CN103289273B - 一种氧化聚合型防蚀填料 - Google Patents

一种氧化聚合型防蚀填料 Download PDF

Info

Publication number
CN103289273B
CN103289273B CN201210517557.3A CN201210517557A CN103289273B CN 103289273 B CN103289273 B CN 103289273B CN 201210517557 A CN201210517557 A CN 201210517557A CN 103289273 B CN103289273 B CN 103289273B
Authority
CN
China
Prior art keywords
filling material
corrosion
corrosion protection
polymerization type
oxidative polymerization
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210517557.3A
Other languages
English (en)
Other versions
CN103289273A (zh
Inventor
侯保荣
小菅雅彦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nitto Denko China Investment Co Ltd
Original Assignee
QINGDAO HAILANRIDONG MATERIAL TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINGDAO HAILANRIDONG MATERIAL TECHNOLOGY Co Ltd filed Critical QINGDAO HAILANRIDONG MATERIAL TECHNOLOGY Co Ltd
Priority to CN201210517557.3A priority Critical patent/CN103289273B/zh
Publication of CN103289273A publication Critical patent/CN103289273A/zh
Application granted granted Critical
Publication of CN103289273B publication Critical patent/CN103289273B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及防腐蚀填充料,具体的说是一种氧化聚合型防蚀填料。防蚀填料包括增稠剂和惰性无机填充剂加入液状橡胶,即为粘土状防蚀填充材料。本发明防蚀填料与矿脂类相比,在低温、高温下的硬度变化小,作业性优良;在高温下不下滴,成型状态好;并且具有难燃性。适用于各种异型管线、突边、凹槽、缝隙、阀门等特殊部位及复杂形状结构物体的填充成型,亦是防腐胶带在粘贴及缠绕时良好的辅助材料。

Description

一种氧化聚合型防蚀填料
技术领域
本发明涉及防腐填充料,具体的说是一种氧化聚合型防蚀填料。
背景技术
滨海电厂以及曝露在室外的机械设备、储罐等钢铁结构,腐蚀情况十分严重。为了确保其安全运行,节约资源,需要有针对性的制定防腐蚀对策。以往采用的防腐蚀方法,比如涂敷防腐涂料、防蚀膏、金属喷涂、环氧覆盖层、水泥覆盖层、防蚀带等包覆方法,对于各种异型管线、突边、凹槽、缝隙、阀门等特殊部位及复杂形状结构物体,即便是多加防腐材料也很难与被保护物吻合、密封性有限,造型不好,成本高,防腐蚀效果差,防腐寿命短。
发明内容
本发明目的在于提供一种氧化聚合型防蚀填料。
为实现上述目的,本发明采用的技术方案为:
一种氧化聚合型防蚀填料,防蚀填料包括增稠剂和惰性无机填充剂加入液状橡胶,即为粘土状防蚀填充材料。
防蚀填料按重量百分比计,聚异戌二烯14-16%、聚α烯烃4-5%、抗氧化剂0.1-1%、有机膨润土3-5%、氢氧化铝40-44%和碳酸钙29-33%
所述抗氧化剂为抗氧剂565(市购产品)。
本发明具有以下优点:本发明防蚀填料与矿脂类相比,在低温、高温下的硬度变化小,作业性优良;即使在高温下也不会下滴,成型状态好;并且具有难燃性。适用于各种异型管线、突边、凹槽、缝隙、阀门等特殊部位及复杂形状结构物体的填充成型,亦是防腐胶带在粘贴及缠绕时良好的辅助材料。
具体实施方式
实施例1
防蚀填料包括增稠剂和惰性无机填充剂加入液状橡胶,即为粘土状防蚀填充材料。
按重量百分比计,聚异戌二烯14%、聚α烯烃5%、抗氧化剂1%、有机膨润土5%、氢氧化铝44%、碳酸钙31%。所述抗氧化剂为抗氧剂565(市购产品)
实施例2
防蚀填料包括增稠剂和惰性无机填充剂加入液状橡胶,即为粘土状防蚀填充材料。
按重量百分比计,聚异戌二烯16%、聚α烯烃4%、抗氧化剂1%、有机膨润土3%、氢氧化铝43%、碳酸钙33%。所述抗氧化剂为抗氧剂565(市购产品)
上述实施例1和实施例2所得防蚀填料效果相同。在低温、高温下的硬度变化小,作业性优良;在高温下不下滴,成型状态好;并且具有难燃性。适用于各种异型管线、突边、凹槽、缝隙、阀门等特殊部位及复杂形状结构物体的填充成型,亦是防腐胶带在粘贴及缠绕时良好的辅助材料。
测定上述所得防蚀填料特性,参见表1
表1氧化聚合型防蚀填料特性
项目 单位 测量值 测试方法
外观 - 白色、方块 -
加热减量 0.11 JIS A 5752
稠度 - 70 JIS K 2220
比重 - 1.65 JIS K 6911
难燃性 - 合格 消防危第57号
引火点 210以上 JIS K 2265

Claims (1)

1.一种氧化聚合型防蚀填料,其特征在于:防蚀填料加入液状橡胶,即为粘土状防蚀填充材料;
所述防蚀填料按重量百分比计由下述组分组成,聚异戌二烯14-16%、聚α烯烃4-5%、抗氧化剂0.1-1%、有机膨润土3-5%、氢氧化铝40-44%和碳酸钙29-33%。
CN201210517557.3A 2012-12-06 2012-12-06 一种氧化聚合型防蚀填料 Active CN103289273B (zh)