Prior art keywords
parts
coating
wear
abrasive resistance
resisting powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310574756.2A
Other languages
English (en)
Inventor
蒋玉俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Southeast University
Original Assignee
Southeast University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Southeast University filed Critical Southeast University
Priority to CN201310574756.2A priority Critical patent/CN103897566A/zh
Publication of CN103897566A publication Critical patent/CN103897566A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Paints Or Removers (AREA)

Abstract

本发明公开了一种高耐磨性涂料,包括以下组分,且各组分的重量份数为:改性有机硅聚酯树脂35-45份;颜料10-15份;耐磨粉10-15份;分散剂1~2份;流平剂1~2份;消泡剂2-3份;增塑剂2-5份;溶剂10-15份。本发明通过在涂料的配方中增加耐磨粉,而由于耐磨粉的超细化粒径,使得所述的涂料涂料不仅具有很好的防腐蚀性和耐侯性,并由于抗刮耐磨粉粒子本身所固有的硬度(莫氏70),能增强涂料的硬度,从而提升其耐擦伤和耐划性。

Description

一种高耐磨性涂料
技术领域
本发明涉及一种涂料,更具体的说是涉及一种具有较高的耐磨性能的涂料配方组成,属于化工技术领域。
背景技术
目前,家装用涂料的耐磨性比较差,且硬度不高,因此,特别容易被刮擦、擦伤等,会严重影响其外观,且增加了反复施工的不便,同时会增加装修成本。
发明内容
为了克服现有技术的不足,本发明的目的在于提供一种硬度高、耐磨性好、成本低的高耐磨性涂料。
本发明是通过以下技术方案来实现的:
一种高耐磨性涂料,其特征在于,包括以下组分,且各组分的重量份数为:
Figure BDA0000414648200000011
进一步,所述的耐磨粉的平均粒径为2.5~3μm。
所述的增塑剂为邻苯二甲酸二丁酯。
所述的溶剂为乙二醇丁醚。
本发明的有益效果为:本发明通过在涂料的配方中增加耐磨粉,而由于耐磨粉的超细化粒径,使得所述的涂料涂料不仅具有很好的防腐蚀性和耐侯性,并由于抗刮耐磨粉粒子本身所固有的硬度(莫氏70),能增强涂料的硬度,从而提升其耐擦伤和耐划性。
具体实施方式
下面将结合具体实施例详细说明本发明的具体实施方式:
实施例1:
一种高耐磨性涂料,包括以下组分,且各组分的重量份数为:改性有机硅聚酯树脂35份;颜料10份;耐磨粉10份;分散剂2份;流平剂1份;消泡剂3份;邻苯二甲酸二丁酯2份;乙二醇丁醚15份。其中,所述的耐磨粉的平均粒径为2.5~3μm。
实施例2:
一种高耐磨性涂料,包括以下组分,且各组分的重量份数为:改性有机硅聚酯树脂45份;颜料15份;耐磨粉15份;分散剂1份;流平剂2份;消泡剂2份;邻苯二甲酸二丁酯5份;乙二醇丁醚10份。其中,所述的耐磨粉的平均粒径为2.5~3μm。
实施例3:
一种高耐磨性涂料,包括以下组分,且各组分的重量份数为:改性有机硅聚酯树脂40份;颜料12份;耐磨粉12份;分散剂1份;流平剂1份;消泡剂2份;邻苯二甲酸二丁酯4份;乙二醇丁醚12份。其中,所述的耐磨粉的平均粒径为2.5~3μm。
本发明通过在涂料的配方中增加耐磨粉,而由于耐磨粉的超细化粒径,使得所述的涂料涂料不仅具有很好的防腐蚀性和耐侯性,并由于抗刮耐磨粉粒子本身所固有的硬度(莫氏70),能增强涂料的硬度,从而提升其耐擦伤和耐划性。
以上已以较佳实施例公开了本发明,然其并非用以限制本发明,凡采用等同替换或者等效变换方式所获得的技术方案,均落在本发明的保护范围之内。

Claims (4)

1.一种高耐磨性涂料,其特征在于,包括以下组分,且各组分的重量份数为:
Figure FDA0000414648190000011
2.根据权利要求1所述的一种高耐磨性涂料,其特征在于,所述的耐磨粉的平均粒径为2.5~3μm。
3.根据权利要求1所述的一种高耐磨性涂料,其特征在于,所述的增塑剂为邻苯二甲酸二丁酯。
4.根据权利要求1所述的一种高耐磨性涂料,其特征在于,所述的溶剂为乙二醇丁醚。
CN201310574756.2A 2013-11-15 2013-11-15 一种高耐磨性涂料 Pending CN103897566A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310574756.2A CN103897566A (zh) 2013-11-15 2013-11-15 一种高耐磨性涂料

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310574756.2A CN103897566A (zh) 2013-11-15 2013-11-15 一种高耐磨性涂料

