CN101934306A - 花纹钢板的平整方法 - Google Patents

花纹钢板的平整方法 Download PDF

Info

Publication number
CN101934306A
CN101934306A CN 201010270346 CN201010270346A CN101934306A CN 101934306 A CN101934306 A CN 101934306A CN 201010270346 CN201010270346 CN 201010270346 CN 201010270346 A CN201010270346 A CN 201010270346A CN 101934306 A CN101934306 A CN 101934306A
Authority
CN
China
Prior art keywords
steel plate
checkered steel
straightener
checkered
levelling method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010270346
Other languages
English (en)
Inventor
张祝得
孙文填
李胜
王建轲
张汉全
胡明樟
李隆基
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGZHOU ZHUJIANG STEEL Co Ltd
Original Assignee
GUANGZHOU ZHUJIANG STEEL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGZHOU ZHUJIANG STEEL Co Ltd filed Critical GUANGZHOU ZHUJIANG STEEL Co Ltd
Priority to CN 201010270346 priority Critical patent/CN101934306A/zh
Publication of CN101934306A publication Critical patent/CN101934306A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种花纹钢板的平整方法,该方法包括有:将整卷的花纹钢板安装于开卷机上;花纹钢板通过入口夹送辊,进入到矫直机内;调整矫直机的上辊的下压力使花纹钢板在矫直机内产生多次变形;通过出口夹送辊将花纹钢板卷于卷取机上。本发明利用矫直机与开卷机之间的张力将花纹钢板拉伸,并利用矫直机上辊对花纹钢板同一部位的多次压力,使花纹钢板产生多次变形,该多次变形恰能够修复花纹钢板在热轧过程中的浪型,消除花纹钢板的缺陷,使其变的平整,且不会产生其他缺陷。

