CN104128358B - 酸化后的磷矿石尾矿 - Google Patents

酸化后的磷矿石尾矿 Download PDF

Info

Publication number
CN104128358B
CN104128358B CN201410379038.4A CN201410379038A CN104128358B CN 104128358 B CN104128358 B CN 104128358B CN 201410379038 A CN201410379038 A CN 201410379038A CN 104128358 B CN104128358 B CN 104128358B
Authority
CN
China
Prior art keywords
rock phosphate
mine tailing
powder
acidifying
powder mine
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410379038.4A
Other languages
English (en)
Other versions
CN104128358A (zh
Inventor
管永祥
朱玫
王子臣
孙华
金白云
许盛英
许庆华
蒋文兰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dalian Earth Environment Technology Co., Ltd.
Original Assignee
许盛英
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 许盛英 filed Critical 许盛英
Priority to CN201410379038.4A priority Critical patent/CN104128358B/zh
Publication of CN104128358A publication Critical patent/CN104128358A/zh
Application granted granted Critical
Publication of CN104128358B publication Critical patent/CN104128358B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种酸化后的磷矿石尾矿,其技术方案的要点是,酸化后的磷矿石尾矿配料由磷矿石尾矿、凹凸棒石粘土、氧化镁、硫酸、速溶硅酸钠、聚乙烯醇、羟丙基甲基纤维素和碳酸钠组成。将酸化后的磷矿石尾矿配料输入磨机中磨粉,磨粉后的粉状物为酸化后的磷矿石尾矿。酸化后的磷矿石尾矿的生产方法可以避免硫酸与速溶硅酸钠、聚乙烯醇、羟丙基甲基纤维素和碳酸钠发生化学反应;磷矿石尾矿经过酸化处理后,可以提高磷矿石尾矿的利用率,不但能带来良好的经济效益、环境效益和社会效益,而且能实现变废为宝。具有较好的吸附性、触变性、可塑性和粘结性的特点,酸化后的磷矿石尾矿适用于生产营养土、耐火材料、建筑材料、环保材料和园林材料。

Description

酸化后的磷矿石尾矿
技术领域
本发明涉及酸化处理,具体涉及一种酸化后的磷矿石尾矿。
背景技术
磷矿石多产于沉积岩,也有产于变质岩和火成岩,除个别情况外,矿物中的磷总是以正磷酸盐形态存在,磷的主要矿物为磷灰石,磷是重要的化工原料,也是农作物生长的必要元素。
在磷矿石矿区有大量的磷矿石尾矿,没有能得到很好的开发利用。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种酸化后的磷矿石尾矿。
酸化后的磷矿石尾矿配料由磷矿石尾矿、凹凸棒石粘土、氧化镁、硫酸、速溶硅酸钠、聚乙烯醇、羟丙基甲基纤维素和碳酸钠组成。
酸化后的磷矿石尾矿的生产方法:将酸化后的磷矿石尾矿配料输入磨机中磨粉,磨粉后的粉状物为酸化后的磷矿石尾矿。
世界上磷矿石的消费结构中约80%左右生产磷肥后用于农业,在农业中用作磷肥、含磷农药、家禽和牲畜的饲料以外,在洗涤剂、冶金、机械、选矿、钻井、电镀、颜料、涂料、纺织、印染、制革、医药、食品、玻璃、陶瓷、搪瓷、水处理、耐火材料、建筑材料、日用化工、造纸、弹药、阻燃及灭火等方面广泛使用。本发明选用粉碎后的磷矿石尾矿,磷矿石尾矿的颗粒细度≤0.5毫米。
凹凸棒石粘土具有独特的层链状结构特征,晶体呈针状,纤维状或纤维集合状。凹凸棒石粘土具有独特的分散、耐高温、抗盐碱等良好的胶体性质和较高的吸附能力,并具有一定的可塑性及粘结力,本发明选用凹凸棒石粘土的颗粒细度≤5毫米。
氧化镁具有碱性氧化物的通性,属于胶凝材料,能提高凹凸棒石粘土的胶体性能。
硫酸选用浓度为98%的浓硫酸。
速溶硅酸钠为白色粉状物料,能快速溶解于水,具有粘结力强、强度较高,耐酸性、耐热性好,耐碱性和耐水性差的特点。
聚乙烯醇系白色固体,外型分絮状、颗粒状、粉末状三种;无毒无味、颗粒状可在80--90℃水中溶解,粉末状的在其他粉料的预分散后可在常温下溶解。具有较好的粘稠度、聚合性、粘结性及保水性。
羟丙基甲基纤维素具有增稠能力、排盐性、pH稳定性、保水性、尺寸稳定性、优良的成膜性以及广泛的耐酶性、分散性和粘结性等特点。
碳酸钠具有盐的通性和热稳定性,易溶于水,其水溶液呈碱性,在本发明中用于调整酸化后的磷矿石尾矿pH值。
本发明通过下述技术方案予以实现:
1、酸化后的磷矿石尾矿配料按重量百分比由下列组分组成:酸化后的磷矿石尾矿半成品90~98%、速溶硅酸钠0.1~5%、聚乙烯醇0.1~5%、羟丙基甲基纤维素0.01~3%和碳酸钠0~3%。
2、酸化后的磷矿石尾矿的生产方法:将酸化后的磷矿石尾矿配料输入磨机中磨粉,颗粒细度≤0.074毫米,磨粉后的粉状物为酸化后的磷矿石尾矿成品。
3、酸化后的磷矿石尾矿半成品的生产方法:⑴先将磷矿石尾矿混合物输入已经运转的搅拌机中搅拌,再将稀硫酸缓慢加入磷矿石尾矿混合物中进行酸化处理;⑵将酸化处理后的磷矿石尾矿混合物,通过对辊机挤压为磷矿石尾矿片状物,磷矿石尾矿片状物的厚度≤3毫米;⑶将磷矿石尾矿片状物输送到回转式烘干炉内焙烧,焙烧时间为1~3小时,焙烧温度控制在250~350℃,焙烧后的磷矿石尾矿片状物含水量≤5%,焙烧后的磷矿石尾矿片状物为酸化后的磷矿石尾矿半成品,含水量百分比为重量百分比。
4、磷矿石尾矿片状物的配料按重量百分比由下列组分组成:磷矿石尾矿混合物75~95%和稀硫酸5~25%。
5、磷矿石尾矿混合物的配料按重量百分比由下列组分组成:磷矿石尾矿68~92%、凹凸棒石粘土7~30%和氧化镁0.1~3%。
6、稀硫酸的配料按重量百分比由下列组分组成:浓度为98%的浓硫酸1~25%和水75~99%,浓度为98%的浓硫酸百分比为重量百分比。
酸化后的磷矿石尾矿的生产方法采取先酸化再进行复合配料,可以避免硫酸与速溶硅酸钠、聚乙烯醇、羟丙基甲基纤维素和碳酸钠发生化学反应,充分发挥配料中原材料的各自特性,并得到互补,确保酸化后的磷矿石尾矿内在质量。
根据产品质量的需要,采用碳酸钠调整酸化后的磷矿石尾矿pH值,方法简单易行。
磷矿石尾矿经过酸化处理后,pH值控制在5.5~7.0,可以提高磷矿石尾矿的利用率,生成一定量的有效磷,不但能带来良好的经济效益、环境效益和社会效益,而且能实现变废为宝。
酸化后的磷矿石尾矿具有较好的吸附性、触变性、可塑性和粘结性的特点。
酸化后的磷矿石尾矿适用于生产营养土、耐火材料、建筑材料、环保材料和园林材料。
具体实施方式
下面结合实施例对本发明作进一步的描述:
1、酸化后的磷矿石尾矿配料按重量百分比由下列组分组成:酸化后的磷矿石尾矿半成品96%、速溶硅酸钠2%、聚乙烯醇1.5%、羟丙基甲基纤维素0.49%和碳酸钠0.01%。
2、酸化后的磷矿石尾矿的生产方法:将酸化后的磷矿石尾矿配料输入磨机中磨粉,颗粒细度≤0.074毫米,磨粉后的粉状物为酸化后的磷矿石尾矿成品。
3、酸化后的磷矿石尾矿半成品的生产方法:⑴先将磷矿石尾矿混合物输入已经运转的搅拌机中搅拌,再将稀硫酸缓慢加入磷矿石尾矿混合物中进行酸化处理;⑵将酸化处理后的磷矿石尾矿混合物,通过对辊机挤压为磷矿石尾矿片状物,磷矿石尾矿片状物的厚度≤3毫米;⑶将磷矿石尾矿片状物输送到回转式烘干炉内焙烧,焙烧时间为2小时,焙烧温度控制在300~350℃,焙烧后的磷矿石尾矿片状物含水量≤5%,焙烧后的磷矿石尾矿片状物为酸化后的磷矿石尾矿半成品。
4、磷矿石尾矿片状物的配料按重量百分比由下列组分组成:磷矿石尾矿混合物88%和稀硫酸12%。
5、磷矿石尾矿混合物的配料按重量百分比由下列组分组成:磷矿石尾矿88%、凹凸棒石粘土10%和氧化镁2%。
6、稀硫酸的配料按重量百分比由下列组分组成:浓度为98%的浓硫酸5%和水95%。

