Prior art keywords
parts
portions
silicon rubber
rubber
molar content
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2008101961960A
Other languages
English (en)
Other versions
CN101654558A (zh
Inventor
王栋葆
徐文俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU TIANCHEN NEW MATERIALS CO., LTD.
Original Assignee
JIANGSU TIANCHENG SILICON CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU TIANCHENG SILICON CO Ltd filed Critical JIANGSU TIANCHENG SILICON CO Ltd
Priority to CN2008101961960A priority Critical patent/CN101654558B/zh
Publication of CN101654558A publication Critical patent/CN101654558A/zh
Application granted granted Critical
Publication of CN101654558B publication Critical patent/CN101654558B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Organic Insulating Materials (AREA)
  • Compositions Of Macromolecular Compounds (AREA)

Abstract

本发明涉及硅橡胶材料的制造,具体是一种用于电气设备绝缘子的绝缘子硅橡胶及其制造方法。该绝缘子硅橡胶其原料组成的重量份为:乙烯基摩尔含量1%的生胶10-25、乙烯基摩尔含量0.14%的生胶60-100、气相白炭黑40-60、二甲基二甲氧基硅烷5-10、氢氧化铝100-300、乙烯基三甲氧基硅烷1-3、二甲基硅油2-4、钛酸酯偶联剂1-3。本发明的产品经过实际检测具有良好的绝缘性能,同时具有够的硬度、强度,不易变形,完全能够满足高压电气绝缘子的使用要求。

Description

绝缘子硅橡胶及其制造方法
技术领域
本发明涉及硅橡胶材料的制造,具体是一种用于电气设备绝缘子的绝缘子硅橡胶及其制造方法。
背景技术
硅橡胶具备良好的耐高低温、耐臭氧、耐候性、绝缘性及生产惰性等很多优异的性能,在国民经济的各个领域有着广泛的应用。硅橡胶本身的特性以及其优异的加工成型性能决定了它有条件成为传统电气绝缘子的替代品。虽然硅橡胶本身即具有较好的电气性能,但是要应用在高压电气方面,还需要针对其综合性能指标进行改性处理,因此,研究绝缘子硅橡胶具有十分积极的意义。
发明内容
本发明所要解决的技术问题是,提供一种绝缘能力强,同时具有较好的硬度、强度并且不易变形的绝缘子硅橡胶及其制造方法。
本发明的绝缘子硅橡胶其原料组成的重量份为:
乙烯基摩尔含量1%的生胶        10-25
乙烯基摩尔含量0.14%的生胶     60-100
气相白炭黑                     40-60
二甲基二甲氧基硅烷             5-10
氢氧化铝                       100-300
乙烯基三甲氧基硅烷             1-3
二甲基硅油        2-4
钛酸酯偶联剂     1-3。
本发明的制造方法是基于上述的原料组成,其步骤依次为:
a.将乙烯基摩尔含量为1%的甲基乙烯基生胶20份,与乙烯基摩尔含量为0.14%的甲基乙烯基生胶70份在捏合机中搅拌2-4分钟;
b.将白炭黑45份和二甲基二甲氧基硅烷8份分多次加入,每次加入后充分搅拌,得到硅橡胶混炼胶;
c.加入氢氧化铝280份、乙烯基三甲氧基硅烷3份、二甲基硅油3份、钛酸酯偶联剂2份捏合成型;
d.捏合成型后,升温到150℃,抽真空,通冷却水降温到80℃,出胶;
f.出胶后冷却至室温,得到产品。
本发明的产品经过实际检测具有良好的绝缘性能,同时具有足够的硬度、强度,不易变形,完全能够满足高压电气绝缘子的使用要求。
具体实施方式
本发明的实施例经过以下步骤制造绝缘子硅橡胶,
a.将乙烯基摩尔含量为1%的甲基乙烯基生胶,与乙烯基摩尔含量为0.14%的甲基乙烯基生胶在捏合机中搅拌2-4分钟;
b.将白炭黑和二甲基二甲氧基硅烷分三次加入,每次加入后搅拌20分钟,得到力学性能优异的硅橡胶混炼胶;
c.加入氢氧化铝,捏合捏合60min,温度控制在130度以下;
d.捏合成型后,升温到150度,抽真空,通冷却水降温到80度,出胶;
F,出胶后冷却至室温,得到产品。使用过程中可再加入硫化剂硫化,在170摄氏度下硫化5分钟,200摄氏度二次硫化4小时。
上述原材料的重量份数为:
乙烯基摩尔含量1%的生胶     23份
乙烯基摩尔含量0.14%的生胶  85份
气相白炭黑                  50份
二甲基二甲氧基硅烷          8份
氢氧化铝                    220份
乙烯基三甲氧基硅烷          2份
二甲基硅油                  3份
钛酸酯偶联剂                3份。
对上述实施例制造的绝缘子硅橡胶,以1mm试片测试绝缘性能,性能如下表:
Figure GSB00000396742300031

