CN101713004B - Method for curling fine fur - Google Patents

Method for curling fine fur Download PDF

Info

Publication number
CN101713004B
CN101713004B CN200910175442A CN200910175442A CN101713004B CN 101713004 B CN101713004 B CN 101713004B CN 200910175442 A CN200910175442 A CN 200910175442A CN 200910175442 A CN200910175442 A CN 200910175442A CN 101713004 B CN101713004 B CN 101713004B
Authority
CN
China
Prior art keywords
fur
pelage
percent
curling
pressure
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN200910175442A
Other languages
Chinese (zh)
Other versions
CN101713004A (en
Inventor
李敬勇
郭艳青
郗铁庄
武艳娥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HUASI HOLDING COMPANY LIMITED
Original Assignee
Huasi Agricultural Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Huasi Agricultural Development Co Ltd filed Critical Huasi Agricultural Development Co Ltd
Priority to CN200910175442A priority Critical patent/CN101713004B/en
Publication of CN101713004A publication Critical patent/CN101713004A/en
Application granted granted Critical
Publication of CN101713004B publication Critical patent/CN101713004B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a method for curling fine fur pelage, which comprises the following steps: 1) preparing reduction processing solution comprising 18 to 22 percent of thioglycollic acid, 38 to 42 percent of ammonia water, 18 to 22 percent of sulfated castor oil and 18 to 22 percent of water; 2) brushing the prepared solution on the fine fur pelage uniformly, and standing the brushed fine fur pelage for 2.5 to 3.5 hours; 3) pressing the reduced fur pelage for 5 minutes by using a pressure machine at the temperature of between 58 and 62 DEG C under the pressure of between 1 and 2 atm; 4) spraying 28 to 32 percent hydrogen peroxide solution after iron extension; and 5) drying, finishing and packaging for warehousing. In the reduced and oxidized pelage, disulfide bonds among keratin chains of fur are broken, so that the fur acquires plasticity, is easy to form, and is stable in curling patterns, washable and friction resistant. In addition, the processing temperature and processing pressure are reduced, so that flipe is soft and good in plasticity.

