CN103880348A - 一种原料含有纳米硅的加气砖及其制作方法 - Google Patents

一种原料含有纳米硅的加气砖及其制作方法 Download PDF

Info

Publication number
CN103880348A
CN103880348A CN201410046842.0A CN201410046842A CN103880348A CN 103880348 A CN103880348 A CN 103880348A CN 201410046842 A CN201410046842 A CN 201410046842A CN 103880348 A CN103880348 A CN 103880348A
Authority
CN
China
Prior art keywords
parts
air
powder
hour
silicon
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410046842.0A
Other languages
English (en)
Other versions
CN103880348B (zh
Inventor
晋元龙
陈德全
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Source, Changtai, Guizhou energy-saving building material limited company
Original Assignee
Ma'an Mountain Bao Long Building Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ma'an Mountain Bao Long Building Material Co Ltd filed Critical Ma'an Mountain Bao Long Building Material Co Ltd
Priority to CN201410046842.0A priority Critical patent/CN103880348B/zh
Publication of CN103880348A publication Critical patent/CN103880348A/zh
Application granted granted Critical
Publication of CN103880348B publication Critical patent/CN103880348B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种原料含有纳米硅的加气砖,其特征在于,由下列重量份的原料制成:磷矿渣20-25、石英砂3-7、水泥5-10、生石灰13-15、锌粉0.06-0.2、海藻粉5-8、聚醚多元醇2-3、脱硫石膏10-13、拉开粉BX0.04-0.06、竹炭粉8-10、稻壳炭5-8、角叉菜胶10-12、纳米硅2-4、薄荷0.2-0.4、花椒0.3-0.5、助剂3-5、适量水;本发明通过添加纳米硅和改性稻壳炭,减轻了砖的容重,同时,使用磷矿渣,减少了能源消耗与环境污染,大大提高加气砖的保温性能,成品强度、抗冻性明显提高。

Description

一种原料含有纳米硅的加气砖及其制作方法
技术领域
本发明涉及加气砖技术领域,具体涉及一种原料含有纳米硅的加气砖及其制作方法。
背景技术
 近年来,随着工业化进程的加快和城市化水平的提高,也带来了各种环境压力和问题,工业生产过程产生的各种固废以及城市建设拆迁重造带来的固废等一直困扰着居民的生活环境,本发明将固废作为原材料添加到加气砖中,实现了废物的循环利用,减少了对环境的污染,符合可持续发展战略要求。
加气砖是通过高温蒸压设备工艺生产的加气混凝土砌块。加气混凝土砌块以水泥、矿渣、砂、石灰等为主要原料,加入发气剂,经搅拌成型、蒸压养护而成的实心砌块,加气混凝土按用途,可分为非承重砌块、承重砌块、保温块、墙板与屋面板五种。
传统实心粘土砖重量大,不仅浪费国家粘土资源、价格高外,而且也无法满足一些特殊建筑用砖的要求,因此现在许多先进地区已经全面禁止红砖使用,取而代之大力提倡加气砖。和传统的粘土砖和普通混凝土砖相比,加气砖不仅重量轻,还具有保温隔热、隔音性能优、抗震能力强、加工性能好、耐高温性能佳、适应性强等优点。但是,目前我国有关加气砖的生产技术还不够成熟,使得加气砖发展技术缓慢,还无法满足多元化市场的需求。
发明内容
本发明的目的就是提供一种原料含有纳米硅的加气砖及其制作方法,以克服现有技术的不足。
本发明的目的是这样实现的:
一种原料含有纳米硅的加气砖,其特征在于,由下列重量份的原料制成:磷矿渣20-25、石英砂3-7、水泥5-10、生石灰13-15、锌粉0.06-0.2、海藻粉5-8、聚醚多元醇2-3、脱硫石膏10-13、拉开粉BX0.04-0.06、竹炭粉8-10、稻壳炭5-8、角叉菜胶10-12、纳米硅2-4、薄荷0.2-0.4、花椒0.3-0.5、助剂3-5、适量水;所述的助剂由下列重量份原料制成:聚苯醚0.03-0.05、碳纳米管0.1-0.4、聚氧乙烯醚0.02-0.04、硅酸钠0.2-0.5、三乙胺1.4-2.7、硅灰石粉1-3、乌洛托品0.01-0.02、樟脑0.1-0.3、柏木油1-3、花生壳2-4、三氯乙基磷酸酯1.2-2.3,其制备方法是将各物料粉碎混合,加热至70-80℃,搅拌反应30-40分钟,即得。
所述的一种原料含有纳米硅的加气砖的制备方法,其特征在于包括以下步骤:
(1)将薄荷、花椒一起在水中煎煮2-3小时过滤,所得滤液真空浓缩提取,得中药提取物;
(2)将步骤(1)的滤渣和磷矿渣、石英砂、脱硫石膏、稻壳炭混匀后,于650-700℃下煅烧3-4小时,冷却,研磨,加入海藻粉、聚醚多元醇、拉开粉BX搅拌均匀;
(3)将步骤(1)、(2)反应物料以及其它剩余成分,投入搅拌机里搅拌混合8-10分钟,得混合料浆;
(4)将所得混合料浆浇筑入模成型,于45-53℃下预养1-3 小时,脱模,切割,得砌块坯;再将砌块坯放入反应釜中蒸压养护12-15 小时,入库即得。
本发明有以下有益效果:本发明通过添加纳米硅和改性稻壳炭,减轻了砖的容重,同时,使用磷矿渣,减少了能源消耗与环境污染,大大提高加气砖的保温性能,成品强度、抗冻性明显提高。
具体实施方式
所述的一种原料含有纳米硅的加气砖,其特征在于,由下列重量份的原料制成:磷矿渣22、石英砂7、水泥10、生石灰13、锌粉0.06、海藻粉5、聚醚多元醇2、脱硫石膏13、拉开粉BX 0.04、竹炭粉9、稻壳炭6、角叉菜胶11、纳米硅2、薄荷0.24、花椒0.3、助剂3、适量水;所述的助剂由下列重量份原料制成:聚苯醚0.03、碳纳米管0.14、聚氧乙烯醚0.04、硅酸钠0.2、三乙胺2.7、硅灰石粉3、乌洛托品0.01、樟脑0.13、柏木油1、花生壳2、三氯乙基磷酸酯1.2,其制备方法是将各物料粉碎混合,加热至70-80℃,搅拌反应30-40分钟,即得。
制作方法包括以下步骤:
(1)将薄荷、花椒一起在水中煎煮2-3小时过滤,所得滤液真空浓缩提取,得中药提取物;
(2)将步骤(1)的滤渣和磷矿渣、石英砂、脱硫石膏、稻壳炭混匀后,于650-700℃下煅烧3-4小时,冷却,研磨,加入海藻粉、聚醚多元醇、拉开粉BX搅拌均匀;
(3)将步骤(1)、(2)反应物料以及其它剩余成分,投入搅拌机里搅拌混合8-10分钟,得混合料浆;
(4)将所得混合料浆浇筑入模成型,于45-53℃下预养1-3 小时,脱模,切割,得砌块坯;再将砌块坯放入反应釜中蒸压养护12-15 小时,入库即得。
通过上述实施例加工得到的加气砖的性能数据如下:本发明制得的加气砖的平均容重为520-680kg/m3,导热系数为0.11-0.15W/MK,在砌块内部具有大量的气孔和微孔,因而有良好的保温隔热性能,平均值抗压强度为6.8-8.2MPa。