Claims (2)

1.一种绝缘子硅橡胶,其特征是:其原料组成的重量份为,
乙烯基摩尔含量1%的生胶         10-25
乙烯基摩尔含量0.14%的生胶      60-100
气相白炭黑                     40-60
二甲基二甲氧基硅烷              5-10
氢氧化铝                       100-300
乙烯基三甲氧基硅烷              1-3
二甲基硅油                     2-4
钛酸酯偶联剂                   1-3。
2.一种如权利要求1所述的绝缘子硅橡胶的制造方法,其特征是:其步骤依次为,
a. 将乙烯基摩尔含量为1%的甲基乙烯基生胶20份,与乙烯基摩尔含量为0.14%的甲基乙烯基生胶70份在捏合机中搅拌2-4分钟;
b. 将白炭黑45份和二甲基二甲氧基硅烷8份分多次加入,每次加入后充分搅拌,得到硅橡胶混炼胶;
c. 加入氢氧化铝280份、乙烯基三甲氧基硅烷3份、二甲基硅油3份、钛酸酯偶联剂2份捏合成型;
d. 捏合成型后,升温到150℃,抽真空,通冷却水降温到80℃,出胶;
f. 出胶后冷却至室温,得到产品。
CN2008101961960A 2008-09-19 2008-09-19 绝缘子硅橡胶及其制造方法 Expired - Fee Related CN101654558B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2008101961960A CN101654558B (zh) 2008-09-19 2008-09-19 绝缘子硅橡胶及其制造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2008101961960A CN101654558B (zh) 2008-09-19 2008-09-19 绝缘子硅橡胶及其制造方法

Publications (2)

Publication Number Publication Date
CN101654558A CN101654558A (zh) 2010-02-24
CN101654558B true CN101654558B (zh) 2011-06-29

Family

ID=41709020

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2008101961960A Expired - Fee Related CN101654558B (zh) 2008-09-19 2008-09-19 绝缘子硅橡胶及其制造方法

Country Status (1)

Country Link
CN (1) CN101654558B (zh)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103360770B (zh) * 2013-07-04 2015-10-28 江苏南瓷绝缘子股份有限公司 高温硫化改性硅橡胶及其生产方法
CN104530717A (zh) * 2014-12-26 2015-04-22 江苏天辰新材料有限公司 低拉伸永久变形的硅橡胶及其制造方法
CN107033602A (zh) * 2017-05-17 2017-08-11 醴陵市时代鑫湘科技有限公司 复合绝缘子用高强度硅橡胶绝缘材料
CN109777112A (zh) * 2018-06-22 2019-05-21 广东聚合科技股份有限公司 一种复合绝缘子用硅橡胶及其制备方法

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1693368A (zh) * 2005-07-21 2005-11-09 江苏宏达化工新材料股份有限公司 用于注射成型复合硅橡胶绝缘子混炼胶专用料的制备方法
CN1923898A (zh) * 2006-02-10 2007-03-07 南方电网技术研究中心 半导体均压层和中导电性硅橡胶及制备合成绝缘子的工艺

