CN101458206A - 一种快速测定造纸网上物料留着率的方法 - Google Patents

一种快速测定造纸网上物料留着率的方法 Download PDF

Info

Publication number
CN101458206A
CN101458206A CNA2007101722838A CN200710172283A CN101458206A CN 101458206 A CN101458206 A CN 101458206A CN A2007101722838 A CNA2007101722838 A CN A2007101722838A CN 200710172283 A CN200710172283 A CN 200710172283A CN 101458206 A CN101458206 A CN 101458206A
Authority
CN
China
Prior art keywords
concentration
white water
retention
paper making
paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2007101722838A
Other languages
English (en)
Inventor
朱勇强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Sustainable Accele Tech Co ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA2007101722838A priority Critical patent/CN101458206A/zh
Publication of CN101458206A publication Critical patent/CN101458206A/zh
Pending legal-status Critical Current

Abstract

本发明是涉及一种快速测定造纸网上物料留着率的方法。本发明提出采用仪器分析方法测试上网料液和白水液体浓度的方法来间接测定留着率。即1.使用浊度仪或分光光度计测试上网和白水的浊度或透光率数值;2.再将以上测得的浊度值或透光率值依次输入相应计算软件中,计算出上网纸料浓度和白水浓度;3.将以上浓度值带入公式:SPR%=(c1-c2)*100%/c1;(式中,c1为上网料液浓度,c2为白水液体浓度),计算出留着率。本发明缩短了测试时间、简化操作程序、减小测试误差,同时结合计算软件还能实现“在线检测”,为造纸湿部化学的“实时控制”创造条件。

