CN103535928B - 一种吸汗手套的制备方法 - Google Patents

一种吸汗手套的制备方法 Download PDF

Info

Publication number
CN103535928B
CN103535928B CN201310556529.7A CN201310556529A CN103535928B CN 103535928 B CN103535928 B CN 103535928B CN 201310556529 A CN201310556529 A CN 201310556529A CN 103535928 B CN103535928 B CN 103535928B
Authority
CN
China
Prior art keywords
temperature
water
heating
glove
absorbing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310556529.7A
Other languages
English (en)
Other versions
CN103535928A (zh
Inventor
王学斌
高尚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhenjiang Huayang Latex Products Co., Ltd.
Original Assignee
ZHENJIANG SUHUI LATEX PRODUCT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHENJIANG SUHUI LATEX PRODUCT CO Ltd filed Critical ZHENJIANG SUHUI LATEX PRODUCT CO Ltd
Priority to CN201310556529.7A priority Critical patent/CN103535928B/zh
Publication of CN103535928A publication Critical patent/CN103535928A/zh
Application granted granted Critical
Publication of CN103535928B publication Critical patent/CN103535928B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种吸汗手套的制备方法,其制备方法如下:(1)在橡胶基胶中加入一定量的吸水性树脂溶液,充分搅拌均匀后加入手套模型中加热,加热温度为70℃-85℃,加热8-12min;(2)对经步骤(1)处理后的手套模型上喷淋余量的吸水性树脂溶液,再经过150℃、25-30分钟的高温干燥;自然冷却至常温,把手套从模具上脱下;(3)对脱下的手套进行高温烘干,烘干温度为80-160℃、烘干时间为10-25分钟,烘干后自然冷却至常温、脱模最终得到成品,本吸汗手套可快速吸收汗水,保持手部干爽。

