CN102225669A - Preparation method of vacuum baking finish film membrane and application thereof - Google Patents

Preparation method of vacuum baking finish film membrane and application thereof Download PDF

Info

Publication number
CN102225669A
CN102225669A CN2011101069509A CN201110106950A CN102225669A CN 102225669 A CN102225669 A CN 102225669A CN 2011101069509 A CN2011101069509 A CN 2011101069509A CN 201110106950 A CN201110106950 A CN 201110106950A CN 102225669 A CN102225669 A CN 102225669A
Authority
CN
China
Prior art keywords
antiadhesion barrier
preparation
baking vanish
gummed paper
true
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2011101069509A
Other languages
Chinese (zh)
Other versions
CN102225669B (en
Inventor
张相如
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 201110106950 priority Critical patent/CN102225669B/en
Publication of CN102225669A publication Critical patent/CN102225669A/en
Application granted granted Critical
Publication of CN102225669B publication Critical patent/CN102225669B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a baking finish film, in particular to a preparation method of a vacuum baking finish film and an application thereof; and the preparation method comprises the following steps of: mounting a release film and a screen on a silk-screen printer; using an oil-ink mixture to silkscreen a pattern; drying the oil-ink mixture on the release film, stoving the release film in an oven; then turning off the power of the oven, taking out the release film when the temperature is cooled; cooling the release film, paving the release film, flattening a gummed paper with a shape in fit with the release film on a plane on which the pattern is silkscreened of the release film, then tearing town the gummed paper so that the pattern is adhered on the gummed paper to form a vacuum baking finish film. The process flow for preparing the vacuum baking finish film is short in manufacturing time, simple in the process procedure, and secure in coloring; the vacuum baking finish can be directly adhered on a glass material, the craft glass can be manufactured without any technology investment; and therefore, a plurality of manpower, material resource and finial resource can be saved.

