CN103706660A - 一种铝型材挤压模套 - Google Patents

一种铝型材挤压模套 Download PDF

Info

Publication number
CN103706660A
CN103706660A CN201310714992.XA CN201310714992A CN103706660A CN 103706660 A CN103706660 A CN 103706660A CN 201310714992 A CN201310714992 A CN 201310714992A CN 103706660 A CN103706660 A CN 103706660A
Authority
CN
China
Prior art keywords
die
die sleeve
sleeve body
sized
diameter
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310714992.XA
Other languages
English (en)
Other versions
CN103706660B (zh
Inventor
刘煌萍
李进洪
丁杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong galuminium Aluminium Co. Ltd.
Original Assignee
GALUMINIUM GROUP CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GALUMINIUM GROUP CO Ltd filed Critical GALUMINIUM GROUP CO Ltd
Priority to CN201310714992.XA priority Critical patent/CN103706660B/zh
Publication of CN103706660A publication Critical patent/CN103706660A/zh
Application granted granted Critical
Publication of CN103706660B publication Critical patent/CN103706660B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种铝型材挤压模套,用于将小规格挤压模具装配到大规格挤压机上,包括模套本体,模套本体后端设有一安装容纳小规格挤压模具的容纳腔,模套本体前端设有与容纳腔相通的预变通道,预变通道的横截面面积小于大规格挤压筒的内腔横截面面积,模套本体前端外缘直径大于大规格挤压筒的内腔直径,小规格挤压模具先嵌入安装在容纳腔后再装配至大规格挤压机上,由于模套本体前端外缘直径远大于大规格挤压筒的内腔直径,从而顺利地将小规格挤压模具安装到大规格挤压机上,通过预变通道,直径较大的铝棒进入小规格挤压模具前,先通过预变通道进行预挤压成型为直径较小的铝棒,再通过小规格挤压模具的模腔形成所需的铝型材。

Description

一种铝型材挤压模套
技术领域
    本发明涉及铝型材挤压技术领域,特别涉及一种铝型材挤压模套。
背景技术
现有的铝型材挤压机主要由模座、挤压筒、挤压杆、挤压垫、模套及模垫等构成,如图1所示,铝型材挤压是对放在挤压筒1内腔中的铝棒2一端施加压力,使之通过挤压模具3的模腔以挤压出各种形状的铝型材4。挤压模具3装配到挤压机中,挤压模具3的外径应该是大于挤压筒1的内腔直径,使得在压力的作用下,挤压模具3的端面与挤压筒1的端面相贴合锁紧。
对于不同能力的挤压机,即不同规格的挤压机,其装备的挤压筒和挤压模具的大小规格是不同的,挤压能力越大的挤压机,其挤压筒内径和挤压模具外径就越大,即规格越大。
当小规格挤压模具装备到大规格挤压机上时,往往挤压模具外径小于挤压筒内径,使得挤压模具的端面与挤压筒的端面无法实现贴合锁紧,不能进行挤压的生产;或者挤压模具止口直径虽然略大于挤压筒内径,但两者接触面太小,锁紧时接触面压强太大,超过挤压筒钢材屈服强度,造成挤压筒的破坏。
 
