CN103232778A - 一种抗裂建筑涂料及其制备方法 - Google Patents

一种抗裂建筑涂料及其制备方法 Download PDF

Info

Publication number
CN103232778A
CN103232778A CN2013101400670A CN201310140067A CN103232778A CN 103232778 A CN103232778 A CN 103232778A CN 2013101400670 A CN2013101400670 A CN 2013101400670A CN 201310140067 A CN201310140067 A CN 201310140067A CN 103232778 A CN103232778 A CN 103232778A
Authority
CN
China
Prior art keywords
refers
crack
fiber
paint
parts
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013101400670A
Other languages
English (en)
Inventor
巢启
傅振宇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hubei Qili New Material Technology Co., Ltd.
Original Assignee
Guangxi Qili New Materials Science And Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangxi Qili New Materials Science And Technology Co Ltd filed Critical Guangxi Qili New Materials Science And Technology Co Ltd
Priority to CN2013101400670A priority Critical patent/CN103232778A/zh
Publication of CN103232778A publication Critical patent/CN103232778A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种抗裂建筑涂料。建筑物墙面经常因各种原因出现0.8-1.2mm的大裂缝,严重影响到建筑物的美观和使用寿命。目前的解决办法是在建筑外墙表面涂上具有抗裂功能的涂料,现有抗裂涂料成本高,附着力、耐水性、透气性、耐污性差。本发明以合成树脂乳液为成膜的主要成分,加入不同粒径的重钙、颜填料、纯水、乙二醇、成膜助剂、纤维、杀菌剂、防沉剂、pH调节剂、消泡剂。利用纤维比重小、比表面积大,具有优良的透气性、耐热性以及优良的柔韧性等特性,加入涂料中增强漆膜连续性能,因而能大大提高漆膜抗冲击性能、耐久性和抗裂性能。解决了普通涂料抗裂性能差、高乳液含量造成的成本过高、附着力下降、耐水、耐候性能差和抗裂不持久等难题。