Description

A kind of preparation method of true baking vanish film and application thereof
 
Technical field
The present invention relates to the baking vanish film, is the preparation method of baking vanish film and the application of baking vanish film on glass material of being made by this method specifically.
Background technology
At present, the ambetti with pattern is more and more used, and its preparation method also has multiple.Wherein a kind of is to adopt traditional silk screen printing process, it need at first make the film and half tone, and the screen frame that stretched tight, then half tone and glass material are installed on the screen printer, and go up printing ink with the pattern silk-screen on glass material, then the figuratum glass material of silk-screen is sent into baking oven and dry, pattern is fixed on the glass material.It is long that this method is made time of finished product, make complex process, and the pattern color of producing can not gradual change.Also having a kind of is to adopt the pearly-lustre film to strengthen film coating process, and it is print pattern on the pearly-lustre film at first, the pearly-lustre film is attached on glassly to dry with baking oven then, although it is simpler that this mode is made, but pattern is relatively poor attached to firmness on glass, is easy to come off, and can not contacts with water.
Summary of the invention
The invention solves above-mentioned technical problem, a kind of preparation method of true baking vanish film is provided, it is the rich color of simple, the consuming time weak point of manufacture craft, pattern not only, and should be pasted on glass by true baking vanish film, can guarantee pattern firm coloration on glass, and can be exposed to the sun under the sun or in water, soak.
The present invention solves the problems of the technologies described above the technical scheme of being taked: a kind of preparation method of true baking vanish film, and it may further comprise the steps:
The first step: antiadhesion barrier is tiled on the platen of screen printer;
Second step: will make figuratum half tone and be installed on the described screen printer;
The 3rd step: be poured on deployed ink mixture on the half tone and start screen printer, after silk-screen on the described antiadhesion barrier goes out pattern on this half tone, close screen printer;
The 4th step: after treating the ink mixture drying on the antiadhesion barrier in the 3rd step, the described half tone of dismantling replaces described half tone with making figuratum at least one other half tone, repeats for second step and the 3rd step successively;
The 5th step: after treating the ink mixture drying on the antiadhesion barrier in the 4th step, this antiadhesion barrier is sent into baking oven dry;
The 6th step: after oven dry is finished, close the baking oven power supply, treat to take out described antiadhesion barrier after temperature descends;
The 7th step: after treating the antiadhesion barrier cooling in the 6th step, at first it is paved, uses the gummed paper that matches with this antiadhesion barrier shape smooth on the figuratum plane of antiadhesion barrier silk-screen, the gummed paper of tearing then, make pattern attached on the gummed paper to form true baking vanish film.
This technical scheme also has following technical characterictic:
Described ink mixture is an epoxy resin printing ink, is added with diluent, curing agent and defoamer in this printing ink.
The baking oven heating-up temperature is 100 ℃ to 130 ℃ a constant temperature in described the 5th step.
Described constant temperature was kept 30 minutes.
After dropping to 50 ℃, temperature in described the 6th step takes out antiadhesion barrier.
With the described gummed paper of doctor blade, make gummed paper smooth in described the 7th step in described antiadhesion barrier.
The another kind of technical scheme that the present invention solves the problems of the technologies described above employing is: will have another relative plane of pattern plane with this true baking vanish film and be pasted on the glass material.
The technical scheme that proposes according to the present invention as can be known, make true baking vanish film by technological process of the present invention, saved the technical process that traditional silk screen printing process is made the film and stretched tight and net, also avoided directly spraying paint to material to be processed, its Production Time is short, technical process is simple, firm coloration, can be exposed to the sun under the sun or soak in water; , true baking vanish of the present invention directly is pasted on the glass material in addition, need not any technology input and just can be made into artistic glass, saved great amount of manpower and material resources and financial resources.
The specific embodiment
Below the present invention is elaborated:
The preparation method of true baking vanish film of the present invention may further comprise the steps, the first step: antiadhesion barrier is tiled on the platen of screen printer; Because antiadhesion barrier is less to the cohesive force of other attachments, be convenient in the 7th step pattern be torn to gummed paper from the antiadhesion barrier commentaries on classics; Second step: will make figuratum half tone and be installed on the described screen printer; The 3rd step: be poured on deployed ink mixture on the half tone and start screen printer, close screen printer after silk-screen on the described antiadhesion barrier goes out pattern on this half tone, silk-screen has gone out the first road color on antiadhesion barrier like this; Ink mixture of the present invention adopts the printing ink of epoxide resin type, add diluent, curing agent and defoamer etc. in it, printing ink wherein: curing agent: the ratio of defoamer is generally 1:(12 ﹪-15 ﹪): (1 ﹪-2 ﹪), and diluent can be selected as required in right amount; The 4th step: after treating the ink mixture air dry on the antiadhesion barrier in the 3rd step, the described half tone of dismantling, replace described half tone with making figuratum at least one other half tone, repeated for second step and the 3rd step successively, can on antiadhesion barrier, go out second road or more color by silk-screen like this, on antiadhesion barrier, wherein the quantity of half tone should rationally be made according to painted needs until the complete silk-screen of whole pattern.
The 5th step: after treating that silk-screen has ink mixture air dry on the antiadhesion barrier of complete pattern, it is rolled gently be put in the baking oven, and open baking oven and heat.In bake process, the temperature in should baking oven is set to constant temperature, and constant temperature is preferably between 100 ℃ to 130 ℃ and selects, and under above-mentioned constant temperature antiadhesion barrier is continued about 30 minutes of baking, and antiadhesion barrier is dried fully.In this process, need the assurance temperature of oven evenly to generate heat formation waste product otherwise the printing ink on the antiadhesion barrier splits easily; The 6th step: close the baking oven power supply after stoving time is finished, oven temperature begins to descend, and when temperature is reduced to about 50 ℃, just can take out the antiadhesion barrier of oven dry.
The 7th step: after treating the antiadhesion barrier cooling, it is divided, entirely be attached to antiadhesion barrier with the adhesive sticker gummed paper and have on the plane of pattern, and wipe off gently, the bubble between gummed paper and the antiadhesion barrier is scraped out with the plastics scraper; Then repeat to scrape several times, between gummed paper and antiadhesion barrier, do not have bubble, and both fit tightly; The antiadhesion barrier of tearing gently then because the characteristic of antiadhesion barrier and gummed paper itself can make pattern firmly be attached on the gummed paper, even be exposed to the sun under the sun or soaking in water, can not come off yet, and the gummed paper of this pattern that takes a turn for the better is true baking vanish film of the present invention.Tear in commentaries on classics and to require dynamics even in the process, surface requirements accomplishes smoothly not wrinkle.
From the above, the present invention has saved traditional silk screen printing process and has made technical process such as the film, the net that stretches tight, also need not material to be processed is sent into the baking oven baking, simultaneously also avoided directly spraying paint, so the present invention makes the method for true baking vanish film, and not only the time is short, technical process is simple to material to be processed; And firm coloration.In the process of using, can another relative plane of pattern plane directly be pasted on glass material with glue etc. or other have on the material of flat surface with having with this true baking vanish film, just can make silk-screen, baking vanish and strengthen the perfect effect that three kinds of technologies of pad pasting are combined as a whole, change the loaded down with trivial details operation of traditional silk-screen, baking vanish and reinforcement process, realized a technologic new breakthrough.When making ambetti, only need true baking vanish film is pasted on and on glassly just can reach decorative effect, so not only can reduce the cost of investment and the production cost of making ambetti, and saving great amount of manpower and material resources and financial resources.
Above-mentioned embodiment is only for the usefulness that the present invention is described; and be not to be limitation of the present invention; the those of ordinary skill in relevant technologies field; without departing from the spirit and scope of the present invention; can also make various variations and modification; therefore all technical schemes that are equal to also should belong to category of the present invention, and scope of patent protection of the present invention should be limited by each claim.

