CN102359266A - 组合式pvc建筑模板 - Google Patents
组合式pvc建筑模板 Download PDFInfo
- Publication number
- CN102359266A CN102359266A CN2011103071363A CN201110307136A CN102359266A CN 102359266 A CN102359266 A CN 102359266A CN 2011103071363 A CN2011103071363 A CN 2011103071363A CN 201110307136 A CN201110307136 A CN 201110307136A CN 102359266 A CN102359266 A CN 102359266A
- Authority
- CN
- China
- Prior art keywords
- dividing plate
- parts
- panel
- connect
- construction formwork
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明涉及建筑领域,尤其涉及一种建筑模板。 组合式PVC建筑模板,该建筑模板包括面板、连接隔板和加强筋板,连接隔板将内、外侧的面板连接成整体,加强筋板与面板和连接隔板相连接用于加强连接强度。本发明大大提高了建筑物水泥浇铸体的横向纵向应力,大大提高了建筑物的安全性能,尤其是抗震性能。并且免除厂房墙面二次粉刷油漆,环保无污染。
Description
技术领域
本发明涉及建筑领域,尤其涉及一种建筑模板。
背景技术
目前,传统建筑行业浇铸水泥墙体、立面和水池等,一般采用竹胶板.木板等钉制模板,在施工过程中,施工工艺复杂,耗时,耗力,而且墙面必须要粉刷,油漆。
中国发明专利(专利号200520035704,申请日2005/10/10)公开了一种木塑复合材料建筑模板的制造方法,其主要采用PVC塑料为主料,配以木粉.竹粉.稳定剂,增塑剂,润滑剂为辅料,注混合造粒、挤出、模具定型、切割成品。该专利主要是替代目前竹胶板.木板等传统材料,使用功能上没有新的突破。
发明内容
为了解决上述的技术问题,本发明的目的是提供一种组合式PVC建筑模板,该建筑模板具有施工方便简捷,大量节约人力,表面光滑,清洁环保,而且大大提高了建筑物的抗震性。
为了实现上述的目的,本发明采用了以下的技术方案:
组合式PVC建筑模板,该建筑模板包括面板、连接隔板和加强筋板;所述的面板的两端朝内侧分别设置有第一“C” 型连接槽,连接隔板的中部设有主钢筋通口,连接隔板的两个端部分别设置有工字型连接头,工字型连接头具有两个第一“T”型连接轨,连接隔板的一端的两个第一“T”型连接轨分别扣在内侧的两块面板的第一“C” 型连接槽内,将内侧的两块面板连接成一体,另一端的两个第一“T”型连接轨分别扣在外侧的两块面板的第一“C” 型连接槽内,将外侧的两块面板连接成一体;内、外侧的面板的内侧面均设有第二“T”型连接轨,连接隔板的两个侧面分别设置有第三“T”型连接轨,所述的加强筋板的两个端部分别设置有第二“C” 型连接槽,两个第二“C” 型连接槽分别与第二“T”型连接轨和第三“T”型连接轨相扣接。
作为进一步改进,上述的内、外侧的面板的内侧面还设有固定连接槽,固定连接槽内设有所述的连接隔板连接内、外侧的面板,固定连接槽由两条“J”型型材构成,所述的连接隔板的两个第一“T”型连接轨分别扣在两条“J”型型材内。
作为进一步改进,上述的连接隔板的两个侧部设有第一次钢筋通口,加强筋板的中部设有第二次钢筋通口,第一次钢筋通口与第二次钢筋通口处于相互贯通的同一位置。
作为进一步改进,上述的加强筋板与面板和连接隔板之间均成45°角。
作为进一步改进,上述的加强筋板、面板和连接隔板均采用以下的材质制成:
