CN102604626A - 高含硫气藏酸压液体 - Google Patents

高含硫气藏酸压液体 Download PDF

Info

Publication number
CN102604626A
CN102604626A CN2011103306104A CN201110330610A CN102604626A CN 102604626 A CN102604626 A CN 102604626A CN 2011103306104 A CN2011103306104 A CN 2011103306104A CN 201110330610 A CN201110330610 A CN 201110330610A CN 102604626 A CN102604626 A CN 102604626A
Authority
CN
China
Prior art keywords
acid
gas reservoir
acid fracturing
high sulfur
fracturing fluid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2011103306104A
Other languages
English (en)
Other versions
CN102604626B (zh
Inventor
王栋
李明志
王稳桃
赵保才
苗红
李国峰
郎学军
孙庆阁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China Petroleum and Chemical Corp
Oil Production Technology Research Institute of Sinopec Zhongyuan Petroleum Engineering Co Ltd
Original Assignee
China Petroleum and Chemical Corp
Oil Production Technology Research Institute of Sinopec Zhongyuan Petroleum Engineering Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China Petroleum and Chemical Corp, Oil Production Technology Research Institute of Sinopec Zhongyuan Petroleum Engineering Co Ltd filed Critical China Petroleum and Chemical Corp
Priority to CN201110330610.4A priority Critical patent/CN102604626B/zh
Publication of CN102604626A publication Critical patent/CN102604626A/zh
Application granted granted Critical
Publication of CN102604626B publication Critical patent/CN102604626B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种高含硫气藏酸压液体,属于油田化学技术领域,特别是适用于深层含硫碳酸岩气藏的压裂改造的酸压液体,含有盐酸、缓蚀剂、胶凝剂、表面活性剂、粘土稳定剂、铁离子稳定剂、硫控制剂和水,其酸压液体耐温可达120℃、粘度大于35mPa·s,残酸粘度小于4.0mPa·s,硫沉积控制率大于80%。对高含硫碳酸盐气藏酸压起到了酸蚀作用距离长,有效地控制硫的沉积的作用。

