CN102220462A - 无机环保水溶性淬火剂 - Google Patents
无机环保水溶性淬火剂 Download PDFInfo
- Publication number
- CN102220462A CN102220462A CN2011101767604A CN201110176760A CN102220462A CN 102220462 A CN102220462 A CN 102220462A CN 2011101767604 A CN2011101767604 A CN 2011101767604A CN 201110176760 A CN201110176760 A CN 201110176760A CN 102220462 A CN102220462 A CN 102220462A
- Authority
- CN
- China
- Prior art keywords
- quenching
- water
- soluble
- quenching agent
- inorganic environment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种无机环保水溶性淬火剂,适用于碳钢和合金钢工件的淬火,属于淬火介质技术领域,本发明是在以水为淬火介质基础上的改进,在水中加入溶解一定配比的碳酸钠、明矾、氯化钠和氢氧化铝,当工件浸入该介质后,在蒸汽膜阶段析出合成盐的晶体并立即爆裂,将蒸汽膜破坏,加速冷却,得到近于水、油之间的冷却速度,以满足不同材料和工件的淬火要求;本发明水性淬火剂无毒,无烟,无腐蚀性,不燃烧,使用安全,无环境污染;本发明的优点是提供了一种冷却速度快,淬火效果好,淬火工件体不裂纹,使用成本低,适用于各种淬火炉淬火的水溶性淬火剂。
Description
技术领域
本发明涉及一种无机环保水溶性淬火剂,尤其是涉及一种适用于碳钢和合金钢工件的淬火,属于淬火介质技术领域。
背景技术
目前传统热处理工序所采用的淬火介质为油类或水,油类适合用于中碳低合金钢,其冷却速度慢,容易出现淬火硬度不够,淬火层浅,烟雾污染等问题;而用水作为淬火介质,因在实际生产过程中水温波动大,且冷却速度快,工件表面很容易产生裂纹。
国内目前也有应用水溶性淬火剂的厂家,但其所含的有机物在生产过程中产生残炭及异味,不利于生产环境保护。
为了落实清洁生产,提高工件合格率,保护改善生产环境,并增加淬火剂在工业应用中的品质,用一种合格环保的无机淬火剂来装备相关企业,具有重要意义。
发明内容
本发明的目的是提供一种冷却速度快,淬火效果价,成本低且使用过程中无环境污染的无机环保水溶性淬火剂。
本发明的技术方案是:一种无机环保水溶性淬火剂,它是在水中加入碳酸钠、明矾、氯化钠和氢氧化铝溶解而成。经淬火生产对比后,其效果明显优于油淬火和水淬火。通过本发明既能满足材料的淬火深度,而表面还不会产生裂纹,且在生产过程中因本发明调配原料均是无机盐类,故无烟雾和气味产生,是一种环境友好型的淬火剂。
本发明无机环保水溶性淬火剂由下述重量份的原料配制而成:氯化钠5~10%,碳酸钠为5%,明矾为7~10%,氢氧化铝为0.5~2%,其余部分是干净的自来水。
配置时,将上述各原料计量好,按顺序先将氯化钠投入水中,充分搅拌待氯化钠溶解完全后,再将碳酸钠投入溶液中,并强烈搅拌20分钟,然后将氢氧化铝投入溶液中并搅拌30分钟,最后把明矾投入溶液中搅拌至完全溶解后即成本发明产品。
所述的氯化钠为工业级氯化钠,其纯度不应小于95%,所述的碳酸钠为工业级碳酸钠,其纯度不能小于90%,所述的氢氧化铝为高活性氢氧化铝,纯度大于99%,所述的明矾为碱式硫酸铝钾。
本发明能用于各种碳钢的高温淬火,也适用于合金钢和工具钢的热处理工艺。
本发明的有益效果是:提供一种冷却速度快,淬火效果佳,工作过程中无有害气体排放的低成本无机环保水溶性淬火剂。
具体实施方式
按氯化钠10%,碳酸钠5%,明矾为7%,氢氧化铝为0.5%,87.5%干净的自来水。按顺序先将氯化钠投入水中,充分搅拌待氯化钠溶解完全后,再将碳酸钠投入溶液中,并强烈搅拌20分钟,然后将氢氧化铝投入溶液中并搅拌30分钟,最后把明矾投入溶液中搅拌至完全溶解。
按氯化钠5%,碳酸钠5%,明矾为10%,氢氧化铝为2%,88%干净的自来水。按顺序先将氯化钠投入水中,充分搅拌待氯化钠溶解完全后,再将碳酸钠投入溶液中,并强烈搅拌20分钟,然后将氢氧化铝投入溶液中并搅拌30分钟,最后把明矾投入溶液中搅拌至完全溶解。
综上所述,以上仅为本发明的较佳实施例之一,并非用于限定本发明的保护范围,因此,凡在本发明的精神和原则之内所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。
Claims (2)
1.一种无机环保水溶性淬火剂,其特征是,所述的淬火剂由水、碳酸钠、明矾、氯化钠和氢氧化铝组成,配比的碳酸钠、明矾、氯化钠和氢氧化铝溶解在水中,其质量百分比氯化钠为5~10%,碳酸钠为5%,明矾为7~10%,氢氧化铝为0.5~2%,其余部分是干净的自来水。
2.根据权利要求1所述的无机环保水溶性淬火剂,其特征是,调整无机盐的浓度,可以取得不同的淬火结果。