CN102225377A - 一种低品位碳酸锰矿浮选后尾矿絮凝处理方法 - Google Patents

一种低品位碳酸锰矿浮选后尾矿絮凝处理方法 Download PDF

Info

Publication number
CN102225377A
CN102225377A CN2011101157181A CN201110115718A CN102225377A CN 102225377 A CN102225377 A CN 102225377A CN 2011101157181 A CN2011101157181 A CN 2011101157181A CN 201110115718 A CN201110115718 A CN 201110115718A CN 102225377 A CN102225377 A CN 102225377A
Authority
CN
China
Prior art keywords
low
manganese carbonate
mine tailing
aluminum sulfate
grade manganese
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011101157181A
Other languages
English (en)
Inventor
石朝军
杨朝霞
麻德立
谢勇
龙秀华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HUAYUAN QIANGHUA MINING CO Ltd
Original Assignee
HUAYUAN QIANGHUA MINING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HUAYUAN QIANGHUA MINING CO Ltd filed Critical HUAYUAN QIANGHUA MINING CO Ltd
Priority to CN2011101157181A priority Critical patent/CN102225377A/zh
Publication of CN102225377A publication Critical patent/CN102225377A/zh
Pending legal-status Critical Current

Abstract

一种低品位碳酸锰矿浮选后尾矿絮凝处理方法,是将阳离子800与硫酸铝溶液配合使用。用本发明的方法对低品位碳酸锰矿浮选后的尾矿进行絮凝处理,可达到较理想的效果,能满足工业生产要求,对废物的再利用、减少环境污染及节约水资源等具有重要的意义。

Description

一种低品位碳酸锰矿浮选后尾矿絮凝处理方法
技术领域
本发明涉及一种低品位碳酸锰矿浮选后尾矿絮凝处理方法。
背景技术
低品位碳酸锰矿由于锰含量低、杂质含量高,通常需要经过浮选。浮选后的精矿用于生产电解金属锰,而浮选后的尾矿一般作废物处理,或可加工成水泥熟料。在浮选后的尾矿中含有一定量的水和可用固形物,用絮凝剂将其絮凝,可促进团粒的下沉、液体的澄清和泥饼的脱水,一方面可加快尾矿的回收利用(如加工成水泥熟料等)时间,另一方面可提高生产效率,减少尾矿流失和水消耗,降低设备投资和加工成本。
发明内容
本发明的目的在于公开一种将低品位碳酸锰矿浮选后的尾矿进行快速有效絮凝的方法。
本发明方法是将阳离子800与硫酸铝溶液配合使用,阳离子800浓度为2g/L,硫酸铝浓度为30g/L,矿浆浓度为15-20%,尾矿溶液、阳离子800、硫酸铝溶液的配比为1500∶8∶20;将浓度为15-20%的尾矿溶液,在50-100r/min的速率下搅拌,然后将阳离子800加入尾矿溶液中,使其大量絮凝后再滴加浓度为30g/L的硫酸铝溶液使浑浊的矿浆继续絮凝澄清。
用本发明的方法对低品位碳酸锰矿浮选后的尾矿进行絮凝处理,可达到较理想的效果,能满足工业生产要求,对废物的再利用、减少环境污染及节约水资源等具有重要的意义。
具体实施方案
取浓度为15%的尾矿溶液1500ml,在50-100r/min的速率下搅拌,然后加入8ml浓度为2g/L的阳离子800,待矿浆中出现大量絮团后再滴加20ml浓度为30g/L的硫酸铝溶液,静置3分钟,可以观察到絮凝较快,沉降较快,溶液较澄清。抽滤后液体澄清,测定其浊度为12,水可回收循环使用,滤渣可用于生产水泥熟料。

Claims (1)

1.一种低品位碳酸锰矿浮选后尾矿絮凝处理方法,其特征在于是将阳离子800与硫酸铝溶液配合使用,阳离子800浓度为2g/L,硫酸铝浓度为30g/L,矿浆浓度为15-20%,尾矿溶液、阳离子800、硫酸铝溶液的配比为1500∶8∶20;将浓度为15-20%的尾矿溶液,在50-100r/min的速率下搅拌,然后将阳离子800加入尾矿溶液中,使其中悬浮的矿粒大量絮凝后再滴加浓度为30g/L的硫酸铝溶液使浑浊的矿浆继续絮凝澄清。
CN2011101157181A 2011-04-28 2011-04-28 一种低品位碳酸锰矿浮选后尾矿絮凝处理方法 Pending CN102225377A (zh)