CN102352682A - Groove type solid wood medium plate and composite plate with same - Google Patents
Groove type solid wood medium plate and composite plate with same Download PDFInfo
- Publication number
- CN102352682A CN102352682A CN2011102190933A CN201110219093A CN102352682A CN 102352682 A CN102352682 A CN 102352682A CN 2011102190933 A CN2011102190933 A CN 2011102190933A CN 201110219093 A CN201110219093 A CN 201110219093A CN 102352682 A CN102352682 A CN 102352682A
- Authority
- CN
- China
- Prior art keywords
- plate
- solid wood
- groove
- wood
- type solid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a groove type solid wood medium plate and a composite plate with the same. Grooves which have inclination angle of 30-90 DEG with a surface and are cut by a saw are distributed on the upper surface and the lower surface of a solid wood medium plate; inside stress of material can be damaged according to the density, the rigidity and the deformability of medium plate materials with different purposes, inside stress of a wood material can be properly and effectively adjusted, and a space for adjusting the expansion or contraction of the wood material is remained during the wood material is wet or dry, so that the smoothness of the surface of the composite plate is better ensured, and the submission with a contact surface is greatly improved; meanwhile, a buffering function when the composite plate is pressed is provided, so that the composite plate has soft and elastic texture when being pressed. The solid wood medium plate provided by the invention can be matched with an upper veneer and a panel on the upper surface and a lower veneer and a veneer or dampproof bottom layer on the lower surface. Both surfaces of a solid wood medium plate with longitudinal wood grains are provided with veneers with cross grains, wood grain fibers can interact due to different constriction and expansion directions, thus, tile-shaped deformation generated on the surface of the composite plate can also be avoided even if the composite plate is affected with damp in seasons with high temperature and high humidity.
Description
Technical field:
The present invention relates to the technical field of solid wood composite board, specifically a kind of resistance to deformation of plough groove type and solid wood composite board with cushioning effect.
Background technology:
It is quite long that solid wood composite board is used in time of indoor decoration and field of furniture; Especially extensive especially in the wood flooring field; The economy that obtains and use based on material; Used in the market wood flooring is generally all adopted grooved and tongued floor; And wherein the solid wood multi-layer composite floor board is low based on its cost; Characteristics such as deflection is little; Also be that the customer is selected gradually; This kind solid wood multi-layer composite floor board is provided with plate in one deck solid wood in the central; Because the hardness of the irregular wood fibre direction of growth of solid wood material itself and wooden body; Density Distribution is uneven; When the humidity in the atmosphere changes greatly; Can expand because of the moisture absorption in the floor; So that the floor board block after the assembling is pushed each other; Form the floor intermediate recess, cause serious watt of shape of floor surface, influence attractive in appearance and practical.
In order to address the above problem; The inventor had once proposed " a kind of plough groove type solid wooden compound floor " utility model patent case Chinese patent CN03256151.2 number; It is the groove that the upper and lower surface of plate is provided with vertical floor surface in solid wood; Effectively destroyed the fiber growth direction of wood floors; Make wood flooring body interior stress drop to minimum; Simultaneously deep-sawing ditch slot space can absorb the unnecessary volume of material that the wooden floor bulking increased again, reduce timber bulking pressure and the floor is pushed each other, thereby solves plate face watt shape situation.
Desired practical effect when above-mentioned patent case has reached design basically in implementing for many years; Only in the utilization of some timber; Because the factor of the fiber growth direction of its wood floors and moisture-absorption characteristics etc.; Add the difference of wood flooring environment for use; Still find to have the part wood flooring to have the partly problem of distortion; The back finds that the wood floors internal stress that the groove of originally vertical floor surface can destroy is limited after deliberation, and still has in addition improved necessity.
Other is exactly that this type of wood flooring is because the characteristic of material; It can't provide preferable vertical cushioning effect; It is comparatively strong when trample on the floor; Though can setting up one deck expanded material or padded coaming in the wood flooring bottom surface, some unit in charge of construction improves its cushioning effect; But as far as the thicker wood flooring of thickness, it is ineffective.
In addition, the composite plate with plate in the solid wood is used furniture and the decoration field of having expanded to, and its requirement for deflection is strict more.