PVC树脂 SG-5 100份 钙锌稳定剂 2.5~6.5份
轻质CaCO3 3~7份 杜邦钛白粉 8~12份
抗冲改性剂CPE 7~11份 紫外光吸收剂UV 0.2~0.8份
增强剂ACR 1~3份。
作为进一步改进,上述的加强筋板、面板和连接隔板均采用以下的材质制成:
PVC树脂 SG-5 100份 钙锌稳定剂 4.5份
轻质CaCO3 5份 杜邦钛白粉 10份
抗冲改性剂CPE 9份 紫外光吸收剂UV 0.5份
增强剂ACR 2份。
本发明采用钙锌稳定剂具有环保无毒的特点,成品铅含量≤200ppm已完全达到欧美技术标准。加入CPE抗冲改性剂,大大提高了制品的抗冲耐压性能,配合独特的卡口卡槽方式,瞬间耐压1200PNS以上,是水泥浇注最大压力600PNS的2倍以上。加入杜邦钛白粉, UV紫外光吸收剂,大大提高了制品的耐候性,户外使用耐老化20年以上。PVC模板均采用挤出成型制得,所以制品表面光滑,清洁。
本发明的使用方法如下:先安装单边面板,连接加强筋板和连接隔板,单边完成后,扎钢筋:然后,安装另一片面板,最后,水泥灌浆浇注;由于,PVC模板重量轻2-4kg/m2,卡扣式安装简便,故具体施工人员2-3名即可。由于本发明采用的是组合式拼装,拼装完毕后再进行浇注,所以施工完毕后,内外立面是PVC模板的面板,而面板又具有光滑清洁环保无毒无污染的功能。
本发明采用的是无限连续拼装方式,浇注完以后,建筑物墙体已完全连成一体,墙体横向拉力已大大增加了。由于连接隔板的钢筋口设计,使连接隔板与横向钢筋,与加强筋板连成一体,而且连接隔板的存在也大大加大了纵向钢筋拉力的密度。
综上所述,采用组合式PVC建筑模板的设计使用方式,大大提高了建筑物水泥浇铸体的横向纵向应力,大大提高了建筑物的安全性能,尤其是抗震性能。同时,本发明大量减少劳动力强度,并且免除厂房墙面二次粉刷油漆,环保无污染。主要适用于水泥浇铸墙体,立面,水槽,圆型水池,贮水池,特别是国外农场,牧场,养殖场等。
附图说明
图1为本发明的结构示意图。
图2为图1中A部放大图。
图3为本发明的面板的结构示意图。
图4为本发明的连接隔板的结构示意图。
图5为图4中A-A的剖视图。
图6为本发明的加强筋板的结构示意图。
图7为图6中B-B的剖视图。
具体实施方式
下面结合附图对本发明的具体实施方式做一个详细的说明。
如图1所示的组合式PVC建筑模板,该建筑模板包括面板1、连接隔板2和加强筋板3构成。如图3所示,面板1的两端朝内侧分别设置有第一“C” 型连接槽11,连接隔板2的中部设有主钢筋通口22。图4、图5所示,连接隔板2的两个端部分别设置有工字型连接头21,工字型连接头21具有两个第一“T”型连接轨24。如图2所示,连接隔板2的一端的两个第一“T”型连接轨24分别扣在内侧的两块面板1的第一“C” 型连接槽11内,将内侧的两块面板1连接成一体,另一端的两个第一“T”型连接轨24分别扣在外侧的两块面板1的第一“C” 型连接槽11内,将外侧的两块面板1连接成一体。并在内、外侧的面板1的内侧面还设有固定连接槽13,固定连接槽13内设有所述的连接隔板2连接内、外侧的面板1,固定连接槽13由两条“J”型型材14构成,所述的连接隔板2的两个第一“T”型连接轨24分别扣在两条“J”型型材14内。如图3所示,内、外侧的面板1的内侧面均设有第二“T”型连接轨12,连接隔板2的两个侧面分别设置有第三“T”型连接轨23。如图6、图7所示,所述的加强筋板3与面板1和连接隔板2之间均成45°角,加强筋板3的两个端部分别设置有第二“C” 型连接槽31,两个第二“C” 型连接槽31分别与第二“T”型连接轨12和第三“T”型连接轨23相扣接。连接隔板2的两个侧部设有第一次钢筋通口25,加强筋板3的中部设有第二次钢筋通口32,第一次钢筋通口25与第二次钢筋通口32处于相互贯通的同一位置。
上述的面板1、连接隔板2、加强筋板3采用以下的材质制成:
PVC树脂 SG-5 100份 钙锌稳定剂 4.5份
