CN103352903A CN201310290770XA CN201310290770A CN103352903A CN 103352903 A CN103352903 A CN 103352903A CN 201310290770X A CN201310290770X A CN 201310290770XA CN 201310290770 A CN201310290770 A CN 201310290770A CN 103352903 A CN103352903 A CN 103352903A
Authority
CN
China
Prior art keywords
bitch
cooled wall
incinerator
aluminium
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310290770XA
Other languages
English (en)
Inventor
袁根芳
许宬铭
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YIXING ZHONGHUAN REFRACTORY MATERIAL CO Ltd
Original Assignee
YIXING ZHONGHUAN REFRACTORY MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YIXING ZHONGHUAN REFRACTORY MATERIAL CO Ltd filed Critical YIXING ZHONGHUAN REFRACTORY MATERIAL CO Ltd
Priority to CN201310290770XA priority Critical patent/CN103352903A/zh
Publication of CN103352903A publication Critical patent/CN103352903A/zh
Pending legal-status Critical Current

Links

Images

Landscapes

  • Furnace Housings, Linings, Walls, And Ceilings (AREA)

Abstract

一种焚烧炉水冷壁用铝焊抓钉,包括焚烧炉水冷壁、附着于水冷壁上的耐磨塑料保护层、以及将两者固定的铝焊抓钉,所述铝焊抓钉一端为圆柱棒体,另一端为“Y”形叉体,圆柱棒体端部中心开设有不通孔,不通孔内设置有铝丝,所述铝焊抓钉的圆柱棒体端部穿过耐磨塑料保护层与水冷壁面焊接固定。有效提高了焊接效率,使不锈钢与普通钢材可有效焊接,提高焊接强度。

Description

一种焚烧炉水冷壁用铝焊抓钉
技术领域
本发明涉及一种焚烧炉用焊接连接件,尤其涉及一种焚烧炉水冷壁与耐磨塑料保护层固定用铝焊抓钉。 
背景技术
焚烧炉水冷壁内衬用耐磨可塑料做保护层,从而保护水冷壁在高温下正常运行,耐磨可塑料的施工厚度为50mm,不可采用立模振动方式进行,只能采用人工捣打方式,但采用人工捣打施工,强度底、容易剥落,现水冷壁材质为普通钢材,耐热不锈钢抓钉为≥1200℃,两者很难进行焊接固定,有待解决。 
发明内容
本发明针对现有技术的不足,提供了一种有效解决焊接问题,焊接牢固,使用寿命长的焚烧炉水冷壁用铝焊抓钉。 
本发明的技术关键在于不改变原有技术的材料和结构,对铝焊抓钉的结构进行改进,加入引火铝丝,有效提高焊接质量。其具体技术方案为:一种焚烧炉水冷壁用铝焊抓钉,包括焚烧炉水冷壁、附着于水冷壁上的耐磨塑料保护层、以及将两者固定的铝焊抓钉,其特征在于所述铝焊抓钉一端为圆柱棒体,另一端为“Y”形叉体,圆柱棒体端部中心开设有不通孔,不通孔内设置有铝丝,所述铝焊抓钉的圆柱棒体端部穿过耐磨塑料保护层与水冷壁面焊接固定。 
作为优选,所述铝焊抓钉为不锈钢。 
本发明的有益效果:本发明有效提高了焊接效率,使不锈钢与普通钢材可有效焊接,提高焊接强度。 
附图说明
图1为本发明的结构示意图。 
图2为图1中铝焊抓钉的结构示意图。 
具体实施方式
一种焚烧炉水冷壁用铝焊抓钉,包括焚烧炉水冷壁001、附着于水冷壁001上的耐磨塑料保护层002、以及将两者固定的铝焊抓钉003,所述铝焊抓钉003一端为圆柱棒体031,另一端为“Y”形叉体032,圆柱棒体031端部中心开设有不通孔311,不通孔311内设置有铝丝004,所述铝焊抓钉003的圆柱棒体031端部穿过耐磨塑料保护层002与水冷壁001面焊接固定。所述铝焊抓钉003为不锈钢。 
对于本领域技术人员来说,在本专利构思及具体实施例启示下,能够从本专利公开内容及常识直接导出或联想到的一些变形,本领域普通技术人员将意识到也可采用其他方法,或现有技术中常用公知技术的替代,以及特征间的相互不同组合,等等的非实质性改动,同样可以被应用,都能实现本专利描述功能和效果,不再一一举例展开细说,均属于本专利保护范围。 

Claims (2)

