CN104110112A CN201410348146.5A CN201410348146A CN104110112A CN 104110112 A CN104110112 A CN 104110112A CN 201410348146 A CN201410348146 A CN 201410348146A CN 104110112 A CN104110112 A CN 104110112A
Authority
CN
China
Prior art keywords
mortar
construction
metope
wall decoration
construction technology
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410348146.5A
Other languages
English (en)
Other versions
CN104110112B (zh
Inventor
朱仁贵
朱安妮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHEJIANG ZILI CONSTRUCTION GROUP CO Ltd
Original Assignee
ZHEJIANG ZILI CONSTRUCTION GROUP CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHEJIANG ZILI CONSTRUCTION GROUP CO Ltd filed Critical ZHEJIANG ZILI CONSTRUCTION GROUP CO Ltd
Priority to CN201410348146.5A priority Critical patent/CN104110112B/zh
Publication of CN104110112A publication Critical patent/CN104110112A/zh
Application granted granted Critical
Publication of CN104110112B publication Critical patent/CN104110112B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Finishing Walls (AREA)

Abstract

本发明涉及一种建筑墙体装饰砂浆施工工艺,通过采用基层处理、底涂施工、分格弹线、抹面层饰面砂浆、去除仿砖型模板或分隔纸以及墙面罩光的工艺步骤,使得建筑墙体具有优良的耐候性、耐水性、不褪色、呼吸性强、防火性好以及具有较强的柔韧性,造型也极为的方便,可以营造从平面到立体的多种造型;整体也非常的耐洗刷、耐沾污,具有很好自洁功能;无毒、无污染、安全,而且非常的绿色环保;省工省料,造价低廉、操作简便、施工快速,而且工期极短。