Description

一种抗裂建筑涂料及其制备方法
技术领域
 本发明涉及一种建筑涂料,尤其涉及一种抗裂建筑涂料及其制备方法,属于建筑涂料技术领域。
背景技术
关于建筑物的外墙装饰,传统上习惯使用外墙砖作为装饰材料,但是外墙砖易随着时间的推移而脱落,墙面不美观的同时,还会给经过该建筑的行人带来危险,而且还难以维修。因此,用外墙涂料代替外墙砖已经越来越被各方面所接受。近年来,建筑材料的研究不断深入,如今的建筑物外墙使用外保温和加气砌块等保温材料已是常规手段,这类材料与各种混合砂浆形成的抹灰基层,受材料干缩应力,冻融破坏,温度变化等因素影响,致使墙面出现0.8-1.2mm的大裂缝,严重影响到建筑物的美观和使用寿命。目前通用的解决办法是在建筑外墙表面涂上具有抗裂功能的涂料,而现有的抗裂涂料存在成本高,附着力、耐水性、透气性、耐污性差等问题。因此开发一种低成本,附着力强,耐水性、透气性好,能抗0.8mm以上砂浆裂缝的建筑涂料是很有意义的。
发明内容
本发明所要解决的技术问题是提供一种抗裂建筑涂料以及制备这种涂料的方法,克服目前使用的外墙涂料成本高,附着力、耐水性、透气性、耐污性差的缺点。
为了解决上述技术问题本发明采用了以下技术措施,一种抗裂建筑涂料,主要由下述重量份原料组成:
合成树脂乳液100-400份  重钙100-800份  纯水70-200份  乙二醇10-50份
成膜助剂5-40份  纤维0.1-40份  颜填料1-300份  杀菌剂2-10份  
防沉剂0.1-10份  PH调节剂1-5份  消泡剂0.1-20份;
所述的合成树脂乳液是指玻璃化转变温度(Tg)在-10℃至40℃,固含在45-60%的纯丙烯酸酯共聚乳液、有机硅改性丙烯酸酯共聚乳液、苯乙烯-丙烯酸酯共聚乳液其中一种或任意配比混合物;
所述的重钙是指方解石、大理石粉碎成的10-2500目的任意配比白色粉体;
所述的纯水是指采用离子交换树脂或反渗透的方法制备,电导率<20μS/cm的去离子水;
所述的乙二醇是指沸点197.3℃,冰点-12.6℃的乙二醇;
所述的成膜助剂是指纯度≥99%,沸点255℃,闪点120℃的市售商品;
所述的纤维是指长度1-10mm的植物纤维、合成纤维、矿物纤维、人造纤维和无机纤维其中的一种或任意配比混合物;
所述的颜填料是指金红石型钛白粉、天然或人工彩砂、岩片和水性色浆其中一种或任意配比混合物;
所述的杀菌剂是指异噻唑啉酮类;
所述的防沉剂是指羟乙基纤维素、碱溶胀型增稠剂其中一种或任意配比混合物;
所述的消泡剂是指矿物油类或有机硅类其中一种或任意混合物。
上述原料,由下述方法制备:
(1)将合成树脂乳液、纯水、乙二醇、成膜助剂、杀菌剂、防沉剂、PH调节剂、消泡剂按照比例混合,然后搅拌均匀得到浆料;
(2)将重钙、纤维、颜填料按比例加入浆料中,混合后,高速搅拌均匀即可得到加纤维的抗裂建筑涂料。
采取上述措施的本发明,以合成树脂乳液为成膜的主要成分。加入不同粒径的重钙、颜填料。利用纤维比重小、比表面积大,具有优良的透气性、耐热性以及优良的柔韧性等特性,加入涂料中增强漆膜连续性能,因而能大大提高漆膜抗冲击性能、耐久性和抗裂性能。解决了普通涂料抗裂性能差、高乳液含量造成的成本过高、附着力下降、耐水、耐候性能差和抗裂不持久等难题。 
具体实施方式
实施例1
(1)浆料的配置:取Tg温度在22℃,固含在48%的纯丙烯酸酯共聚乳液150份,纯水100份,乙二醇10份,成膜助剂5份,杀菌剂2份,羟乙基纤维素1份,PH调节剂1份,矿物油类消泡剂1份,将上述材料料混合均匀后待用。
(2)取20目重钙50份,40目重钙200份,80目重钙300份,100目重钙80份,取长度 2mm植物纤维3份,40目彩砂90份,投入浆料中搅拌20分钟后,得到加纤维的抗裂建筑涂料。
实施例2
(1)浆料的配置:取Tg温度在28℃,固含在48%的有机硅改性丙烯酸酯共聚乳液160份,纯水90份,乙二醇10份,成膜助剂7份,杀菌剂2份,羟乙基纤维素0.5份,碱溶胀型增稠剂0.2份,PH调节剂1份,矿物油类消泡剂1份,将上述材料料混合均匀后待用。
(2)取40目重钙200份,60目重钙100份,80目重钙200份,100目重钙80份,取长度 3mm合成纤维2份,60目彩砂100份,投入浆料中搅拌20分钟后,得到加纤维的抗裂建筑涂料。
实施例3
(1)浆料的配置:取Tg温度在23℃,固含在46%的苯乙烯-丙烯酸酯共聚乳液140份,纯水90份,乙二醇12份,成膜助剂6份,杀菌剂2份,羟乙基纤维素1份,PH调节剂1份,有机硅类消泡剂1份,将上述材料料混合均匀后待用。
(2)取30目重钙100份,40目重钙200份,80目重钙300份,100目重钙30份,取长度 3mm矿物纤维1份,30目彩砂100份,投入浆料中搅拌20分钟后,得到加纤维的抗裂建筑涂料。
实施例4
(1)浆料的配置:取Tg温度在28℃,固含在48%的纯丙烯酸酯共聚乳液350份,纯水80份,乙二醇12份,成膜助剂20份,杀菌剂2份,羟乙基纤维素0.5份,碱溶胀型增稠剂0.1份,PH调节剂1份,有机硅类消泡剂2份,将上述材料料混合均匀后待用。
(2)取800目重钙200份,1250目重钙150份,金红石型钛白粉100份,取长度 2mm人造纤维2份,投入浆料中高速分散25分钟后,得到加纤维的抗裂建筑涂料。
实施例5
(1)浆料的配置:取Tg温度在28℃,固含在48%的有机硅改性丙烯酸酯共聚乳液320份,纯水90份,乙二醇12份,成膜助剂26份,杀菌剂2份,羟乙基纤维素0.5份,碱溶胀型增稠剂0.2份,PH调节剂1份,矿物油类消泡剂2份,将上述材料料混合均匀后待用。
(2)取800目重钙100份,1250目重钙150份,金红石型钛白粉150份,取长度 2mm无机纤维3份,投入浆料中高速分散25分钟后,得到加纤维的抗裂建筑涂料。
实施例6
(1)浆料的配置:取Tg温度在23℃,固含在46%的苯乙烯-丙烯酸酯共聚乳液300份,纯水90份,乙二醇11份,成膜助剂18份,杀菌剂2份,羟乙基纤维素1份,PH调节剂1份,有机硅类消泡剂2份,将上述材料料混合均匀后待用。
(2)取800目重钙250份,1250目重钙150份,金红石型钛白粉80份,取长度 2mm合成纤维6份,投入浆料中高速分散25分钟后,得到加纤维的抗裂建筑涂料。

