CN103578746A - 电容器用复合型安全防爆金属化薄膜 - Google Patents

电容器用复合型安全防爆金属化薄膜 Download PDF

Info

Publication number
CN103578746A
CN103578746A CN201310479740.3A CN201310479740A CN103578746A CN 103578746 A CN103578746 A CN 103578746A CN 201310479740 A CN201310479740 A CN 201310479740A CN 103578746 A CN103578746 A CN 103578746A
Authority
CN
China
Prior art keywords
film
capacitor
explosion
metallized
metallized film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310479740.3A
Other languages
English (en)
Inventor
荚朝辉
康仙文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TONGLING QILI ELECTRONIC MATERIALS CO Ltd
Original Assignee
TONGLING QILI ELECTRONIC MATERIALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGLING QILI ELECTRONIC MATERIALS CO Ltd filed Critical TONGLING QILI ELECTRONIC MATERIALS CO Ltd
Priority to CN201310479740.3A priority Critical patent/CN103578746A/zh
Publication of CN103578746A publication Critical patent/CN103578746A/zh
Pending legal-status Critical Current

Abstract

一种电容器用复合型安全防爆金属化薄膜,涉及电容器技术领域,包括基膜和蒸镀在基膜上金属镀层,所述金属镀层蒸镀在基膜的上下两面上,所述基膜的两边呈锯齿状,该锯齿状设计能够提高膜卷质量,减少成品膜的静电,所述金属镀层内附网状金属化容断丝。本发明结构简单,设计新颖,能够提高金属化薄膜的整体性能,同时在金属化层增加硅油涂层,等于为金属层增加了一个“油封”,减少金属化层和空气的接触,增加金属化膜的抗氧化能力。

Description

电容器用复合型安全防爆金属化薄膜
技术领域
本发明涉及电容器技术领域,具体涉及一种电容器用复合型安全防爆金属化薄膜。
背景技术
薄膜电容器是一种性能优越的电容器,其具有如下主要特性:无极性,绝缘阻抗很高,频率特性优异,介质损失很小,并且体积小容量大。因此,薄膜电容器有着较为广泛的用途,可以形成不同的系列产品,如高比能储能电容器、抗电磁干扰电容器、抗辐射电容器、安全膜电容器、长寿命电容器、高可靠电容器、高压全膜电容器等。随着电子整机向数字化、高频化、多功能化以及向薄、轻、小、便携等方向发展,电容器不可避免的要向体积小、性能优、价格更低的方向发展。研发小型电容器用金属化膜,可以有效减少电容器体积,改善电容器的产品性能。
发明内容
本发明所要解决的技术问题在于提供一种降低生产成本,减小产品体积的电容器用复合型安全防爆金属化薄膜。
本发明所要解决的技术问题采用以下技术方案来实现:
一种电容器用复合型安全防爆金属化薄膜,包括基膜和蒸镀在基膜上金属镀层,所述金属镀层蒸镀在基膜的上下两面上,所述基膜的两边呈锯齿状,该锯齿状设计能够提高膜卷质量,减少成品膜的静电,所述金属镀层内附网状金属化容断丝。
所述金属镀层为镀铝层。
所述镀铝层外部蒸镀有一层渐变方阻金属化膜。
所述渐变方阻金属化膜的表面上涂覆有硅油层。
本发明的有益效果是:本发明结构简单,设计新颖,能够提高金属化薄膜的整体性能,同时在金属化层增加硅油涂层,等于为金属层增加了一个“油封”,减少金属化层和空气的接触,增加金属化膜的抗氧化能力,内附网状金属化容断丝作为防爆结构,当金属化极板上局部范围内发生自愈击穿,该局部范围的金属化熔断丝熔断,与其周围的金属化极板断开,电容量变化极小,完成自愈后电容器照常工作,提高了电容器的可靠性,不至于因容量损失太大而逐渐失效,更不会因引起发热而导致外壳爆裂,大大提高了电容器的寿命。
附图说明
图1为本发明结构示意图。
具体实施方式
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体图示,进一步阐述本发明。
如图1所示,一种电容器用复合型安全防爆金属化薄膜,包括基膜10和蒸镀在基膜10上金属镀层20,金属镀层20蒸镀在基膜10的上下两面上,基膜10的两边呈锯齿状,该锯齿状设计能够提高膜卷质量,减少成品膜的静电,金属镀层20内附网状金属化容断丝,金属镀层20为镀铝层,镀铝层20外部蒸镀有一层渐变方阻金属化膜30,渐变方阻金属化膜30的表面上涂覆有硅油层。
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。

Claims (4)

1.一种电容器用复合型安全防爆金属化薄膜,其特征在于:包括基膜和蒸镀在基膜上金属镀层,所述金属镀层蒸镀在基膜的上下两面上,所述基膜的两边呈锯齿状,所述金属镀层内附网状金属化容断丝。
2.根据权利要求1所述的电容器用复合型安全防爆金属化薄膜,其特征在于:所述金属镀层为镀铝层。
3.根据权利要求2所述的电容器用复合型安全防爆金属化薄膜,其特征在于:所述镀铝层外部蒸镀有一层渐变方阻金属化膜。
4.根据权利要求3所述的电容器用复合型安全防爆金属化薄膜,其特征在于:所述渐变方阻金属化膜的表面上涂覆有硅油层。
CN201310479740.3A 2013-10-15 2013-10-15 电容器用复合型安全防爆金属化薄膜 Pending CN103578746A (zh)