Description

建筑墙体装饰砂浆施工工艺
技术领域
本发明涉及建筑施工工艺的技术领域,尤其是涉及一种建筑墙体装饰砂浆施工工艺。
背景技术
随着社会的快速发展和生活水平的提高,人们对生活质量和居住环境有了更高的要求,从单调的建筑外墙立面和室内装饰效果,已转变到建筑环境美观、色彩时尚以及节能环保等更高层次的需求。目前传统的装饰砂浆试内外墙抹灰及装饰材料,这种抹灰和装饰的方式已有几百年的历史。传统装饰砂浆因使用耐候性很好的天然矿物材料作为原材料,虽然有着很好的物理特性,耐久性好,整体比较古朴自然。但是缺少艳丽的色彩,靠彩色涂料来弥补其不足,但使用年限不长,返修率极高。
发明内容
针对上述现有技术存在的不足,本发明的目的是提供一种具有优良的耐候性、耐水性、不褪色、呼吸性强、防火性好以及具有较强的柔韧性,造型也极为的方便,整体也非常的耐洗刷、耐沾污,具有很好的自洁功能,省工省料,造价低廉的建筑墙体装饰砂浆施工工艺。
为实现上述的目的,本发明提供了以下技术方案:
一种建筑墙体装饰砂浆施工工艺,采用以下步骤:
a、基层处理:
基层为保温型墙面时,将墙面上残余砂浆、污垢、灰尘清理干净,墙面保持平整,在保温型墙面干燥后即进行底漆施工;
或基层为非保温型墙面时,将墙面上残余泥土、污垢、灰尘清理干净,墙面保持平整,在非保温型墙面干燥后即进行底漆施工;
b、底涂施工:基层清理干净后,均匀涂刷底漆,不可漏刷;底漆干燥后,再刷饰面砂浆底涂,要求涂刷均匀,不得漏刷;
c、分格弹线:底涂未干燥时,根据设计要求弹出分格线,按照分格线粘贴美纹纸;
d、抹面层饰面砂浆:将仿砖型模板或分隔纸粘贴在分格线分隔的基层底涂墙面上,然后抹面层饰面砂浆,砂浆厚度为1-3mm,要求平整、均匀;
e、去除仿砖型模板或分隔纸:将饰面砂浆面层进行搓毛工序完成后立即撕掉仿砖型模板或分隔纸;
f、墙面罩光:饰面砂浆面层干燥后,将墙面进行清理干净,再涂刷罩面,涂刷要求均匀,不得漏刷。
本发明进一步设置为:所述步骤b中的底涂粉料与水的重量比为1:0.48。
本发明进一步设置为:所述底涂粉料的加水量的控制方法为:先将水导入一半至搅拌器内,再将量好的砂浆底涂粉料全部加入,机械搅拌1-3分钟,然后再倒入剩余的水,继续搅拌1-3分钟,后静置3-5分钟,再搅拌15-30秒至均匀。
本发明进一步设置为:所述砂浆底涂浆料须在1小时内用完。
本发明进一步设置为:所述步骤e中的去除仿砖型模板或分隔纸后,需对墙面养护60—80小时。
本发明进一步设置为:所述步骤f中涂刷罩面需2-3遍。
本发明进一步设置为:所述步骤b或/和步骤d或/和步骤f中的涂刷方式由上至下进行喷涂或涂抹。
本发明进一步设置为:所述步骤d中的抹面层饰面砂浆采用的方式为喷涂方式或者抹灰方式。
本发明进一步设置为:所述采用喷涂方式中砂浆与清水的重量比为1:(0.38-0.4),喷涂次数至少为2次,每次喷涂时间间隔为2小时。
本发明进一步设置为:所述采用抹灰方式中砂浆与清水的重量比为3:1。
通过采用上述技术方案,本发明所达到的技术效果为:
1、具有优良的耐候性、耐水性、不褪色、呼吸性强、防火性好以及具有较强的柔韧性;
2、造型也极为的方便,可以营造从平面到立体的多种造型;
3、装饰的墙面整体柔和典雅、纹理清晰、色泽艳丽以及材源也极为丰富;
4、整体也非常的耐洗刷、耐沾污,具有很好的自洁功能;
5、无毒、无污染、安全,而且非常的绿色环保;
6、省工省料,造价低廉、操作简便、施工快速,而且工期极短。
具体实施方式
本发明公开的一种建筑墙体装饰砂浆施工工艺,采用以下步骤:
a、基层处理:基层表面不得粘有灰尘、油迹、铁锈及砂浆、砼块,应去除灰尘、油渍以及疏松物质;
基层为保温型墙面时,将墙面上残余砂浆、污垢、灰尘清理干净,墙面保持平整,在保温型墙面干燥后即进行底漆施工;
或基层为非保温型墙面时,将墙面上残余泥土、污垢、灰尘清理干净,墙面保持平整,在非保温型墙面干燥后即进行底漆施工;
b、底涂施工:基层清理干净后,均匀涂刷底漆,不可漏刷;底漆干燥后,再刷饰面砂浆底涂,要求涂刷均匀,不得漏刷;在进行施工时,应使用专用刷子从上至下施工,先竖向涂刷,再横向涂刷,不允许斜向涂刷;
所述步骤b中的底涂粉料与水的重量比为1:0.48。所述底涂粉料的加水量的控制方法为:先将水导入一半至搅拌器内,再将量好的砂浆底涂粉料全部加入,机械搅拌1-3分钟,然后再倒入剩余的水,继续搅拌1-3分钟,后静置3-5分钟,再搅拌15-30秒至均匀。所述砂浆底涂浆料须在1小时内用完。
c、分格弹线:底涂未干燥时,根据设计要求弹出分格线,按照分格线粘贴美纹纸;
d、抹面层饰面砂浆:将仿砖型模板或分隔纸粘贴在分格线分隔的基层底涂墙面上,然后抹面层饰面砂浆,砂浆厚度为1-3mm,要求平整、均匀;在这里砂浆的厚度优选为2mm;在进行施工时,应使用专用刷子从上至下施工;
e、去除仿砖型模板或分隔纸:将饰面砂浆面层进行搓毛工序完成后立即撕掉仿砖型模板或分隔纸;
所述步骤e中的去除仿砖型模板或分隔纸后,需对墙面养护60—80小时。本实施例中,优选采用对墙面养护72小时。
f、墙面罩光:饰面砂浆面层干燥后,将墙面进行清理干净,再涂刷罩面,涂刷要求均匀,不得漏刷。在进行施工时,应使用专用刷子从上至下施工。
所述步骤f中涂刷罩面需2-3遍。
综上,所述步骤b或/和步骤d或/和步骤f中的涂刷方式由上至下进行喷涂或涂抹。
所述步骤d中的抹面层饰面砂浆采用的方式为喷涂方式或者抹灰方式。所述采用喷涂方式中砂浆与清水的重量比为1:(0.38-0.4),喷涂次数至少为2次,每次喷涂时间间隔为2小时;所述采用抹灰方式中砂浆与清水的重量比为3:1。
上述实施例仅为本发明的较佳实施例,并非依此限制本发明的保护范围,故:凡依本发明的结构、形状、原理所做的等效变化,均应涵盖于本发明的保护范围之内。

