CN103880467B - 一种抗裂加气砖及其制作方法 - Google Patents

一种抗裂加气砖及其制作方法 Download PDF

Info

Publication number
CN103880467B
CN103880467B CN201410046829.5A CN201410046829A CN103880467B CN 103880467 B CN103880467 B CN 103880467B CN 201410046829 A CN201410046829 A CN 201410046829A CN 103880467 B CN103880467 B CN 103880467B
Authority
CN
China
Prior art keywords
aerated bricks
present
hour
cracking resistance
ore deposit
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410046829.5A
Other languages
English (en)
Other versions
CN103880467A (zh
Inventor
晋元龙
陈德全
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Gaohang Intellectual Property Operation Co ltd
Sihui Afterburner Cement Products Co ltd
Original Assignee
Hefei Lanke New Materials Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hefei Lanke New Materials Co Ltd filed Critical Hefei Lanke New Materials Co Ltd
Priority to CN201410046829.5A priority Critical patent/CN103880467B/zh
Publication of CN103880467A publication Critical patent/CN103880467A/zh
Application granted granted Critical
Publication of CN103880467B publication Critical patent/CN103880467B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种抗裂加气砖,其特征在于,由下列重量份的原料制成:矾矿尾渣18-20、水泥6-8、滑石粉2-4、镁粉0.3-0.5、左旋酒石酸钾0.1-0.3、右旋酒石酸0.5-1、平平加0.02-0.04、聚丙烯纤维0.1-0.2、二氧化硅7-8、田菁胶4-6、纯碱5-7、氢氧化铝0.01-0.02、茉莉花0.1-0.3、川楝子0.3-0.5、助剂4-6、适量水;本发明通过采用矾矿尾渣作为加气砖的成分,弥补了粉煤灰加气砖抗裂效果低的不足,完全可以取代粘土砖,使用范围广,本发明的方法工艺简单,产品能耗低。同时本发明通过优化配方用料,本发明的保温性能优良,还具有较高的抗压强度。

Description

一种抗裂加气砖及其制作方法
技术领域
本发明涉及加气砖技术领域,具体涉及一种抗裂加气砖及其制作方法。
背景技术
近年来,随着工业化进程的加快和城市化水平的提高,也带来了各种环境压力和问题,工业生产过程产生的各种固废以及城市建设拆迁重造带来的固废等一直困扰着居民的生活环境,本发明将固废作为原材料添加到加气砖中,实现了废物的循环利用,减少了对环境的污染,符合可持续发展战略要求。
加气砖是通过高温蒸压设备工艺生产的加气混凝土砌块。加气混凝土砌块以水泥、矿渣、砂、石灰等为主要原料,加入发气剂,经搅拌成型、蒸压养护而成的实心砌块,加气混凝土按用途,可分为非承重砌块、承重砌块、保温块、墙板与屋面板五种。
传统实心粘土砖重量大,不仅浪费国家粘土资源、价格高外,而且也无法满足一些特殊建筑用砖的要求,因此现在许多先进地区已经全面禁止红砖使用,取而代之大力提倡加气砖。和传统的粘土砖和普通混凝土砖相比,加气砖不仅重量轻,还具有保温隔热、隔音性能优、抗震能力强、加工性能好、耐高温性能佳、适应性强等优点。但是,目前我国有关加气砖的生产技术还不够成熟,使得加气砖发展技术缓慢,还无法满足多元化市场的需求。
发明内容
本发明的目的就是提供一种抗裂加气砖及其制作方法,以克服现有技术的不足。
本发明的目的是这样实现的:
一种抗裂加气砖,其特征在于,由下列重量份的原料制成:矾矿尾渣18-20、水泥6-8、滑石粉2-4、镁粉0.3-0.5、左旋酒石酸钾0.1-0.3、右旋酒石酸0.5-1、平平加0.02-0.04、聚丙烯纤维0.1-0.2、二氧化硅7-8、田菁胶4-6、纯碱5-7、氢氧化铝0.01-0.02、茉莉花0.1-0.3、川楝子0.3-0.5、助剂4-6、适量水;所述的助剂由下列重量份原料制成:聚苯醚0.03-0.05、碳纳米管0.1-0.4、聚氧乙烯醚0.02-0.04、硅酸钠0.2-0.5、三乙胺1.4-2.7、硅灰石粉1-3、乌洛托品0.01-0.02、樟脑0.1-0.3、柏木油1-3、花生壳2-4、三氯乙基磷酸酯1.2-2.3,其制备方法是将各物料粉碎混合,加热至70-80℃,搅拌反应30-40分钟,即得。
所述的一种抗裂加气砖的制备方法,其特征在于包括以下步骤:
(1)将茉莉花、川楝子一起在水中煎煮2-3小时过滤,所得滤液真空浓缩提取,得中药提取物;
(2)将步骤(1)的滤渣和矾矿尾渣、二氧化硅、聚丙烯纤维混匀后,于800-900℃下煅烧3-4小时,冷却,研磨,加入田菁胶、平平加搅拌均匀;
(3)将步骤(1)、(2)反应物料以及其它剩余成分,投入搅拌机里搅拌混合8-10分钟,得混合料浆;
(4)将所得混合料浆浇筑入模成型,于43-53℃下预养1-3小时,脱模,切割,得砌块坯;再将砌块坯放入反应釜中蒸压养护12-15小时,入库即得。
本发明有以下有益效果:本发明通过采用矾矿尾渣作为加气砖的成分,弥补了粉煤灰加气砖抗裂效果低的不足,完全可以取代粘土砖,使用范围广,本发明的方法工艺简单,产品能耗低。同时本发明通过优化配方用料,本发明的保温性能优良,还具有较高的抗压强度。
具体实施方式
所述的一种抗裂加气砖,其特征在于,由下列重量份的原料制成:矾矿尾渣19、水泥6、滑石粉2、镁粉0.3、左旋酒石酸钾0.1、右旋酒石酸0.5、平平加0.02-、聚丙烯纤维0.1、二氧化硅7、田菁胶4、纯碱5、氢氧化铝0.01、茉莉花0.1-0.3、川楝子0.3-0.5、助剂4-6、适量水;所述的助剂由下列重量份原料制成:聚苯醚0.03、碳纳米管0.1、聚氧乙烯醚0.02、硅酸钠0.5、三乙胺2.7、硅灰石粉1、乌洛托品0.01、樟脑0.3、柏木油1、花生壳2、三氯乙基磷酸酯1.2,其制备方法是将各物料粉碎混合,加热至70-80℃,搅拌反应30-40分钟,即得。
制作方法包括以下步骤:
(1)将茉莉花、川楝子一起在水中煎煮2-3小时过滤,所得滤液真空浓缩提取,得中药提取物;
(2)将步骤(1)的滤渣和矾矿尾渣、二氧化硅、聚丙烯纤维混匀后,于800-900℃下煅烧3-4小时,冷却,研磨,加入田菁胶、平平加搅拌均匀;
(3)将步骤(1)、(2)反应物料以及其它剩余成分,投入搅拌机里搅拌混合8-10分钟,得混合料浆;
(4)将所得混合料浆浇筑入模成型,于43-53℃下预养1-3小时,脱模,切割,得砌块坯;再将砌块坯放入反应釜中蒸压养护12-15小时,入库即得。
通过上述实施例加工得到的加气砖的性能数据如下:本砌块的平均容重为535-690kg/m3,保温性能好,在砌块内部具有大量的气孔和微孔,因而有良好的保温隔热性能,平均值抗压强度为6.5-7.8MPa。