轻质CaCO3 5份 杜邦钛白粉 10份
抗冲改性剂CPE 9份 紫外光吸收剂UV 0.5份
增强剂ACR 2份。
上述组合式PVC建筑模板板材的生产方法,包括以下步骤:
①PVC树脂、轻质碳酸钙、CPE抗冲改性剂、ACR增强剂、钙锌稳定剂、杜邦钛白粉、UV紫外光吸收剂、投入热锅共混;
②热锅温度至118℃时,下料至冷锅,冷混至40℃,下料至盛料车;
③共混料在盛料车堆放24小时后挤出机挤出,挤出料筒一段温度162℃,料筒二段温度162℃,料筒三段温度166℃,料筒四172℃,合流芯178℃,模头温度192℃;
④挤出后牵引成型,牵引速度3.0m/wm;
⑤面板1清洁打包,连接隔板2和加强筋板3冲床冲孔。
所制得产品主要技术指标如下:
比重:1.47
拉伸强度:2800Mpa
抗拉强度:45.3Mpa
弯曲模量:2850Mpa
抗弯强度:88.5Mpa
计示硬度:79
扭曲负荷下,塑料边缘位置弯曲温度:72.7℃
热膨胀系数:0.000065cm/cm/℃
铅含量:110PPM。
本发明的使用方法如下:先安装单边面板1,连接加强筋板3和连接隔板2,单边完成后,扎钢筋,横向钢筋分别通过主钢筋通口22以及第一次钢筋通口25与第二次钢筋通口32;然后,安装另一片面板1,最后,水泥灌浆浇注。
Claims (6)
1.组合式PVC建筑模板,该建筑模板包括面板(1)、连接隔板(2)和加强筋板(3);其特征在于:面板(1)的两端朝内侧分别设置有第一“C” 型连接槽(11),连接隔板(2)的中部设有主钢筋通口(22),连接隔板(2)的两个端部分别设置有工字型连接头(21),工字型连接头(21)具有两个第一“T”型连接轨(24),连接隔板(2)的一端的两个第一“T”型连接轨(24)分别扣在内侧的两块面板(1)的第一“C” 型连接槽(11)内,将内侧的两块面板(1)连接成一体,另一端的两个第一“T”型连接轨(24)分别扣在外侧的两块面板(1)的第一“C” 型连接槽(11)内,将外侧的两块面板(1)连接成一体;并在内、外侧的面板(1)的内侧面均设有第二“T”型连接轨(12),连接隔板(2)的两个侧面分别设置有第三“T”型连接轨(23),所述的加强筋板(3)的两个端部分别设置有第二“C” 型连接槽(31),两个第二“C” 型连接槽(31)分别与第二“T”型连接轨(12)和第三“T”型连接轨(23)相扣接。
2.根据权利要求1所述的组合式PVC建筑模板,其特征在于:内、外侧的面板(1)的内侧面还设有固定连接槽(13),固定连接槽(13)内设有所述的连接隔板(2)连接内、外侧的面板(1),固定连接槽(13)由两条“J”型型材(14)构成,所述的连接隔板(2)的两个第一“T”型连接轨(24)分别扣在两条“J”型型材(14)内。
3.根据权利要求1所述的组合式PVC建筑模板,其特征在于:连接隔板(2)的两个侧部设有第一次钢筋通口(25),加强筋板(3)的中部设有第二次钢筋通口(32),第一次钢筋通口(25)与第二次钢筋通口(32)处于相互贯通的同一位置。
4.根据权利要求1所述的组合式PVC建筑模板,其特征在于:加强筋板(3)与面板(1)和连接隔板(2)之间均成45°角。
5.根据权利要求1~4任意一项权利要求所述的组合式PVC建筑模板,其特征在于:面板(1)、连接隔板(2)和加强筋板均采用以下的材质制成:
PVC树脂 SG-5 100份 钙锌稳定剂 2.5~6.5份
轻质CaCO3 3~7份 杜邦钛白粉 8~12份
抗冲改性剂CPE 7~11份 紫外光吸收剂UV 0.2~0.8份
增强剂ACR 1~3份。
6.根据权利要求5所述的组合式PVC建筑模板,其特征在于:面板(1)、连接隔板(2)和加强筋板均采用以下的材质制成:
PVC树脂 SG-5 100份 钙锌稳定剂 4~5份
轻质CaCO3 5份 杜邦钛白粉 9~10份
抗冲改性剂CPE 8~10份 紫外光吸收剂UV 0.5份
增强剂ACR 2份。