Claims (10)

1.一种建筑墙体装饰砂浆施工工艺,其特征在于采用以下步骤:
a、基层处理:
基层为保温型墙面时,将墙面上残余砂浆、污垢、灰尘清理干净,墙面保持平整,在保温型墙面干燥后即进行底漆施工;
或基层为非保温型墙面时,将墙面上残余泥土、污垢、灰尘清理干净,墙面保持平整,在非保温型墙面干燥后即进行底漆施工;
b、底涂施工:基层清理干净后,均匀涂刷底漆,不可漏刷;底漆干燥后,再刷饰面砂浆底涂,要求涂刷均匀,不得漏刷;
c、分格弹线:底涂未干燥时,根据设计要求弹出分格线,按照分格线粘贴美纹纸;
d、抹面层饰面砂浆:将仿砖型模板或分隔纸粘贴在分格线分隔的基层底涂墙面上,然后抹面层饰面砂浆,砂浆厚度为1—3mm,要求平整、均匀;
e、去除仿砖型模板或分隔纸:将饰面砂浆面层进行搓毛工序完成后立即撕掉仿砖型模板或分隔纸;
f、墙面罩光:饰面砂浆面层干燥后,将墙面进行清理干净,再涂刷罩面,涂刷要求均匀,不得漏刷。
2.根据权利要求1所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述步骤b中的底涂粉料与水的重量比为1:0.48。
3.根据权利要求2所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述底涂粉料的加水量的控制方法为:先将水导入一半至搅拌器内,再将量好的砂浆底涂粉料全部加入,机械搅拌1-3分钟,然后再倒入剩余的水,继续搅拌1-3分钟,后静置3-5分钟,再搅拌15-30秒至均匀。
4.根据权利要求3所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述砂浆底涂浆料须在1小时内用完。
5.根据权利要求1所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述步骤e中的去除仿砖型模板或分隔纸后,需对墙面养护60—80小时。
6.根据权利要求1所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述步骤f中涂刷罩面需2-3遍。
7.根据权利要求1所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述步骤b或/和步骤d或/和步骤f中的涂刷方式由上至下进行喷涂或涂抹。
8.根据权利要求1-7任意一项所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述步骤d中的抹面层饰面砂浆采用的方式为喷涂方式或者抹灰方式。
9.根据权利要求8所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述采用喷涂方式中砂浆与清水的重量比为1:(0.38-0.4),喷涂次数至少为2次,每次喷涂时间间隔为2小时。
10.根据权利要求8所述的建筑墙体装饰砂浆施工工艺,其特征在于:所述采用抹灰方式中砂浆与清水的重量比为3:1。
CN201410348146.5A 2014-07-21 2014-07-21 建筑墙体装饰砂浆施工工艺 Expired - Fee Related CN104110112B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410348146.5A CN104110112B (zh) 2014-07-21 2014-07-21 建筑墙体装饰砂浆施工工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410348146.5A CN104110112B (zh) 2014-07-21 2014-07-21 建筑墙体装饰砂浆施工工艺

Publications (2)

Publication Number Publication Date
CN104110112A true CN104110112A (zh) 2014-10-22
CN104110112B CN104110112B (zh) 2017-02-22

Family

ID=51707088

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410348146.5A Expired - Fee Related CN104110112B (zh) 2014-07-21 2014-07-21 建筑墙体装饰砂浆施工工艺

Country Status (1)

Country Link
CN (1) CN104110112B (zh)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104775576A (zh) * 2015-04-17 2015-07-15 湖南博通新型建材有限公司 使用墙漆装饰建筑物墙面并形成美纹网格线的方法
CN105113730A (zh) * 2015-07-21 2015-12-02 平江县长城建筑工程有限公司 防裂保色零voc零泛碱水性干粉建筑彩色涂料外墙施工方法
CN109184210A (zh) * 2018-10-11 2019-01-11 鼎宸建设管理有限公司 一种3d打印装饰造型模板施工工艺
CN109372204A (zh) * 2018-10-26 2019-02-22 安徽安兴装饰工程有限责任公司 无机干粉条纹状外墙装饰砂浆涂料系统施工工法
CN110374282A (zh) * 2019-07-26 2019-10-25 陕西古建园林建设有限公司 耐侵蚀性麦草泥抹面施工方法
CN114934643A (zh) * 2022-05-28 2022-08-23 龙德建设有限公司 一种复古装修墙面结构、施工设备及施工方法

