CN103483939A - 一种聚氯乙烯粉末涂料 - Google Patents

一种聚氯乙烯粉末涂料 Download PDF

Info

Publication number
CN103483939A
CN103483939A CN201310393239.5A CN201310393239A CN103483939A CN 103483939 A CN103483939 A CN 103483939A CN 201310393239 A CN201310393239 A CN 201310393239A CN 103483939 A CN103483939 A CN 103483939A
Authority
CN
China
Prior art keywords
parts
powder paint
polyvinyl
polyvinyl chloride
chloride powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310393239.5A
Other languages
English (en)
Other versions
CN103483939B (zh
Inventor
张洪滨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Ruichi new materials Co., Ltd
Original Assignee
BENGBU HONGAN PRECISION MACHINERY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BENGBU HONGAN PRECISION MACHINERY Co Ltd filed Critical BENGBU HONGAN PRECISION MACHINERY Co Ltd
Priority to CN201310393239.5A priority Critical patent/CN103483939B/zh
Publication of CN103483939A publication Critical patent/CN103483939A/zh
Application granted granted Critical
Publication of CN103483939B publication Critical patent/CN103483939B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种聚氯乙烯粉末涂料,它是由下述重量份的原料组成的:聚氯乙烯树脂90-100、三氧化二铝6-10、竹炭粉13-18、硬脂酸钙4-6、氧化铁黑3-4、2-羟基-4-正辛氧基二苯甲酮0.2-0.4、苯二甲酸二丁酯10-13、脂肪醇聚氧乙烯醚1-2、甲基硫醇锡1-2、复合填料10-20;本发明粉末涂料具备原料易得,陈本低,成品流动性好,稳定性好等特点,可应用于对耐腐蚀、耐气候要求较高的产品上。

Description

一种聚氯乙烯粉末涂料
技术领域
    本发明主要涉及一种涂料,尤其涉及一种聚氯乙烯粉末涂料。
背景技术
粉末涂料的其特性有:1、该产品不含毒性,不含溶剂和不含挥发有毒性的物质,故无中毒、无火灾、无“三废”的排放等公害的问题,完全符合国家环保法的要求。2、原材料利用率高,一些知名品牌的粉末供应商生产的粉末,其过喷的粉末可回收利用,最高的利用率甚至能达99%以上。3、被涂物前处理后, 一次性施工,无需底涂,即可得到足够厚度的涂膜,易实现自动化操作,生产效率高, 可降低成本。4、涂层致密、附着力、抗冲击强度和韧性均好,边角覆盖率高,具有优良的耐化学药品腐蚀性能和电气绝缘性能。5、粉末涂料存贮、运输安全和方便。
发明内容
本发明目的就是为了提供一种聚氯乙烯粉末涂料。
本发明是通过以下技术方案实现的:
一种聚氯乙烯粉末涂料,其特征在于它是由下述重量份的原料组成的:
聚氯乙烯树脂90-100、三氧化二铝6-10、竹炭粉13-18、硬脂酸钙4-6、氧化铁黑3-4、2-羟基-4-正辛氧基二苯甲酮0.2-0.4、苯二甲酸二丁酯10-13、脂肪醇聚氧乙烯醚1-2、甲基硫醇锡1-2、复合填料10-20;
所述的复合填料是由下述重量份的原料组成的:
三水铝石30-40、凹凸棒土20-30、碳化硅6-10、氢氧化镁3-5、羧甲基纤维素1-2、霍霍巴油2-3;
将上述三水铝石、凹凸棒土、碳化硅混合,在600-800℃下保温煅烧2-4小时,出料冷却后送入球磨机中进行球磨混合,再加入氢氧化镁和羧甲基纤维素,继续球磨1-2小时,将霍霍巴油加热到25-30℃后加入,球磨,过80-100目筛,即得所述复合填料。
一种聚氯乙烯粉末涂料的制备方法,包括以下步骤:
将上述聚氯乙烯树脂与甲基硫醇锡混合加热到80-90℃,保温搅拌3-5分钟,加入苯二甲酸二丁酯,充分搅拌后降低温度为45-50℃,加入剩余各原料,充分混合,过筛,即得所述聚氯乙烯粉末涂料。
本发明的优点是:
    本发明粉末涂料具备原料易得,陈本低,成品流动性好,稳定性好等特点,可应用于对耐腐蚀、耐气候要求较高的产品上。
具体实施方式
实施例1,
一种聚氯乙烯粉末涂料,它是由下述重量份(公斤)的原料组成的:
聚氯乙烯树脂100、三氧化二铝10、竹炭粉18、硬脂酸钙4、氧化铁黑3、2-羟基-4-正辛氧基二苯甲酮0.4、苯二甲酸二丁酯13、脂肪醇聚氧乙烯醚2、甲基硫醇锡2、复合填料20;
所述的复合填料是由下述重量份的原料组成的:
三水铝石40、凹凸棒土20、碳化硅10、氢氧化镁3、羧甲基纤维素1-2、霍霍巴油2-3;
将上述三水铝石、凹凸棒土、碳化硅混合,在800℃下保温煅烧2小时,出料冷却后送入球磨机中进行球磨混合,再加入氢氧化镁和羧甲基纤维素,继续球磨1小时,将霍霍巴油加热到30℃后加入,球磨,过100目筛,即得所述复合填料。
一种聚氯乙烯粉末涂料的制备方法,包括以下步骤:
将上述聚氯乙烯树脂与甲基硫醇锡混合加热到90℃,保温搅拌5分钟,加入苯二甲酸二丁酯,充分搅拌后降低温度为50℃,加入剩余各原料,充分混合,过筛,即得所述聚氯乙烯粉末涂料。
性能测试:
耐溶剂:240小时,无变化;
盐雾试验(1000h):无变化。

Claims (2)

1.一种聚氯乙烯粉末涂料,其特征在于它是由下述重量份的原料组成的:
聚氯乙烯树脂90-100、三氧化二铝6-10、竹炭粉13-18、硬脂酸钙4-6、氧化铁黑3-4、2-羟基-4-正辛氧基二苯甲酮0.2-0.4、苯二甲酸二丁酯10-13、脂肪醇聚氧乙烯醚1-2、甲基硫醇锡1-2、复合填料10-20;
所述的复合填料是由下述重量份的原料组成的:
三水铝石30-40、凹凸棒土20-30、碳化硅6-10、氢氧化镁3-5、羧甲基纤维素1-2、霍霍巴油2-3;
将上述三水铝石、凹凸棒土、碳化硅混合,在600-800℃下保温煅烧2-4小时,出料冷却后送入球磨机中进行球磨混合,再加入氢氧化镁和羧甲基纤维素,继续球磨1-2小时,将霍霍巴油加热到25-30℃后加入,球磨,过80-100目筛,即得所述复合填料。
2.一种如权利要求1所述的聚氯乙烯粉末涂料的制备方法,其特征在于包括以下步骤:
将上述聚氯乙烯树脂与甲基硫醇锡混合加热到80-90℃,保温搅拌3-5分钟,加入苯二甲酸二丁酯,充分搅拌后降低温度为45-50℃,加入剩余各原料,充分混合,过筛,即得所述聚氯乙烯粉末涂料。
CN201310393239.5A 2013-09-03 2013-09-03 一种聚氯乙烯粉末涂料 Active CN103483939B (zh)