Description

花纹钢板的平整方法
技术领域
本发明涉及一种钢板的平整方法,尤其是指一种热轧花纹钢板的平整方法。
背景技术
花纹钢板亦称为网纹钢板,其是指表面具有菱形或凸(或凹)棱的钢板。花纹钢板具有良好的防滑和装饰作用,且组合型花纹板的防滑能力、抗弯能力、节约金属量及外观等方面的综合效果,均明显优于单一型花纹板。花纹钢板广泛用于造船、锅炉、汽车、拖拉机、火车车厢及建筑等行业。
近年来随着市场需求的变化,要求热轧花纹钢板的厚度越来越薄,由于板材热加工工艺的特殊性,热轧薄规格板材很容易产生浪形缺陷。一般的薄规格热轧板可以通过平整机修复板型缺陷,而花纹钢板由于板面上存在花纹,无法采用一般的平整工艺来修复板型缺陷。如何消除热轧薄规格花纹钢板的浪型缺陷,提高产品质量,是热轧花纹钢板生产企业面临的一个技术难题。
因此,本发明提供一种花纹钢板的平整方法,其能够克服现有技术的缺陷,在平整花纹钢板的基础上,不产生新的缺陷。
发明内容
本发明提供一种花纹钢板的平整方法,其利用花纹钢板在压力和张力的作用下产生一定的变形,恰用于修复花纹钢板在热轧过程中产生的浪型缺陷。
本发明是这样实现的:
一种花纹钢板的平整方法,该方法包括有:
(1)将整卷的花纹钢板安装于开卷机上;
(2)花纹钢板通过入口夹送辊,进入到矫直机内;
(3)调整矫直机的上辊的下压力使花纹钢板在矫直机内产生多次变形;
(4)通过出口夹送辊将花纹钢板卷于卷取机上。
利用矫直机上辊对花纹钢板同一部位的多次压力,使花纹钢板产生多次变形,该多次变形恰能够修复花纹钢板在热轧过程中的浪型,消除花纹钢板的缺陷,使其变的平整,且不会产生其他缺陷。
为了更进一步达到消除该花纹钢板的浪型,在步骤(2)时,调节矫直机与开卷机之间的张力,使通过该开卷机送入该矫直机的花纹钢板受到拉伸。
优选的是,该开卷机与该矫直机之间的张力值范围为0-20t。
优选的是,该矫直机的上辊对该花纹钢板施加压力,其压力值范围为0-8t,根据花纹钢的厚度及浪型缺陷的弯曲程度调整压力的大小。
优选的是,该压力随该张力变大而依次变小,反之亦然,该张力可随该压力的变大而变小。
优选的是,该花纹钢板在该矫直机内受到至少5次弯曲。
优选的是,该矫直机为15辊矫直机,该花纹钢板在该矫直机内受到5-15次弯曲。
经过开卷机的张力和矫直机的压力之后,该花纹钢板的长度延伸0-3%。
本发明的技术效果:
本发明一种花纹钢的平整方法,其通过开卷机对花纹钢施加张力,再通过矫直机的上辊对花纹钢的压力,使花纹钢在热轧时产生的浪型经过拉伸和多次压力之后,能够修复,消除花纹钢在热热轧时产生的缺陷。
附图说明
图1为本发明花纹钢板的平整方法的流程图;
图2为本发明花纹钢板的平整方法的工作示意图。
具体实施方式
下面结合附图对本发明的实施例进行详细说明:
参阅图1及图2。本发明一种花纹钢板的平整方法,其包括有如下步骤:
步骤一100:将整卷的花纹钢板安装于开卷机上;
步骤二200:花纹钢板通过入口夹送辊,进入到矫直机内;
步骤三300:调整矫直机的上辊的下压力使花纹钢板在矫直机内产生多次变形;
步骤四400:通过出口夹送辊将花纹钢板卷于卷取机上。
步骤一100通过开卷机1将整卷的花纹钢板10依次展开;步骤二200花纹钢板10通过入口夹送辊的上辊6和下辊2的作用,将花纹钢板10送入矫直机8,此时,通过调节矫直机8的控制系统调整矫直机8与开卷机1之间的张力,使花纹钢板10收到拉伸,在一定程度上,消除浪型缺陷;花纹钢板10进入矫直机8后,花纹钢板10在矫直机8内快速上、下运动,根据花纹钢板10不同的弯曲程度,再通过调整矫直机8的油缸的动力调节上辊3对花纹钢板10的压力,使花纹钢板10产生多次变形而恢复平整;最后再通过出口夹送辊的上辊7和下辊4的作用,将花纹钢板卷于卷取机5上。经过开卷机1与矫直机8对花纹钢板10的张力的作用,及矫直机8的上辊3对花纹钢板10的压力作用,花纹钢板10的浪型消除,花纹钢板的长度延伸0-3%。
优选的是,该开卷机与该矫直机之间具有张力,其张力值范围为0-20t,该矫直机10的上辊对该花纹钢板施加的压力值范围为0-8t,可根据不同型号的花纹钢板、或花纹钢板的变形程度,选取不同的压力值和张力值。并且,该压力随该张力的变大而变小;该张力随该压力的变大而变小。例如,当张力为1t时,压力位5t;当张力为4t时,压力位3t;当张力为8t时,压力为2t。
为了适应不同型号的花纹钢板,可根据花纹钢板10的型号不同选取不同的矫直机,使花纹钢板10在矫直机内收到不同个数的上辊的压力而弯曲,因而,对花纹钢板10的修复程度亦不同。本发明优选实施例矫直机8优选为15辊矫直机,该花纹钢板10在该15辊矫直机8内受到5-15次弯曲变形,使花纹钢板恰能恢复平整,消除热轧过程中的产生的浪型缺陷。
以上仅为本发明的具体实施例,并不以此限定本发明的保护范围;在不违反本发明构思的基础上所作的任何替换与改进,均属本发明的保护范围。

Claims (9)

1.一种花纹钢板的平整方法,其特征在于,该方法包括有:
(1)将整卷的花纹钢板安装于开卷机上;
(2)花纹钢板通过入口夹送辊,进入到矫直机内;
(3)调整矫直机的上辊的下压力使花纹钢板在矫直机内产生多次变形;
(4)通过出口夹送辊将花纹钢板卷于卷取机上。
2.如权利要求1所述的花纹钢板的平整方法,其特征在于,在步骤(2)时,调节矫直机与开卷机之间的张力,使通过该开卷机送入该矫直机的花纹钢板受到拉伸。
3.如权利要求2所述的花纹钢板的平整方法,其特征在于,该开卷机与该矫直机之间的张力值范围为0-20t。
4.如权利要求1所述的花纹钢板的平整方法,其特征在于,该矫直机的上辊对该花纹钢板施加的压力值范围为0-8t。
5.如权利要求2或3或4所述的花纹钢板的平整方法,其特征在于,该压力随该张力的变大而变小。
6.如权利要求2或3或4所述的花纹钢板的平整方法,其特征在于,该张力随该压力的变大而变小。
7.如权利要求1-4任一项所述的花纹钢板的平整方法,其特征在于,该花纹钢板在该矫直机内受到至少5次弯曲。
8.如权利要求7所述的花纹钢板的平整方法,其特征在于,该矫直机为15辊矫直机,该花纹钢板在该矫直机内受到5-15次弯曲。
9.如权利要求1所述的花纹钢板的平整方法,其特征在于,该花纹钢板的长度延伸0-3%。
CN 201010270346 2010-08-31 2010-08-31 花纹钢板的平整方法 Pending CN101934306A (zh)