CN102013462A - 消除铅酸蓄电池极柱胶气泡的工艺及其装置 - Google Patents
消除铅酸蓄电池极柱胶气泡的工艺及其装置 Download PDFInfo
- Publication number
- CN102013462A CN102013462A CN201010552313XA CN201010552313A CN102013462A CN 102013462 A CN102013462 A CN 102013462A CN 201010552313X A CN201010552313X A CN 201010552313XA CN 201010552313 A CN201010552313 A CN 201010552313A CN 102013462 A CN102013462 A CN 102013462A
- Authority
- CN
- China
- Prior art keywords
- glue
- bubble
- firelock
- polar column
- battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明系提供一种消除铅酸蓄电池极柱胶气泡的工艺及其装置,所述工艺步骤具体如下:第一步:按照常规的铅酸蓄电池极柱胶滴加工序操作,确认铅酸蓄电池极柱胶滴加完毕,胶量适中。第二步:开启并调节火枪装置,使火枪装置喷头喷出的火焰呈淡蓝色。第三步:将火枪装置喷头喷出的火焰的外焰对准电池极柱胶,均匀快速的摆动喷头,确保每一个电池的极柱胶都能够烘烤到。第四步:每间隔静置5分钟后再烘烤一次极柱胶,极柱胶烘烤3次。第五步:检查极柱胶上是否有气泡,确保极柱胶无气泡后再将电池推进烘箱,进行后续的固化操作。本发明所述的工艺及其装置操作起来很是方便,速度快,生产效率高,提高了企业生产效率。
Description
技术领域
本发明涉及电池生产过程中消除气泡的工艺及其装置,尤其涉及消除铅酸蓄电池极柱胶气泡的工艺及其装置。
背景技术
在阀控密封铅酸蓄电池生产过程中,极柱胶是阀控式密封铅酸蓄电池必不可少的一部分,其主要作用是密封和标明端子的正负极性。但是由于其固有的特性,极柱胶主剂和固化剂混合搅拌之后,会产生大量的热量并产生气泡。这些气泡不但影响电池外观,而且会影响电池质量。传统的做法是用细针将这些气泡逐个挑破,该方法虽然解决了气泡的问题,但按照该方法操作起来很是不方便,速度慢,生产效率低下。针对于此,本发明改良了消除气泡的工艺,加快了气泡消除的速度,提高了企业生产效率。
发明内容
本发明的目的在于针对上述现有技术的不足之处,克服现有技术的缺陷,提出了一种用于消除铅酸蓄电池极柱胶气泡的工艺及其装置,可以快速的消除极柱胶中的气泡。
本发明采用如下技术方案:
一种消除铅酸蓄电池极柱胶气泡的工艺,其特征在于:所述工艺步骤具体如下:
第一步:给铅酸蓄电池极柱进行胶滴工序,确认铅酸蓄电池极柱胶滴加完毕,胶量适中;
第二步:开启并调节火枪装置,使火枪装置喷头喷出的火焰呈淡蓝色。
第三步:将火枪装置喷头喷出的火焰的外焰对准电池极柱胶,均匀快速的摆动喷头,确保每一个电池的极柱胶都能够烘烤到。
第四步:每间隔静置5分钟后再烘烤一次极柱胶,极柱胶烘烤3次。
第五步:停止烘烤,检查极柱胶上是否有气泡;
第六步:如果还有气泡,则继续用火枪装置烘烤,直至完全消除气泡;如果没气泡则将电池推进烘箱,进行后续的固化操作。
一种消除铅酸蓄电池极柱胶气泡的装置,所述装置为火枪装置,火枪装置包含有液化气罐,液化气罐通过煤气专用管连接焊枪,煤气专用管靠近液化气罐端设有减压阀,焊枪前端设有枪头罩。
