CN102979053B - 一种公路护栏清洗养护方法 - Google Patents

一种公路护栏清洗养护方法 Download PDF

Info

Publication number
CN102979053B
CN102979053B CN201210515513.7A CN201210515513A CN102979053B CN 102979053 B CN102979053 B CN 102979053B CN 201210515513 A CN201210515513 A CN 201210515513A CN 102979053 B CN102979053 B CN 102979053B
Authority
CN
China
Prior art keywords
cleaning
guardrail
coating
highway barrier
maintenance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210515513.7A
Other languages
English (en)
Other versions
CN102979053A (zh
Inventor
周心德
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangxi Gude Industrial Co., Ltd.
Original Assignee
周心德
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 周心德 filed Critical 周心德
Priority to CN201210515513.7A priority Critical patent/CN102979053B/zh
Publication of CN102979053A publication Critical patent/CN102979053A/zh
Application granted granted Critical
Publication of CN102979053B publication Critical patent/CN102979053B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明就是要提供一种公路护栏清洗养护方法,包括对公路护栏表面进行清洗和养护,按如下方法进行:1)用清洗液清洗护栏表面;2)用水蒸汽喷洗护栏表面;3)养护,对2)步清洗后的护栏表面依次涂覆防锈涂层,亚光亮涂层及光亮涂层。其采用清洗和养护相结合的方法,清洗速度快,清洗效率高,使护栏的防腐性能和使用寿命大为改善。具有较好的经济和社会效益。

