CN101615453B - 一种漆包线涂漆活动模具 - Google Patents
一种漆包线涂漆活动模具 Download PDFInfo
- Publication number
- CN101615453B CN101615453B CN2009101830225A CN200910183022A CN101615453B CN 101615453 B CN101615453 B CN 101615453B CN 2009101830225 A CN2009101830225 A CN 2009101830225A CN 200910183022 A CN200910183022 A CN 200910183022A CN 101615453 B CN101615453 B CN 101615453B
- Authority
- CN
- China
- Prior art keywords
- carbide alloy
- alloy bar
- hard alloy
- chute
- moveable die
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明公开了一种活动模具,该活动模具由一组四个硬质合金条组成,在单个硬质合金条的轴向上设有滑槽,在单个硬质合金条的一侧端部设有与滑槽相配合的滑头,单个硬质合金条的滑头镶嵌在与其相邻单个硬质合金条的滑槽内,相互配合的四个硬质合金条共同构成模具腔。该活动模具使得漆膜厚度像固定模具一样精确,可重复利用,节省了大量买模具、加工模具、修模具的工作及人员,降低劳动强度,节省了调节时间,提高了效率,也节省了原材料及能源的浪废。
Description
技术领域
本发明涉及一种模具,具体地说是一种漆包线涂漆活动模具。
背景技术
目前国内漆包线涂漆工艺一般有两种,一种使用毛毡涂漆,一种使用固定模具。毛毡涂漆优点是更换不同线规时只须将裸铜扁线直接对焊起来,就可以顺利牵引,操作简便,速度快,浪费少。缺点是漆膜厚度不易控制、需要经常换毛毡且绝缘漆易污染影响绝缘性能。固定模具优点是根据不同线规及屈服强度选择对应尺寸的模具,漆膜厚度较精确;缺点是每种线规有十道涂漆烘焙过程,因此至少需要十个固定模具,生产中也存在磨损报废,每种产品线规的大小也不同,现有模具很难重复利用,因此固定模具需求量较大;另外十道涂漆模具在换线规时都必须一道一道剪断裸铜扁线,穿上相应模具,再焊接起来,牵引到下一个模具,重复上一道工作,劳动量大,浪费较多;每当一个模具发生问题需要更换时,必须剪断现有的扁线,导致十道线全部报废。
发明内容
为了克服现有技术存在的问题,本发明的目的是提供一种漆包线涂漆活动模具,该活动模具可调节尺寸,且漆膜厚度精确。使用该活动模具进行漆包线涂漆,漆膜厚度精确,节省了大量买模具、加工模具、修模具的工作及人员,降低了劳动强度,节省了调节时间,提高了效率。
本发明的目的是通过以下技术方案来实现的:
一种漆包线涂漆活动模具,其特征在于:该活动磨具由一组四个硬质合金条组成,在单个硬质合金条的轴向上设有滑槽,在单个硬质合金条的一侧端部设有与滑槽相配合的滑头,单个硬质合金条的滑头镶嵌在与其相邻单个硬质合金条的滑槽内,相互配合的四个硬质合金条共同构成模具腔。
本发明所述滑槽设置在单个硬质合金条的轴向中部。
所述硬质合金条的截面形状为“凹”型。
所述滑头深度等于或者小于滑槽的深度。所述滑头深度等于或者小于滑槽的深度。
本发明使用时,具有与固定模具一样精确的漆膜厚度。由于活动模具可调节尺寸,可重复利用,节省了大量买模具、加工模具、修模具的工作及人员;更换线规时只须焊接一次,通过调节活动模具就可一次通过,降低劳动强度,节省了调节时间,提高了效率,也节省了原材料及能源的浪废;另外,活动模具在线可调节,一道模具有问题,可立即在线处理,无须剪断,用不着十道模全部报废,也提高了工作效率、减少了浪费。
与现有技术相比,本发明漆膜厚度精确,节省了大量买模具、加工模具、修模具的工作及人员,降低了劳动强度,节省了调节时间,提高了效率,也节省了原材料,减少了能源的浪废。
附图说明
图1是本发明结构示意图;
图2是本发明中单个硬质合金条的结构示意图;
图3是本发明中单个硬质合金条的右视图。
具体实施方式
一种本发明所述的漆包线涂漆活动模具,见图1、图2和图3,该活动磨具由一组四个硬质合金条1组成,在单个硬质合金条1的轴向上设有滑槽2,在单个硬质合金条1的一侧端部设有与滑槽2相配合的滑头3。滑头3能在其他硬质合金的滑槽2内滑动。滑头3深度等于或者小于滑槽2的深度。硬质合金条1的截面形状为“凹”型。单个硬质合金条的滑头3镶嵌在与其相邻单个硬质合金条的滑槽2内,相互配合的四个硬质合金条1共同构成模具腔4。
使用时,如图1,将第一条硬质合金1的滑头3插入第二条硬质合金1的滑槽2中,再将第二条硬质合金1的滑头3插入第三条硬质合金1的滑槽2中,以此类推,最后将第四条硬质合金1的滑头3插入第一条硬质合金1的滑槽2中,构成封闭的模具腔5。通过调节四条硬质合金,可使得中央模具腔5尺寸符合涂漆模具要求的尺寸,精度可达到0.01mm,再通过相应的旋紧装置予以固定,使得在生产中不会变形。
该活动模具漆膜厚度精确,由于活动模具可调节尺寸,可重复利用,节省了大量买模具、加工模具、修模具的工作及人员;更换线规时只须焊接一次,通过调节活动模具就可一次通过,降低劳动强度,节省了调节时间,提高了效率,也节省了原材料及能源的浪废;另外,活动模具在线可调节,一道模具有问题,可立即在线处理,无须剪断,用不着十道模全部报废,也提高了工作效率、减少了浪费。最后,密闭的漆缸代替原来简易敞开式的漆缸,最大可能地杜绝了绝缘漆的污染,使产品绝缘性能更可靠。
Claims (4)
1.一种漆包线涂漆活动模具,其特征在于:该活动模具由一组四个硬质合金条(1)组成,在单个硬质合金条(1)的轴向上设有滑槽(2),在单个硬质合金条(1)的一侧端部设有与滑槽(2)相配合的滑头(3),单个硬质合金条(1)的滑头(3)镶嵌在与其相邻单个硬质合金条(1)的滑槽(2)内,相互配合的四个硬质合金条(1)共同构成模具腔(4)。
2.根据权利要求1所述漆包线涂漆活动模具,其特征在于:所述滑槽(2)设置在单个硬质合金条(1)的轴向中部。
3.根据权利要求1所述漆包线涂漆活动模具,其特征在于:所述硬质合金条(1)的截面形状为“凹”型。
4.根据权利要求1所述漆包线涂漆活动模具,其特征在于:所述滑头(3)深度等于或者小于滑槽(2)的深度。