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1693368A (zh) * 2005-07-21 2005-11-09 江苏宏达化工新材料股份有限公司 用于注射成型复合硅橡胶绝缘子混炼胶专用料的制备方法
CN1923898A (zh) * 2006-02-10 2007-03-07 南方电网技术研究中心 半导体均压层和中导电性硅橡胶及制备合成绝缘子的工艺

Non-Patent Citations (2)

* Cited by examiner, † Cited by third party
Title
JP特开2007-180044A 2007.07.12
黄文润.混炼硅橡胶的配合技术(五).《有机硅材料》.2006,第20卷(第5期),第268-272页. *

Also Published As

Publication number Publication date
CN101654558A (zh) 2010-02-24

Similar Documents

Publication Publication Date Title
CN111019357B (zh) 高性能硅基导热泥及其制备方法
CN111057379B (zh) 一种含有碳纤维的高导热绝缘硅橡胶复合材料及其制备方法
CN102618041B (zh) 一种高导热绝缘硅橡胶及其制备方法
CN109735112B (zh) 加成型有机硅导热凝胶及其制备方法
CN101704975B (zh) 一种电缆用绝缘橡皮
CN103694709B (zh) 加成型液体硅橡胶用耐漏电起痕剂及其制备方法和应用
CN101654558B (zh) 绝缘子硅橡胶及其制造方法
CN103030862B (zh) 耐温125℃硅烷交联聚乙烯绝缘料及其制备方法
CN104610754A (zh) 一种复合绝缘子用的微纳硅橡胶复合胶料及其制备方法
CN102757648A (zh) 一种导热硅橡胶复合材料及其制备方法
CN107033602A (zh) 复合绝缘子用高强度硅橡胶绝缘材料
CN101775216A (zh) 一种高导热有机硅复合物的生产方法
CN101654557A (zh) 耐油甲基乙烯基硅橡胶及其制造方法
CN110791103A (zh) 一种新型导电液体硅橡胶及其制备方法与应用
CN112063176A (zh) 一种灌封变压器用的加成型灌封硅橡胶及其制备方法
CN105131413A (zh) 高强度耐高温硅烷交联电缆用半导电屏蔽料及其制备方法
CN102585506B (zh) 一种具有优良耐电弧性能的硅橡胶及其制备方法
CN109880375A (zh) 一种耐老化硅橡胶复合材料及其制备方法
CN111334045A (zh) 一种单组分快速室温固化导热凝胶及其制作工艺
CN114031945A (zh) 一种具有良好憎水性及阻燃性的硅橡胶材料及其制备方法
CN102070906A (zh) 一种挤出硅橡胶及其制备方法
CN103333505A (zh) 一种高强度绝缘子硅胶及其制备方法
CN111647271A (zh) 一种耐高温阻燃有机硅弹性体电缆料及其制备方法
CN101575454A (zh) 一种用于电应力控制的液体导电硅橡胶及其制备方法
CN103602068A (zh) 一种导电橡胶

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
ASS Succession or assignment of patent right

Owner name: JIANGSU TIANCHEN SILICON MATERIALS CO., LTD.

Free format text: FORMER OWNER: ZHENJIANG DONGCHEN NEW MATERIALS CO., LTD.

Effective date: 20110128

C41 Transfer of patent application or patent right or utility model
TA01 Transfer of patent application right

Effective date of registration: 20110128

Address after: 212216, Jiangsu province Yangzhong Mayor Wang Industrial Park

Applicant after: Jiangsu Tiancheng Silicon Co., Ltd.

Address before: 212216, Jiangsu province Yangzhong Mayor Wang Industrial Park

Applicant before: Zhenjiang Dongchen New Materials Co., Ltd.

C14 Grant of patent or utility model
GR01 Patent grant
C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20150911

Address after: Yangzhong City Development Zone, Jiangsu city of Zhenjiang province 212211 Hong Kong Road No. 568

Patentee after: JIANGSU TIANCHEN NEW MATERIALS CO., LTD.

Address before: 212216, Jiangsu province Yangzhong Mayor Wang Industrial Park

Patentee before: Jiangsu Tiancheng Silicon Co., Ltd.

CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20110629

Termination date: 20180919