Prior art keywords
valve seat
seat ring
air valve
powder metal
metal materials
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410135305.3A
Other languages
English (en)
Inventor
孙恒香
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HANSHAN COUNTY QUANXING GAS ENGINE FITTINGS CO Ltd
Original Assignee
HANSHAN COUNTY QUANXING GAS ENGINE FITTINGS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HANSHAN COUNTY QUANXING GAS ENGINE FITTINGS CO Ltd filed Critical HANSHAN COUNTY QUANXING GAS ENGINE FITTINGS CO Ltd
Priority to CN201410135305.3A priority Critical patent/CN103912332A/zh
Publication of CN103912332A publication Critical patent/CN103912332A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Lift Valve (AREA)

Abstract

本发明公开了一种内燃机气门座圈,所述的气门座圈是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C0.4-1.6%、Mo1-5%、Co2.5-8%、Mn0.6-1.8%、Cr2.0-5.0%、P0.05-1.2%、V0.2-0.5%、S0.01-0.08%、Ni0.3-2.2%、余量为Fe。本发明的配方合理,加入多种耐磨损和耐高温的材料,有效提高了耐磨性、耐高温性,通过合理的配比及烧结,最高能高温环境下运行长时间,而不出现塌陷及变形。

Description

一种内燃机气门座圈
技术领域
本发明涉及一种内燃机配件,具体涉及一种内燃机气门座圈。
背景技术
汽车发动机气门座圈是发动机上重要的部件,是内燃机燃料燃烧时进入空气和燃
烧后排出废气的门户,其主要目的是保证燃烧室的密封。由于工作条件的恶劣,需要在高温环境下承受气门的冲击、磨损,以及进、排气流的冲蚀、氧化等作用,因此,对气门座圈的耐高温、耐磨损、抗氧化等特性具有极高的要求。随着科学技术的发展,人们对发动机气门座圈的要求越来越严,希望气门座圈具有更高的耐热性、耐磨性和耐腐蚀性。
发明内容
本发明目的是提供一种耐高温、耐磨损的气门座圈。
本发明的方案如下:一种内燃机气门座圈,所述的气门座圈是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C0.4-1.6%、Mo1-5%、Co2.5-8%、Mn0.6-1.8%、Cr2.0-5.0%、P 0.05-1.2%、V 0.2-0.5%、S0.01-0.08%、Ni 0.3-2.2%、余量为Fe。
进一步,所述的气门座圈是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C0.4-1.3%、Mo1-3%、Co2.5-8%、Mn0.6-1.2%、Cr2.0-3.9%、P0.05-1.2%、V 0.3-0.5%、S0.01-0.04%、Ni0.3-1.2%、余量为Fe。
进一步,所述的气门座圈是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C1.2%、Mo3%、Co 5.2%、Mn1.2%、Cr3%、P0.6%、V 0.3%、S0.058%、Ni 1.1%、余量为Fe。
本发明的配方合理,加入多种耐磨损和耐高温的材料,有效提高了耐磨性、耐高温性,通过合理的配比及烧结,最高能高温环境下运行长时间,而不出现塌陷及变形。
具体实施方式
实施例1
一种内燃机气门座圈,所述的气门座圈是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C1.2%、Mo3%、Co5%、Mn0.9%、Cr2.9%、P 0.08%、V 035%、S0.02%、Ni 0.4.2%、余量为Fe。
实施例2
粉末金属材料的重量百分含量组成为:C0.6%、Mo2%、Co8%、Mn1.1%、Cr2.9%、P0. 2%、V 0. 5%、S0.03%、Ni0.32%、余量为Fe。
实施例3
粉末金属材料的重量百分含量组成为:C1.2%、Mo3%、Co 5.2%、Mn1.2%、Cr3%、P0.6%、V 0.3%、S0.058%、Ni 1.1%、余量为Fe。
尽管上文对本发明的具体实施方式给予了详细描述和说明,但是应该指明的是,我们可以依据本发明的构想对上述实施方式进行各种等效改变和修改,其所产生的功能作用仍未超出说明书所涵盖的精神时,均应在本发明的保护范围之内。 

Claims (3)

1.一种内燃机气门座圈,其特征在于,所述的气门座圈是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C 0.4-1.6%、Mo1-5%、Co 2.5-8%、Mn0.6-1.8%、Cr2.0-5.0%、P 0.05-1.2%、V 0.2-0.5%、S0.01-0.08%、Ni 0.3-2.2%、余量为Fe。
2.根据权利要求1所述的一种内燃机气门座圈,其特征在于,所述的气门座是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C 0.4-1.3%、Mo1-3%、Co 2.5-8%、Mn0.6-1.2%、Cr2.0-3.9%、P 0.05-1.2%、V 0.3-0.5%、S0.01-0.04%、Ni 0.3-1.2%、余量为Fe。
3.根据权利要求1所述的一种内燃机气门座圈,其特征在于,所述的气门座是由粉末金属材料制成的,其中,粉末金属材料的重量百分含量组成为:C 1.2%、Mo3%、Co 5.2%、Mn1.2%、Cr3%、P0.6%、V 0.3%、S0.058%、Ni 1.1%、余量为Fe。
CN201410135305.3A 2014-04-04 2014-04-04 一种内燃机气门座圈 Pending CN103912332A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410135305.3A CN103912332A (zh) 2014-04-04 2014-04-04 一种内燃机气门座圈