发明内容
本发明所要解决的技术问题是提供一种可将小规格挤压模具装配到大规格挤压机上的铝型材挤压模套。
为解决上述技术问题所采用的技术方案:一种铝型材挤压模套,用于将小规格挤压模具装配到大规格挤压机上,包括模套本体,所述模套本体后端设有一安装容纳小规格挤压模具的容纳腔,所述模套本体前端设有与容纳腔相通的预变通道,所述大规格挤压机具有一大规格挤压筒,所述预变通道的横截面面积小于大规格挤压筒的内腔横截面面积,所述预变通道的横截面面积大于小规格挤压模具的模腔横截面面积,所述模套本体前端外缘直径大于大规格挤压筒的内腔直径。
进一步作为本发明技术方案的改进,所述模套本体前端外缘直径与大规格挤压筒的内腔直径之间的差值大于75mm。
进一步作为本发明技术方案的改进,所述预变通道的横截面形状与大规格挤压筒的内腔横截面形状相似。
有益效果:小规格挤压模具先嵌入安装在模套本体的容纳腔内与模套本体成为一整体,再将该模套本体的前端面与大规格挤压机中大规格挤压筒的端面相贴合锁紧,由于模套本体前端外缘直径远大于大规格挤压筒的内腔直径,从而顺利地将小规格挤压模具安装到大规格挤压机上;在模套本体前端还设有一预变通道,直径较大的铝棒进入小规格挤压模具前,先通过预变通道进行预挤压成型为直径较小的铝棒,再通过小规格挤压模具的模腔形成所需的铝型材。通过设计本发明挤压模套实现小规格挤压模具装配到大规格挤压机上,充分解决了小规格挤压机生产量满负荷,而大规格挤压机开工不足的问题,从而提高生产效率和降低生产成本。
附图说明
下面结合附图和实施例对本发明做进一步的说明;
图1为现有技术中铝型材挤压成型示意图;
图2为本发明实施例挤压模套的装配示意图;
图3为本发明实施例挤压模套的结构示意图。
具体实施方式
参照图2和图3,本发明一种铝型材挤压模套,用于将小规格挤压模具20装配到大规格挤压机上,包括模套本体10,模套本体10后端设有一安装容纳小规格挤压模具20的容纳腔11,模套本体10前端设有与容纳腔11相通的预变通道12,大规格挤压机具有一大规格挤压筒30,预变通道12的横截面面积小于大规格挤压筒30的内腔31横截面面积,预变通道12的横截面面积大于小规格挤压模具20的模腔21横截面面积,模套本体10前端外缘13直径大于大规格挤压筒30的内腔31直径。
本发明通过在采用一专用挤压模套可使小规格挤压模具20安装到大规格挤压机的模座上,具体地,小规格挤压模具20先嵌入安装到模套本体10的容纳腔11内,使之与模套本体20成为一整体,带有小规格挤压模具20的模套本体10再安装到大规格挤压机的模座上,模套本体10的前端面与大规格挤压机中大规格挤压筒30的端面相贴合锁紧,从而顺利将小规格挤压模具20安装到大规格挤压机上。
一定规格大小的挤压模具相应要求一定规格大小的铝棒,传统中即使小规格的挤压模具勉强装到大规格的挤压机上,也难以完成挤压成型工序,即大直径铝棒难以直接通过小规格的挤压模具挤压成型,在本实施例中,将小规格挤压模具20安装到大规格挤压机后,由于大规格挤压机中的铝棒直径较大,难以顺利直接通过小规格挤压模具20挤压得到所需的铝型材,必须先成型小直径铝棒,故在模套本体10前端还设有一预变通道12,直径较大的铝棒进入小规格挤压模具20前,先通过预变通道12进行预挤压成型为直径较小的铝棒,再通过小规格挤压模具20的模腔形成所需的铝型材,通过在模套本体10中设置预变通道12使得一次挤压完成两道挤压工序,即大直径铝棒挤压成小直径铝棒的预挤压工序和小直径铝棒挤压成预定形状铝型材的成型工序,通过本发明挤压模套使得小规格挤压模具20装配到大规格挤压机成为可能,且大直径铝棒直接利用小规格挤压模具20挤压预定形状的铝型材。
通过设计本发明挤压模套实现小规格挤压模具20装配到大规格挤压机上,充分解决了小规格挤压机生产量满负荷,而大规格挤压机开工不足的问题,从而提高生产效率和降低生产成本。
作为本发明的优选实施方式,模套本体前端外缘直径与大规格挤压筒的内腔直径之间的差值大于75mm。
作为本发明的优选实施方式,预变通道的横截面形状与大规格挤压筒的内腔横截面形状相似。
上面结合附图对本发明的实施方式作了详细说明,但是本发明不限于上述实施方式,在所述技术领域普通技术人员所具备的知识范围内,还可以在不脱离本发明宗旨的前提下作出各种变化。

Claims (3)

1.一种铝型材挤压模套,用于将小规格挤压模具装配到大规格挤压机上,其特征在于:包括模套本体,所述模套本体后端设有一安装容纳小规格挤压模具的容纳腔,所述模套本体前端设有与容纳腔相通的预变通道,所述大规格挤压机具有一大规格挤压筒,所述预变通道的横截面面积小于大规格挤压筒的内腔横截面面积,所述预变通道的横截面面积大于小规格挤压模具的模腔横截面面积,所述模套本体前端外缘直径大于大规格挤压筒的内腔直径。
2.根据权利要求1所述的铝型材挤压模套,其特征在于:所述模套本体前端外缘直径与大规格挤压筒的内腔直径之间的差值大于75mm。
3.根据权利要求1或2所述的铝型材挤压模套,其特征在于:所述预变通道的横截面形状与大规格挤压筒的内腔横截面形状相似。
CN201310714992.XA 2013-12-20 2013-12-20 一种铝型材挤压模套 Active CN103706660B (zh)