CN102922223A - 汽车转向凸缘外套冷锻工艺 - Google Patents
汽车转向凸缘外套冷锻工艺 Download PDFInfo
- Publication number
- CN102922223A CN102922223A CN2011102290058A CN201110229005A CN102922223A CN 102922223 A CN102922223 A CN 102922223A CN 2011102290058 A CN2011102290058 A CN 2011102290058A CN 201110229005 A CN201110229005 A CN 201110229005A CN 102922223 A CN102922223 A CN 102922223A
- Authority
- CN
- China
- Prior art keywords
- flange
- motor turning
- cold
- phosphatization
- forging technique
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种汽车转向凸缘外套冷锻工艺,该冷锻工艺通过一次正挤预成形、一次刚性平移反挤成形和镦挤收口,使得产品流线连续,不但满足了产品的凸圆及内腔尺寸的精确性,而且还能够消除挤压工艺造成的中间强度薄弱点,提高了产品的强度,完全符合现代高级轿车对汽车零件节材减重提高强度的要求。
Description
技术领域
本发明涉及凸缘外套加工工艺,更具体地说,涉及一种汽车转向凸缘外套冷锻工艺,属于冷锻精密成形工艺技术领域。
背景技术
请参阅图1所示,该凸缘外套1是汽车转向系统重要零件,对于产品受力和耐摩擦力要求很高,其结构特点是外表面要求具有大凸缘2,内孔3要求为球形面,还有收口4部分呈斜面。其制作工艺有很大难度,即要保证表面凸缘和内腔尺寸达到各图纸要求,又要保证通过冷锻之后产品的受力和耐摩擦力及强度达到客户要求。然而,采用目前的切削加工工艺来生产,其产品存在机械强度低、易断裂的缺陷,更是很难满足设计及客户要求。
发明内容
针对现有技术中存在的上述缺点,本发明的目的是提供一种汽车转向凸缘外套冷锻工艺,能够满足产品的质量及尺寸要求。
为实现上述目的,本发明采用如下技术方案:
该汽车转向凸缘外套冷锻工艺,包括以下步骤:
A.采用圆锯机进行坯料落料;
B.退火磷化,用以锻前软化;
C.采用高强度模具钢分别制造正挤模具、反挤模具和镦挤模具;
D.通过正挤模具对坯料进行一次正挤预成形,挤压出具有球形面内孔及凸缘直径的毛坯;
E.再次退火磷化,用以锻前软化;
F.通过反挤模具进行一次刚性平移反挤成形,挤压出凸缘外套的凸缘下端部分形状;
G.通过镦挤模具进行镦挤,将凸缘外套的凸缘上端部分及斜面收口部分挤压成形;
H.精整、车边角及表面处理。
在步骤B中,退火温度为900℃,保温6小时;磷化温度为80℃,时间为20分钟。
在步骤D中,所述的正挤内孔时,其内壁厚度公差<0.02mm。
在步骤E中,退火温度为900℃,保温6小时;磷化温度为80℃,时间为20分钟。
在步骤H中,表面处理为表面镀锌。
在上述技术方案中,本发明的汽车转向凸缘外套冷锻工艺通过一次正挤预成形、一次刚性平移反挤成形和镦挤收口,使得产品流线连续,不但满足了产品的凸圆及内腔尺寸的精确性,而且还能够消除挤压工艺造成的中间强度薄弱点,提高了产品的强度,完全符合现代高级轿车对汽车零件节材减重提高强度的要求。
附图说明
图1是本发明的汽车转向凸缘外套的结构图。
具体实施方式
下面结合附图和实施例进一步说明本发明的技术方案。
同样也参考图1所示,本发明的汽车转向凸缘外套冷锻工艺包括以下具体步骤:
A.采用圆锯机进行坯料落料;
B.退火磷化;
C.采用高强度模具钢分别制造正挤模具、反挤模具和镦挤模具;
D.通过正挤模具对坯料进行一次正挤预成形,挤压出具有球形面内孔3及凸缘2直径的毛坯;
E.再次退火磷化;
F.通过反挤模具进行一次刚性平移反挤成形,挤压出凸缘外套1的凸缘2下端部分形状;
G.通过镦挤模具进行镦挤,将凸缘外套1的凸缘2上端部分及斜面收口部分挤压成形;
H.精整、车边角及表面处理。
在步骤B和E中,退火温度均为900℃,保温6小时;磷化温度为80℃,时间为20分钟。
在步骤D中,所述的正挤内孔时,其内壁厚度公差<0.02mm。
在步骤H中,表面处理为表面镀锌。
本发明通过采用一次正挤成形、一次反挤成形、一次镦挤收口的三次冷锻工艺,能够使得加工的产品流线连续,不但满足了产品的凸缘2及内腔尺寸的精确性,而且还能够消除挤压工艺造成的中间强度薄弱点,提高了产品的强度,可以完全用冷锻工艺技术替代原有的切削加工,符合现代高级轿车对汽车零件节材减重提高强度的要求。
本技术领域中的普通技术人员应当认识到,以上的实施例仅是用来说明本发明,而并非用作为对本发明的限定,只要在本发明的实质精神范围内,对以上所述实施例的变化、变型都将落在本发明的权利要求书范围内。
Claims (5)
1.一种汽车转向凸缘外套冷锻工艺,其特征在于,包括以下步骤:
A.采用圆锯机进行坯料落料;
B.退火磷化;
C.采用高强度模具钢分别制造正挤模具、反挤模具和镦挤模具;
D.通过正挤模具对坯料进行一次正挤预成形,挤压出具有球形面内孔及凸缘直径的毛坯;
E.再次退火磷化;
F.通过反挤模具进行一次刚性平移反挤成形,挤压出凸缘外套的凸缘下端部分形状;
G.通过镦挤模具进行镦挤,将凸缘外套的凸缘上端部分及斜面收口部分挤压成形;
H.精整、车边角及表面处理。
2.如权利要求1所述的汽车转向凸缘外套冷锻工艺,其特征在于:
在步骤B中,退火温度为900℃,保温6小时;磷化温度为80℃,时间为20分钟。
3.如权利要求1所述的汽车转向凸缘外套冷锻工艺,其特征在于:
在步骤D中,所述的正挤内孔时,其内壁厚度公差<0.02mm。
4.如权利要求1所述的汽车转向凸缘外套冷锻工艺,其特征在于:
在步骤E中,退火温度为900℃,保温6小时;磷化温度为80℃,时间为20分钟。
5.如权利要求1所述的汽车转向凸缘外套冷锻工艺,其特征在于:
在步骤H中,表面处理为表面镀锌。