848A CN 104131301 B CN104131301 B CN 104131301B
Authority
CN
China
Prior art keywords
polishing fluid
auxiliary agent
water
iron
steel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410308848.0A
Other languages
English (en)
Other versions
CN104131301A (zh
Inventor
王慧
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Hong Energy Saving Equipment Co ltd
Original Assignee
Anhui Hong Energy Saving Equipment Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Hong Energy Saving Equipment Co ltd filed Critical Anhui Hong Energy Saving Equipment Co ltd
Priority to CN201410308848.0A priority Critical patent/CN104131301B/zh
Publication of CN104131301A publication Critical patent/CN104131301A/zh
Application granted granted Critical
Publication of CN104131301B publication Critical patent/CN104131301B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种添加杀菌防腐剂的适用于钢铁的抛光液,其特征在于,由下列重量份的原料制成:柠檬酸2-3、硫酸亚铁3-5、硅酸钠4-6、次氯酸钠1-2、二硫化钼4-6、尼泊金甲酯2-4、偏硼酸钠2-4、葡糖糖酸钠3-4、甲醇4-6、氧化铬1-2、OP-10?3-5、助剂5-7、去离子水300;本发明配方合理,除了具有传统的柠檬酸等成分,加入了表面活性剂以及助剂,具有良好的分散、润滑、成膜性,能够在钢铁表面形成一层保护膜,防止空气对高温工件的腐蚀,而且抛光液为水基配方,提升了冷却效果;本发明抛光液添加了尼泊金甲酯等杀菌防腐成分,保存更长久,质量均以稳定,抛光效果好。

Description

一种添加杀菌防腐剂的适用于钢铁的抛光液及其制备方法
技术领域
本发明涉及表面处理技术领域,特别是一种添加杀菌防腐剂的适用于钢铁的抛光液及其制备方法。
背景技术
钢铁材料在加工成形后表面通常会附着一层油污或其它化学制剂,使用一段时间后由使用环境的腐蚀,在表面会产生锈迹,为了美观和延长使用寿命,常用专用的金属清洗剂或抛光剂来清理表面的污物,但现有抛光剂产品存在返锈快、清洗不彻底、抛光性能较弱,容易产生气味、抛光后表面挂灰、抛光后容易生锈,抛光液容易腐败等问题,本发明即对该混合抛光液的技术改进,发现通过将磨料研磨过与表面活性剂混合,不仅可以起到润滑磨料的效果,而且可以在金属加工表面形成一层保护膜,防止表层被空气腐蚀,而且采用水基制成,在钢铁工件抛光时产生的大量热量,冷却的效果良好。
发明内容
本发明的目的是提供一种添加杀菌防腐剂的适用于钢铁的抛光液及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种添加杀菌防腐剂的适用于钢铁的抛光液,由下列重量份的原料制成:柠檬酸2-3、硫酸亚铁3-5、硅酸钠4-6、次氯酸钠1-2、二硫化钼4-6、尼泊金甲酯2-4、偏硼酸钠2-4、葡糖糖酸钠3-4、甲醇4-6、氧化铬1-2、OP-10 3-5、助剂5-7、去离子水300;
所述助剂由以下重量份的原料制成:三氧化二铝4-6、纳米二氧化钛5-7、硅酸钠1-2、丙二醇甲醚醋酸酯3-4、十二碳醇酯2-3、丙烯酸甲酯2-4、交联羧甲基纤维素钠2-3、乳化剂BP4-5、水50-54;制备方法是首先将三氧化二铝、纳米二氧化钛、交联羧甲基纤维素钠、乳化剂BP加入一半量的水中,研磨1-2小时,然后缓慢加入其余剩余成分,缓慢加热至70℃-80℃,在300-500转/分条件下搅拌反应30-50分钟,冷却至室温即得。
本发明所述一种添加杀菌防腐剂的适用于钢铁的抛光液,由以下具体步骤制成:
(1)将二硫化钼、氧化铬、OP-10混合均匀,加入适量的去离子水,加热至30℃-40℃,研磨30-40分钟,得到混合A料;
(2)将除助剂之外的其余剩余成分加入到反应釜中,搅拌混合均匀,缓慢加热至35℃-45℃,保温1-1.5小时,得到混合B料;
(3)将保温的混合B料边搅拌边缓慢加入到混合A料中,充分搅拌后加入助剂,继续搅拌20-30分钟,冷却至室温即得。
本发明的优异效果是:本发明配方合理,除了具有传统的柠檬酸等成分,加入了表面活性剂以及助剂,具有良好的分散、润滑、成膜性,能够在钢铁表面形成一层保护膜,防止空气对高温工件的腐蚀,而且抛光液为水基配方,提升了冷却效果;本发明抛光液添加了尼泊金甲酯等杀菌防腐成分,保存更长久,质量均以稳定,抛光效果好。
具体实施方式
下面通过具体实例对本发明进行详细说明。
一种添加杀菌防腐剂的适用于钢铁的抛光液,由下列重量份(公斤)的原料制成:柠檬酸2、硫酸亚铁3、硅酸钠4、次氯酸钠1、二硫化钼4、尼泊金甲酯2、偏硼酸钠2、葡糖糖酸钠3、甲醇4、氧化铬1、OP-10 3、助剂5、去离子水300;
所述助剂由以下重量份(公斤)的原料制成:三氧化二铝4、纳米二氧化钛5、硅酸钠1、丙二醇甲醚醋酸酯3、十二碳醇酯2、丙烯酸甲酯2、交联羧甲基纤维素钠2、乳化剂BP4、水50;制备方法是首先将三氧化二铝、纳米二氧化钛、交联羧甲基纤维素钠、乳化剂BP加入一半量的水中,研磨1-2小时,然后缓慢加入其余剩余成分,缓慢加热至70℃-80℃,在300-500转/分条件下搅拌反应30-50分钟,冷却至室温即得。
本发明所述一种添加杀菌防腐剂的适用于钢铁的抛光液,由以下具体步骤制成:
(1)将二硫化钼、氧化铬、OP-10混合均匀,加入适量的去离子水,加热至30℃-40℃,研磨30-40分钟,得到混合A料;
(2)将除助剂之外的其余剩余成分加入到反应釜中,搅拌混合均匀,缓慢加热至35℃-45℃,保温1-1.5小时,得到混合B料;
(3)将保温的混合B料边搅拌边缓慢加入到混合A料中,充分搅拌后加入助剂,继续搅拌20-30分钟,冷却至室温即得。
实验检测结果:肉眼观察各钢铁工件的表面,工件表面外观均匀、无异色或有轻微色差、且无雪花;采用微型光泽仪A-4430(德国BYK公司)测试各抛光钢铁工件表面的光泽度,光泽度为47 Gu。