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH08158580A (ja) * 1994-12-09 1996-06-18 Marukoo Pooro Kako:Kk コンクリート壁面の表面処理工法
CN101319552A (zh) * 2008-07-23 2008-12-10 勾希杰 真石漆仿面砖建筑外墙施工方法
CN101899899A (zh) * 2009-05-26 2010-12-01 内蒙古兴泰建筑有限责任公司 外墙仿真石漆面层的施工方法
CN102776994A (zh) * 2012-08-13 2012-11-14 上海大学 仿花岗岩多彩涂料墙面的施工方法
CN103233574A (zh) * 2013-05-08 2013-08-07 内蒙古兴泰建筑有限责任公司 一种外墙仿真石漆面层施工方法

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH08158580A (ja) * 1994-12-09 1996-06-18 Marukoo Pooro Kako:Kk コンクリート壁面の表面処理工法
CN101319552A (zh) * 2008-07-23 2008-12-10 勾希杰 真石漆仿面砖建筑外墙施工方法
CN101899899A (zh) * 2009-05-26 2010-12-01 内蒙古兴泰建筑有限责任公司 外墙仿真石漆面层的施工方法
CN102776994A (zh) * 2012-08-13 2012-11-14 上海大学 仿花岗岩多彩涂料墙面的施工方法
CN103233574A (zh) * 2013-05-08 2013-08-07 内蒙古兴泰建筑有限责任公司 一种外墙仿真石漆面层施工方法

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
于克,等: "保温外墙柔性仿石砖砂浆面层施工技术", 《烟台职业学院学报》 *

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104775576A (zh) * 2015-04-17 2015-07-15 湖南博通新型建材有限公司 使用墙漆装饰建筑物墙面并形成美纹网格线的方法
CN105113730A (zh) * 2015-07-21 2015-12-02 平江县长城建筑工程有限公司 防裂保色零voc零泛碱水性干粉建筑彩色涂料外墙施工方法
CN109184210A (zh) * 2018-10-11 2019-01-11 鼎宸建设管理有限公司 一种3d打印装饰造型模板施工工艺
CN109372204A (zh) * 2018-10-26 2019-02-22 安徽安兴装饰工程有限责任公司 无机干粉条纹状外墙装饰砂浆涂料系统施工工法
CN110374282A (zh) * 2019-07-26 2019-10-25 陕西古建园林建设有限公司 耐侵蚀性麦草泥抹面施工方法
CN114934643A (zh) * 2022-05-28 2022-08-23 龙德建设有限公司 一种复古装修墙面结构、施工设备及施工方法

Also Published As

Publication number Publication date
CN104110112B (zh) 2017-02-22

Similar Documents

Publication Publication Date Title
CN104110112B (zh) 建筑墙体装饰砂浆施工工艺
CN103952052A (zh) 仿洞石弹性质感涂料及其制备方法
CN104449169A (zh) 一种天然岩片漆的制备方法
CN105089232B (zh) 一种多层复合结构柔性饰面产品及其生产方法
CN102094496A (zh) 仿砖墙面的制作方法
CN101899899A (zh) 外墙仿真石漆面层的施工方法
CN100532756C (zh) 一种墙面喷涂方法
CN106869428A (zh) 一种隔热反射彩色砂浆施工工艺
CN108930374A (zh) 一种具有隔热反射功能的环保型真石漆外墙施工方法
CN111171614A (zh) 一种批刮型仿大理石漆及其制备方法与应用
CN103755219B (zh) 仿澳洲砂岩硅藻土壁材及其施工方法
CN109651905A (zh) 一种新型双组份防水装饰一体化涂料及其施工方法
CN203626162U (zh) 仿火烧石涂层结构
CN113802844B (zh) 一种建筑墙面仿夯土制作用辅衬曲线模条
CN102259085A (zh) 一种水性金属漆在拉毛涂装工艺中的应用
CN203049968U (zh) 装饰饰面漆复合结构
CN106497285A (zh) 玉瓷漆
CN203097163U (zh) 外墙天然真石涂层结构
CN205171914U (zh) 一种岩彩石墙面墙体
CN203097164U (zh) 外墙质感仿砂岩涂层结构
CN207211590U (zh) 一种新型外墙装饰板
CN203097165U (zh) 内外墙仿瓷砖艺术质感涂层结构
CN205476176U (zh) 一种高仿石灰石墙身饰层结构
CN205153198U (zh) 一种莱姆石涂料墙面的墙体
CN104761179A (zh) 一种抹涂型仿花岗岩石涂料

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20170222

Termination date: 20180721