Description

一种公路护栏清洗养护方法
技术领域:本发明涉及一种公路护栏清洗养护方法。
背景技术:目前,我国公路护栏如高速公路的波形梁钢护栏,需求量每年就大约在300万吨以上,随着我国高速公路的快速发展,每年需求量还将大大增加。当前,我国高速公路护栏如波形梁钢护栏都采用的热浸镀锌工艺,其设计寿命为30年以上,但实际使用寿命只有10年左右。 
其原因这一方面是:由于现代工业大规模发展,生态环境受到不同程度的破坏,工业排放的废气、城市汽车排放的尾气,造成空气中的一氧化碳(CO)、二氧化碳(CO2)、二氧化硫(SO2)等有害物质含量不断升高,这些有害物质散发在空气中,充分与锌层接触,造成对镀锌层的破坏。这种产品10年以后,一方面实际使用强度明显降低,存在严重的安全隐患;另一方面由于发黑、锈蚀,景观环保效果差。再一就是没能对高速公路护栏进行有效的防护与清洗,有害物质长期附着于护栏表面,对护栏造成腐蚀缩短了护栏的使用寿命。
针对目前的这种情况,如何提高公路护栏的使用寿命,降低生产使用成本,提高管理效益,节约资源的现实需要。
如中国专利申请号为2009100582783的《高速公路护栏的清洁与护理方法》其生产是对护栏板先进行清洁表面,吹风干燥,喷涂油漆,打蜡,采用上述方法生产效率低,速度慢,相对清洗成本更高,清洗不彻底,护栏使用寿命短,效果不甚理想。
发明内容:本发明就是要提供一种公路护栏清洗养护方法,其采用清洗和养护相结合的方法,清洗速度快,清洗效率高,使护栏的防腐性能和使用寿命大为改善。具有较好的经济和社会效益。
本发明一种公路护栏清洗养护方法,包括对公路护栏表面进行清洗和养护,其是依次按如下方法进行:1)用清洗液清洗护栏表面;2)用水蒸汽喷洗护栏表面;3)养护,对2)步清洗后的护栏表面依次涂覆防锈涂层,亚光亮涂层及光亮涂层。
本发明一种公路护栏清洗养护方法,所述方法是优选按如下方法进行:
1)、用清洗装置将清洗液喷洒于护栏表面清洗灰尘与油污,控制清洗液压力为10-50㎏/cm2,清洗装置清洗刷旋转速度为300-1200转/分钟,清洗时行进速度为3-10千米/小时;2)、用高温高压水蒸汽喷洗护栏表面,控制蒸汽的压力为8-20㎏/cm2,温度在120-250℃;3)、养护,对2)步清洗后的护栏表面,依次涂覆富锌防锈漆底层涂料,丙稀酸亚光亮及光亮漆涂层。
本发明所述3)步养护在晴天进行,工作温度为20-37℃。
本发明采用自动强力清洗装置、全自动高温高压蒸汽清洗装置及全自动喷涂养护装置。 对公路护栏清洗速度快,使用效率高,清洗后的公路护栏美观,防腐效果好。起到清洗养护双重效果。性能可靠;使用寿命长,完全能满足设计使用要求,性价比可提高200% 。具有较大的经济和社会效益。
大量节约资源,一块高速公路波形梁钢护栏,相当于现有的产品三块使用,加上节约出来的制作费、安装施工费和维修费,一并折算成钢材、锌锭,每年至少为国家节约钢材210万吨,锌锭5.25万吨,
具体实施方式:下面结合实施例对本发明作进一步的详细说明。
 下面公路护栏以波形梁钢护栏为产品对本发明进行说明,即本发明对高速公路波形梁钢护栏进行清洗养护工艺。 
实施例1
本发明对波形梁钢护栏清洗工艺过程是:先对公路护栏进行强力清洗、高温高压清洗、防锈底层涂料喷涂、半光亮涂料喷涂光亮涂料喷涂。
具体清洗为用全自动强力清洗机是将无毒、无害、无污染的清洗液,利用一定压力喷洒到公路护栏波形梁钢护栏上,通过清洗机的高速旋转的仿形毛刷,洗去沉积在波形梁钢护栏上的灰尘和油污。控制清洗液的液体压力=10-50㎏/cm2,清洗液通过市售获得,将清洗液与水调合为重量浓度为2-5%清洗液溶液;清洗机清洗装置的仿形毛刷旋转速度为300-1200转/分钟。     清洗工作时,清洗机的运行速度为3-10千米/小时,最佳的清洗运行速度为5米/小时;这样将公路护栏表面上的灰尘及油渍大部分清洗干净。然后用全自动高温高压清洗机,将高温高压蒸汽喷洒到经上步清洗后的波形梁钢护栏表面上,利用高温高压蒸汽进一步对公路护栏表面进行清洗,控制全自动高温高压清洗机的水蒸汽的压力为8-20㎏/cm2,温度在120-250℃;较佳温度在150℃,然后又通过高速旋转的仿形纱布轮进一步清洗上道工序未清洗干的油污,使公路护栏表面彻底暴露锌层的致密的氧化膜。控制全自动高温高压清洗机的仿形纱布轮旋转速度为300-1200转/分钟 ,清洗过程中工作运行速度为2-10千米/小时。
最后是养护,对经清洗后的公路护栏用全自动喷涂养护机,将绿色、环保的防锈底层涂料、半光亮涂料、光亮涂料依次喷涂在波形梁钢护栏上。养护工艺条件为:全自动喷涂养护机工作运行速度为2-10千米/小时;漆的稀释度为10-40秒/杯,防锈底层涂料的底漆为环氧富锌防锈漆 ,半光亮涂料的中间层为丙稀酸半光亮漆,公路护栏的表面层光亮涂料为为光亮丙稀酸漆 ;工作温度为晴天一般在30度为佳;养护所用涂料均可通过市售获得。
经本发明方法对公路护栏进行清洗与养护,以达到高速公路波形梁钢护栏色彩鲜艳,防腐性能和使用寿命大为改善,成倍提高高速公路波形梁钢护栏使用寿命。

Claims (2)

1.一种公路护栏清洗养护方法,包括对公路护栏表面进行清洗和养护,其特征是依次按如下方法进行:1)用清洗液清洗护栏表面,是用清洗装置将清洗液喷洒于护栏表面清洗灰尘与油污,控制清洗液压力为10-50㎏/cm2,清洗装置清洗刷旋转速度为300-1200转/分钟,清洗时行进速度为3-10千米/小时;
2)用水蒸汽喷洗护栏表面,是用高温高压水蒸汽喷洗护栏表面,控制蒸汽的压力为8-20㎏/cm2,温度在120-250℃;
3)养护,对2)步清洗后的护栏表面依次涂覆防锈涂层,亚光亮涂层及光亮涂层,即是对清洗后的护栏表面,依次涂覆富锌防锈漆底层涂料,丙稀酸亚光亮及光亮漆涂层。
2.依据权利要求1所述的一种公路护栏清洗养护方法,其特征是所述3)步养护在晴天进行,工作温度为20-37℃。
CN201210515513.7A 2012-12-05 2012-12-05 一种公路护栏清洗养护方法 Active CN102979053B (zh)