CN103711009A - Production method of wool sea-island pile blended fabric - Google Patents
Production method of wool sea-island pile blended fabric Download PDFInfo
- Publication number
- CN103711009A CN103711009A CN201310726797.9A CN201310726797A CN103711009A CN 103711009 A CN103711009 A CN 103711009A CN 201310726797 A CN201310726797 A CN 201310726797A CN 103711009 A CN103711009 A CN 103711009A
- Authority
- CN
- China
- Prior art keywords
- fabric
- wool
- raw material
- production method
- oxygen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention provides a production method of a wool sea-island pile blended fabric, and belongs to the technical field of wool sea-island pile blended fabric processing. The production method comprises the following steps: selecting a face texture raw material and a bottom texture raw material, and warping the raw materials; weaving the warped raw materials on a warp knitting machine so as to obtain a double-faced loop pile fabric grey fabric with double-faced looped piles; carrying out oxygen bleaching; dyeing; washing with water; dyeing; fixing color; slitting, and cutting piles. The production method disclosed by the invention has the advantage that the method can be used for ensuring that the obtained fabric has good size stability and a good antibacterial deodorization effect, is unlikely to ladder and does not generate peculiar smell and foul smell.
Description
Technical field
The invention belongs to the processing technique field of wool island suede mixed fabric, be specifically related to the production method of a kind of wool island suede mixed fabric.
Background technology
Wool island suede mixed fabric has dimensional instability, easily reels off raw silk from cocoons, and fabric can produce the shortcomings such as foreign odor taste under long-time moist situation.
Therefore, be necessary to be explored technically, to make wool island suede mixed fabric both there is good DIMENSIONAL STABILITY, be difficult for reeling off raw silk from cocoons, have again desirable hygroscopicity, wash and wear and have excellent antibiosis and deodorization effects, technical scheme described below produces under this background.
Summary of the invention
Task of the present invention is to provide a kind of production method of the wool island suede mixed fabric that had both had good DIMENSIONAL STABILITY, has been difficult for reeling off raw silk from cocoons.
Task of the present invention completes like this, the production method of a kind of wool island suede mixed fabric, and it comprises the following steps:
1) select raw material, choose covering weave raw material and the end and organize raw material and carry out warping;
2) weave, the raw material after warping is weaved on warp knitting machine, obtain having the two-sided circle pile fabric grey cloth of two-sided terry;
3) oxygen floats, and to two-sided circle pile fabric rayon gray fabric oxygen bleaching, steam pressure when oxygen floats is to be 0.6~0.8MPa by Steam pressure control; Described control grey cloth gait of march is to be 20~25m/min by the gait of march control of grey cloth; The time that described control oxygen floats and bath temperature are that oxygen is floated to time and bath temperature control is respectively 40~50min and 90~95 ℃, and wherein, it is hydrogen peroxide that oxygen floats agent, and the addition of hydrogen peroxide is 5~8g/L;
4) dyeing, dye formulation is: the DISPERSE DYES 2~3% of fabric weight ratio, metabisulfite solution 4~6g/L, sodium carbonate liquor 15~20g/L, dichloroacetic acid 3~4g/L and dimethylethanolamine 3~4g/L, dyeing temperature is 100~110 ℃, pressure is 250~280KPa, and the time is 20~25min;
5) adopt 4~5% alkaline reduction washings of fabric quality ratio;
6) dry, bake out temperature is 180~200 ℃, cloth speed 8~10m/min;
7) fixation adds 5-nitrofuran methylene acetone 3~4g/L and arhat pitch 10~15g/L when fixation, adds 12~25g/L softener in fixation process;
8) cut open width and clipping, obtain wool island suede mixed fabric.
The advantage of technical scheme provided by the present invention is: disclosed method can ensure that the fabric obtaining possesses good DIMENSIONAL STABILITY, is difficult for reeling off raw silk from cocoons, owing to having added antibacterial, arhat pitch in fixation step, thereby can make fabric there is antibiosis and deodorization effects, under long-time moist situation, can not produce foreign odor taste.
The specific embodiment
Below in conjunction with the specific embodiment, be described further:
Task of the present invention completes like this, the production method of a kind of wool island suede mixed fabric, and it comprises the following steps:
1) select raw material, choose covering weave raw material and the end and organize raw material and carry out warping;
2) weave, the raw material after warping is weaved on warp knitting machine, obtain having the two-sided circle pile fabric grey cloth of two-sided terry;
3) oxygen floats, and to two-sided circle pile fabric rayon gray fabric oxygen bleaching, steam pressure when oxygen floats is to be 0.6~0.8MPa by Steam pressure control; Described control grey cloth gait of march is to be 20~25m/min by the gait of march control of grey cloth; The time that described control oxygen floats and bath temperature are that oxygen is floated to time and bath temperature control is respectively 40~50min and 90~95 ℃, and wherein, it is hydrogen peroxide that oxygen floats agent, and the addition of hydrogen peroxide is 5~8g/L;
4) dyeing, dye formulation is: the DISPERSE DYES 2~3% of fabric weight ratio, metabisulfite solution 4~6g/L, sodium carbonate liquor 15~20g/L, dichloroacetic acid 3~4g/L and dimethylethanolamine 3~4g/L, dyeing temperature is 100~110 ℃, pressure is 250~280KPa, and the time is 20~25min;
5) adopt 4~5% alkaline reduction washings of fabric quality ratio;
6) dry, bake out temperature is 180~200 ℃, cloth speed 8~10m/min;
7) fixation adds 5-nitrofuran methylene acetone 3~4g/L and arhat pitch 10~15g/L when fixation, adds 12~25g/L softener in fixation process;
8) cut open width and clipping, obtain wool island suede mixed fabric.
The advantage of technical scheme provided by the present invention is: disclosed method can ensure that the fabric obtaining possesses good DIMENSIONAL STABILITY, is difficult for reeling off raw silk from cocoons, owing to having added antibacterial, arhat pitch in fixation step, thereby can make fabric there is antibiosis and deodorization effects, under long-time moist situation, can not produce foreign odor taste.
Claims (1)
1. a production method for wool island suede mixed fabric, is characterized in that it comprises the following steps:
1) select raw material, choose covering weave raw material and the end and organize raw material and carry out warping;
2) weave, the raw material after warping is weaved on warp knitting machine, obtain having the two-sided circle pile fabric grey cloth of two-sided terry;
3) oxygen floats, and to two-sided circle pile fabric rayon gray fabric oxygen bleaching, steam pressure when oxygen floats is to be 0.6~0.8MPa by Steam pressure control; Described control grey cloth gait of march is to be 20~25m/min by the gait of march control of grey cloth; The time that described control oxygen floats and bath temperature are that oxygen is floated to time and bath temperature control is respectively 40~50min and 90~95 ℃, and wherein, it is hydrogen peroxide that oxygen floats agent, and the addition of hydrogen peroxide is 5~8g/L;
4) dyeing, dye formulation is: the DISPERSE DYES 2~3% of fabric weight ratio, metabisulfite solution 4~6g/L, sodium carbonate liquor 15~20g/L, dichloroacetic acid 3~4g/L and dimethylethanolamine 3~4g/L, dyeing temperature is 100~110 ℃, pressure is 250~280KPa, and the time is 20~25min;
5) adopt 4~5% alkaline reduction washings of fabric quality ratio;
6) dry, bake out temperature is 180~200 ℃, cloth speed 8~10m/min;
7) fixation adds 5-nitrofuran methylene acetone 3~4g/L and arhat pitch 10~15g/L when fixation, adds 12~25g/L softener in fixation process;
8) cut open width and clipping, obtain wool island suede mixed fabric.