CN103952074B - 一种防臭氧氧化保护物质的生产方法 - Google Patents
一种防臭氧氧化保护物质的生产方法 Download PDFInfo
- Publication number
- CN103952074B CN103952074B CN201410172076.2A CN201410172076A CN103952074B CN 103952074 B CN103952074 B CN 103952074B CN 201410172076 A CN201410172076 A CN 201410172076A CN 103952074 B CN103952074 B CN 103952074B
- Authority
- CN
- China
- Prior art keywords
- rubber
- protection material
- production method
- ozone
- unsaturated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明公开了一种防臭氧氧化保护物质的生产方法,包括不饱和橡胶,其特征在于:将不饱和橡胶或老化后的橡胶打碎放置在60℃的密封空间内,在密封空间内设置一个臭氧发生装置,氧化24小时,将氧化后的不饱和橡胶制造成粉末状,加入到液态硅橡胶中,搅拌均匀。将按重量比例:不饱和橡胶氧化物粉末30份,液态硅橡胶70份混合后涂于橡胶外表面。发明的目的是克服现有技术的不足,生产一种防臭氧氧化保护物质,生产方法简单,原料可以采用老化后的橡胶或不饱和的橡胶,使老化后的橡再胶回收利用,节约成本的同时使资源再生,市场前景广阔。
Description
技术领域
本发明涉及橡胶防护技术领域,属于一种防臭氧氧化保护物质的生产方法。
背景技术
橡胶制品容易老化是因为大气中含有臭氧,因为臭氧比央企更活泼,所以它对橡胶尤其是不饱和的的橡胶的侵袭要比氧气厉害得多。
据了解,不饱和的橡胶很容易和臭氧发生氧化,并且臭氧化后的外观特征和热氧老化不一样,臭氧化是在橡胶制品的表面进行的,是由表及里的过程,而且橡胶和臭氧发生反应的时候会生成一层银白色的硬膜(大约10nm厚),在静态的条件下这层膜能够阻止臭氧和橡胶深层接触。只要没有外力使薄膜龟裂,橡胶将不再继续臭氧化。如若对已经臭氧化的橡胶拉伸或使其产生动态变形,生成的臭氧化薄膜将出现龟裂,露出新的橡胶表面又会与臭氧发生反应,这使得裂纹继续增长。
发明内容
本发明的目的是克服现有技术的不足,提供一种防臭氧氧化保护物质的生产方法,将不饱和橡胶或老化后的橡胶打碎放置在60℃的密封空间内,在密封空间内设置一个臭氧发生装置,氧化24小时,将氧化后的不饱和橡胶制造成粉末状,加入到液态硅橡胶中,搅拌均匀。将按重量比例:不饱和橡胶氧化物粉末30份,液态硅橡胶70份混合后涂于橡胶外表面,由于该混合物中的物质不易与臭氧发生反应,达到保护橡胶制品的目的,同时此混合物干燥后为软性,不会应橡胶变形而开裂。
为了实现上述目的本发明采用如下技术方案:
一种防臭氧氧化保护物质的生产方法,包括不饱和橡胶,其特征在于:将不饱和橡胶或老化后的橡胶打碎放置在60℃的密封空间内,在密封空间内设置一个臭氧发生装置,氧化24小时,将氧化后的不饱和橡胶制造成粉末状,加入到液态胶中,搅拌均匀。
所述的防臭氧氧化保护物质按重量比例:不饱和橡胶氧化物粉末30份,液态胶70份。
所述的液态胶为液态硅橡胶。
与已有技术相比,本发明的有益效果如下:
本发明采用防臭氧氧化保护物质的生产方法,生产方法简单,原料可以采用老化后的橡胶或不饱和的橡胶,使老化后的橡胶再回收利用,节约成本的同时使资源再生,市场前景广阔。
具体实施方式
下面结合实施例对本发明作进一步的描述,但本发明不仅限于这些实例,在为脱离本发明宗旨的前提下,所为任何改进均落在本发明的保护范围之内。
实施例:
一种防臭氧氧化保护物质的生产方法,包括不饱和橡胶,其特征在于:将不饱和橡胶或老化后的橡胶打碎放置在60℃的密封空间内,在密封空间内设置一个臭氧发生装置,氧化24小时,将氧化后的不饱和橡胶制造成粉末状,加入到液态硅橡胶中,搅拌均匀。将按重量比例:不饱和橡胶氧化物粉末30份,液态硅橡胶70份混合后涂于橡胶外表面。
Claims (1)
1.一种防臭氧氧化保护物质的生产方法,包括不饱和橡胶,其特征在于:将不饱和橡胶打碎放置在60℃的密封空间内,在密封空间内设置一个臭氧发生装置,氧化24小时,将氧化后的不饱和橡胶制造成粉末状,加入到液态硅橡胶中,搅拌均匀;
所述的防臭氧氧化保护物质按重量比例:不饱和橡胶氧化物粉末30份,液态硅橡胶70份。