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410135305.3A CN103912332A (zh) 2014-04-04 2014-04-04 一种内燃机气门座圈

Publications (1)

Publication Number Publication Date
CN103912332A true CN103912332A (zh) 2014-07-09

Family

ID=51038294

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410135305.3A Pending CN103912332A (zh) 2014-04-04 2014-04-04 一种内燃机气门座圈

Country Status (1)

Country Link
CN (1) CN103912332A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104791041A (zh) * 2015-05-18 2015-07-22 夏志清 一种汽车发动机气缸盖
CN108757079A (zh) * 2018-05-23 2018-11-06 合肥众机群机械制造有限公司 一种发动机气门油封组件

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5350560A (en) * 1993-07-12 1994-09-27 Triten Corporation Wear resistant alloy
US6251157B1 (en) * 1998-08-19 2001-06-26 Hitachi Powdered Metals Co., Ltd. Sintered alloy having superb wear resistance and process for producing the same
US20060278038A1 (en) * 2005-06-13 2006-12-14 Hitachi Powdered Metals Co., Ltd. Sintered valve seat and production method therefor
CN101505910A (zh) * 2006-08-09 2009-08-12 Ing商事株式会社 铁基耐蚀耐磨损性合金以及用于获得该合金的堆焊材料
CN102172775A (zh) * 2005-10-12 2011-09-07 日立粉末冶金株式会社 烧结阀座的制造方法

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5350560A (en) * 1993-07-12 1994-09-27 Triten Corporation Wear resistant alloy
US6251157B1 (en) * 1998-08-19 2001-06-26 Hitachi Powdered Metals Co., Ltd. Sintered alloy having superb wear resistance and process for producing the same
US20060278038A1 (en) * 2005-06-13 2006-12-14 Hitachi Powdered Metals Co., Ltd. Sintered valve seat and production method therefor
CN102172775A (zh) * 2005-10-12 2011-09-07 日立粉末冶金株式会社 烧结阀座的制造方法
CN101505910A (zh) * 2006-08-09 2009-08-12 Ing商事株式会社 铁基耐蚀耐磨损性合金以及用于获得该合金的堆焊材料

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104791041A (zh) * 2015-05-18 2015-07-22 夏志清 一种汽车发动机气缸盖
CN108757079A (zh) * 2018-05-23 2018-11-06 合肥众机群机械制造有限公司 一种发动机气门油封组件
CN108757079B (zh) * 2018-05-23 2020-06-26 合肥众机群机械制造有限公司 一种发动机气门油封组件

Similar Documents

Publication Publication Date Title
CN103924162A (zh) 一种耐高温耐磨气门座圈
CN103480849A (zh) 一种天然气发动机粉末冶金气门座圈材料
BR112016012537A2 (pt) Liga à base de níquel, inserto de sede de válvula para um motor de combustão interna, método de fabricação do inserto de sede de válvula e método de fabricação de um motor de combustão interna
CN104169649A (zh) 环形燃烧室旁通装置
CN102330583B (zh) 汽车发动机气门座圈
CN103912332A (zh) 一种内燃机气门座圈
BR112014026950A2 (pt) filtro de partículas
PL88655B1 (zh)
CN103362652A (zh) 级间密封系统及包括级间密封系统的系统
WO2012175271A3 (de) Verwendung einer heissgaskorrosionsbeständigen duktilen legierung
WO2011135579A3 (en) Carbon black reactor
Vardar et al. Investigation of exhaust valve failure in heavy â?? duty diesel engine
CN106282783B (zh) 发动机的进排气门座圈和进排气门组合
RU2013154782A (ru) Газообменный клапан, а также способ производства газообменного клапана
CN103600064B (zh) 一种粉末冶金进排气阀座圈及其制备方法
CN104674062A (zh) 一种碲镍铬合金材料
CN103014544A (zh) 一种高耐磨粉末冶金气门座
RU2017102992A (ru) Нагнетатель системы волнового наддува
CN103216288B (zh) 一种乙醇汽油发动机的进排气门座圈
CN104878309A (zh) 一种汽车发动机气门座圈及其制备方法
CN101907003A (zh) 低排放天然气发动机气门座圈
JP5875072B2 (ja) 溶射材料焼結体及び溶射材料の製造方法
CN104928599A (zh) 一种用于制作汽门座圈的材料的配方
CN104165073A (zh) 一种防止气门座圈脱落的气缸盖
CN102618789B (zh) 铸钢合金和铸造组件

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20140709