CN103666280B - Polishing wax emulsion for leather finishing and preparation method thereof - Google Patents
Polishing wax emulsion for leather finishing and preparation method thereof Download PDFInfo
- Publication number
- CN103666280B CN103666280B CN201310563477.6A CN201310563477A CN103666280B CN 103666280 B CN103666280 B CN 103666280B CN 201310563477 A CN201310563477 A CN 201310563477A CN 103666280 B CN103666280 B CN 103666280B
- Authority
- CN
- China
- Prior art keywords
- wax
- leather
- minutes
- temperature
- reactor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention provides a polishing wax emulsion for leather finishing and a preparation method thereof. The preparation method comprises the following steps: (1) putting 3.5-4.6% of oxidized petroleum wax, 1.4-1.9% of lignite wax, 3.3-4.8% of rice bran wax, 5.5-6.5% of paraffin, 8.4-10.8% of comprehensive wax emulsifier, 0.5-1.5% of co-emulsifier and 1.0-1.5% of sodium hydroxide solution into a reaction kettle, and heating to 100 DEG C, thus melting the materials; (2) starting to stir, controlling the rotation speed to be 85 r/min, and ensuring that the materials are uniformly mixed; (3) turning on cooling water, reducing the temperature in the reaction kettle to 90 DEG C, adding distilled water (95 DEG C) accounting for 50% of the total amount into the reaction kettle, increasing the stirring speed to 400 r/min, and emulsifying for 40-50 minutes; (4) reducing the temperature to 60 DEG C, adding the residual distilled water (60 DEG C) into the reaction kettle, ensuring that the stirring speed is 800 r/min, and emulsifying for 60-75 minutes; and (5) reducing the temperature to 35 DEG C, further stirring for 30-40 minutes, filtering, and discharging. The prepared leather polishing wax emulsion can increase the gloss of the leather, improve the hand feeling of the leather and reinforce the wear resistance of the leather.
Description
Technical field
The present invention relates to the preparation method of leather finish cerate, more particularly, that the present invention relates to is a kind of preparation method of the buffing wax emulsion for leather finish.
Background technology
Emulsifying wax in leather industry mainly as leather finish auxiliary agent, for the end, in, top be coated with, there is good performance.
Wax had both had the general character of water-repellancy and oilness, had again the characteristic of such as oiliness, viscosity, fragility, toughness, fusibleness and gloss aspect, had a great difference to each other.There is as paraffin the advantages such as dryness, glossiness and the transparency, but its shortcoming to be film more crisp; Beeswax has good toughness, but difference in quality is larger because the place of production is different; It is high that carnauba wax and Insect Wax have fusing point, and hardness is large, wipes luminance brightness good, and oil number is large, the features such as easy emulsification.
In actual applications, a kind of wax can not have all character met required for a certain specific end use.Therefore, when selecting the raw material of leather finish emulsifying wax, the use properties of wax be considered, improving the Spraying technique of leather finish.
Summary of the invention
The object of this invention is to provide a kind of preparation method of the buffing wax emulsion for leather finish, obtain remarkable back cover and polishing, burn effect, and can hand feel and drape be obtained after hot iron, sense organ nature, the covering with paint style that surface is fine and smooth, to make up the deficiencies in the prior art.
For achieving the above object, the technical solution used in the present invention is:
(1) by oxidized petroleum wax 3.5% ~ 4.6%, montanin wax 1.4% ~ 1.9%, rice bran wax 3.3% ~ 4.8%, paraffin 5.5% ~ 6.5%, comprehensive wax emulsifying agent 8.4% ~ 10.8%, assistant for emulsifying agent 0.5% ~ 1.5%, oxygen sodium oxide 1.0% ~ 1.5% is placed in reactor, is heated to 100 DEG C and makes it melt.
(2) open stirring, control rotating speed at 85r/min, make mixing of materials even.
(3) open water coolant, make reactor temperature be reduced to 90 DEG C, add the distilled water (95 DEG C) accounting for total amount 50% in reactor, improve stirring velocity 400r/min, emulsification times is 40 ~ 50 minutes
(4) temperature is reduced to 60 DEG C, adds remaining distilled water (60 DEG C) in reactor, stirring velocity is at 800r/min, and emulsification times is 60 ~ 75 minutes.
