CN102408814A - 一种金属罐头内壁用涂料的制备方法 - Google Patents

一种金属罐头内壁用涂料的制备方法 Download PDF

Info

Publication number
CN102408814A
CN102408814A CN2011103111784A CN201110311178A CN102408814A CN 102408814 A CN102408814 A CN 102408814A CN 2011103111784 A CN2011103111784 A CN 2011103111784A CN 201110311178 A CN201110311178 A CN 201110311178A CN 102408814 A CN102408814 A CN 102408814A
Authority
CN
China
Prior art keywords
parts
weight
metal
mass parts
food
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011103111784A
Other languages
English (en)
Inventor
肖伟荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wujiang Tianyuan Plastic Co Ltd
Original Assignee
Wujiang Tianyuan Plastic Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wujiang Tianyuan Plastic Co Ltd filed Critical Wujiang Tianyuan Plastic Co Ltd
Priority to CN2011103111784A priority Critical patent/CN102408814A/zh
Publication of CN102408814A publication Critical patent/CN102408814A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种金属罐头内壁用涂料的制备方法,该方法的制备步骤如下:将100质量份苯酚、40-45质量份甲醛、5质量份氨水、10份三乙基铝和30-40质量份丁醇加热至沸腾1h,与70℃下真空脱水,然后将200质量份的环氧树脂加入其中进行搅拌均匀。本发明方法生产出的产品经工业试验证明,对金属罐头内表面进行涂饰处理,无毒且不与食品发生反应,还能保持食品的色香味不变。

Description

一种金属罐头内壁用涂料的制备方法
技术领域
本发明涉及一种金属罐头内壁用涂料的制备方法,属于化工涂料技术领域。
技术背景
    近年来,罐头加工工业长足发展与进步,罐头食品随包装材料和形式的扩大,除用马口铁罐、玻璃罐、铝合金罐外,其它如用铝塑复合包装材料制成的各种软罐头和无菌大包装;而玻璃罐头属于易碎产品,所以长途运输时,很容易打碎,造成损失。而金属罐头就比较安全,但是由于罐头内装的食品种类繁多,所以食品直接与金属罐头接触的话,有的会与金属发生反应,影响食品的卫生安全,所以罐头的内层必须要有一层隔绝层,避免食品与金属罐头直接接触。
发明内容
本发明目的是提供一种无毒且不与食品发生反应的金属罐头内壁用涂料的制备方法,。
    为了达到上述目的,本发明采用一个技术方案是:一种金属罐头内壁用涂料的制备方法,该方法的制备步骤如下:将100质量份苯酚、40-45质量份甲醛、5质量份氨水、10份三乙基铝和30-40质量份丁醇加热至沸腾1h,与70℃下真空脱水,然后将200质量份的环氧树脂加入其中进行搅拌均匀。
本发明方法生产出的产品经工业试验证明,对金属罐头内表面进行涂饰处理,无毒且不与食品发生反应,还能保持食品的色香味不变。
具体实施方式
实施例1
一种金属罐头内壁用涂料的制备方法,该方法的制备步骤如下:将100质量份苯酚、40-45质量份甲醛、5质量份氨水、10份三乙基铝和30-40质量份丁醇加热至沸腾1h,与70℃下真空脱水,然后将200质量份的环氧树脂加入其中进行搅拌均匀。

Claims (1)

1.一种金属罐头内壁用涂料的制备方法,其特征在于该方法的制备步骤如下:将100质量份苯酚、40-45质量份甲醛、5质量份氨水、10份三乙基铝和30-40质量份丁醇加热至沸腾1h,与70℃下真空脱水,然后将200质量份的环氧树脂加入其中进行搅拌均匀。
CN2011103111784A 2011-10-14 2011-10-14 一种金属罐头内壁用涂料的制备方法 Pending CN102408814A (zh)