Claims (2)

1.一种抗裂建筑涂料,其特征是所述的建筑涂料主要由下述重量份原料组成:
合成树脂乳液100-400份  重钙100-800份  纯水70-200份  乙二醇10-50份
成膜助剂5-40份  纤维0.1-40份  颜填料1-300份  杀菌剂2-10份  
防沉剂0.1-10份  PH调节剂1-5份  消泡剂0.1-20份;
所述的合成树脂乳液是指玻璃化转变温度(Tg)在-10℃至40℃,固含在45-60%的纯丙烯酸酯共聚乳液、有机硅改性丙烯酸酯共聚乳液、苯乙烯-丙烯酸酯共聚乳液其中一种或任意配比混合物;
所述的重钙是指方解石、大理石粉碎成的10-2500目的任意配比白色粉体;
所述的纯水是指采用离子交换树脂或反渗透的方法制备,电导率<20μS/cm的去离子水;
所述的乙二醇是指沸点197.3℃,冰点-12.6℃的乙二醇;
所述的成膜助剂是指纯度≥99%,沸点255℃,闪点120℃的市售商品;
所述的纤维是指长度1-10mm的植物纤维、合成纤维、矿物纤维、人造纤维和无机纤维其中的一种或任意配比混合物;
所述的颜填料是指金红石型钛白粉、天然或人工彩砂、岩片和水性色浆其中一种或任意配比混合物;
所述的杀菌剂是指异噻唑啉酮类;
所述的防沉剂是指羟乙基纤维素、碱溶胀型增稠剂其中一种或任意配比混合物;
所述的消泡剂是指矿物油类或有机硅类其中一种或任意混合物。
2.如权利要求1所述的一种抗裂建筑涂料的制备方法,其特征是所述制备方法主要包括下述步骤:
(1)将合成树脂乳液、纯水、乙二醇、成膜助剂、杀菌剂、防沉剂、PH调节剂、消泡剂按照比例混合,然后搅拌均匀得到浆料;
(2)将重钙、纤维、颜填料按比例加入浆料中,混合后,高速搅拌均匀即可得到加纤维的抗裂建筑涂料。
CN2013101400670A 2013-04-22 2013-04-22 一种抗裂建筑涂料及其制备方法 Pending CN103232778A (zh)