Summary of the invention:
The problem that the present invention will solve is to overcome the not good some shortcomings of cushioning effect when the inner stress of solid wood multi-layer composite plate timber causes composite plate distortion, composite surface pressurized in the prior art.
To achieve these goals, technical scheme of the present invention provides plate in a kind of plough groove type solid wood, it is characterized in that: in this solid wood the surface of plate be provided with the angular range of surface tilt for more than or equal to the grooves of 30 degree less than 90 degree.
The angular range of said groove and surface tilt is smaller or equal to 85 degree more than or equal to 30 degree.
The surface of plate is provided with the groove that is 90 degree with the angle on surface in addition in the said solid wood.
Said groove is first longitudinal groove of plate upper surface in this solid wood.
Said groove is second longitudinal groove of plate soffit in this solid wood.
Said groove is first lateral trench of plate upper surface in the solid wood.
Said groove is second lateral trench of plate soffit in the solid wood.
Said groove is first longitudinal groove of plate upper surface in this solid wood and second longitudinal groove of soffit, is provided with in the same way or oppositely between first longitudinal groove of plate and second longitudinal groove in this solid wood.
First longitudinal groove of plate and the second longitudinal groove space are provided with in this solid wood; The groove pitch of first, second longitudinal groove is 10-60mm; The groove width of first, second longitudinal groove is 0.5-3mm, and the degree of depth of first, second longitudinal groove of plate is the 20%-95% of plate thickness in the solid wood in this solid wood.
Plate is a slash grain in this solid wood, and the thickness of plate is 5-50mm in the solid wood.
The present invention proposes a kind of composite plate with plate in the plough groove type solid wood as previously mentioned in addition, and it is characterized in that: the upper surface of plate is provided with veneer in this solid wood, and the soffit of plate is provided with down veneer in the solid wood, and upper and lower veneer is horizontal wood grain.
Said composite plate upper surface is provided with panel, and the thickness of panel is 0.05-10mm.
Said panel adopts solid wood plate, wooden skin, wood-based plate, facing paper or the wear-resisting graining paper of melamine-impregnated.
Said composite plate soffit is provided with moistureproof bottom.
Said moistureproof bottom adopts tinfoil, aluminium-foil paper, moistureproof paper, color printing facial tissue, the shockproof moistureproof sound insulating pad film in floor, elastic material bed course, wood-based plate (density board), kraft, wooden skin or single-coated foam.
During use; The plate upper and lower surface distributes corresponding sawing more than or equal to the longitudinal groove of 30 degree less than 90 degree in the solid wood of the present invention; Can be along with the middle panel material density of difference use; Hardness; Degree of deformation destroys material internal stress and can appropriateness effectively adjust the inner stress of timber; When moist or dry, give the adjusting space of swelling of wood or contraction; Better the smooth of floor surface that guarantee; Simultaneously; The two sides of plate is equipped with the band base plate in the solid wood; Because the difference of wood grain filament contraction expansion direction; The wood grain fiber can pin down each other; When even the floor makes moist at high-temperature high humidity season, the advantage that watt shape that can avoid floor to produce is out of shape.
Description of drawings:
Fig. 1 has the STRUCTURE DECOMPOSITION sketch map of composite plate one preferred embodiment of plate in the plough groove type solid wood for the present invention.
Fig. 2 is the arrange in pairs or groups STRUCTURE DECOMPOSITION sketch map of a preferred embodiment of moistureproof bottom of the composite plate that has plate in the plough groove type solid wood among Fig. 1 of the present invention.
Fig. 3 is for having the finished product cut-away section structural representation of the composite plate preferred embodiment of plate in the plough groove type solid wood among Fig. 2 of the present invention.
Fig. 4 has the STRUCTURE DECOMPOSITION sketch map of another preferred embodiment of composite plate of plate in the plough groove type solid wood for the present invention.
Fig. 5 is for having the finished product cut-away section structural representation of the composite plate preferred embodiment of plate in the plough groove type solid wood among Fig. 4 of the present invention.
Fig. 6 has the STRUCTURE DECOMPOSITION sketch map of another preferred embodiment of composite plate of plate in the plough groove type solid wood for the present invention.
