Prior art keywords
titanium alloy
cylindrical part
alloy cylindrical
vacuum
foundry goods
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210353649.2A
Other languages
English (en)
Other versions
CN103658548A (zh
Inventor
孙敏杰
王宝兵
李宝辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Space Precision Machinery Research Institute
Original Assignee
Shanghai Space Precision Machinery Research Institute
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Space Precision Machinery Research Institute filed Critical Shanghai Space Precision Machinery Research Institute
Priority to CN201210353649.2A priority Critical patent/CN103658548B/zh
Publication of CN103658548A publication Critical patent/CN103658548A/zh
Application granted granted Critical
Publication of CN103658548B publication Critical patent/CN103658548B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Manufacture And Refinement Of Metals (AREA)

Abstract

本发明公开了一种钛合金筒形件石墨型铸造方法,该方法包括下述工艺步骤:1)钛合金筒形件浇注系统设计;2)石墨模具的制备;3)石墨模具除气;4)石墨模具按照铸件组型图组成铸型;5)钛合金真空自耗电极凝壳熔炼工艺。本发明通过钛合金筒形铸件石墨型铸造工艺的研究,成功浇注出了表面质量和机械性能合格的钛合金筒形铸件,避免了钛合金筒形件对机加工制备方式的依赖,降低了生产成本,提高了生产效率。

Description

一种钛合金筒形件的石墨型铸造方法
技术领域
本发明涉及一种钛合金铸造工艺,具体涉及一种钛合金筒形件的石墨型铸造工艺。
背景技术
舵机舱和控制舱一般均为钛合金筒形件,由于其内部结构复杂、凸台较多、壁厚相差较大,前期的研制生产过程中铸造件中存在着很多裂纹、气孔等缺陷,这大大影响了产品的生产进度,成为型号研制和生产的瓶颈,造成制造成本居高不下,研制节点难以保证,必需加以解决。
发明内容
本发明的所要解决的技术问题在于提供一种合适的钛合金筒形件的铸造工艺,使其能够浇注出表面质量和机械性能合格的钛合金筒形件。
为了解决本发明的上述技术问题,本发明提供的解决方案是:一种钛合金筒形件的铸造工艺,包括以下步骤:
第一步:钛合金筒形件石墨模具的选材采用TSK石墨,同时根据浇注系统设计进行加工、组装;
第二步:将组装好的钛合金筒形件石墨模具在真空度为6×10-1~8×10-1Pa,700~900℃下焙烧2~3小时,随炉冷却到200~300℃后出炉。
第三步:将组装好的石墨模具放入真空自耗熔炼炉内,并调整合金锭使其电极对中度达到100%。
第四步:关闭好炼炉门后对真空自耗炉进行抽真空,当真空度达到0.2~0.4Pa时进行熔炼,熔炼过程中真空度保持在0.5~0.6Pa左右。
第五步:熔炼过程中电压控制在25~35V,电流控制在6~8KA,熔炼时间在2~7min,静置1~6分钟后进行浇注。
浇注完成后铸件随炉冷却到室温后,将铸件从真空自耗电极熔炼炉中取出。对铸件打磨处理后得到质量合格的铸件。
进一步地,所述浇注系统采用顶铸式形式的浇注方式,包括一个浇口杯,一个直浇道,两个横浇道和12个内浇道,铸件浇注时液体从顶部引入液流。
本发明相对于现有技术的有益效果是:解决了铸造件中存在很多裂纹、气孔等缺陷,加快了生产进度,为型号研制和生产的提供便利,节约了制造成本。
具体实施方式
下面结合具体实施例,进一步阐述本发明。
本发明实施例提供的钛合金筒形件铸造工艺,具体实施方法如下:
钛合金筒形件浇注系统采用顶铸式形式的浇注方式,包括一个浇口杯,一个直浇道,两个横浇道和12个内浇道,铸件浇注时液体从顶部引入液流。
本发明包括浇注系统设计、石墨模具的选材、制备、组装、焙烧工艺研究、钛合金真空自耗电极凝壳熔炼工艺研究。
钛合金筒形件石墨模具的选材采用TSK石墨,同时根据浇注系统设计进行加工、组装。
组装好的钛合金筒形件石墨模具在真空度为6×10-1~8×10-1Pa,700~900℃下焙烧2~3小时,随炉冷却到200~300℃后出炉。
将组装好的石墨模具放入真空自耗熔炼炉内,并调整合金锭使其电极对中度达到100%。
关闭好炉门后对真空自耗炉进行抽真空,当真空度达到0.2~0.4Pa时进行熔炼,熔炼过程中真空度保持在0.5~0.6Pa左右。
熔炼过程中电压控制在25~35V,电流控制在6~8KA,熔炼时间在2~7min,静置1~6分钟后进行浇注。
浇注完成后铸件随炉冷却到室温后,将铸件从真空自耗电极熔炼炉中取出。对铸件打磨处理后得到质量合格的铸件。
上述实施例应理解为仅用于说明本发明而不用于限制本发明的保护范围。在阅读了本发明记载的内容之后,本领域技术人员可以对本发明作各种改动或修改,这些等效变化和修饰同样落入本发明权利要求所限定的范围。

Claims (3)

