CN103265831B - A kind of heat-resisting antiwear paint containing 2-methyl methacrylate - Google Patents

A kind of heat-resisting antiwear paint containing 2-methyl methacrylate Download PDF

Info

Publication number
CN103265831B
CN103265831B CN201310209053.XA CN201310209053A CN103265831B CN 103265831 B CN103265831 B CN 103265831B CN 201310209053 A CN201310209053 A CN 201310209053A CN 103265831 B CN103265831 B CN 103265831B
Authority
CN
China
Prior art keywords
parts
methyl methacrylate
heat
paint containing
coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310209053.XA
Other languages
Chinese (zh)
Other versions
CN103265831A (en
Inventor
林耀朋
张旭
吴军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU AITESI ENVIRONMENTAL PROTECTION EQUIPMENT CO Ltd
Original Assignee
Suzhou Aitesi Environmental Protection Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Aitesi Environmental Protection Material Co Ltd filed Critical Suzhou Aitesi Environmental Protection Material Co Ltd
Priority to CN201310209053.XA priority Critical patent/CN103265831B/en
Publication of CN103265831A publication Critical patent/CN103265831A/en
Application granted granted Critical
Publication of CN103265831B publication Critical patent/CN103265831B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of heat-resisting antiwear paint containing 2-methyl methacrylate, be made up of according to weight ratio following composition: 2-methyl methacrylate 30 ~ 40 parts, ethyl 2-methacrylate 20 ~ 30 parts, 10 ~ 20 parts, silicon carbide, aluminium sesquioxide 10 ~ 20 parts, silica 10 ~ 20 part, terra alba 5 ~ 10 parts, propyl carbinol 50 ~ 70 parts.The coating containing 2-methyl methacrylate made has good heat resistant and wear resistant effect.

Description

A kind of heat-resisting antiwear paint containing 2-methyl methacrylate
Technical field
The present invention relates to a kind of heat-resisting antiwear paint, particularly relate to the heat-resisting antiwear paint containing 2-methyl methacrylate.
Background technology
At present, the field of application of paints is very wide, coating according to unlike material can be applied to different market, existing market is coated of a great variety, there is different application functions, in some professional domains, client has higher requirement to the high temperature resistant of coating and wear resistance, but in the market not only can be high temperature resistant but also to have the coating of excellent abrasive resistance few, because the high temperature resistant of coating and wear resistance are poor, result in the waste of ample resources, therefore, exploitation one can be used for specific environment as hot environment, simultaneously not only high temperature resistant but also to have the coating of excellent abrasive resistance very urgent.
Summary of the invention
The problem solved: the problem of conventional coating heat resistant and wear resistant weak effect.
Technical scheme is as follows: a kind of heat-resisting antiwear paint containing 2-methyl methacrylate, be made up of according to weight ratio following composition: 2-methyl methacrylate 30 ~ 40 parts, ethyl 2-methacrylate 20 ~ 30 parts, 10 ~ 20 parts, silicon carbide, aluminium sesquioxide 10 ~ 20 parts, silica 10 ~ 20 part, terra alba 5 ~ 10 parts, propyl carbinol 50 ~ 70 parts.
Beneficial effect: beneficial effect of the present invention: by above-mentioned coating even application on tinplate surface, carry out thermal test after finish-drying.Thermal test temperature is 700 ~ 900 DEG C, and the time is 30h.Adopted by coating the method described in GB23988-2009 to carry out cut resistance test, measure its wear resistance.Result shows, the present invention has good high temperature resistant and abrasion resistant effect, and withstand high temperatures can reach 700 ~ 900 DEG C, and wear resistance is 1150 ~ 1300L/ μm.
Embodiment
embodiment 1
Get 2-methyl methacrylate 40kg, drop in reactor, add ethyl 2-methacrylate 20kg, stir, add silicon carbide 20kg again, do not stop to stir, add aluminium sesquioxide 10kg, add silica 1 0kg again, add terra alba 5 parts, then add propyl carbinol 50kg.Both finished product can be obtained after abundant stirring.By above-mentioned coating even application on tinplate surface, after finish-drying, carry out thermal test.Thermal test temperature is 700 DEG C, and the time is 30h.There is not foaming cracking phenomena in 30h inside courtyard, coating has good thermotolerance.Adopted by coating the method described in GB23988-2009 to carry out cut resistance test, measure its wear resistance.Wear resistance is 1150 L/ μm, and coating has good wear resistance.
embodiment 2
Get 2-methyl methacrylate 30kg, drop in reactor, add ethyl 2-methacrylate 30kg, stir, add silicon carbide 10kg again, do not stop to stir, add aluminium sesquioxide 20kg, add silicon-dioxide 20kg again, add terra alba 10 parts, then add propyl carbinol 70kg.Both finished product can be obtained after abundant stirring.By above-mentioned coating even application on tinplate surface, after finish-drying, carry out thermal test.Thermal test temperature is 900 DEG C, and the time is 30h.There is not foaming cracking phenomena in 30h inside courtyard, coating has good thermotolerance.Adopted by coating the method described in GB23988-2009 to carry out cut resistance test, measure its wear resistance.Wear resistance is 1250 L/ μm, and coating has good wear resistance.
embodiment 3
Get 2-methyl methacrylate 35kg, drop in reactor, add ethyl 2-methacrylate 25kg, stir, add silicon carbide 15kg again, do not stop to stir, add aluminium sesquioxide 15kg, add silica 1 5kg again, add terra alba 5 parts, then add propyl carbinol 60kg.Both finished product can be obtained after abundant stirring.By above-mentioned coating even application on tinplate surface, after finish-drying, carry out thermal test.Thermal test temperature is 800 DEG C, and the time is 30h.There is not foaming cracking phenomena in 30h inside courtyard, coating has good thermotolerance.Adopted by coating the method described in GB23988-2009 to carry out cut resistance test, measure its wear resistance.Wear resistance is 1300 L/ μm, and coating has good wear resistance.

Claims (5)

1. the heat-resisting antiwear paint containing 2-methyl methacrylate, it is characterized in that: be made up of according to weight ratio following composition: 2-methyl methacrylate 30 ~ 40 parts, ethyl 2-methacrylate 20 ~ 30 parts, 10 ~ 20 parts, silicon carbide, aluminium sesquioxide 10 ~ 20 parts, silica 10 ~ 20 part, terra alba 5 ~ 10 parts, propyl carbinol 50 ~ 70 parts.
2. a kind of heat-resisting antiwear paint containing 2-methyl methacrylate as claimed in claim 1, is characterized in that in coating composition, 2-methyl methacrylate is 40 parts.
3. a kind of heat-resisting antiwear paint containing 2-methyl methacrylate as claimed in claim 1, is characterized in that in coating composition for ethyl 2-methacrylate is 30 parts.
4. a kind of heat-resisting antiwear paint containing 2-methyl methacrylate as claimed in claim 1, is characterized in that in coating composition, silicon carbide is 10 parts.
5. a kind of heat-resisting antiwear paint containing 2-methyl methacrylate as claimed in claim 1, is characterized in that in coating composition, silicon-dioxide is 20 parts.
CN201310209053.XA 2013-05-30 2013-05-30 A kind of heat-resisting antiwear paint containing 2-methyl methacrylate Active CN103265831B (en)