Claims (2)

1.一种原料含有纳米硅的加气砖,其特征在于,由下列重量份的原料制成:磷矿渣20-25、石英砂3-7、水泥5-10、生石灰13-15、锌粉0.06-0.2、海藻粉5-8、聚醚多元醇2-3、脱硫石膏10-13、拉开粉BX0.04-0.06、竹炭粉8-10、稻壳炭5-8、角叉菜胶10-12、纳米硅2-4、薄荷0.2-0.4、花椒0.3-0.5、助剂3-5、适量水;所述的助剂由下列重量份原料制成:聚苯醚0.03-0.05、碳纳米管0.1-0.4、聚氧乙烯醚0.02-0.04、硅酸钠0.2-0.5、三乙胺1.4-2.7、硅灰石粉1-3、乌洛托品0.01-0.02、樟脑0.1-0.3、柏木油1-3、花生壳2-4、三氯乙基磷酸酯1.2-2.3,其制备方法是将各物料粉碎混合,加热至70-80℃,搅拌反应30-40分钟,即得。
2.根据权利要求1所述的一种原料含有纳米硅的加气砖的制作方法,其特征在于包括以下步骤:
(1)将薄荷、花椒一起在水中煎煮2-3小时过滤,所得滤液真空浓缩提取,得中药提取物;
(2)将步骤(1)的滤渣和磷矿渣、石英砂、脱硫石膏、稻壳炭混匀后,于650-700℃下煅烧3-4小时,冷却,研磨,加入海藻粉、聚醚多元醇、拉开粉BX搅拌均匀;
(3)将步骤(1)、(2)反应物料以及其它剩余成分,投入搅拌机里搅拌混合8-10分钟,得混合料浆;
(4)将所得混合料浆浇筑入模成型,于45-53℃下预养1-3 小时,脱模,切割,得砌块坯;再将砌块坯放入反应釜中蒸压养护12-15 小时,入库即得。
CN201410046842.0A 2014-02-11 2014-02-11 一种原料含有纳米硅的加气砖及其制作方法 Active CN103880348B (zh)