1.一种钛合金筒形件石墨型铸造方法,其特征在于,包括以下步骤:
第一步:钛合金筒形件石墨模具的选材采用TSK石墨,同时根据浇注系统设计进行加工、组装;
第二步:将组装好的钛合金筒形件石墨模具在真空度为6×10-1~8×10-1Pa,700~900℃下焙烧2~3小时,随炉冷却到200~300℃后出炉;
第三步:将组装好的石墨模具放入真空自耗熔炼炉内,并调整合金锭使其电极对中度达到100%;
第四步:关闭好炼炉门后对真空自耗炉进行抽真空,当真空度达到0.2~0.4Pa时进行熔炼,熔炼过程中真空度保持在0.5~0.6Pa;
第五步:熔炼过程中电压控制在25~35V,电流控制在6~8KA,熔炼时间在2~7min,静置1~6分钟后进行浇注;
浇注完成后铸件随炉冷却到室温后,将铸件从真空自耗电极熔炼炉中取出。
2.根据权利要求1所述的钛合金筒形件石墨型铸造方法,其特征在于:对铸件打磨处理后得到质量合格的铸件。
3.根据权利要求1所述的钛合金筒形件石墨型铸造方法,其特征在于:所述浇注系统采用顶铸式的浇注方式,包括一个浇口杯,一个直浇道,两个横浇道和12个内浇道,铸件浇注时从顶部引入液流。
CN201210353649.2A 2012-09-21 2012-09-21 一种钛合金筒形件的石墨型铸造方法 Active CN103658548B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201210353649.2A CN103658548B (zh) 2012-09-21 2012-09-21 一种钛合金筒形件的石墨型铸造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201210353649.2A CN103658548B (zh) 2012-09-21 2012-09-21 一种钛合金筒形件的石墨型铸造方法

Publications (2)

Publication Number Publication Date
CN103658548A CN103658548A (zh) 2014-03-26
CN103658548B true CN103658548B (zh) 2016-02-10

Family

ID=50298010

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201210353649.2A Active CN103658548B (zh) 2012-09-21 2012-09-21 一种钛合金筒形件的石墨型铸造方法

Country Status (1)

Country Link
CN (1) CN103658548B (zh)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105880464B (zh) * 2016-06-01 2018-02-06 洛阳双瑞精铸钛业有限公司 一种大型薄壁钛合金铸件的石墨型铸造方法
CN107790626A (zh) * 2017-10-23 2018-03-13 魏至成 一种利用数字化加工的石墨块组合成铸造模具的铸造方法
CN109332592A (zh) * 2018-12-10 2019-02-15 上海航天精密机械研究所 一种大型复杂圆台型钛合金铸造方法
CN110000336B (zh) * 2019-04-17 2020-12-22 包头市神润高新材料股份有限公司 采用石墨模具的热装热送铸造方法
CN110465630A (zh) * 2019-08-30 2019-11-19 北京星航机电装备有限公司 一种大型薄壁弱刚性钛合金铸件的铸造方法
CN111036855A (zh) * 2019-11-18 2020-04-21 洛阳双瑞精铸钛业有限公司 一种钛合金前罩壳体的成型方法
CN114713775B (zh) * 2022-03-28 2024-01-19 洛阳双瑞精铸钛业有限公司 一种带开口的大型圆筒型钛铸件的制备方法

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2005152957A (ja) * 2003-11-26 2005-06-16 Kobe Steel Ltd 球状黒鉛鋳鉄鋳物およびその製造方法
CN101733641A (zh) * 2009-12-18 2010-06-16 西北有色金属研究院 一种大口径无缝钛合金筒体的制造方法

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6799627B2 (en) * 2002-06-10 2004-10-05 Santoku America, Inc. Castings of metallic alloys with improved surface quality, structural integrity and mechanical properties fabricated in titanium carbide coated graphite molds under vacuum

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2005152957A (ja) * 2003-11-26 2005-06-16 Kobe Steel Ltd 球状黒鉛鋳鉄鋳物およびその製造方法
CN101733641A (zh) * 2009-12-18 2010-06-16 西北有色金属研究院 一种大口径无缝钛合金筒体的制造方法

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
航空航天用钛合金的铸造工艺及发展;聂小武;《金属加工(热加工)》;20100715(第13期);第26-29、32页 *

Also Published As

Publication number Publication date
CN103658548A (zh) 2014-03-26

Similar Documents

Publication Publication Date Title
CN103658548B (zh) 一种钛合金筒形件的石墨型铸造方法
CN101733383B (zh) 石墨型-陶瓷芯钛合金精密铸造方法
CN102605190A (zh) 模具钢电渣重熔渣系及使用方法
CN105750515A (zh) 一种小容量母合金浇铸系统
CN104745917A (zh) 曲轴的铸造工艺
CN103862000A (zh) 一种端盖铸件芯壳垂直分型水平浇注铸造工艺
CN102990043A (zh) 一种壳体的铸造生产工艺
CN104741574A (zh) 铝合金转向节的低压铸造工艺
CN102873310A (zh) 一种端盖的铸造生产工艺
CN102485377B (zh) 非晶带用铬锆铜冷却辊的制造方法
CN101875090A (zh) 一种法兰的铸造生产工艺
CN109986056A (zh) 一种铸铝转子低压铸铝工艺方法
CN101530899B (zh) 采用离心铸造技术制作轴承环的方法
CN201442974U (zh) 用于冶炼轧辊的电渣炉结晶器
CN204052806U (zh) 一种金属模具
CN104550740A (zh) 大型薄壁回旋体高强度铝合金铸件铸造方法
CN104741562A (zh) 法兰铸件的离心铸造方法
CN111947456B (zh) 一种连续铸造真空感应熔炼炉
CN104607594A (zh) 合金弹簧座的铸造生产工艺
CN105665649A (zh) 高强度轴承连接器的铸造工艺
CN210755019U (zh) 双模壳室四室定向单晶真空感应精密铸造炉
CN103128268B (zh) 用于大型特厚板坯的中低温打箱的方法
CN107457366A (zh) 一种汽车用油泵盖生产工艺
CN104874744A (zh) 曲轴箱的铸造方法
CN111533568A (zh) 一种耐火陶瓷制品

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant