CN101789655A - 发电机变流器馈电状态下转子抗老化绝缘设计 - Google Patents
发电机变流器馈电状态下转子抗老化绝缘设计 Download PDFInfo
- Publication number
- CN101789655A CN101789655A CN 201010119984 CN201010119984A CN101789655A CN 101789655 A CN101789655 A CN 101789655A CN 201010119984 CN201010119984 CN 201010119984 CN 201010119984 A CN201010119984 A CN 201010119984A CN 101789655 A CN101789655 A CN 101789655A
- Authority
- CN
- China
- Prior art keywords
- generator converter
- insulation design
- aging insulation
- slot
- tape
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种发电机变流器馈电状态下转子抗老化绝缘设计,包括槽楔、槽绝缘、扁铜线、云母带、浸漆玻璃丝带、层间垫条和槽底垫条。本发明发电机变流器馈电状态下转子抗老化绝缘设计的层间垫条和槽底垫条的材质采用双马来酰亚胺层压玻璃布板,此种材料的强度、柔韧性等性能都优于普通的玻璃层压板。槽楔选用引拔槽楔,此种材料在200℃时,弯曲强度≥350MPa,抗劈强度≥2000N/10mm,沿面耐电压12kY/1min,表面电阻≥1×1010Ω,这样能够达到设计要求。
Description
技术领域
本发明涉及一种发电机变流器馈电状态下转子抗老化绝缘设计。
背景技术
在以往的转子硬绕组的绝缘选择上,一般是端部绝缘为聚酰亚胺薄膜,外层为无碱带;直线部分绝缘为粉云母箔,第二层为聚酰亚胺薄膜,最外层为硅有机上胶玻璃带;但用于风力发电机上时,这种绝缘结构不能满足设计要求;由于风力发电机在变流器馈电状态下,转子产生高频脉冲电流,在此电流长期作用下,绝缘材料老化速度加快,从而电机寿命降低,这样对转子绝缘材料的选取来说就十分重要。
发明内容
本发明的目的是提供一种可使转子绝缘性大大提高,抗老化的发电机变流器馈电状态下转子抗老化绝缘设计。
本发明为实现上述目的所采用的技术方案是:一种发电机变流器馈电状态下转子抗老化绝缘设计,其特征在于:包括槽楔、槽绝缘、浸漆玻璃丝带、云母带、扁铜线、层间垫条和槽底垫条。
所述层间垫条和槽底垫条为双马来酰亚胺层压玻璃布板。
所述槽楔为引拔槽楔。
所述云母带为耐电晕聚酰亚胺薄膜少胶粉云母带。
本发明发电机变流器馈电状态下转子抗老化绝缘设计的优点在于:
1、层间垫条和槽底垫条的材质采用9334双马来酰亚胺层压玻璃布板,此种材料的强度、柔韧性等性能都优于普通的玻璃层压板。槽楔选用3955引拔槽楔,此种材料在200℃时,弯曲强度≥350Mpa,抗劈强度≥2000N/10mm,沿面耐电压12kV/1min,表面电阻≥1×1010Ω,这样能够达到设计要求。
2、槽绝缘选取的是两层0.2厚的NHN,槽内放置两层NHN后,即可以起到绝缘作用,也可避免扁铜线外层绝缘在穿线时被破坏,以往会加一层聚酰亚胺薄膜,由于此种材料的耐电晕性能差,转子线圈穿过铁心时,容易将其破坏。
3、扁铜线外的第一层绝缘材料为耐电晕聚酰亚胺薄膜少胶粉云母带(DY7329B-1),此种材料在温度90℃,电压3kV,频率20kHz,脉冲上升时间400ns等条件下试验,式样至终止时间未发生击穿。扁铜线最外层绑扎浸漆玻璃丝带,以保护里层绝缘。
附图说明
下面结合附图和具体实施方式对本发明作进一步说明。
图1是本发明发电机变流器馈电状态下转子抗老化绝缘设计结构图。
具体实施方式
如图1所示,该发电机变流器馈电状态下转子抗老化绝缘设计,包括槽楔1、槽绝缘2、扁铜线5、云母带4、浸漆玻璃丝带3、层间垫条6和槽底垫条7,该层间垫条6和槽底垫条7为双马来酰亚胺层压玻璃布板,槽楔为引拔槽楔,云母带为耐电晕聚酰亚胺薄膜少胶粉云母带。
该层间垫条6和槽底垫条7的材质均为9334双马来酰亚胺层压玻璃布板,此种材料的强度、柔韧性等性能都优于普通的玻璃层压板。槽楔选用3955引拔槽楔,此种材料在200℃时,弯曲强度≥350Mpa,抗劈强度≥2000N/10mm,沿面耐电压12kV/1min,表面电阻≥1×1010Ω,这样能够达到设计要求。槽绝缘选取的是两层0.2厚的NHN,槽内放置两层NHN后,即可以起到绝缘作用,也可避免扁铜线外层绝缘在穿线时被破坏,以往会加一层聚酰亚胺薄膜,由于此种材料的耐电晕性能差,转子线圈穿过铁心时,容易将其破坏。扁铜线外的第一层绝缘材料为耐电晕聚酰亚胺薄膜少胶粉云母带(DY7329B-1),此种材料在温度90℃,电压3kV,频率20kHz,脉冲上升时间400ns等条件下试验,式样至终止时间未发生击穿。扁铜线最外层绑扎浸漆玻璃丝带,以保护里层绝缘。采用上诉绝缘材料后,再采用真空压力浸漆,使得转子绝缘性能大大提高,以满足设计需要。
Claims (4)
1.一种发电机变流器馈电状态下转子抗老化绝缘设计,其特征在于:包括槽楔、槽绝缘、扁铜线、云母带、浸漆玻璃丝带、层间垫条和槽底垫条。
2.根据权利要求1所述的一种发电机变流器馈电状态下转子抗老化绝缘设计,其特征在于:所述层间垫条和槽底垫条为双马来酰亚胺层压玻璃布板。
3.根据权利要求1所述的一种发电机变流器馈电状态下转子抗老化绝缘设计,其特征在于:所述槽楔为引拔槽楔。
4.根据权利要求1所述的一种发电机变流器馈电状态下转子抗老化绝缘设计,其特征在于:所述云母带为耐电晕聚酰亚胺薄膜少胶粉云母带。