Claims (7)

1. the preparation method of a true baking vanish film, it may further comprise the steps:
The first step: antiadhesion barrier is tiled on the platen of screen printer;
Second step: will make figuratum half tone and be installed on the described screen printer;
The 3rd step: be poured on deployed ink mixture on the half tone and start screen printer, after silk-screen on the described antiadhesion barrier goes out pattern on this half tone, close screen printer;
The 4th step: after treating the ink mixture drying on the antiadhesion barrier in the 3rd step, the described half tone of dismantling replaces described half tone with making figuratum at least one other half tone, repeats for second step and the 3rd step successively;
The 5th step: after treating the ink mixture drying on the antiadhesion barrier in the 4th step, this antiadhesion barrier is sent into baking oven dry;
The 6th step: after oven dry is finished, close the baking oven power supply, treat to take out described antiadhesion barrier after temperature descends;
The 7th step: after treating the antiadhesion barrier cooling in the 6th step, at first it is paved, uses the gummed paper that matches with this antiadhesion barrier shape smooth on the figuratum plane of antiadhesion barrier silk-screen, the gummed paper of tearing then, make pattern attached on the gummed paper to form true baking vanish film.
2. the preparation method of a kind of true baking vanish film according to claim 1 is characterized in that: described ink mixture is an epoxy resin printing ink, is added with diluent, curing agent and defoamer in this printing ink.
3. the preparation method of a kind of true baking vanish film according to claim 1 is characterized in that: the baking oven heating-up temperature is 100 ℃ to 130 ℃ a constant temperature in described the 5th step.
4. the preparation method of a kind of true baking vanish film according to claim 3 is characterized in that: described constant temperature was kept 30 minutes.
5. the preparation method of a kind of true baking vanish film according to claim 1 is characterized in that: take out antiadhesion barrier after the temperature in described the 6th step drops to 50 ℃.
6. the preparation method of a kind of true baking vanish film according to claim 1 is characterized in that: with the described gummed paper of doctor blade, make gummed paper smooth in described antiadhesion barrier in described the 7th step.
7. according to the application of the true baking vanish film of any described method making in the claim 1 to 6, it is characterized in that: will have another relative plane of pattern plane with this true baking vanish film and be pasted on the glass material.
CN 201110106950 2011-04-27 2011-04-27 Preparation method of vacuum baking finish film membrane and application thereof Expired - Fee Related CN102225669B (en)