Claims (1)

1.一种抗裂加气砖,其特征在于,由下列重量份的原料制成:矾矿尾渣18-20、水泥6-8、滑石粉2-4、镁粉0.3-0.5、左旋酒石酸钾0.1-0.3、右旋酒石酸0.5-1、平平加0.02-0.04、聚丙烯纤维0.1-0.2、二氧化硅7-8、田菁胶4-6、纯碱5-7、氢氧化铝0.01-0.02、茉莉花0.1-0.3、川楝子0.3-0.5、助剂4-6、适量水;所述的助剂由下列重量份原料制成:聚苯醚0.03-0.05、碳纳米管0.1-0.4、聚氧乙烯醚0.02-0.04、硅酸钠0.2-0.5、三乙胺1.4-2.7、硅灰石粉1-3、乌洛托品0.01-0.02、樟脑0.1-0.3、柏木油1-3、花生壳2-4、三氯乙基磷酸酯1.2-2.3,其制备方法是将各物料粉碎混合,加热至70-80℃,搅拌反应30-40分钟,即得;
所述的抗裂加气砖的制作方法包括以下步骤:
(1)将茉莉花、川楝子一起在水中煎煮2-3小时过滤,所得滤液真空浓缩提取,得中药提取物;
(2)将步骤(1)的滤渣和矾矿尾渣、二氧化硅、聚丙烯纤维混匀后,于800-900℃下煅烧3-4小时,冷却,研磨,加入田菁胶、平平加搅拌均匀;
(3)将步骤(1)、步骤(2)反应物料以及其它剩余成分,投入搅拌机里搅拌混合8-10分钟,得混合料浆;
(4)将所得混合料浆浇筑入模成型,于43-53℃下预养1-3小时,脱模,切割,得砌块坯;再将砌块坯放入反应釜中蒸压养护12-15小时,入库即得。
CN201410046829.5A 2014-02-11 2014-02-11 一种抗裂加气砖及其制作方法 Expired - Fee Related CN103880467B (zh)