CN103468385A - 一种全合成铝合金拉丝液 - Google Patents

一种全合成铝合金拉丝液 Download PDF

Info

Publication number
CN103468385A
CN103468385A CN2013103723879A CN201310372387A CN103468385A CN 103468385 A CN103468385 A CN 103468385A CN 2013103723879 A CN2013103723879 A CN 2013103723879A CN 201310372387 A CN201310372387 A CN 201310372387A CN 103468385 A CN103468385 A CN 103468385A
Authority
CN
China
Prior art keywords
parts
water
add
aluminum alloy
nitride powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013103723879A
Other languages
English (en)
Inventor
何康
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TIANCHANG KANGHE METAL MATERIAL Co Ltd
Original Assignee
TIANCHANG KANGHE METAL MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TIANCHANG KANGHE METAL MATERIAL Co Ltd filed Critical TIANCHANG KANGHE METAL MATERIAL Co Ltd
Priority to CN2013103723879A priority Critical patent/CN103468385A/zh
Publication of CN103468385A publication Critical patent/CN103468385A/zh
Pending legal-status Critical Current

Abstract

一种全合成铝合金拉丝液,由下列重量份的原料制成:三乙醇胺1-2、正辛酸2-3、硼酸1-2、乙二醇3-4、苯骈三氮唑1-2、钼酸钠1-2、2,6-苯并异噻唑啉酮0.6-0.8、聚乙烯醇3-4、扩散剂NNO1-2、叔丁基过氧化氢1-2、改性氮化铝粉末2-3、水1200。

Description

一种全合成铝合金拉丝液
技术领域
本发明涉及铜、铝导线拉丝技术领域,是一种全合成铝合金拉丝液及其制备方法。
背景技术
现有拉丝工艺中多采用润滑油作为拉丝介质,拉拔出的导线表面圆润、细腻、光滑、透亮、无杂物滞留,断丝率降低,产品质量大大提高。但是润滑油散热慢,损毁模具,影响产品质量,同时高温易引燃油品或使油品蒸发冒烟导致现场环境恶化。
发明内容
本发明的目的是提供一种全合成铝合金拉丝液。
本发明的技术方案如下:
    一种全合成铝合金拉丝液,其特征在于由下列重量份的原料制成:三乙醇胺1-2、正辛酸2-3、硼酸1-2、乙二醇3-4、苯骈三氮唑1-2、钼酸钠1-2、2,6-苯并异噻唑啉酮0.6-0.8、聚乙烯醇3-4、扩散剂NNO1-2、叔丁基过氧化氢1-2、改性氮化铝粉末2-3、水1200;
改性氮化铝粉末由下列重量份的原料制成:
三聚磷酸钠2.0-2.2、壳聚糖1.6-1.8、硅烷偶联剂KH570 0.1-0.2,过硫酸铵1.0-1.2、1-羟乙基-2-油基咪唑啉2.0-2.3、纳米氮化铝3.4-3.8、纳米碳1.2-1.4、十二烷基苯磺酸钠0.5-0.8、羟甲基脲2.0-2.3、聚乙烯吡咯烷酮2.4-2.8、水50;
所述的改性氮化铝粉末的制备方法如下:将壳聚糖溶解于水中,加热至80-85℃,再加入三聚磷酸钠,搅拌反应15-20分钟,然后,再加入纳米氮化铝,45-50℃搅拌10-20分钟,然后,加入其它剩余原料,搅拌均匀后,烘干,磨粉即得。
     所述的全合成铝合金拉丝液,其特征在于,
制备方法如下:先将三乙醇胺、乙二醇加入水中,加热至40-45℃,500-800转/分搅拌反应50-60分钟,然后,再添加其它剩余原料,升温至80-90℃,900-1000转/分继续搅拌反应1-2小时,即得。
本发明的有益效果为:  
    本发明具有优异的润滑性能、清洗性和铝防护性能,能够满足加工精度要求。具体实施方式
  一种全合成铝合金拉丝液,由下列重量份(kg)的原料制成:三乙醇胺1.8、正辛酸3、硼酸2、乙二醇4、苯骈三氮唑2、钼酸钠1、2,6-苯并异噻唑啉酮0.8、聚乙烯醇4、扩散剂NNO  2、叔丁基过氧化氢1、改性氮化铝粉末3、水1200;
改性氮化铝粉末由下列重量份的原料制成:
三聚磷酸钠2.2、壳聚糖1.6、硅烷偶联剂KH570  0.2,过硫酸铵 1.2、1-羟乙基-2-油基咪唑啉 2.3、纳米氮化铝3.8、纳米碳1.4、十二烷基苯磺酸钠0.8、羟甲基脲2.3、聚乙烯吡咯烷酮2.8、水50;
所述的改性氮化铝粉末的制备方法如下:将壳聚糖溶解于水中,加热至80℃,再加入三聚磷酸钠,搅拌反应20分钟,然后,再加入纳米氮化铝,50℃搅拌20分钟,然后,加入其它剩余原料,搅拌均匀后,烘干,磨粉即得。
     所述的全合成铝合金拉丝液,
制备方法如下:先将三乙醇胺、乙二醇加入水中,加热至45℃,800转/分搅拌反应50分钟,然后,再添加其它剩余原料,升温至80℃,1000转/分继续搅拌反应2小时,即得。
使用本实施例拉丝液,最高拉丝速度可达22m/sec。生产出的铜丝工序间防锈时间在8天以上;集中油池换油周期为3 年,单机油池换油周期为11个月,减少了废液处理和排放,保护了环境。

Claims (2)

1.一种全合成铝合金拉丝液,其特征在于由下列重量份的原料制成:三乙醇胺1-2、正辛酸2-3、硼酸1-2、乙二醇3-4、苯骈三氮唑1-2、钼酸钠1-2、2,6-苯并异噻唑啉酮0.6-0.8、聚乙烯醇3-4、扩散剂NNO1-2、叔丁基过氧化氢1-2、改性氮化铝粉末2-3、水1200;
改性氮化铝粉末由下列重量份的原料制成:
三聚磷酸钠2.0-2.2、壳聚糖1.6-1.8、硅烷偶联剂KH570 0.1-0.2,过硫酸铵1.0-1.2、1-羟乙基-2-油基咪唑啉2.0-2.3、纳米氮化铝3.4-3.8、纳米碳1.2-1.4、十二烷基苯磺酸钠0.5-0.8、羟甲基脲2.0-2.3、聚乙烯吡咯烷酮2.4-2.8、水50;
所述的改性氮化铝粉末的制备方法如下:将壳聚糖溶解于水中,加热至80-85℃,再加入三聚磷酸钠,搅拌反应15-20分钟,然后,再加入纳米氮化铝,45-50℃搅拌10-20分钟,然后,加入其它剩余原料,搅拌均匀后,烘干,磨粉即得。
2.根据权利要求1所述的全合成铝合金拉丝液,其特征在于,
制备方法如下:先将三乙醇胺、乙二醇加入水中,加热至40-45℃,500-800转/分搅拌反应50-60分钟,然后,再添加其它剩余原料,升温至80-90℃,900-1000转/分继续搅拌反应1-2小时,即得。
CN2013103723879A 2013-08-24 2013-08-24 一种全合成铝合金拉丝液 Pending CN103468385A (zh)