CN102151726A - 钢管弯管热弯成型工艺及设备 - Google Patents

钢管弯管热弯成型工艺及设备 Download PDF

Info

Publication number
CN102151726A
CN102151726A CN2010105709177A CN201010570917A CN102151726A CN 102151726 A CN102151726 A CN 102151726A CN 2010105709177 A CN2010105709177 A CN 2010105709177A CN 201010570917 A CN201010570917 A CN 201010570917A CN 102151726 A CN102151726 A CN 102151726A
Authority
CN
China
Prior art keywords
steel pipe
pipe
running roller
hot bending
thruster
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010105709177A
Other languages
English (en)
Inventor
黄杰生
陈展宏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHUJIANG STEEL PIPE CO Ltd PANYU
Original Assignee
ZHUJIANG STEEL PIPE CO Ltd PANYU
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHUJIANG STEEL PIPE CO Ltd PANYU filed Critical ZHUJIANG STEEL PIPE CO Ltd PANYU
Priority to CN2010105709177A priority Critical patent/CN102151726A/zh
Publication of CN102151726A publication Critical patent/CN102151726A/zh
Pending legal-status Critical Current

Abstract

本发明钢管弯管热弯成型工艺及设备属于钢管制造和加工领域,先将需弯曲的钢管吊放到工位上,再由推送装置把钢管推出,伸出至中频感应加热圈前,导向辊装置的两组导向辊夹紧钢管,在垂直于钢管推出方向安装有水平弯管成型进给装置,并将进给装置上的侧推辊轮调整好与管端外圆接触,中频感应加热圈对钢管加热后,推送装置再把钢管向前推出,同时水平弯管成型进给装置上的侧推辊轮开始垂直于钢管推出方向对钢管成型进给,侧推辊轮对钢管热弯成型的切入点到达预先计算好的成型后的坐标点之后,侧推辊轮停止对钢管的切入进给,获得所需曲率的管件。本发明生产效率高,不受生产场地面积的局限,可以随意生产不同曲率半径的弯管。