Fig. 7 is the arrange in pairs or groups STRUCTURE DECOMPOSITION sketch map of a preferred embodiment of moistureproof bottom of the composite plate that has plate in the plough groove type solid wood among Fig. 6 of the present invention.
Fig. 8~10 are made into the end face structure sketch map of three kinds of preferred embodiments of matched boards for plate in the plough groove type solid wood of the present invention.
Figure 11~15 are the end face structure sketch map of five kinds of preferred embodiments of plate in the plough groove type solid wood of the present invention.
The specific embodiment:
Below in conjunction with accompanying drawing and preferred embodiment the present invention is done further description.
See Figure 1, which is the invention, the plate having a grooved wood composite sheet structure of a preferred embodiment of the exploded view of the embodiment shown in the present invention include solid plate 3, the wood in the board upper surface of the panel 1 and the upper board 2, the wood in the lower surface plate 3a of the board 4, the solid upper surface of the plate 3a, a first longitudinal groove 8a and the first lateral grooves 9a , a lower surface provided with a second longitudinal grooves 6a and the second lateral grooves 7a, the solid surface plate 3a of the first longitudinal groove 8a and the lower surface of the longitudinal grooves 6a and the second surface is inclined, the tilt angle range of 30 degrees or greater than 90 degrees; plate 3a and the upper surface of the wood in a first lower lateral grooves 9a and a second lateral surface of the groove inclination angle of the surface 7a range greater than or equal to 30 degrees Less than or equal to 90 degrees;
Fig. 2 is the arrange in pairs or groups STRUCTURE DECOMPOSITION sketch map of a preferred embodiment of moistureproof bottom of the composite plate that has plate in the plough groove type solid wood among Fig. 1 of the present invention; Fig. 3 is for having the finished product cut-away section structural representation of the composite plate preferred embodiment of plate in the plough groove type solid wood among Fig. 2 of the present invention; Wherein demonstrating composite plate of the present invention bottom surface can be provided with the moistureproof bottom 5 of one deck (this protection against the tide bottom 5 can be the moistureproof counterdie of film like; Also can be to have certain thickness moistureproof bottom; In explanation, explain with moistureproof bottom), this protection against the tide bottom 5 adopts tinfoil; Aluminium-foil paper; Moistureproof paper; The color printing facial tissue; The shockproof moistureproof sound insulating pad film in floor; The elastic material bed course; Wood-based plate (density board); Kraft; Wood skin or single-coated foam.
The STRUCTURE DECOMPOSITION sketch map that has another preferred embodiment of composite plate of plate in the plough groove type solid wood shown in Fig. 4 for the present invention; Cooperate the finished product cut-away section structural representation of Fig. 5 to know; Its overall structure configuration identical with shown in Fig. 2, Fig. 3; It is variant to have the direction that the second longitudinal groove 6b of the first longitudinal groove 8b and the lower surface of plate 3b upper surface in its solid wood tilts only; Can know shown in the embodiment that thus the direction that second longitudinal groove of first longitudinal groove of the present invention and lower surface tilts can do various collocation, between first longitudinal groove and second longitudinal groove in the same way or reverse the setting.
Fig. 6 has the STRUCTURE DECOMPOSITION sketch map of another preferred embodiment of composite plate of plate in the plough groove type solid wood for the present invention; And Fig. 7 is the arrange in pairs or groups STRUCTURE DECOMPOSITION sketch map of a preferred embodiment of moistureproof bottom of the composite plate among Fig. 6 of the present invention; Its overall structure configuration identical with shown in Fig. 2, Fig. 3 has that plate 3c upper surface and soffit can not be provided with lateral trench in its solid wood only.