Description

一种快速测定造纸网上物料留着率的方法
技术领域
本发明是涉及一种快速测定造纸网上物料留着率的方法,是采用仪器分析测试上网料液浓度和白水液体浓度的方法来间接测定留着率。
技术背景
随着社会经济的快速发展,品质、成本、环境三大要素已成为现代造纸工业的竞争核心。如何提升产品的品质,降低生产成本,并减少环境负荷就成了我们每个造纸工作者努力的重点,提高纸页抄造过程中的留着效率无疑是达到这三个目的的重要途径之一。
目前,我国许多造纸企业广泛地采用较传统的测试方法:取上网料液和白水液体各1000ml,用滤纸过滤,再烘干至恒重,称重计算出浓度(c1,c2),再由此计算出留着率SPR%。SPR%=(c1-c2)*100%/c1(式中,c1为上网料液的浓度,c2为白水液体的浓度)。
但该方法存在诸多不足:1.费时;2.误差大,准确性低(白水浓度为0.1%时,1000ml样品仅有1g固形物)。
然而留着率的高低在很大程度上影响了造纸的产量、质量及造纸废水的污染负荷。因此快速准确测定留着率,及时调整生产工艺以达到最佳状态已成为造纸企业的迫切需要。
发明内容
本发明的目的在于提供一种快速测定造纸网上物料留着率的方法。该方法缩短了测试时间,简化了操作程序减小误差,同时结合造纸软件还能实现“在线检测”,为造纸湿部化学的“实时控制”提供依据。
为了达到上述目的,本发明提出采用仪器分析测试上网料液和白水液体的方法间接测定留着率。即1.使用浊度仪或分光光度计测试上网料液和白水液体的浊度数值或透光度值;;2.将以上所有浊度值或透光度值依次输入计算软件中,计算上网浓度和白水浓度;3.再将以上浓度值带入公式SPR%=(c1-c2)*100%/c1(式中,c1为上网料液浓度,c2为白水液体浓度),计算出留着率。
根据上述构思,本发明采用下述技术方案:
一种快速测定造纸网上物料留着率的方法,计算留着率所需的上网纸料的浓度(c1)和造纸白水的浓度(c2),是通过仪器分析方法来间接测定的。
上述间接测量上网纸料浓度和白水浓度的仪器为可以测定液体浊度的浊度计,或可以测定液体透光率的分光光度计。
上述上网纸料浓度和白水浓度的数值是通过浓度的实际数值(C)与间接测量值(IC)之间的回归关系方程式,或相应的计算软件计算得出。
上述留着率(SPR%)的计算公式为:SPR%=(c1-c2)*100%/c1。
上述采用浊度计,或分光光度计来测定上网纸料浓度和白水浓度的间接数值时,需要在试样中加入一种透明的聚合物液体,增加待测样品的粘稠度,以保证测试的准确度。
上述造纸生产线的上网纸料浓度与白水浓度的在线测量是采用浊度计或分光光度计进行“在线测量”,并由计算机自动采集测量数据并计算出留着率。
本发明与传统方法相比较,具有如下显而易见的突出特点和显著优点:
1.可快速测定造纸网上物料留着率。
2.由于该方法缩短了测试时间,简化操作程序,进而减小误差。
3.同时该方法结合计算软件还可以实现“在线检测”,为造纸湿部化学的“实时控制”提供依据。
附图说明
附图是本发明专利中纸料在线检测的装置流程图。其中:
1-造纸机流浆箱         2-造纸机网部的白水盘
3-上网纸料取样泵       4-白水取样泵
5-浊度计1              6-浊度计2
7-计算机(计算留着率)
具体实施方式
一.实施例一
1.浊度数值的测定方法
(1)分别取上网纸料与造纸白水样品各一份,充分均匀搅拌后用量筒各取50ml,均加150ml蒸馏水稀释4倍,摇匀备用。
(2)依次将上述制备好的样品倒入测试用样品池中,加入测试稳定液2滴,均匀振动,然后把瓶中气泡赶走,再放到浊度仪上测试,10秒后读取的结果即为浓度的间接测量值。
(3)完毕后摇匀一下再重复操作(2),各样品取3次有效数据。
2.样品实际浓度的计算
将所有测试好的数据依次输入下面的回归方程或计算软件中,试样浓度c%。按如下公式计算可得出浓度实际值:
C=10-3*nK0*(2.41291+0.18095N-4.87834*10-5N2+6.59505*10-9N3)
式中,n为测定时稀释倍数
K0为校正常数
N为仪器测定的浊度数值
3.计算留着率
将以上各样品浓度值带入公式:
SPR%=(c1-c2)*100%/c1
式中,c1为上网料液浓度,c2为白水液体浓度。
计算出留着率SPR%
二.实施例二
1.测试透光率的方法
(1)分别取上网纸料与造纸白水样品各1ml,用50ml蒸馏水稀释,再用分光光度计测定透光率。
(2)完毕后重复操作(1),各样品取3次有效数据。
2.样品实际浓度的计算
将所有测试好的数据依次输入下面的回归方程或计算软件中,试样浓度c%。
按如下公式计算可得出浓度实际值:
C%=-2.7551-3.5153*K0*log10(T/100)
式中,K0为实验常数
T为透光率
3.计算留着率
将以上各样品浓度值带入公式:
SPR%=(c1-c2)*100%/c1
式中,c1为上网料液浓度,c2为白水液体浓度。
计算出留着率SPR%。
三.实施例三
通过在线取样装置在线取样,所取样品自动进入检测仪器进行测量。测量完毕,数据被计算机采集并计算出留着率。
流程如附图所示。

Claims (6)

1.一种快速测定造纸网上物料留着率的方法。其特征在于计算留着率所需的上网纸料的浓度(c1)和造纸白水的浓度(c2),是通过仪器分析方法来间接测定的。
2.根据权利要求1所述的快速测定造纸网上物料留着率的方法。其特征在于间接测量上网纸料浓度和白水浓度的仪器为可以测定液体浊度的浊度计,或可以测定液体透光率的分光光度计。
3.根据权利要求2所述的快速测定造纸网上物料留着率的方法。其特征在于上网纸料浓度和白水浓度的数值是通过浓度的实际数值(C)与间接测量值(IC)之间的回归关系方程式,或相应的计算机软件计算得出。
4.根据权利要求1所述的快速测定造纸网上物料留着率的方法。其特征在于留着率(SPR%)的计算公式为:SPR%=(c1-c2)*100%/c1。
5.根据权利要求1所述的快速测定造纸网上物料留着率的方法。其特征在于采用浊度计,或分光光度计来测定上网纸料浓度和白水浓度的间接数值时,需要在试样中加入一种透明的聚合物液体,增加待测样品的粘稠度,以保证测试的准确度。
6.根据权利要求2所述的快速测定造纸网上物料留着率的方法。其特征在于造纸生产线的上网纸料浓度与白水浓度的间接测量是采用浊度计或分光光度计进行“在线连续测量”,计算机自动采集测量数据并计算出留着率。
CNA2007101722838A 2007-12-14 2007-12-14 一种快速测定造纸网上物料留着率的方法 Pending CN101458206A (zh)