1.一种焚烧炉水冷壁用铝焊抓钉,包括焚烧炉水冷壁、附着于水冷壁上的耐磨塑料保护层、以及将两者固定的铝焊抓钉,其特征在于所述铝焊抓钉一端为圆柱棒体,另一端为“Y”形叉体,圆柱棒体端部中心开设有不通孔,不通孔内设置有铝丝,所述铝焊抓钉的圆柱棒体端部穿过耐磨塑料保护层与水冷壁面焊接固定。
2.根据权利要求1所述的一种焚烧炉水冷壁用铝焊抓钉,其特征在于所述铝焊抓钉为不锈钢。
CN201310290770XA 2013-07-11 2013-07-11 一种焚烧炉水冷壁用铝焊抓钉 Pending CN103352903A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310290770XA CN103352903A (zh) 2013-07-11 2013-07-11 一种焚烧炉水冷壁用铝焊抓钉

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310290770XA CN103352903A (zh) 2013-07-11 2013-07-11 一种焚烧炉水冷壁用铝焊抓钉

Publications (1)

Publication Number Publication Date
CN103352903A true CN103352903A (zh) 2013-10-16

Family

ID=49309305

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310290770XA Pending CN103352903A (zh) 2013-07-11 2013-07-11 一种焚烧炉水冷壁用铝焊抓钉

Country Status (1)

Country Link
CN (1) CN103352903A (zh)

Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2004053166A (ja) * 2002-07-22 2004-02-19 Takuma Co Ltd 空冷型耐火壁
CN201373702Y (zh) * 2008-12-31 2009-12-30 施国梁 高熔点金属搪涂低熔点金属表层的焊接制品
CN201507921U (zh) * 2009-08-28 2010-06-16 无锡海源重工股份有限公司 循环流化床锅炉炉膛密相区与稀相过渡区域防磨结构
CN201547802U (zh) * 2009-11-30 2010-08-11 上海锅炉厂有限公司 一种给煤管与炉膛接口处的耐磨结构
CN202675310U (zh) * 2012-07-03 2013-01-16 杭州海陆重工有限公司 纯燃垃圾炉全绝热炉膛
CN203394951U (zh) * 2013-07-11 2014-01-15 宜兴市中环耐火材料有限公司 一种焚烧炉水冷壁用铝焊抓钉

Patent Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2004053166A (ja) * 2002-07-22 2004-02-19 Takuma Co Ltd 空冷型耐火壁
CN201373702Y (zh) * 2008-12-31 2009-12-30 施国梁 高熔点金属搪涂低熔点金属表层的焊接制品
CN201507921U (zh) * 2009-08-28 2010-06-16 无锡海源重工股份有限公司 循环流化床锅炉炉膛密相区与稀相过渡区域防磨结构
CN201547802U (zh) * 2009-11-30 2010-08-11 上海锅炉厂有限公司 一种给煤管与炉膛接口处的耐磨结构
CN202675310U (zh) * 2012-07-03 2013-01-16 杭州海陆重工有限公司 纯燃垃圾炉全绝热炉膛
CN203394951U (zh) * 2013-07-11 2014-01-15 宜兴市中环耐火材料有限公司 一种焚烧炉水冷壁用铝焊抓钉

Similar Documents

Publication Publication Date Title
CN203231632U (zh) 水泥回转窑前窑口结构
CN103949630A (zh) 一种用于混铁车罐口封闭的保温盖
CN102248345A (zh) 封头堆焊工装及制备方法
CN203394951U (zh) 一种焚烧炉水冷壁用铝焊抓钉
CN103352903A (zh) 一种焚烧炉水冷壁用铝焊抓钉
CN210368944U (zh) 一种灌注桩主筋与加强筋连接结构及灌注桩钢筋笼
CN204565103U (zh) 一种安全分体式透气套砖
CN204923875U (zh) 一种可拆卸式金属锚固件结构
CN201416605Y (zh) 钢箍制动鼓
CN205021072U (zh) 不锈钢薄板焊接夹具
CN103993136A (zh) 高强度炉底辊
CN106855357A (zh) 一种退火炉炉衬用陶瓷纤维模块异位固定方法
CN102941392A (zh) 一种适用于低合金高强板与低合金铸钢件的焊接方法
CN204756189U (zh) 高断裂伸长率给水用聚乙烯管材
CN202667631U (zh) 一种透气砖复合安全标识
CN204051891U (zh) 一种新型滚筒端盖防护板
CN201184022Y (zh) 出屋面高温钢烟囱与砼屋面连接的构造
CN204100781U (zh) 回转窑窑口护铁
CN204043402U (zh) 一种沸腾炉墙体加固拉钩
CN204311074U (zh) 一种简单耐用的高炉铁水沟流咀
CN203824312U (zh) 一种高温取向硅钢电磁感应加热炉炉口密封装置
CN103212915B (zh) 船舶铸件焊补方法
CN215593115U (zh) 钢包用直通狭缝式透气砖
CN204359118U (zh) 塔式熔铝炉熔化室炉床结构
CN204035552U (zh) 一种预制扒渣耙前板

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20131016