Description

高含硫气藏酸压液体
技术领域  本发明涉及一种含硫气藏酸压液体,属于油田化学技术领域,特别是适用于深层含硫碳酸岩气藏的压裂改造的酸压液体。
背景技术  现有的碳酸岩气藏所用的酸压液体,由盐酸、缓蚀剂、胶凝剂、铁离子稳定剂组成,由于胶凝酸液体在25℃和80℃的条件下粘度相对较低,在压裂施工中液体滤失速度大、有效酸蚀距离短,压后残酸粘度高,破胶不彻底,返排和排出后处理困难大,易造成地面环境污染。尤其是高含硫气井,随着残酸的pH值逐步上升,溶解的Fe2+将和H2S发生进一步的反应,生成FeS沉淀,引起地层严重伤害。
申请号为90106162.X的专利,公开了一种用于碳酸盐地层油气井酸化或压裂酸化的胶凝酸包括有:(A)盐酸;(B)以醛酮胺缩合物为主要组份的盐酸酸化缓蚀剂;(C)表面活性剂OP-10或SD-1;(D)水溶性耐酸阳离子2-(甲基丙烯酰氧)乙基三甲基胺盐/丙烯酰胺共聚物;(E)水,其含量(质量%)依次为15~28,0.5~1.5,0.2~1.5,1~1.5,其余为水,D系采用“W/O”型“反”乳液聚合法,使用油水两相引发剂引发2-(甲基丙烯酰氧)乙基三甲铵盐和丙烯酰胺的单体混合物而制成的共聚物,该胶凝酸同样存在对高含硫气井不能控制硫沉积的缺陷。
发明内容
本发明的目的在于克服现有技术存在的高含硫气藏酸压改造中胶凝酸粘度低、残酸粘度高、不能控制硫沉积的缺陷,提供一种酸压推进距离长,返排顺利,并在酸压过程中有效抑制硫沉积,减少对地层的污染的高含硫气藏酸压液体。
本发明的目的通过以下方案实现:
一种高含硫气藏酸压液体,含有盐酸、缓蚀剂、胶凝剂、表面活性剂、粘土稳定剂、铁离子稳定剂、硫控制剂和水,按以下质量百分比配制:
盐酸占48.3-64.5%;
胶凝剂占1.0-2.0%;
缓蚀剂占2.0-3.0%;
表面活性剂占0.1-0.5%;
粘土稳定剂占0.1-1.0%;
铁离子稳定剂占1.0-2.0%;
硫控制剂占1.0-3.0%;
余量为水。
所述的胶凝剂为亚甲基聚丙烯酰胺或聚乙烯吡咯烷酮;
所述的表面活性剂为全氟壬酸钾或全氟辛酸;
所述的硫控制剂为吖啶或喹啉。
本发明有益效果:在现有酸压液体的组分中添加配伍性良好的化合物硫控制剂吖啶或喹啉,该化合物抗盐抗温性能好,具有较强的稳定性,能吸收硫化氢,形成可溶性含硫有机化合物,同时还将三价铁离子还原成二价铁离子,起到了抑制了硫沉积和稳定铁离子的作用。
具体实施方式
实施例1:预配30吨酸液,在40吨的配液罐中加入清水6.9吨,然后加工业盐酸19.35吨,混合均匀后再加入亚甲基聚丙烯酰胺0.9吨、咪唑啉硫代磷酸酯0.9吨、全氟壬酸钾0.15吨、环氧丙基三甲基氯化铵0.3吨、EDTA 0.6吨、吖啶0.9吨,充分搅拌均匀即可实施酸压施工。
实施例2:预配30吨酸液在40方的配液罐中加入清水10.455吨,然后加入工业盐酸16.92吨,混合均匀后再加入亚甲基聚丙烯酰胺0.6吨、咪唑啉硫代磷酸酯0.75吨、全氟壬酸钾0.075吨、环氧丙基三甲基氯化铵0.15吨、EDTA0.45吨、吖啶0.6吨,充分搅拌均匀即可实施酸压施工。
实施例3:预配30吨酸液在40方的配液罐中加入清水13.94方,然后加入工业盐酸14.5方,混合均匀后再加入亚甲基聚丙烯酰胺0.3吨、咪唑啉硫代磷酸酯0.6吨、全氟壬酸钾0.03吨、环氧丙基三甲基氯化铵0.03吨、EDTA0.3方、吖啶0.3吨,充分搅拌均匀即可实施酸压施工。
实施例4、5、6与实施例1、2、3配制方法相同,具体配比见表1,表2为实施例实验的效果指标。
表1为高含硫气藏酸压液体实施例
Figure BDA0000102504660000031
表2为实施例实验的效果指标
由表2可知,本发明酸压液体耐温可达120℃、粘度大于35mPa·s,残酸粘度小于4.0mPa·s,硫沉积控制率大于80%。对高含硫碳酸盐气藏酸压起到了酸蚀作用距离长,有效地控制硫的沉积的作用。

Claims (4)

1.一种高含硫气藏酸压液体,其特征是,主要含有盐酸、缓蚀剂、胶凝剂、表面活性剂、粘土稳定剂、铁离子稳定剂、硫控制剂和水,按以下质量百分比配制:
盐酸占48.3-64.5%;
缓蚀剂占2.0—3.0%;
胶凝剂占1.0-2.0%;
表面活性剂占0.1-0.5%;
粘土稳定剂占0.1-1.0%;
铁离子稳定剂占1.0-2.0%;
硫控制剂占1.0-3.0%;
余量为水。
2.根据权利要求1所述的高含硫气藏酸压液体,其特征是:所述的胶凝剂为亚甲基聚丙烯酰胺或聚乙烯吡咯烷酮。
3.根据权利要求1或2所述的高含硫气藏酸压液体,其特征是:所述的表面活性剂为全氟壬酸钾或全氟辛酸。
4.根据权利要求3所述的高含硫气藏酸压液体,其特征是:所述的硫控制剂为吖啶或喹啉。
CN201110330610.4A 2011-10-26 2011-10-26 高含硫气藏酸压液体 Active CN102604626B (zh)