Description

Method for curling fine fur pelage
Affiliated technical field
The invention belongs to a kind of treatment process of animal skin, is to relate to a kind of method for curling fine fur pelage particularly.
Background technology
In industry, usually mink skin, raw fox skin, raccoon fur, raw weasel skin, rabbit etc. are referred to as thin skin, and the skin of animals such as ox, horse, sheep, pig, dog is called tertia.In the prior art, the processing that thin fur is curled is to utilize thermodynamics, adopts pressing machine under 150 ℃ of high temperature, high pressure 4-5atm, time 15min condition, to press, and makes thin fur curved by rolling, carries out the later stage arrangement after the pressure, beats the chi warehouse-in.The deficiency of its existence is: the fleece of just under condition under the physics HTHP, handling, and the feather keratin disulfide linkage of hair does not rupture, the just simple and mechanical bending of hair, so the flower shape of curling is unstable, not water-fast washing, not rub resistance.And the dermatotome that HTHP is processed down is harder, and plasticity-is bad.
Summary of the invention
The present invention's purpose is to overcome the above-mentioned deficiency of prior art, and a kind of thin fur new method for processing that is curled is provided, the frizzle skin of its production, and the flower shape of curling is stable, water-fastly washes, rub resistance, and dermatotome is soft, and plasticity-is good.
For realizing above-mentioned purpose, method for curling fine fur pelage of the present invention is taked following steps:
1. dispose the reduction treatment soln: ethyl thioglycollic acid 18-22%; Ammoniacal liquor 38-42%; Sulfated castor oil 18-22%; Water 18-22%;
2. use the solution of being joined to brush on thin fur quilt quiet putting 2.5~3.5 hours uniformly;
With pressing machine under temperature 58-62 ℃, pressure 1-2atm condition, the fur of handling through reduction is carried out pressing treatment 5min;
4. press the hydrogen peroxide solution of stretching back spray 28-32% on fleece;
5. carry out the later stage arrangement after the drying, beat the chi warehouse-in.
The present invention takes technique scheme, has following beneficial effect: the present invention handles the back fleece through reduction-oxidation, and the Keratin sulfate interchain disulfide bonds of hair makes hair obtain a plasticity, and easy-formation, can obtain to stablize, water-fastly washes, the curling colored shape of rub resistance.In addition, hard because the dermatotome fiber can become tight under HTHP, so the present invention reduced treatment temp and pressure, makes the dermatotome softness, plasticity-is good.
Embodiment
Below in conjunction with embodiment the present invention is described in detail.
Embodiment 1:
Method for curling fine fur pelage of the present invention is taked following steps:
1. dispose the reduction treatment soln: ethyl thioglycollic acid 18%; Ammoniacal liquor 42%; Sulfated castor oil 22%; Water 18%;
2. use the solution of being joined to brush on thin fur quilt quiet putting 2.5 hours uniformly;
With pressing machine under 58 ℃ of temperature, pressure 1atm condition, the fur of handling through reduction is carried out pressing treatment 5min;
4. press the hydrogen peroxide solution of stretching back spray 28% on fleece;
5. carry out the later stage arrangement after the drying, beat the chi warehouse-in.
Embodiment 2:
Method for curling fine fur pelage of the present invention is taked following steps:
1. dispose the reduction treatment soln: ethyl thioglycollic acid 20%; Ammoniacal liquor 40%; Sulfated castor oil 20%; Water 20%;
2. use the solution of being joined to brush on thin fur quilt quiet putting 3 hours uniformly;
With pressing machine under 60 ℃ of temperature, pressure 1.5atm condition, the fur of handling through reduction is carried out pressing treatment 5min;
4. press the hydrogen peroxide solution of stretching back spray 30% on fleece;
5. carry out the later stage arrangement after the drying, beat the chi warehouse-in.
Embodiment 3:
Method for curling fine fur pelage of the present invention is taked following steps:
1. dispose the reduction treatment soln: ethyl thioglycollic acid 22%; Ammoniacal liquor 38%; Sulfated castor oil 18%; Water 22%;
2. use the solution of being joined to brush on thin fur quilt quiet putting 3.5 hours uniformly;
With pressing machine under 62 ℃ of temperature, pressure 2atm condition, the fur of handling through reduction is carried out pressing treatment 5min;
4. press the hydrogen peroxide solution of stretching back spray 32% on fleece;
5. carry out the later stage arrangement after the drying, beat the chi warehouse-in.

Claims (2)

1. method for curling fine fur pelage is characterized in that it takes following steps:
1) configuration reduction treatment soln: Thiovanic acid 18-22%; Ammoniacal liquor 38-42%; Sulfated castor oil 18-22%; Water 18-22%;
2) use the solution of being joined to brush on thin fur quilt quiet putting 2.5~3.5 hours uniformly;
3) with pressing machine under temperature 58-62 ℃, pressure 1-2atm condition, the fur of handling through reduction is carried out pressing treatment 5min;
4) press the hydrogen peroxide solution of stretching back spray 28-32% on fleece;
5) carry out the later stage arrangement after the drying, beat the chi warehouse-in.
2. a kind of method for curling fine fur pelage according to claim 1 is characterized in that it takes following steps:
1) configuration reduction treatment soln: Thiovanic acid 20%; Ammoniacal liquor 40%; Sulfated castor oil 20%; Water 20%;
2) use the solution of being joined to brush on thin fur quilt quiet putting 3 hours uniformly;
3) with pressing machine under 60 ℃ of temperature, pressure 1.5atm condition, the fur of handling through reduction is carried out pressing treatment 5min;
4) press the hydrogen peroxide solution of stretching back spray 30% on fleece;
5) carry out the later stage arrangement after the drying, beat the chi warehouse-in.
CN200910175442A 2009-11-18 2009-11-18 Method for curling fine fur Active CN101713004B (en)