CN103521614A - 钢管打头机打头模具内腔工作面型线 - Google Patents

钢管打头机打头模具内腔工作面型线 Download PDF

Info

Publication number
CN103521614A
CN103521614A CN201310486927.6A CN201310486927A CN103521614A CN 103521614 A CN103521614 A CN 103521614A CN 201310486927 A CN201310486927 A CN 201310486927A CN 103521614 A CN103521614 A CN 103521614A
Authority
CN
China
Prior art keywords
operation section
deformation
molded line
deformation operation
working face
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310486927.6A
Other languages
English (en)
Other versions
CN103521614B (zh
Inventor
王刚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Changzhou Changbao Precision & Special Steel Tube Co Ltd
Original Assignee
Changzhou Changbao Precision & Special Steel Tube Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Changzhou Changbao Precision & Special Steel Tube Co Ltd filed Critical Changzhou Changbao Precision & Special Steel Tube Co Ltd
Priority to CN201310486927.6A priority Critical patent/CN103521614B/zh
Publication of CN103521614A publication Critical patent/CN103521614A/zh
Application granted granted Critical
Publication of CN103521614B publication Critical patent/CN103521614B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种钢管打头机打头模具内腔工作型线,其工作面型线由导向工作段(1)、变形工作段(2)和定径工作段(3)依次过渡连接构成,以其所述变形工作段(2)沿钢管前进方向,呈等间距、等缩径率而逐步缩小其内径的等变形比例的结构形式为主要特征,具有变形工作段的变形比例自始至终均等,模具不易磨损变形,而使用寿命长等特点。

Description

钢管打头机打头模具内腔工作面型线
技术领域
本发明涉及一种钢管打头机打头模具内腔工作面型线,属于钢管生产装备技术。
背景技术
钢管打头机的打头模具,一般为四开合模具,其每一爿模具占整个模具的1/4,通过装置令其4爿模具组合成一体,且可开可合十分灵活。
而所述打头模具的内腔工作面,由导向工作段,变形工作段和定径工作段沿钢管前进方向依次过渡连接构成。
已有的所述变形工作段的内腔工作面为锥形,其工作面型线为斜直线,而在钢管打头过程中,钢管由导向工作段进入变形工作段后,由于钢管变形的绝对量不变,在钢管由变形工作段进入定径工作段的全程中,由钢管变形所造成的模具受力越来越大,而在变形工作段与定径工作段连接处的受力最大,由此对模具造成异常磨损和变形,降低了模具的使用寿命,而迫切需要对打头模具内腔工作面型线进行改进。
发明内容
本发明的目的在于提供一种钢管变形比例全程相等的钢管打头机打头模具内腔工作面线,以克服已有技术的不足。
本发明实现其目的的技术方案是:
一种钢管打头机打头模具内腔工作面型线,其工作面型线由导向工作段、变形工作段和定径工作段依次过渡连接构成,其创新点在于,所述变形工作段沿钢管前进方向,呈等间距、等缩径率而逐步缩小其内径的等变形比例的结构形式。
在上述技术方案中,本发明优选的所述等间距、等缩径率而逐步缩小其内径的等变形比例结构各分段的内径,要满足以下计算式:
Dn=D1×△n-1
式中:n为所述变形工作段轴线上等间距分开所设的若干个变形分段的段点序号;
Dn为位于变形分段段点部位的变形工作段的内径;
D1为所述变形工作段入口处的内径;
△为缩径百分率(%)
参与变形工作段的轴向长度=100~150mm,
△=98~96%;
且采用若干个变形分段描点,圆弧过渡连接构成所述变形工作段沿钢管前进方向的各分段等变形比例的结构形式。
由以上所给出的技术方案可以明了,本发明在其变形工作段,由于钢管所接受的是相等运动距离的相等变形比例的缩径变形,从而解决了由于变形比例不均对模具所造成的受力不均等且越来越大的问题,提高了模具的使用寿命,实现了本发明的目的。
附图说明
图1是本发明所述打头模具的主视示意图;
图2是图1的左视图;
图3是本发明一种具体实施方式采用计算式Dn=D1×△n-1所得出的变形工作段2的型线示意图。
具体实施方式
以下结合附图,通过具体实施方式的描述,对本发明作进一步说明。
典型的具体实施例,如附图1~3所示.
一种钢管打头机打头模具内腔工作型线,其工作面型线由导向工作段1、变形工作段2和定径工作段3依次过渡连接构成,所述变形工作段2沿钢管前进方向,呈等间距、等缩径率而逐步缩小其内径的等变形比例的结构形式。
而所述等间距、等缩径率而逐步缩小其内径的等变形比例结构各分段的内径,满足以下计算式:
Dn=D1×△n-1
式中:n为所述变形工作段2轴线上等间距分开所设的若干个变形分段的段点序号;
Dn为位于变形分段段点部位的变形工作段2的内径;
D1为所述变形工作段2入口处的内径;
△为缩径百分率%
变形工作段2轴向长度=100~150mm,
△=98~96%;
且采用若干个变形分段描点,圆弧过渡连接构成所述变形工作段2沿钢管前进方向的各分段等变形比例的结构形式。
而变形工作段2采用Dn=D1×△n-1计算式所得出变形工作段2的型线的计算绘制过程是:
以φ90mm外径成品钢管打头为例;
设毛坯钢管外径为φ100mm,则
取n=21,设定的参与变形工作段2的轴向长度为100mm,则每一分段长度为5mm,D1=φ100mm
△=98%
计算:D1=φ100mm
D2=D1×98%=φ100×98%=φ98mm
D3=D2×98%=φ100×(98%)2=φ96.04mm
D4=D3×98%=φ100×(98%)3=φ94.12mm
D5=D4×98%=φ100×(98%)4=φ92.04mm
D6=D5×98%=φ100×(98%)5=φ90.39mm
以下依次类推、分段逐个计算得:
D7=88.58;D8=86.81;D9=85.08;
D10=83.37;D11=81.71;D12=80.07;
D13=78.47;D14=76.90;D15=75.36;
D16=73.86;D17=72.38;D18=70.93;
D19=69.51;D20=68.12;D21=66.76(即定径工作段直径)。
然后如附图3分段描点,圆弧过渡构成打头模具变形工作段2的工作型线。
本发明初样在机试用状况很好。由于解决了变形比例不均等的问题,所述打头模具的使用寿命,比已有技术提高近一倍。取得了明显的技术经济效果。

Claims (2)

1.一种钢管打头机打头模具内腔工作面型线,其工作面型线由导向工作段(1)、变形工作段(2)和定径工作段(3)依次过渡连接构成,其特征在于,所述变形工作段(2)沿钢管前进方向,呈等间距、等缩径率而逐步缩小其内径的等变形比例的结构形式。
2.根据权利要求1所述的工作面型线,其特征在于,所述等间距、等缩径率而逐步缩小其内径的等变形比例结构各分段的内径,要满足以下计算式:
Dn=D1×△n-1
式中:
n为所述变形工作段(2)轴线上等间距分开所设的若干个变形分段的段点序号;
Dn为位于变形分段段点部位的变形工作段(2)的内径;
D1为所述变形工作段(2)入口处的内径;
△为缩径百分率(%)
参与变形工作段的轴向长度=100~150mm,
△=98~96%;
且采用若干个变形分段描点,圆弧过渡连接构成所述变形工作段(2)沿钢管前进方向的各分段等变形比例的结构形式。
CN201310486927.6A 2013-10-17 2013-10-17 钢管打头机打头模具内腔工作面型线 Active CN103521614B (zh)