(5) temperature is reduced to 35 DEG C, Keep agitation 30 ~ 40 minutes, filters discharging.
This leather buffing wax emulsion can improve the gloss of leather, improves leather hand feeling, strengthens leather wear resistance.
Embodiment
Below by embodiment, the present invention is specifically described.
Embodiment 1
By oxidized petroleum wax 3.8%, montanin wax 1.9%, rice bran wax 3.5%, paraffin 5.9%, comprehensive wax emulsifying agent 9.6%, assistant for emulsifying agent 1.2%, sodium hydroxide 1.5% is placed in reactor, is heated to 100 DEG C and makes it melt.Open and stir, control rotating speed at 85r/min, make mixing of materials even.Control temperature 90 DEG C, adds the hot water (95 DEG C) accounting for total amount 50% in reactor, and improve stirring velocity 400r/min, emulsification times is 40 minutes.Temperature is reduced to 60 DEG C, in reactor, add the hot water (60 DEG C) accounting for total amount 22.6%, stirring velocity is at 800r/min, and emulsification times is 65 minutes.Temperature is reduced to 35 DEG C, Keep agitation 35 minutes, filters discharging.
Embodiment 2
By oxidized petroleum wax 3.5%, montanin wax 1.5%, rice bran wax 3.7%, paraffin 5.8%, comprehensive wax emulsifying agent 9.0%, is placed in reactor, is heated to 100 DEG C and makes it melt.Open and stir, control rotating speed at 85r/min, make mixing of materials even.Control temperature 90 DEG C, adds the hot water (95 DEG C) accounting for total amount 50% in reactor, and improve stirring velocity 400r/min, emulsification times is 40 minutes.Temperature is reduced to 60 DEG C, in reactor, add the hot water (60 DEG C) accounting for total amount 24.3%, stirring velocity is at 800r/min, and emulsification times is 65 minutes.Temperature is reduced to 35 DEG C, Keep agitation 35 minutes, filters discharging.
Claims (2)
1., for a buffing wax emulsion for leather finish, it comprises the component of following weight proportioning:
Described oxidized petroleum wax is the oxide compound of refined paraffin wax, montanin wax is deep processed product essence wax, rice bran wax is deep processed product essence wax, paraffin is refined paraffin wax, comprehensive wax emulsifying agent is nonionogenic tenside, by polyoxyethylene sorbitan fatty acid ester, and fatty alcohol-polyoxyethylene ether composition, wherein said polyoxyethylene sorbitan fatty acid ester is polyoxyethylene sorbitan fatty acid ester (80), is (60), fatty alcohol-polyoxyethylene ether is fatty alcohol-polyoxyethylene ether (9), assistant for emulsifying agent is positive Lauryl Alcohol and/or positive 16 carbon alcohol, sodium hydroxide solution mass percent is 15%.
2. a preparation method for the buffing wax emulsion for leather finish according to claim 1, its processing step is:
(1) by oxidized petroleum wax 3.5% ~ 4.6%, montanin wax 1.4% ~ 1.9%, rice bran wax 3.3% ~ 4.8%, paraffin 5.5% ~ 6.5%, comprehensive wax emulsifying agent 8.4% ~ 10.8%, assistant for emulsifying agent 0.5% ~ 1.5%, sodium hydroxide solution 1.0% ~ 1.5% is placed in reactor, is heated to 100 DEG C and makes it melt;
(2) open stirring, control rotating speed at 85r/min, make mixing of materials even;
(3) open water coolant, make reactor temperature be reduced to 90 DEG C, add the 95 DEG C of distilled water accounting for total amount 50% in reactor, improve stirring velocity 400r/min, emulsification times is 40 ~ 50 minutes;
(4) temperature is reduced to 60 DEG C, adds remaining 60 DEG C of distilled water in reactor, stirring velocity is at 800r/min, and emulsification times is 60 ~ 75 minutes;
(5) temperature is reduced to 35 DEG C, Keep agitation 30 ~ 40 minutes, filters discharging.