The present invention has grooved wood boards wood composite panels with the upper surface of the plate first longitudinal groove and the first lateral grooves, solid wood in the lower surface of the plate has a second longitudinal groove and a second lateral grooves, these grooves can be used with different plate material density, hardness, degree of deformation and destruction moderately effective stress within the material inside the timber to adjust the stress, in wet or dry expansion or contraction of the timber when the conditioned space, to better ensure the smoothness of the surface of the composite sheet; these longitudinal grooves in the wood board surface tilt angle of 30 degrees or greater than 90 degrees, which is different from the existing wood panels opened in a groove perpendicular to the surface, representing the one hand, a groove depth ratio of solid in the same thickness of the plate 3, the other inclined grooves can be cut open more fiber composite board body that minimizes the internal stress, the other of the inclined groove opened Composite plate surface to provide a cushioning effect when the pressure as trampling on the floor with soft texture, and when the groove surface of the wood plate tilt angle less than 90 degrees, to provide the composite plate surface of the compression buffer its tilt angle smaller, the higher the groove density, which can be better damage, adjusting wood plate material deformation stress and pressure on the surface of composite panels provide cushioning effect when the better.
The degree of depth of first longitudinal groove of plate and second longitudinal groove is the 20%-95% of plate thickness in the solid wood in the solid wood of the present invention.Upper and lower veneer 2,4 is horizontal wood grain, and panel 1 is a slash grain, and the thickness of upper and lower veneer 2,4 is 0.5-8mm, and the thickness of panel 1 is 0.05-10mm, and the thickness of plate is 5-50mm in the solid wood.It is the wear-resisting graining paper of the solid wood plate of 0.10.05-10mm, wooden skin, wood-based plate, facing paper or melamine-impregnated that panel 1 adopts thickness, and the both sides of plate can be respectively equipped with the tongue and groove that supplies assembling in the solid wood.
The present invention has in the solid wood of the composite plate of plate in the plough groove type solid wood purpose for can reach design more than or equal to 30 degree less than 90 degree time of the angular range of plate 3 surface tilt in these grooves of plate and solid wood; Only if will provide general user can experience actual foot-operated buffering sense as the floor use, the preferred angle scope of plate surface tilt is to spend smaller or equal to 85 degree more than or equal to 30 in these grooves and the solid wood.
First longitudinal groove and second longitudinal groove of the present invention with plate in the solid wood of the composite plate of plate in the plough groove type solid wood adopted the structure that is inclination with the surface again; First lateral trench and second lateral trench then can be adopted the structure of existing vertical surface, also can reach effect of the presently claimed invention.
In Fig. 8~10 is the end face structure sketch map that plate is made into three kinds of preferred embodiments of matched boards in the plough groove type solid wood of the present invention; Wherein can find out plate 3d in the solid wood of the present invention clearly; 3e; The first longitudinal groove 8d of 3f upper surface; 8e; The second longitudinal groove 6d of 8f and soffit, 6e, 6f can have various angle to change and different directions changes.
Figure 11~15 are the end face structure sketch map of five kinds of preferred embodiments of plate in the plough groove type solid wood of the present invention; Wherein demonstrating first longitudinal groove of plate upper surface in the solid wood of the present invention and second longitudinal groove of soffit singly can not have various angle to change and different direction variations; The plate surface is vertical longitudinal groove and arranges in pairs or groups mutually and use in the longitudinal groove that plate surface in the present invention and the solid wood can also be simultaneously inclination and the existing solid wood, can also reach practicality effect of the present invention.
The present invention has after plate is got the raw materials ready among the following a of preparation method, solid wood of the composite plate of plate in the plough groove type solid wood; The upper and lower surface of plate is opened saw first longitudinal groove and second longitudinal groove respectively in solid wood, and the upper and lower surface of plate is opened saw first lateral trench and second lateral trench respectively in solid wood again; B, in solid wood the upper and lower surface coated cold pressing glue or the hot pressing glue of plate; To go up veneer and following veneer again and be fitted in the upper and lower surface of plate in the solid wood respectively; Employing cold pressing the press of glue application cold pressing or use hot pressing glue pass through the hot pressing of precompressed hot repressing machine, three ply board is shown consideration for is closed; C, at the surface coated cold pressing glue or the hot pressing glue of last veneer, panel is fitted in the surface of veneer, adopt the press of the glue application of colding pressing to cold pressing or use the hot press hot pressing after the precompressed of passing through of hot pressing glue, make the applying of panel and last veneer; D, with the composite plate sawing itemize behind the aforementioned applying panel, offer tongue and groove at the composite plate edge; E, composite plate oil paint coating are examined according to composite plate lacquer painting quality requirement sheet again; Moistureproof bottom is pasted in f, following veneer bottom, at last the packing warehouse-in.Wherein, The angular range of first longitudinal groove and first lateral trench is less than 90 degree more than or equal to 30 degree; The angular range of second longitudinal groove and second lateral trench is less than 90 degree more than or equal to 30 degree; Angle described here be meant plate in the solid wood on; Angle between soffit and each groove; Be provided with in the same way or oppositely between first longitudinal groove and second longitudinal groove; Be provided with in the same way or oppositely between each groove of first longitudinal groove; Be provided with in the same way or oppositely between each groove of second longitudinal groove, first longitudinal groove and second longitudinal groove are for be provided with in the same way or oppositely.