Description

钢管弯管热弯成型工艺及设备
技术领域
本发明钢管弯管热弯成型工艺及设备属于钢管制造和加工领域,特别是涉及一种钢管弯管热弯成型工艺及设备。
背景技术
在管道铺设工程方面,由于地形多变,热弯管的应用十分广范和重要,而且在实地施工上对热弯管的曲率半径范围要求很广。但现在的热弯管生产企业中,对钢管热弯成型的工艺方法是先将钢管安装在导向辊装置上,通过旋臂回转装置上的丝杠丝母传动装置调整好弯管需要的弯曲半径,同时旋臂上夹紧座夹紧钢管突出中频感应加热圈的部分,然后采用中频感应加热圈对钢管加热到一定温度后进行弯曲,弯曲时以液压为动力,由推送装置把钢管向前推出,钢管受旋臂约束,则沿调整好的弯曲半径在加热处发生变形而弯曲,从而获得所需弯管管件。但这样的方法会受到机组旋臂回转半径、生产场地的面积的局限,不能生产大半径规格弯管,一般只能生产最大弯曲半径为9m~10m的弯管。
发明内容
本发明的目的在于克服现有技术的不足之处,而提供一种减少成型机组的占地面积,可生产任意弯曲半径的钢管弯管热弯成型工艺及设备。
本发明的目的是通过以下措施来达到的:先将需弯曲的钢管吊放到工位上,再由推送装置把钢管推出,伸出至中频感应加热圈前,导向辊装置的两组导向辊夹紧钢管,在垂直于钢管推出方向安装有水平弯管成型进给装置,并将进给装置上的侧推辊轮调整好与管端外圆接触,中频感应加热圈对钢管加热后,推送装置再把钢管向前推出,同时水平弯管成型进给装置上的侧推辊轮开始垂直于钢管推出方向对钢管成型进给,侧推辊轮对钢管热弯成型的切入点到达预先计算好的成型后的坐标点之后,侧推辊轮停止对钢管的切入进给,获得所需曲率的管件。
钢管本身与导向辊装置的两组导向辊装置以及水平弯管成型进给装置的侧推辊轮形成三点受力弯曲,当在推送装置的推力作用下,使在加热圈处的钢管发生渐进式的弯曲变形,从而获得所需曲率的管件,不会因旋臂回转半径和生产场地面积的局限,可以随意生产不同曲率半径的弯管。
中频感应加热圈对钢管加热到920±20°。
推送装置向前以推进速度为45±5mm/min的速度推出。
侧推辊轮以50±5mm/min速度垂直于钢管推出方向对钢管成型进给。
本发明的钢管弯管热弯成型设备是包括由推送装置、导向辊装置、中频感应加热圈组成,水平弯管成型进给装置包括由底座、侧推辊轮、丝杆丝母、减速机组成,丝杆丝母安装在底座上,在丝杆丝母上安装一对侧推辊轮,减速机连接丝杆丝母,侧推辊轮上部安装有辊轮。一对侧推辊轮相对安装在丝杆丝母上。
本发明生产效率高,不受生产场地面积的局限,可以随意生产不同曲率半径的弯管。
附图说明
附图1为本发明示意图。
附图2为本发明侧推辊轮结构示意图。
具体实施方式
下面结合附图和实施例对本发明作进一步说明。
图中:水平弯管成型进给装置1,钢管2,推送装置3,导向辊装置4,中频感应加热圈5,侧推辊轮6,丝杆丝母7,减速机8,辊轮9,侧推辊轮10。
如附图1、附图2所示,钢管弯管热弯成型工艺采用的设备是包括由推送装置3、导向辊装置4、中频感应加热圈5、水平弯管成型进给装置1组成,开始时先将需弯曲的钢管2吊放到工位上,再由推送装置3把钢管推出,伸出至中频感应加热圈5前1.8m处,导向辊装置4的两组导向辊夹紧钢管2,在垂直于钢管2推出方向安装有水平弯管成型进给装置1,并将进给装置上的侧推辊轮6调整好与管端外圆接触。中频感应加热圈5对钢管2加热到920±20℃后,推送装置3再把钢管2向前以推进速度为45±5mm/min的速度推出,同时水平弯管成型进给装置1上的侧推辊轮6开始以50±5mm/min速度垂直于钢管推出方向对钢管成型进给。当侧推辊轮6对钢管2热弯成型的切入点到达跟据订单要求的管件数据预先计算好的成型后的坐标点之后,侧推辊轮6停止对钢管的切入进给。钢管2本身与导向辊装置4的两组导向辊装置以及侧推辊轮6形成三点受力弯曲,当在推送装置3的推力作用下,使在加热圈处的钢管发生渐进式的弯曲变形。从而获得所需曲率管件。
如附图2所示,钢管弯管热弯成型设备包括由底座、侧推辊轮、丝杆丝母、减速机组成,丝杆丝母7安装在底座上,在丝杆丝母上安装侧推辊轮6和侧推辊轮10,减速机8连接丝杆丝母,侧推辊轮上部安装有辊轮9。一对侧推辊轮安装在丝杆丝母上,辊轮相对。减速机8与丝杆丝母相连接传动动力到侧推辊轮,使侧推辊轮在钢管热弯成型时对钢管成型进给。

Claims (4)

1.一种钢管弯管热弯成型工艺,先将需弯曲的钢管吊放到工位上,再由推送装置把钢管推出,伸出至中频感应加热圈前,导向辊装置的两组导向辊夹紧钢管,在垂直于钢管推出方向安装有水平弯管成型进给装置,并将进给装置上的侧推辊轮调整好与管端外圆接触,中频感应加热圈对钢管加热后,推送装置再把钢管向前推出,其特征是水平弯管成型进给装置上的侧推辊轮开始垂直于钢管推出方向对钢管成型进给,侧推辊轮对钢管热弯成型的切入点到达预先计算好的成型后的坐标点之后,侧推辊轮停止对钢管的切入进给,获得所需曲率的管件。
2.根据权利要求1所述的钢管弯管热弯成型工艺,其特征是中频感应加热圈对钢管加热到920±20°,推送装置向前以推进速度为45±5mm/min的速度推出,侧推辊轮以50±5mm/min速度垂直于钢管推出方向对钢管成型进给。
3.一种钢管弯管热弯成型设备,其特征是包括底座、侧推辊轮、丝杆丝母、减速机组成,丝杆丝母安装在底座上,在丝杆丝母上安装一对侧推辊轮,减速机连接丝杆丝母,侧推辊轮上部安装有辊轮。
4.根据权利要求3所述的钢管弯管热弯成型设备,其特征是一对侧推辊轮相对安装在丝杆丝母上。
CN2010105709177A 2010-11-24 2010-11-24 钢管弯管热弯成型工艺及设备 Pending CN102151726A (zh)