CN102757529A - 一种水性丙烯酸树脂的制备方法 - Google Patents
一种水性丙烯酸树脂的制备方法 Download PDFInfo
- Publication number
- CN102757529A CN102757529A CN2012102215070A CN201210221507A CN102757529A CN 102757529 A CN102757529 A CN 102757529A CN 2012102215070 A CN2012102215070 A CN 2012102215070A CN 201210221507 A CN201210221507 A CN 201210221507A CN 102757529 A CN102757529 A CN 102757529A
- Authority
- CN
- China
- Prior art keywords
- temperature
- acrylic resin
- water
- preparation
- borne acrylic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (2)