In a step; Plate employing thickness is that 5-50mm, dry moisture content are lower than 12% artificial growth woods material in the solid wood; General China fir, poplar, pine, Eucalyptus or the birch that adopts growth fast; It is subsequent use that above-mentioned material blocks the back; First longitudinal groove of plate and the second longitudinal groove space are provided with in the solid wood; The groove pitch of first, second longitudinal groove is 15-60mm; The groove width of first, second longitudinal groove is 0.5-3mm, and the gash depth of first, second longitudinal groove is the 20%-95% for plate thickness in the solid wood; First lateral trench of plate and the second lateral trench space are provided with in the solid wood; The groove pitch of first, second lateral trench is 10-80cm; The groove width of first, second lateral trench is 0.5-3mm; The gash depth of first, second lateral trench is the 20%-80% of plate thickness in the solid wood; Sawing is had laterally at last, plate carries out jigsaw in the solid wood of longitudinal groove, the length of jigsaw is 90-2650cm, width 90-135cm.In the b step, the upper and lower surface of plate adopts dual-layer adhesive machine to be coated with in the solid wood, and the cold pressing glue coating weight is 100-200g/m
2, hot pressing glue coating weight is 120-220g/m
2, the pressure of colding pressing is 6-15kg/cm2, the time 10-60 branch of colding pressing, and the environment temperature of the work of colding pressing is 10-35 ℃, the pressure of hot pressing is 6-15kg/cm
2, hot pressing time 5-20 branch, hot pressing temperature is a 100-125 degree Celsius, plate in last veneer, the solid wood, the veneer three ply board shows consideration for that to close the two-sided sanding in back fixed thick down, make plate body thickness evenly, the plate face is smooth bright and clean.
In the c step, the surface of last veneer adopts the single spreading machine to be coated with, and the cold pressing glue coating weight is 100-200g/m
2, hot pressing glue coating weight is 120-220g/m
2, the pressure of colding pressing is 6-15kg/cm
2, the time 15-60 branch of colding pressing, the pressure of hot pressing is 6-15kg/cm
2, hot pressing time 5-20 branch, hot pressing temperature is a 100-125 degree Celsius, it is the wear-resisting graining paper of the solid wood plate of 0.05-10mm, wooden skin, wood-based plate, facing paper or melamine-impregnated that panel adopts thickness.In the f step, moistureproof bottom adopts tinfoil, aluminium-foil paper, moistureproof paper, color printing facial tissue, the shockproof moistureproof sound insulating pad film in floor, elastic material bed course, wood-based plate (density board), kraft, wooden skin or single-coated foam.
Illustrate that through subordinate list the present invention uses and the difference and the improvements that have the ground plate technique now as the floor below:
Content by subordinate list 1 and subordinate list 2 can draw; Composite plate with plate in the plough groove type solid wood of the present invention uses as the floor that not only cost of production is low; Mat formation conveniently; Technological process is simple; Have the not available advantages of wooden floor such as anti-damp resist drying simultaneously; The needs that more meet the underground heat ground heater laying; The feel and the visual effect that have general wooden floor again; Content of formaldehyde is significantly less than common solid wooden compound floor again; We can say that composite plate that the present invention has a plate in the plough groove type solid wood combines the advantage of wooden floor and common solid wooden compound floor, has opened up the frontier of solid wooden compound floor.
