CN103218020A - 耐摩印刷笔记本电脑外壳 - Google Patents
耐摩印刷笔记本电脑外壳 Download PDFInfo
- Publication number
- CN103218020A CN103218020A CN2013101519410A CN201310151941A CN103218020A CN 103218020 A CN103218020 A CN 103218020A CN 2013101519410 A CN2013101519410 A CN 2013101519410A CN 201310151941 A CN201310151941 A CN 201310151941A CN 103218020 A CN103218020 A CN 103218020A
- Authority
- CN
- China
- Prior art keywords
- antifriction
- printing
- notebook computer
- film
- outer shell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种耐摩印刷笔记本电脑外壳,包括基材和印刷于基材表面的油墨层,在所述油墨层的表面覆盖有薄膜保护层。本发明通过增加薄膜作为保护层改变产品结构使其达到耐摩,不影响印刷字符效果,使印刷外观修饰效果在产品夹层中,表面受薄膜保护,从而达到耐摩效果。
Description
技术领域
本发明涉及一种笔记本电脑外壳,特别是涉及一种耐摩印刷笔记本电脑外壳。
背景技术
目前行业中将文字、图画、照片等原稿经制版、施墨、加压等工序,使油墨转移到纸张、织品、皮革,塑胶制品等材料表面上,批量复制原稿内容的技术,称之为印刷,以物理化学为主的传统领域,对于印刷而言如何保证印刷好的图档耐摩,现有主要处理技术是增加油墨溶剂提高耐摩损性能,以及防止材料表面划伤,提高滑动性,降低材料间的摩擦等,但是这种方法得到的产品耐磨效果并不好。
发明内容
针对现有技术的不足,本发明的目的在于,提供一种耐摩印刷笔记本电脑外壳,通过增加薄膜改变产品结构使其达到耐摩,不影响印刷字符效果,使印刷外观修饰效果在产品夹层中,表面受薄膜保护,从而达到耐摩效果。
为解决上述技术问题,本发明采用的技术方案是:耐摩印刷笔记本电脑外壳,包括基材和印刷于基材表面的油墨层,其特征在于:在所述油墨层的表面覆盖有保护层。
前述的耐摩印刷笔记本电脑外壳,其特征在于:所述油墨层和保护层之间设有贴合胶。
前述的耐摩印刷笔记本电脑外壳,其特征在于:所述保护层为薄膜。
前述的耐摩印刷笔记本电脑外壳,其特征在于:所述薄膜为1层。
前述的耐摩印刷笔记本电脑外壳,其特征在于:所述薄膜的材质为PVC、PC、PET、PMMA中的一种。
前述的耐摩印刷笔记本电脑外壳,其特征在于:所述薄膜的厚度为0.1~0.25 mm。
本发明的有益效果是:
1.表面耐磨达2H,色彩可多选,表面可做强立体效果,符合环保要求;
2.实现三维表面的高精度装饰,装饰图案内藏,永不磨损; 3.更高抗刮性和透光性,轻松实现永久清晰显示;
4.防水,防尘,耐用,可反复清洗,保持外观亮丽如新。
附图说明
图1是本发明的结构示意图。
具体实施方式
为进一步揭示本发明的技术方案,下面结合附图详细说明本发明的实施方式:如图1所示,耐摩印刷笔记本电脑外壳,包括基材1和印刷于基材1表面的油墨层2,在油墨层2的表面覆盖有1层薄膜保护层3,油墨层2和薄膜保护层3之间设有贴合胶4。
基材1为热塑性材料,主要由碳、氧、氢和氮及其它有机或无机元素所构成,成品为固体,在制造过程中是熔融状的液体,因此可以籍加热使其熔化、加压力使其流动、冷却使其固化,而形成各种形状。是由高分子合成树脂(聚合物)为主要成份,渗入各种辅助料或添加剂,在特定温度,压力下,具有可塑性和流动性,可被模塑成一定形状,且在一定条件下保持形状不变的材料。
油墨层2通过印刷将图案、文字表现在基材上,油墨中包括主要成分和辅助成分,它们均匀地混合并经反复轧制而成一种粘性胶状流体。由颜料、连结料、助剂和溶剂等组成,用于塑胶件外现装饰,书刊、包装装潢、建筑装饰等,是用于外观包装的重要材料。将油墨层印在薄膜上,再进行同基材无缝连接,使其外观通过保护层散发不同光学效果,表面永久耐摩。
薄膜保护层3的材质为PVC、PC、PET、PMMA中的一种,所述薄膜的厚度为0.178 mm。主要颜色为透明色,用于导光,透光,外观保护。光学效果多样;力学结构合理,有一定的隔音隔热特性;同时在采用不同表面材料后,可以显着增加抗UV和抗自然侵蚀的能力,使绚丽的图档表面耐腐蚀、耐摩、不脱落、色彩鲜艳。
本发明通过增加薄膜改变产品结构使其达到耐摩,不影响印刷字符效果,使印刷外观修饰效果在产品夹层中,表面受薄膜保护,从而达到耐摩效果。
加工步骤:
a.将基材表面处理的外观印刷效果印在基材反面,通过增加贴合胶的方式让油墨与薄膜粘合附着;
b.将印好的薄膜进行烘烤,使油墨充分附着在薄膜上;
c.将烘好的薄膜进行热塑性成型,使薄膜成型成基材的仿形,以便进行贴合处理;
d.再将仿形后的薄膜放入贴合型腔内;
e.注塑贴合成型完成。
以上通过对所列实施方式的介绍,阐述了本发明的基本构思和基本原理。但本发明绝不限于上述所列实施方式,凡是基于本发明的技术方案所作的等同变化、改进及故意变劣等行为,均应属于本发明的保护范围。
Claims (6)
1.耐摩印刷笔记本电脑外壳,包括基材和印刷于基材表面的油墨层,其特征在于:在所述油墨层的表面覆盖有保护层。
2.根据权利要求1所述的耐摩印刷笔记本电脑外壳,其特征在于:所述油墨层和保护层之间设有贴合胶。
3.根据权利要求1所述的耐摩印刷笔记本电脑外壳,其特征在于:所述保护层为薄膜。
4.根据权利要求3所述的耐摩印刷笔记本电脑外壳,其特征在于:所述薄膜为1层。
5.根据权利要求3所述的耐摩印刷笔记本电脑外壳,其特征在于:所述薄膜的材质为PVC、PC、PET、PMMA中的一种。
6.根据权利要求3所述的耐摩印刷笔记本电脑外壳,其特征在于:所述薄膜的厚度为0.1~0.25 mm。