CN101215189A - 新型户外冷光源(发光砖石,夜光砖,荧光砖) - Google Patents
新型户外冷光源(发光砖石,夜光砖,荧光砖) Download PDFInfo
- Publication number
- CN101215189A CN101215189A CNA2008100192970A CN200810019297A CN101215189A CN 101215189 A CN101215189 A CN 101215189A CN A2008100192970 A CNA2008100192970 A CN A2008100192970A CN 200810019297 A CN200810019297 A CN 200810019297A CN 101215189 A CN101215189 A CN 101215189A
- Authority
- CN
- China
- Prior art keywords
- brick
- luminous
- noctilucent
- glaze
- fluorescent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及光源领域,具体是由基础釉熔块,发光材料和添加剂等原材料烧制而成的新型户外冷光源(发光砖石,夜光砖,荧光砖)。该材料能够吸收自然光,在夜间持续发出冷光,光亮度可以超过目前国际市场上花园太阳能灯所发出的光强。其发光时间根据稀土材质的区别,可以连续发光达2至12小时不等。也是节能,绿色环保型的户外新型光源。
Description
技术领域
本发明涉及光源领域,具体是由基础釉熔块,发光材料和添加剂等原材料烧制而成的新型户外冷光源(发光砖石,夜光砖,荧光砖)。
背景技术
目前,在市场现有的晚间夜光源(发光砖石,夜光砖,荧光砖),一般都是用在室内,在室外有的技术无法解决,如果在室外有的话,晚间发光时间也不会太长,而且全部采用挤压方法作成成品,所以一直在困扰着人们很多问题。
发明内容
为了解决以上现有夜光源技术不足,发光时间短、硬度不够,寿命短等特点。
本发明解决其技术问题所采用的技术方案是:
发光陶瓷釉料的制备过程:按配方组成称取各种原材料,经球磨充分混合均匀,将混合好的物料置于熔块炉中,在极端高温下熔制,水淬,烘干,球磨,过筛(50 500目)再将过筛后的基础釉熔块粉末与一定量的夜光粉及少量添加剂在球磨机中球磨,釉浆细度达到万孔筛余(0.001-0.5%)即可。
将发光陶瓷釉料与印油按照1:(0.02-0.95)比例混合均匀,搅拌成浓稠壮,用10-90目丝网印于釉面砖上,彻底干燥再套印陶瓷颜料,最后用20---90目丝网印堆釉干粉。在采用快速烧成的辊道窑中烧成。时间大约10-200分钟烧成夜光陶瓷。
本发明技术产品适用于:路缘石,城市交通事故频发带,犯罪案件频发区域,省道/国道/城郊结合部事故频发带,公路弯道,公园/景区弯道和小径,居民小区干道。停车场分隔带,分隔线,车道分隔线。花园装饰,民用建筑墙体,门窗,台阶,屋顶等外部装饰。
本发明的有益效果具有以下特点:
1)无放射性危害发光强度高。
2)可以连续发光达2至12小时不等。
3)节能,绿色环保型的户外新型光源。
具体实施方法
具体做法是:先制成发光陶瓷釉料,将体发光陶瓷釉料施于陶瓷胚表面,烧制成表面发光的陶瓷制品。发光陶瓷釉料的制备过程:按配方组成称取各种原材料,经球磨充分混合均匀,将混合好的物料置于熔块炉中,在极端高温下熔制,水淬,烘干,球磨,过筛(50-500目)再将过筛后的基础釉熔块粉末与一定量的夜光粉及少量添加剂在球磨机中球磨,釉浆细度达到万孔筛余(0.001-0.5%)即可。
将发光陶瓷釉料与印油按照1:(0.02-0.95)比例混合均匀,搅拌成浓稠壮,用10-90目丝网印于釉面砖上,彻底干燥再套印陶瓷颜料,最后用20---90目丝网印堆釉干粉。在采用快速烧成的辊道窑中烧成。时间大约10-200分钟烧成夜光陶瓷。
除说明书所述的技术特征外,均为本专业技术人员的已知技术。
Claims (4)
1.本发明涉及光源领域,具体是由基础釉熔块,发光材料和添加剂等原材料烧制而成的新型户外冷光源(发光砖石,夜光砖,荧光砖)。
发光陶瓷釉料的制备过程:按配方组成称取各种原材料,经球磨充分混合均匀,将混合好的物料置于熔块炉中,在极端高温下熔制,水淬,烘干,球磨,过筛(50-500目)再将过筛后的基础釉熔块粉末与一定量的夜光粉及少量添加剂在球磨机中球磨,釉浆细度达到万孔筛余(0.001-0.5%)即可。将发光陶瓷釉料与印油按照1∶(0.02-0.95)比例混合均匀,搅拌成浓稠壮,用10 90目丝网印于釉面砖上,彻底干燥再套印陶瓷颜料,最后用20---90目丝网印堆釉干粉。在采用快速烧成的辊道窑中烧成。时间大约10-200分钟烧成夜光陶瓷。
2.根据权利要求1所述新型户外冷光源(发光砖石,夜光砖,荧光砖),其特征在于经球磨充分混合均匀,将混合好的物料置于熔块炉中,在极端高温下熔制,水淬,烘干,球磨,过筛(50-500目)再将过筛后的基础釉熔块粉末与一定量的夜光粉及少量添加剂在球磨机中球磨,釉浆细度达到万孔筛余(0.001-0.5%)
3.根据权利要求1所述新型户外冷光源(发光砖石,夜光砖,荧光砖),其特征在于发光陶瓷釉料与印油按照1∶(0.02-0.95)比例混合均匀,搅拌成浓稠壮,用10-90目丝网印于釉面砖上,彻底干燥再套印陶瓷颜料,最后用20---90目丝网印堆釉干粉。在采用快速烧成的辊道窑中烧成。时间大约10-200分钟烧成夜光陶瓷。
4.根据权利要求1所述新型户外冷光源(发光砖石,夜光砖,荧光砖),其特征在于由其制成的发光夜光系列产品的发光特点可以经年保持,也是节能,绿色环保型的户外新型光源。