Claims (3)

1.一种酸化后的磷矿石尾矿,其特征在于,酸化后的磷矿石尾矿配料按重量百分比由下列组分组成:酸化后的磷矿石尾矿半成品90~98%、速溶硅酸钠0.1~5%、聚乙烯醇0.1~5%、羟丙基甲基纤维素0.01~3%和碳酸钠0~3%;
所述酸化后的磷矿石尾矿半成品的生产方法:⑴先将磷矿石尾矿混合物输入已经运转的搅拌机中搅拌,再将稀硫酸缓慢加入磷矿石尾矿混合物中进行酸化处理;⑵将酸化处理后的磷矿石尾矿混合物,通过对辊机挤压为磷矿石尾矿片状物,磷矿石尾矿片状物的厚度≤3毫米;⑶将磷矿石尾矿片状物输送到回转式烘干炉内焙烧,焙烧时间为1~3小时,焙烧温度控制在250~350℃,焙烧后的磷矿石尾矿片状物含水量≤5%,焙烧后的磷矿石尾矿片状物为酸化后的磷矿石尾矿半成品;
磷矿石尾矿片状物的配料按重量百分比由下列组分组成:磷矿石尾矿混合物75~95%和稀硫酸5~25%;磷矿石尾矿混合物的配料按重量百分比由下列组分组成:磷矿石尾矿68~92%、凹凸棒石粘土7~30%和氧化镁0.1~3%;稀硫酸的配料按重量百分比由下列组分组成:浓度为98%的浓硫酸1~25%和水75~99%。
2.根据权利要求1所述的酸化后的磷矿石尾矿,其特征在于,酸化后的磷矿石尾矿的生产方法:将酸化后的磷矿石尾矿配料输入磨机中磨粉,颗粒细度≤0.074毫米,磨粉后的粉状物为酸化后的磷矿石尾矿成品。
3.根据权利要求1所述的酸化后的磷矿石尾矿,其特征在于,磷矿石尾矿的颗粒细度≤0.5毫米,凹凸棒石粘土的颗粒细度≤5毫米。
CN201410379038.4A 2014-08-04 2014-08-04 酸化后的磷矿石尾矿 Active CN104128358B (zh)