CN103881427A - 一种制备水性仿花岗岩石型涂料的原料及其制备方法 - Google Patents

一种制备水性仿花岗岩石型涂料的原料及其制备方法 Download PDF

Info

Publication number
CN103881427A
CN103881427A CN201310518068.4A CN201310518068A CN103881427A CN 103881427 A CN103881427 A CN 103881427A CN 201310518068 A CN201310518068 A CN 201310518068A CN 103881427 A CN103881427 A CN 103881427A
Authority
CN
China
Prior art keywords
parts
water
coating
raw material
polyvinyl alcohol
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310518068.4A
Other languages
English (en)
Inventor
郭新立
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Southeast University
Original Assignee
Southeast University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Southeast University filed Critical Southeast University
Priority to CN201310518068.4A priority Critical patent/CN103881427A/zh
Publication of CN103881427A publication Critical patent/CN103881427A/zh
Pending legal-status Critical Current

Abstract

本发明公开一种制备水性仿花岗岩石型涂料的原料,包括如下质量份材料:聚乙烯醇20-50份,乳化剂0.5-3份,邻苯二甲酸二丁酯0.5-2份,乙二醇1-3份,丙二醇1-3份,羧甲基纤维素0.2-1份,磷酸三丁酯0.1-1份,六偏磷酸钠0.1-2份,硼酸钠1-20份,水600-1000份,木质素1-20份,钛白粉2-10份,立德粉5-30份,轻质碳酸钙300-500份,重质碳酸钙50-150份,滑石粉20-100份;本发明所述的制备水性仿花岗岩石型涂料的原料及其制备方法制得的涂料在干燥后可保持原来的花纹而不收缩变形,并能增加涂料表面的硬度和韧性,因而能喷涂出花岗岩石型花纹图案,其装饰效果好,施工简便,价格低廉,满足了普通百姓对美化环境的要求。

Description

一种制备水性仿花岗岩石型涂料的原料及其制备方法
技术领域
本发明涉及一种建筑涂料,尤其涉及一种制备水性仿花岗岩石型涂料的原料及其制备方法。
背景技术
用于建筑装饰和保护的涂料统称为建筑涂料。从本质上讲,建筑涂料与一般涂料并没有本质的区别,而只是涂料的一个应用领域而已。在我国,将涂料用作建筑物的装饰和保护材料已有几千年的历史,但是将建筑涂料单独分类却只有近几十年的事。早期的涂料主要是由天然动物油脂(牛油、鱼油等)、植物油脂(桐油、亚麻子油等)和天然树脂(松香、生漆)等制成,因此涂料又称油漆。20实际50年代以来,世界石油化学工业和高分子合成工业的迅速发展,为涂料工业的发展提供了良好的物质基础,因此,当前的涂料除了少量采用天然树脂和油脂外,主要是以合成树脂为成膜物质。随着各种需要,还出现了各种功能性涂料,如防火涂料、防水涂料、防霉涂料、防结露涂料、杀虫灭蚊涂料、隔热涂料和隔声涂料等。
发明内容
发明目的:本发明的目的在于提供一种制备水性仿花岗岩石型涂料的原料及其制备方法,所述制得的涂料装饰效果好,施工简便,价格低廉,满足了普通百姓对美化环境的要求。
技术方案:本发明所述的一种制备水性仿花岗岩石型涂料的原料,包括如下质量份材料:聚乙烯醇20-50份,乳化剂0.5-3份,邻苯二甲酸二丁酯0.5-2份,乙二醇1-3份,丙二醇1-3份,羧甲基纤维素0.2-1份,磷酸三丁酯0.1-1份,六偏磷酸钠0.1-2份,硼酸钠1-20份,水600-1000份,木质素1-20份,钛白粉2-10份,立德粉5-30份,轻质碳酸钙300-500份,重质碳酸钙50-150份,滑石粉20-100份。
作为优选:上述制备水性仿花岗岩石型涂料的原料,包括如下质量份材料:聚乙烯醇30份,乳化剂1份,邻苯二甲酸二丁酯1份,乙二醇2份,丙二醇2份,羧甲基纤维素0.5份,磷酸三丁酯0.5份,六偏磷酸钠1份,硼酸钠10份,水750份,木质素10份,钛白粉5份,立德粉15份,轻质碳酸钙400份,重质碳酸钙100份,滑石粉50份。
一种利用上述原料制备水性仿花岗岩石型涂料的方法,首先,向带有夹套和搅拌的反应器内加入所述计量的水,加热至70-80摄氏度,缓慢地分批加入聚乙烯醇,升温至95-99摄氏度,保温30-50分钟;然后,待聚乙烯醇全部溶解后,加入乳化剂、邻苯二甲酸二丁酯,开始降温至70摄氏度,加入羧甲基纤维素、乙二醇和丙二醇,反应30分钟后降温至60摄氏度,再加入硼酸钠、磷酸三丁酯、木质素和六偏磷酸钠,冷却后过筛除去未溶解物,然后将制得的基材与钛白粉、立德粉、轻质碳酸钙、重质碳酸钙及滑石粉混合搅拌均匀,即制得成品。
上述方法制得的涂料只要用作室内装饰涂料,具体施工方法为:施工前,先对墙体进行平整、清除尘埃与油垢等处理,施工机具采用1.5-2匹自控型压缩泵和内径2.5mm喷嘴的喷枪,喷枪压力要求:施工压力为0.2-0.3MPa,并将喷枪调节至进气量中等,出料量中等,喷枪口到墙面距离为30-50cm,喷枪与墙面的角度为90度,即可得到仿真造型图案。
本发明与现有技术相比,其有益效果是:本发明所述的制备水性仿花岗岩石型涂料的原料及其制备方法制得的涂料在干燥后可保持原来的花纹而不收缩变形,并能增加涂料表面的硬度和韧性,因而能喷涂出花岗岩石型花纹图案,其装饰效果好,施工简便,价格低廉,满足了普通百姓对美化环境的要求。
具体实施方式
下面对本发明技术方案进行详细说明,但是本发明的保护范围不局限于所述实施例。
实施例1:一种制备水性仿花岗岩石型涂料的原料,包括如下质量份材料:聚乙烯醇30份,乳化剂1份,邻苯二甲酸二丁酯1份,乙二醇2份,丙二醇2份,羧甲基纤维素0.5份,磷酸三丁酯0.5份,六偏磷酸钠1份,硼酸钠10份,水750份,木质素10份,钛白粉5份,立德粉15份,轻质碳酸钙400份,重质碳酸钙100份,滑石粉50份。
利用上述原料制备水性仿花岗岩石型涂料的方法,首先,向带有夹套和搅拌的反应器内加入所述计量的水,加热至70-80摄氏度,缓慢地分批加入聚乙烯醇,升温至95-99摄氏度,保温30-50分钟;然后,待聚乙烯醇全部溶解后,加入乳化剂、邻苯二甲酸二丁酯,开始降温至70摄氏度,加入羧甲基纤维素、乙二醇和丙二醇,反应30分钟后降温至60摄氏度,再加入硼酸钠、磷酸三丁酯、木质素和六偏磷酸钠,冷却后过筛除去未溶解物,然后将制得的基材与钛白粉、立德粉、轻质碳酸钙、重质碳酸钙及滑石粉混合搅拌均匀,即制得成品。
上述原料和方法制得的涂料在干燥后可保持原来的花纹而不收缩变形,并能增加涂料表面的硬度和韧性,因而能喷涂出花岗岩石型花纹图案。
如上所述,尽管参照特定的优选实施例已经表示和表述了本发明,但其不得解释为对本发明自身的限制。在不脱离所附权利要求定义的本发明的精神和范围前提下,可对其在形式上和细节上作出各种变化。