Can be provided with the moistureproof bottom 5 that floor moistureproof paper, shockproof moistureproof sound insulating pad film, elastic material bed course etc. are processed at following the following of veneer 4; Effectively isolated bottom surface, floor contacts with the direct of ground moisture; Can prevent effectively more that make moist distortion, situation such as rotten of floor from maximum moistureproof, anticorrosion, the sound-absorbing shockproof effect in floor that improves taking place.The deep-sawing groove has destroyed the wooden irregular machine direction in floor; It is minimum that wood floors internal stress, degree of deformation are reduced to; For making the more smooth docile not warpage in floor; And improve because of dry or high temperature sunshine shining directly; The floor internal moisture runs off in a large number; The gap of the wood flooring that causes and floor cracking; Through the bonding reorganization of the staggered up and down vertical and horizontal sawing groove of plate in the solid wood and upper and lower surface with the wooden thin slice of transverse direction; Wood fibre pins down each other, can avoid the cracking of wood flooring gap and floor panel face.Reasonable in design of the present invention; Except that panel 1 uses the nobler raw material; Other all can use artificial growth fast-growing woods wood skin or adopt moistureproof bottom 5 materials in below of veneer 4 down; Material uses more environmental protection; Comprehensive utilization ratio is higher; Adopt moistureproof bottom 5 materials; Reduce glue 50%-70% use amount than solid wood multi-layer composite floor board again in addition; Formaldehyde is hanged down in environmental protection; Moistureproof; Anticorrosion non-deformability is stronger; Production procedure is shortened; Manufacturing cost is lower; Product be specially adapted to the popular heating floor of existing market over the ground plate hight quality high standard require to use that (winter, floor bottoms was born 50-60 degree Celsius left and right sides high temperature for a long time; Material is dried contraction for a long time; The expansion of making moist of the damp and hot humidity in summer, material).
Plate adopts length 930mm in the solid wood; Width 135mm; Thickness is 12mm; Gan Zao moisture content is lower than 12% China fir plate; The full on four sides light processing of above-mentioned material back is subsequent use; In solid wood plate on; Soffit is opened saw first longitudinal groove and second longitudinal groove respectively; First longitudinal groove and the second longitudinal groove rightabout are provided with; Again in solid wood plate on; Soffit is opened saw first lateral trench and second lateral trench respectively; First longitudinal groove of plate and the second longitudinal groove space are provided with in the solid wood; In the solid wood (raised line) limit of plate start to the groove pitch of first groove be 20mm; First; The groove pitch of second longitudinal groove is 20mm, first; The groove width of second longitudinal groove is 1mm first; The gash depth of second longitudinal groove be in the solid wood plate thickness 80%; First lateral trench of plate and the second lateral trench space are provided with in the solid wood; The groove pitch of first, second lateral trench is 20cm; The groove width of first, second lateral trench be the gash depth of 1mm, second lateral trench be in the solid wood plate thickness 60%, sawing is had laterally at last, plate is combined into the big plate of opening with jigsaw string rope machine in the solid wood of longitudinal groove.Then, the upper and lower surface of plate adopts dual-layer adhesive machine to be coated with in solid wood, and hot pressing glue coating weight is 200g/m
2, after will going up veneer and following veneer again and being fitted in the upper and lower surface of plate in the solid wood respectively, to put into the oil pressure preformer and cold pressing, the pressure of colding pressing is 10kg/cm
2, to cold pressing 40 minutes time, the environment temperature of the work of colding pressing is 25 ℃ ± 5 ℃, the pressure of hot pressing is 12kg/cm
2, hot pressing time 10 minutes, hot pressing temperature is 110 degree Celsius, plate in last veneer, the solid wood, the veneer three ply board is shown consideration for and is closed the two-sided sanding in back and decide thickly down, makes the plate face thickness even, smooth bright and clean.The surface of last veneer adopts the single spreading machine to be coated with, and the cold pressing glue coating weight is 180g/m
2, the pressure of colding pressing is 12kg/cm
2, to cold pressing 30 minutes time, the environment temperature of the work of colding pressing is 25 ℃ ± 5 ℃, it is the solid wood plate of 2mm that panel adopts thickness.Carry out the floor itemize then; Tongue and groove is offered on the floor; Floor UV coats with lacquer application; Examine according to floor lacquer painting quality requirement sheet again; Bottom sticks the moistureproof bottom in floor on the floor at last; Material can be a tinfoil; Aluminium-foil paper; Moistureproof paper; The color printing facial tissue; The shockproof moistureproof sound insulating pad film in floor; The elastic material bed course; Wood-based plate (density board); Kraft; The wood skin; Single-coated foam etc.; Make floor bottoms can better effectively reach moistureproof; Anticorrosion; Shockproof; Soundproof effect; Use the color printing facial tissue can be printed with various wood grains attractive in appearance in floor bottoms simultaneously; Also can on this moistureproof bottom, stamp trade mark; Producer's title; The patent No.; Anti-counterfeiting mark and product build date etc.; Make the customer find out manufacturer at a glance; Product company reaches better products propaganda effect and prevents that product personation situation of poor quality from taking place.