Claims (2)

1.一种添加杀菌防腐剂的适用于钢铁的抛光液,其特征在于,由下列重量份的原料制成:柠檬酸2-3、硫酸亚铁3-5、硅酸钠4-6、次氯酸钠1-2、二硫化钼4-6、尼泊金甲酯2-4、偏硼酸钠2-4、葡糖糖酸钠3-4、甲醇4-6、氧化铬1-2、OP-10 3-5、助剂5-7、去离子水300;
所述助剂由以下重量份的原料制成:三氧化二铝4-6、纳米二氧化钛5-7、硅酸钠1-2、丙二醇甲醚醋酸酯3-4、十二碳醇酯2-3、丙烯酸甲酯2-4、交联羧甲基纤维素钠2-3、乳化剂BP4-5、水50-54;制备方法是首先将三氧化二铝、纳米二氧化钛、交联羧甲基纤维素钠、乳化剂BP加入一半量的水中,研磨1-2小时,然后缓慢加入其余剩余成分,缓慢加热至70℃-80℃,在300-500转/分条件下搅拌反应30-50分钟,冷却至室温即得。
2.根据权利要求1所述一种添加杀菌防腐剂的适用于钢铁的抛光液,其特征在于,由以下具体步骤制成:
(1)将二硫化钼、氧化铬、OP-10混合均匀,加入适量的去离子水,加热至30℃-40℃,研磨30-40分钟,得到混合A料;
(2)将除助剂之外的其余剩余成分加入到反应釜中,搅拌混合均匀,缓慢加热至35℃-45℃,保温1-1.5小时,得到混合B料;
(3)将保温的混合B料边搅拌边缓慢加入到混合A料中,充分搅拌后加入助剂,继续搅拌20-30分钟,冷却至室温即得。
CN201410308848.0A 2014-07-01 2014-07-01 一种添加杀菌防腐剂的适用于钢铁的抛光液及其制备方法 Expired - Fee Related CN104131301B (zh)