本发明的优点在于:
本发明改良了消除气泡的工艺,加快了气泡消除的速度,本发明所述的工艺及其装置操作起来很是方便,速度快,生产效率高,提高了企业生产效率。
附图说明
图1是工艺流程图;
图2是火枪装置的结构示意图。
具体实施方式
为能进一步了解本发明的特征、技术手段以及所达到的具体目的、功能,下面对本发明作进一步详细描述。
一种消除铅酸蓄电池极柱胶气泡的工艺,所述工艺步骤具体如下:
第一步:给铅酸蓄电池极柱进行胶滴工序,确认铅酸蓄电池极柱胶滴加完毕,胶量适中。此步骤是阀控密封铅酸蓄电池生产过程中,滴加极柱胶的工艺,在滴加极柱胶后,由于极柱胶固有的特性,极柱胶主剂和固化剂混合搅拌之后,会产生大量的热量并产生气泡。这些气泡不但影响电池外观,而且会影响电池质量。传统的做法是用细针将这些气泡逐个挑破,该方法虽然解决了气泡的问题,但按照该方法操作起来很是不方便,速度慢,生产效率低下。针对于此,本发明尝试用高温火焰烘烤的方法来消除气泡,具体见如下步骤:
第二步:开启并调节火枪装置,使火枪装置喷出的火焰呈淡蓝色。
第三步:将火枪装置喷出的火焰的外焰对准电池极柱胶,均匀快速的摆动喷头,确保每一个电池的极柱胶都能够烘烤到,电池加了极柱胶后,通过火焰的快速烘烤,可以使极柱胶内的气泡膨胀破裂,气泡可以迅速消除干净。
此步骤注意事项:煤气火苗不得停留在某一点长时间烘烤,否则会烘烤坏电池壳。
第四步:每间隔静置5分钟后再烘烤一次极柱胶,极柱胶烘烤3次。
第五步:停止烘烤,检查极柱胶上是否有气泡;
第六步:如果还有气泡,则继续用火枪装置烘烤,直至完全消除气泡;如果没气泡则将电池推进烘箱,进行后续的固化操作。
一种消除铅酸蓄电池极柱胶气泡的装置,所述装置为火枪装置,火枪装置包含有液化气罐1,液化气罐1通过煤气专用管3连接焊枪4,煤气专用管3靠近液化气罐1端设有减压阀2,减压阀2可以调节气压,必不可少,焊枪4前端设有枪头罩5,枪头罩5可以更好的确保焊枪4喷出的火焰达到最好的效果。
该装置是特为本发明所述的消除极柱胶气泡的工艺所设置的,由液化气罐1与焊枪4等连接而成,制作简单,操作方便。
综上所述,本发明通过所述火枪装置替代了现有技术中的人工针挑气泡,加快了工作效率,节约成本,给企业带来显著的经济效益。
以上所述实施例仅表达了本发明的一种实施方式,其描述较为具体和详细,但并不能因此而理解为对本发明范围的限制。应当指出的是,对于本领域的普通技术人员来说,在不脱离本发明构思的前提下,还可以做出若干变形和改进,这些都属于本发明的保护范围。因此,本发明的保护范围应以所附权利要求为准。
Claims (2)
1.一种消除铅酸蓄电池极柱胶气泡的工艺,其特征在于:所述工艺步骤具体如下:
第一步:给铅酸蓄电池极柱进行胶滴工序,确认铅酸蓄电池极柱胶滴加完毕,胶量适中;
第二步:开启并调节火枪装置,使火枪装置喷出的火焰呈淡蓝色;
第三步:将火枪装置喷出的火焰的外焰对准电池极柱胶,均匀快速的摆动喷头,确保每一个电池的极柱胶都能够烘烤到;
第四步:每间隔静置5分钟后再烘烤一次极柱胶,极柱胶烘烤3次;
第五步:停止烘烤,检查极柱胶上是否有气泡;
第六步:如果还有气泡,则继续用火枪装置烘烤,直至完全消除气泡;如果没气泡则将电池推进烘箱,进行后续的固化操作。
2.一种消除铅酸蓄电池极柱胶气泡的装置,其特征在于:所述装置为火枪装置,火枪装置包含有液化气罐(1),液化气罐(1)通过煤气专用管(3)连接焊枪(4),煤气专用管(3)靠近液化气罐(1)端设有减压阀(2),焊枪(4)前端设有枪头罩(5)。