Claims (15)
1. plate in the plough groove type solid wood is characterized in that: in this solid wood the surface of plate be provided with the angular range of surface tilt for more than or equal to the grooves of 30 degree less than 90 degree.
2. plate in the plough groove type solid wood according to claim 1 is characterized in that: the angular range of said groove and surface tilt is for spending smaller or equal to 85 more than or equal to 30 degree.
3. plate in the plough groove type solid wood according to claim 1 is characterized in that: the surface of plate is provided with the groove that is 90 degree with the angle on surface in addition in the said solid wood.
4. according to plate in claim 1, the 2 or 3 described plough groove type solid woods, it is characterized in that: said groove is first longitudinal groove of plate upper surface in this solid wood.
5. according to plate in claim 1, the 2 or 3 described plough groove type solid woods, it is characterized in that: said groove is second longitudinal groove of plate soffit in this solid wood.
6. according to plate in claim 1, the 2 or 3 described plough groove type solid woods, it is characterized in that: said groove is first lateral trench of plate upper surface in this solid wood.
7. according to plate in claim 1, the 2 or 3 described plough groove type solid woods, it is characterized in that: said groove is second lateral trench of plate soffit in the high solid wood.
8. plate in the plough groove type solid wood according to claim 1; It is characterized in that: said groove is first longitudinal groove of plate upper surface in this solid wood and second longitudinal groove of soffit, is provided with in the same way or oppositely between first longitudinal groove of plate and second longitudinal groove in this solid wood.
9. plate in the plough groove type solid wood according to claim 8; It is characterized in that: first longitudinal groove of plate and the second longitudinal groove space are provided with in the said solid wood; The groove pitch of first, second longitudinal groove is 10-60mm; The groove width of first, second longitudinal groove is 0.5-3mm, and the degree of depth of first, second longitudinal groove is the 20%-95% of plate thickness in the solid wood.
10. plate in the plough groove type solid wood according to claim 1 is characterized in that: plate is a slash grain in the said solid wood, and the thickness of plate is 5-50mm in the solid wood.
11. one kind has like the composite plate of plate in the plough groove type solid wood as described in each in the claim 1,2,3,8,9,10; It is characterized in that: the upper surface of plate is provided with veneer in the said solid wood; The soffit of plate is provided with down veneer in the solid wood, and upper and lower veneer is horizontal wood grain.
12. the composite plate with plate in the plough groove type solid wood according to claim 11 is characterized in that: said composite plate upper surface is provided with panel, and the thickness of panel is 0.05-10mm.
13. the composite plate with plate in the plough groove type solid wood according to claim 12 is characterized in that: panel adopts solid wood plate, wooden skin, wood-based plate, facing paper or the wear-resisting graining paper of melamine-impregnated.
14. the composite plate with plate in the plough groove type solid wood according to claim 11 is characterized in that: said composite plate soffit is provided with moistureproof bottom.
15. the composite plate with plate in the plough groove type solid wood according to claim 14 is characterized in that: moistureproof bottom adopts tinfoil, aluminium-foil paper, moistureproof paper, color printing facial tissue, the shockproof moistureproof sound insulating pad film elasticity material bed course in floor, wood-based plate, kraft, wooden skin or single-coated foam.