Description

一种吸汗手套的制备方法
技术领域
本发明涉及一种吸汗手套的制造方法。
背景技术
目前,传统的橡胶手套在手部干燥时很容易穿戴,但当手部潮湿或有水迹时却不易穿戴;即便手部干燥时容易穿戴,但当手部出汗时,手套粘手,很不舒适。国外虽然有湿手易穿戴的手套,可它是通过加深氯化程度,在内层加水凝胶的方法来实现的,由于氯化过度,大大影响了手套的物理性能和储存期。
发明内容
本发明所要解决的技术问题是针对以上弊端提供一种吸汗手套的制备方法。
为解决上述技术问题,本发明的技术方案是:
一种吸汗手套的制备方法,其制备方法如下:
(1)在橡胶基胶中加入一定量的吸水性树脂溶液,充分搅拌均匀后加入手套模型中加热,加热温度为70℃—85℃,加热8—12min;
(2)对经步骤(1)处理后的手套模型上喷淋余量的吸水性树脂溶液,再经过150℃、25-30分钟的高温干燥;自然冷却至常温,把手套从模具上脱下;
(3)对脱下的手套进行高温烘干,烘干温度为80-160℃、烘干时间为10-25分钟,烘干后自然冷却至常温、脱模最终得到成品。
上述一种吸汗手套的制备方法,其中,所述的吸水性树脂溶液组分按重量份数计为:
聚丙烯酸及其共聚物  100份
聚氨酯胶粘剂        25—500份
水                  10—50份。
本发明的有益效果为:可以吸收水份,手套内层的吸水性树脂溶液层不会剥离或脱落,可快速吸收汗水,保持手部干爽,当手部干燥时,本发明和普通手套一样易穿戴;当手部潮湿或有水迹时,水份被迅速吸收,所以仍然很容易穿戴,保持了手套的舒适度,使用更加方便、安全。
具体实施方式
以下通过具体实施例对本发明的具体实施方式作进一步详细的说明。
本发明所述聚氨酯胶粘剂购于上海寿兴实业有限公司;所述聚丙烯酸及其共聚物购于苏州市天诚商贸有限公司。
实例一:
一种吸汗手套的制备方法,其制备方法如下:
(1)配置吸水性树脂溶液,将10kg聚丙烯酸及其共聚物,5kg聚氨酯胶粘剂和3kg水混合均匀进行加热,加热温度为120℃,加热10min;
(2)在150kg橡胶基胶中加入3kg吸水性树脂溶液,充分搅拌均匀后加入手套模型中加热,加热温度为70℃,加热8min;
(3)对经步骤(2)处理后的手套模型上喷淋15kg的吸水性树脂溶液,再经过150℃、25分钟的高温干燥;自然冷却至常温,把手套从模具上脱下;
(4)对脱下的手套进行高温烘干,烘干温度为120℃、烘干时间为25分钟,烘干后自然冷却至常温、脱模最终得到成品。
实例二:
一种吸汗手套的制备方法,其制备方法如下:
(1)配置吸水性树脂溶液,将50kg聚丙烯酸及其共聚物,25kg聚氨酯胶粘剂和15kg水混合均匀进行加热,加热温度为120℃,加热10min;
(2)在750kg橡胶基胶中加入15kg吸水性树脂溶液,充分搅拌均匀后加入手套模型中加热,加热温度为70℃—85℃,加热8—12min;
(3)对经步骤(2)处理后的手套模型上喷淋75kg的吸水性树脂溶液,再经过150℃、25-30分钟的高温干燥;自然冷却至常温,把手套从模具上脱下;
(4)对脱下的手套进行高温烘干,烘干温度为80-160℃、烘干时间为10-25分钟,烘干后自然冷却至常温、脱模最终得到成品。
综上所述,普通手套5分钟内的吸水率为3.4%,而本吸汗手套的吸水率能达到9.8%,效果明显,且该手套在干燥状态的摩擦系数与普通手套差别不大,但在潮湿状态下的摩擦系数却大大低于普通丁腈手套,所以它不论在干燥还是潮湿状态下,都容易穿戴。
这里本发明的描述和应用是说明性的,并非想将本发明的范围限制在上述实施例中,因此,本发明不受本实施例的限制,任何采用等效替换取得的技术方案均在本发明保护的范围内。

Claims (2)

1.一种吸汗手套的制备方法,其特征为,其制备方法如下:
(1)配置吸水性树脂溶液,将10kg聚丙烯酸及其共聚物,5kg聚氨酯胶粘剂和3kg水混合均匀进行加热,加热温度为120℃,加热10min;
(2)在150kg橡胶基胶中加入3kg吸水性树脂溶液,充分搅拌均匀后加入手套模型中加热,加热温度为70℃,加热8min;
(3)对经步骤(2)处理后的手套模型上喷淋15kg的吸水性树脂溶液,再经过150℃、25分钟的高温干燥;自然冷却至常温,把手套从模具上脱下;
(4)对脱下的手套进行高温烘干,烘干温度为120℃、烘干时间为25分钟,烘干后自然冷却至常温、脱模最终得到成品。
2.一种吸汗手套的制备方法,其制备方法如下:
(1)配置吸水性树脂溶液,将50kg聚丙烯酸及其共聚物,25kg聚氨酯胶粘剂和15kg水混合均匀进行加热,加热温度为120℃,加热10min;
(2)在750kg橡胶基胶中加入15kg吸水性树脂溶液,充分搅拌均匀后加入手套模型中加热,加热温度为70℃—85℃,加热8—12min;
(3)对经步骤(2)处理后的手套模型上喷淋75kg的吸水性树脂溶液,再经过150℃、25-30分钟的高温干燥;自然冷却至常温,把手套从模具上脱下;
(4)对脱下的手套进行高温烘干,烘干温度为80-160℃、烘干时间为10-25分钟,烘干后自然冷却至常温、脱模最终得到成品。
CN201310556529.7A 2013-11-11 2013-11-11 一种吸汗手套的制备方法 Active CN103535928B (zh)