Claims (3)

1.一种制备水性仿花岗岩石型涂料的原料,其特征在于,包括如下质量份材料:聚乙烯醇20-50份,乳化剂0.5-3份,邻苯二甲酸二丁酯0.5-2份,乙二醇1-3份,丙二醇1-3份,羧甲基纤维素0.2-1份,磷酸三丁酯0.1-1份,六偏磷酸钠0.1-2份,硼酸钠1-20份,水600-1000份,木质素1-20份,钛白粉2-10份,立德粉5-30份,轻质碳酸钙300-500份,重质碳酸钙50-150份,滑石粉20-100份。
2.根据权利要求1所述的一种制备水性仿花岗岩石型涂料的原料,其特征在于,包括如下质量份材料:聚乙烯醇30份,乳化剂1份,邻苯二甲酸二丁酯1份,乙二醇2份,丙二醇2份,羧甲基纤维素0.5份,磷酸三丁酯0.5份,六偏磷酸钠1份,硼酸钠10份,水750份,木质素10份,钛白粉5份,立德粉15份,轻质碳酸钙400份,重质碳酸钙100份,滑石粉50份。
3.一种利用权利要求1所述的原料制备水性仿花岗岩石型涂料的方法,其特征在于,首先,向带有夹套和搅拌的反应器内加入所述计量的水,加热至70-80摄氏度,缓慢地分批加入聚乙烯醇,升温至95-99摄氏度,保温30-50分钟;然后,待聚乙烯醇全部溶解后,加入乳化剂、邻苯二甲酸二丁酯,开始降温至70摄氏度,加入羧甲基纤维素、乙二醇和丙二醇,反应30分钟后降温至60摄氏度,再加入硼酸钠、磷酸三丁酯、木质素和六偏磷酸钠,冷却后过筛除去未溶解物,然后将制得的基材与钛白粉、立德粉、轻质碳酸钙、重质碳酸钙及滑石粉混合搅拌均匀,即制得成品。
CN201310518068.4A 2013-10-28 2013-10-28 一种制备水性仿花岗岩石型涂料的原料及其制备方法 Pending CN103881427A (zh)