CN1028896C - 内外有涂料的镀锌钢铁管和连接件及其加工方法 - Google Patents

内外有涂料的镀锌钢铁管和连接件及其加工方法 Download PDF

Info

Publication number
CN1028896C
CN1028896C CN 92107666 CN92107666A CN1028896C CN 1028896 C CN1028896 C CN 1028896C CN 92107666 CN92107666 CN 92107666 CN 92107666 A CN92107666 A CN 92107666A CN 1028896 C CN1028896 C CN 1028896C
Authority
CN
China
Prior art keywords
coating
galvanized steel
parts
resin
steel pipe
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 92107666
Other languages
English (en)
Other versions
CN1081750A (zh
Inventor
宣定智
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 92107666 priority Critical patent/CN1028896C/zh
Publication of CN1081750A publication Critical patent/CN1081750A/zh
Application granted granted Critical
Publication of CN1028896C publication Critical patent/CN1028896C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

内外有涂料的镀锌钢铁管和连接件及加工方法是一种防腐输水管道件及加工工艺。内外有涂料的镀锌钢铁管及连接件有本体,本体外表有镀锌层,在外表镀锌层和内壁上或内外表镀锌层上均有由树脂、香蕉水、正丁醇和无水乙醇混合而成的涂料,选合标准的镀锌钢铁管及连接件,对内外表清洁处理,清理好后放入涂料液中,10分钟后提起淋去多余的涂料,放入230℃温度下烘烤取出。该方法比较简单,涂料有耐酸碱、抗硫化和防氧化的性能。

Description

本发明是一种防腐输水管道件及其加工方法。
现有输水管道的铁管及配套连接件,为防止腐蚀,有外表镀锌铁管,有外包或内衬外包塑料管的铁管,有外表或内外表涂防腐材料的铁管,只在铁管外表增加防腐层不能解决铁管内壁防腐问题;内衬外包塑料管工艺比较复杂,成本比较高,管材长管径小的铁管内壁涂布防腐涂料一般方法比较困难,而且有的防腐材料在金属表面所形成的钝化膜与钢铁基体结合力较差,易起泡、开裂或脱落。
本发明的目的是:提供一种内外表面有防腐涂料的镀锌钢铁管和镀锌钢铁连接件及加工方法,该工艺方法比较简单,对管材长、长径小的钢铁管内壁涂布比较容易,涂料与镀锌钢铁基体结合较好,不易起泡、开裂或脱落,具有耐酸碱、抗硫化、防氧化的性能。
本发明的技术方案是:内外有涂料的镀锌钢铁管及连接件、有钢铁管及钢铁连接件本体,本体外表有镀锌层,在外表镀锌层和内壁上或内外表镀锌层上均涂有由树脂、香蕉水、正丁醇和无水乙醇按比例混合而成的防腐涂料层。
内外有涂料的镀锌钢铁管及连接件的加工方法是:先选用符合标准的镀锌钢铁管及连接件,对其内外表面清洁处理,如酸洗,清理好后浸没在由树脂、香蕉水、正丁醇和无水乙醇按比例混合而成的涂料液中,一定时间后提起淋去多余的涂料,放入一定温度下烘烤一断时间后取出。连接件有二通、三通、四通和弯头等。涂料液由树脂、香蕉水、正丁醇和无水乙醇混合而成,其配比是:树脂100份、香蕉水10份、正丁醇25份、无水乙醇15份。树脂由酚醛树脂和环氧树脂混合而成,其配比是:酚醛树脂100份,环氧树脂40份。
本发明的主要优点是:在一般镀锌层上面覆盖了一层有耐酸碱、抗硫化、防氧化性能的防腐涂料,且镀锌钢铁管及连接件内外表面上均有防腐涂料层,增加了防腐性能,克服了内表面易锈蚀的问题,比一般镀锌钢铁管使用寿命延长5倍以上。
下面结合附图和实施例对本发明进一步说明:
附图是内外表有涂料的镀锌钢铁管示图,图中:1、外表涂料层,2、外表镀锌层、3、钢铁管本体,4、外表镀锌层,5、内表涂料层。
先选符合标准的镀锌钢铁管及连接件,对内外表清洁处理,如酸洗,清理好后放入预先配制好的涂料液中,10~20分钟后提起,淋去多余的涂料,放入230℃的温度下烘烤20~30分钟取出。
涂料液的配制:先用酚醛树脂100份和环氧树脂40份混合,再用混合好的树脂100份、香蕉水10份、正丁醇25份和无水乙醇15份混合(均按质量)。无水乙醇含量大于或等于99.5%,正丁醇含量大于或等于98%,树脂固体含量53%,粘度20-30秒。
经烘烤后的内外有涂料的镀锌钢铁管和连接件取样放入盐酸或硫酸液中,经30分钟,无腐蚀、无硫化、无脱落时,再放入沸水中煮15分钟,涂料不发白、不脱落,不锈蚀即成合格产品,如不合格,采用上述方法再涂一次,直至合格为止。

Claims (5)

1、内外有涂料的镀锌钢铁管和连接件,有钢铁管及钢铁连接件本体,本体外表有镀锌层、其特征是:在外表镀锌层和内壁上或内外表镀锌层上均有由树脂、香蕉水、正丁醇和无水乙醇按比例混合成的防腐涂料层。
2、内外有涂料的镀锌钢铁管和连接件的加工方法,其特征是:先选合标准的镀锌钢铁管及连接件,对其内外表面清洁处理,清理好后浸没在由树脂、香蕉水、正丁醇和无水乙醇按比例混合而成的涂料液中,一定时间后提起淋去多余的涂料,放入一定温度下烘烤一断时间后取出。
3、按照权利要求2所说的方法,其特征是:树脂由酚醛树脂和环氧树脂按比例混合而成。
4、按照权利要求3所说的方法,其特征是:树脂由酚醛树脂100份和环氧树脂40份混合而成。
5、按照权利要求2或3所说的方法,其特征是:涂料液由树脂100份、香蕉水10份、正丁醇25份和无水乙醇15份混合而成。
CN 92107666 1992-07-30 1992-07-30 内外有涂料的镀锌钢铁管和连接件及其加工方法 Expired - Fee Related CN1028896C (zh)