CN101126387A - 高精度柱塞的生产方法 - Google Patents

高精度柱塞的生产方法 Download PDF

Info

Publication number
CN101126387A
CN101126387A CNA2007101318717A CN200710131871A CN101126387A CN 101126387 A CN101126387 A CN 101126387A CN A2007101318717 A CNA2007101318717 A CN A2007101318717A CN 200710131871 A CN200710131871 A CN 200710131871A CN 101126387 A CN101126387 A CN 101126387A
Authority
CN
China
Prior art keywords
minutes
plunger
temperature
furnace
carbon potential
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2007101318717A
Other languages
English (en)
Other versions
CN100447417C (zh
Inventor
陆建秋
程道广
张京谊
蔡中辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuxi Yingbei Precision Hydraulic Co., Ltd
Original Assignee
WUXI YINGBEI MACHINERY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI YINGBEI MACHINERY CO Ltd filed Critical WUXI YINGBEI MACHINERY CO Ltd
Priority to CNB2007101318717A priority Critical patent/CN100447417C/zh
Publication of CN101126387A publication Critical patent/CN101126387A/zh
Application granted granted Critical
Publication of CN100447417C publication Critical patent/CN100447417C/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种高精度柱塞的生产方法,材料选用合金钢或轴承钢,工艺采用车+热处理+磨,热处理具体步骤:柱塞在350~400℃下预热40~50分钟;柱塞投入渗碳热处理炉中,升温至840℃,保温30分钟,碳势控制在CP=0.4,之后升温至880℃,同时升碳势到CP=0.8,时间为20分钟,在880℃炉温和CP=0.8碳势下进行表面渗碳180分钟,之后下降碳势至0.7,时间为10分钟,炉温保持在880℃,再在880℃炉温和0.7碳势下进行表面渗碳30分钟,之后冷却至100℃,时间50分钟,最后再升温至800℃,时间10分钟,在800℃下保温50分钟出炉;在油中淬火15~25分钟,控制油温80℃;清洗;在175~185℃的回火炉中回火170~190分钟。本发明方法环保、生产的柱塞精度高。

