CN101780642B - 耐高温磨损复合导位托辊的制备方法 - Google Patents
耐高温磨损复合导位托辊的制备方法 Download PDFInfo
- Publication number
- CN101780642B CN101780642B CN2010101263701A CN201010126370A CN101780642B CN 101780642 B CN101780642 B CN 101780642B CN 2010101263701 A CN2010101263701 A CN 2010101263701A CN 201010126370 A CN201010126370 A CN 201010126370A CN 101780642 B CN101780642 B CN 101780642B
- Authority
- CN
- China
- Prior art keywords
- powder
- carrying roller
- carrier roller
- guide carrier
- resistant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (3)