Publications (1)

Publication Number Publication Date
CN103897566A true CN103897566A (zh) 2014-07-02

Family

ID=50989155

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310574756.2A Pending CN103897566A (zh) 2013-11-15 2013-11-15 一种高耐磨性涂料

Country Status (1)

Country Link
CN (1) CN103897566A (zh)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104449262A (zh) * 2014-12-08 2015-03-25 成都锦汇科技有限公司 一种耐候性钢板用涂料组合物的制备方法
CN105399914A (zh) * 2015-12-11 2016-03-16 江门市凌云涂料有限公司 一种耐磨哑光聚氨酯清漆及其制备方法
CN108384297A (zh) * 2018-03-09 2018-08-10 浙江鸿道环保有限公司 一种可加强玻璃钢耐磨性的涂料
CN108893053A (zh) * 2018-05-31 2018-11-27 郑州朗纽防护材料有限公司 一种高温带温耐热涂料

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1246503A (zh) * 1998-08-28 2000-03-08 曲树蓁 一种耐磨防结垢涂料
CN1278543A (zh) * 2000-06-14 2001-01-03 上海市建筑科学研究院 聚氨酯树脂涂料及其生产方法
DE102009056187A1 (de) * 2008-11-28 2010-07-15 Basf Se Polyesterharz auf Basis von 2-Propylheptansäureglycidester und/oder 4-Methyl-2 propylhexansäureglycidester
CN101885944A (zh) * 2010-07-19 2010-11-17 昆山市东亚树脂涂料厂有限公司 有机硅聚酯树脂涂料及其生产方法

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1246503A (zh) * 1998-08-28 2000-03-08 曲树蓁 一种耐磨防结垢涂料
CN1278543A (zh) * 2000-06-14 2001-01-03 上海市建筑科学研究院 聚氨酯树脂涂料及其生产方法
DE102009056187A1 (de) * 2008-11-28 2010-07-15 Basf Se Polyesterharz auf Basis von 2-Propylheptansäureglycidester und/oder 4-Methyl-2 propylhexansäureglycidester
CN101885944A (zh) * 2010-07-19 2010-11-17 昆山市东亚树脂涂料厂有限公司 有机硅聚酯树脂涂料及其生产方法

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104449262A (zh) * 2014-12-08 2015-03-25 成都锦汇科技有限公司 一种耐候性钢板用涂料组合物的制备方法
CN105399914A (zh) * 2015-12-11 2016-03-16 江门市凌云涂料有限公司 一种耐磨哑光聚氨酯清漆及其制备方法
CN108384297A (zh) * 2018-03-09 2018-08-10 浙江鸿道环保有限公司 一种可加强玻璃钢耐磨性的涂料
CN108893053A (zh) * 2018-05-31 2018-11-27 郑州朗纽防护材料有限公司 一种高温带温耐热涂料

Similar Documents

Publication Publication Date Title
CN102051096B (zh) 一种环保高性能水性木器漆及其使用方法
CN103897566A (zh) 一种高耐磨性涂料
CN104817946A (zh) 单组分水性木器涂料
CN107916024B (zh) 一种水性常温超快干车间预涂底漆及其制备方法和应用
CN107523193B (zh) 一种镁合金基材高耐盐雾强耐候防护涂料、制备方法及使用方法
CN103450760A (zh) 一种室内外金属制件用装饰漆及其加工工艺
CN102863892A (zh) 风机叶片用水性聚氨酯涂料及其制备方法
CN104371465A (zh) 基于单组份水性耐污白面面漆
AU2014100870A4 (en) Transparent, heat-insulting, UV-blocking coatings
CN103725138A (zh) 一种硅溶胶高渗透多功能透明罩面漆
CN105400038A (zh) 一种电子产品外壳材料
CN103146272B (zh) 一种增强闪光效果的金属粉末涂料及其制备方法
CN102746747B (zh) 一种硝基耐磨亚光黑色漆
CN103113543A (zh) 一种正丁醇混合醚化三聚氰胺树脂
CN102952451A (zh) 水性过氯乙烯防腐漆制备方法
CN103102465A (zh) 一种异丁醇混合醚化三聚氰胺树脂
CN104293111A (zh) 一种负载二氧化硅纳米球的高效防锈环氧面漆及其制备方法
CN103073971A (zh) 新型无溶剂防静电抗菌环氧自流平地坪涂料
CN105885648A (zh) 自清洁高分散性卷材用粉末涂料及其制备方法
CN105348974A (zh) 一种新型防腐面漆
CN103773196A (zh) 一种醇酸底漆的配方
CN103122193A (zh) 一种环氧地坪涂料
CN104419283A (zh) 一种高性能水性烘漆
CN103265864B (zh) 一种湿固化双组分环氧中间漆及其制备方法
CN103571284A (zh) 一种玻璃墙用防尘涂料

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20140702