Description

高精度柱塞的生产方法
技术领域
本发明涉及一种液压柱塞泵,具体涉及一种液压柱塞泵的柱塞的生产方法。属液压控制元件技术领域。
背景技术
液压柱塞泵广泛应用在液压系统的控制和液压系统的执行等控制工程。主要装机类型有汽车工程、航空工程、工程机械等行业。
目前同类精度较低的液压柱塞泵的柱塞的生产方法是:车+磨+电镀。柱塞材料主要选择碳钢,表面采用镀铬工艺,其主要缺点是:
1、柱塞外圆部分精度较低,圆度和直线度都在3μm以上,表面粗糙度在Ra0.2μm以上,造成配选装配、运行不平稳等现象。
2、柱塞球头部分精度较低,圆度在5μm以上,表面粗糙度在Ra0.4μm以上,造成运行不平稳,泄漏等现象。
3、表面镀铬工艺容易造成环境污染,而且镀层容易脱落,造成设备卡死等现象。
发明内容
本发明的目的在于克服上述不足,提供一种精度高、环保的高精度柱塞的生产方法。
本发明的目的是这样实现的:一种高精度柱塞的生产方法,柱塞材料选用合金钢或轴承钢,先对柱塞外圆部分和球头部分进行车削加工,再对车削加工后的柱塞进行渗碳淬火热处理,再将热处理后的柱塞外圆部分和球头部分进行磨加工,所述渗碳淬火热处理的具体工艺步骤如下:
步骤一、柱塞零件在清洗机中清洗,烘干;
步骤二、烘干后的柱塞零件在350~400℃下预热40~50分钟;
步骤三、预热后的柱塞零件投入渗碳热处理炉中,升温至840℃±10℃,保温30分钟±5分钟,碳势控制在CP=0.4,之后升温至880℃±5℃,同时升碳势到CP=0.8,时间为20分钟±5分钟,在880℃±5℃炉温和CP=0.8碳势下进行表面渗碳180分钟±5分钟,之后下降碳势至0.7,时间为10分钟±5分钟,炉温保持在880℃±5℃,再在880℃±5℃炉温和0.7碳势下进行表面渗碳30分钟±5分钟,之后冷却至100℃±5℃,时间50分钟±5分钟,最后再升温至800℃±5℃,时间10分钟±5分钟,在800℃±5℃下保温50分钟±5℃,出炉,零件表面有效渗碳层在0.6~0.7mm;
步骤四、渗碳后的柱塞零件在油中淬火20分钟±5分钟,控制油温80℃±5℃;
步骤五、淬火后的柱塞零件在清洗机中清洗;
步骤六、清洗后柱塞零件在175~185℃的回火炉中回火170~190分钟。
本发明生产工艺采用车+热处理+磨,与现有同类方法相比较有以下优势:
1、外圆精度高,圆度、直线度在0.76μm以上,表面粗糙度在Ra0.08μm以下;
2、球面精度高,圆度在0.76μm以上,表面粗糙度在Ra0.08μm以下;
3、装配后运行平稳,无泄漏;
4、生产过程无污染,符合环保要求,无镀层脱落造成设备卡死等现象。
附图说明
图1为本发明高精度柱塞热处理温度-时间曲线图。
具体实施方式
本发明为一种高精度柱塞的生产方法,柱塞材料选用强度较高的合金钢或轴承钢,对柱塞外圆部分和球头部分进行车削加工,然后对车削加工后的柱塞进行渗碳淬火热处理,达到零件的耐磨要求,最后将热处理后的柱塞外圆部分和球头部分进行磨加工。
所述渗碳淬火热处理的具体工艺参数如下(参见图1):
1、柱塞零件在清洗机中清洗,烘干60分钟;
2、烘干后的柱塞零件在350~400℃下预热40~50分钟;
3、预热后的柱塞零件投入渗碳热处理炉中,升温至840℃,零件在840℃下保温30分钟,碳势控制在CP=0.4,之后升温至880℃,同时升碳势到CP=0.8,时间为20分钟,在880℃炉温和0.8碳势下进行表面渗碳180分钟,之后进行880℃炉温下降碳势至0.7,时间为10分钟,再在880℃炉温和0.7碳势下进行表面渗碳30分钟,之后在0.7碳势下冷却至100℃,时间50分钟,最后再升温至800℃,时间10分钟,在800℃下保温50分钟,保证零件表面有效渗碳层达到0.6~0.7mm;
4、渗碳后的柱塞零件在油中淬火15~25分钟,控制油温80℃;
5、淬火后的柱塞零件在清洗机中清洗55~65分钟;
6、清洗后柱塞零件在175~185℃的回火炉中回火170~190分钟,保证零件的表面硬度。

Claims (1)

1.一种高精度柱塞的生产方法,其特征在于:柱塞材料选用合金钢或轴承钢,对柱塞外圆部分和球头部分进行车削加工,对车削加工后的柱塞进行渗碳淬火热处理,将热处理后的柱塞外圆部分和球头部分进行磨加工,所述渗碳淬火热处理的具体工艺步骤如下:
步骤一、柱塞零件在清洗机中清洗,烘干;
步骤二、烘干后的柱塞零件在350~400℃下预热40~50分钟;
步骤三、预热后的柱塞零件投入渗碳热处理炉中,升温至840℃,保温30分钟,碳势控制在CP=0.4,之后升温至880℃,同时升碳势到CP=0.8,时间为20分钟,在880℃炉温和CP=0.8碳势下进行表面渗碳180分钟,之后下降碳势至0.7,时间为10分钟,炉温保持在880℃,再在880℃炉温和0.7碳势下进行表面渗碳30分钟,之后冷却至100℃,时间50分钟,最后再升温至800℃,时间10分钟,在800℃下保温50分钟出炉,零件表面有效渗碳层在0.6~0.7mm;
步骤四、渗碳后的柱塞零件在油中淬火15~25分钟,控制油温80℃;
步骤五、淬火后的柱塞零件在清洗机中清洗55~65分钟;
步骤六、清洗后柱塞零件在175~185℃的回火炉中回火170~190分钟。
CNB2007101318717A 2007-09-07 2007-09-07 高精度柱塞的生产方法 Active CN100447417C (zh)