CN101117513A - 金属表面防腐蚀涂料的制备方法 - Google Patents

金属表面防腐蚀涂料的制备方法 Download PDF

Info

Publication number
CN101117513A
CN101117513A CNA2006100150822A CN200610015082A CN101117513A CN 101117513 A CN101117513 A CN 101117513A CN A2006100150822 A CNA2006100150822 A CN A2006100150822A CN 200610015082 A CN200610015082 A CN 200610015082A CN 101117513 A CN101117513 A CN 101117513A
Authority
CN
China
Prior art keywords
coating
heated
gram
preparation
metal surface
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CNA2006100150822A
Other languages
English (en)
Inventor
张云波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin Zhendong Paints Co Ltd
Original Assignee
Tianjin Zhendong Paints Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin Zhendong Paints Co Ltd filed Critical Tianjin Zhendong Paints Co Ltd
Priority to CNA2006100150822A priority Critical patent/CN101117513A/zh
Publication of CN101117513A publication Critical patent/CN101117513A/zh
Withdrawn legal-status Critical Current

Abstract

一种金属表面防腐蚀涂料的制备方法,20克铝粉及980克H04-1绿环氧磁漆混合与200克H-2固化剂搅拌均匀即为底层涂料,面层为501-3聚氨酯清漆,铝合金试片用有机溶液除油,用200目刚玉粉吹砂,表面均匀喷涂底层后,放入循环热风炉,加热至100℃,保温2小时,取出空冷;再喷涂一层底层涂料,用同样方法固化并冷却后喷涂一层面层,放入循环热风炉,加热至150℃,保温1小时。本发明具有以下优点:既耐冲刷又防腐蚀,涂覆工艺简单,涂层具有较高的耐腐蚀性、韧性、耐冲刷性以及与金属基体的结合力。

Description

金属表面防腐蚀涂料的制备方法
技术领域
本发明涉及一种金属表面防腐蚀涂料的制备方法。
背景技术
目前,对于铝合金表面耐冲刷防腐蚀涂料,通常是提高涂料的防腐蚀性能,就无法兼顾涂层的抗冲刷性。
发明内容
本发明的目的在于克服上述的缺陷,提供一种金属表面防腐蚀涂料的制备方法。
本发明的技术方案是:一种金属表面防腐蚀涂料的制备方法,其特征在于:该金属表面涂料内层由H04-1绿环氧磁漆与超细锌铝粉或超细铝粉,由501-3聚氨酯清漆为面层组成的双层结构;底面涂料由两组分组成,A组分由85-98%的H04-1绿环氧磁漆与2-15%超细锌铝粉或超细铝粉组成,B组分由H-2固化剂组成,A组分:B组分配比为5-6∶1。
本发明具有以下优点:既耐冲刷又防腐蚀,涂覆工艺简单,涂层具有较高的耐腐蚀性、韧性、耐冲刷性以及与金属基体的结合力。
具体实施方式
实施例1:20克铝粉及980克H04-1绿环氧磁漆混合与200克H-2固化剂搅拌均匀即为底层涂料,面层为501-3聚氨酯清漆,铝合金试片用有机溶液除油,用200目刚玉粉吹砂,表面均匀喷涂底层后,放入循环热风炉,加热至100℃,保温2小时,取出空冷;再喷涂一层底层涂料,用同样方法固化并冷却后喷涂一层面层,放入循环热风炉,加热至150℃,保温1小时。
实施例2:80克锌铝片及920克HO4-1绿环氧磁漆混合与167克H-2固化剂搅拌均匀即为底层涂料,面层为501-3聚氨酯清漆,用有机溶液除油,用200目刚玉粉吹砂,表面均匀喷涂底层后,放入循环热风炉,加热至100℃,保温2小时,取出空冷;再喷涂一层底层涂料,用同样方法固化并冷却后喷涂一层面层,放入循环热风炉,加热至150℃,保温1小时。

Claims (1)

1.一种金属表面防腐蚀涂料的制备方法,其特征在于:20克铝粉及980克H04-1绿环氧磁漆混合与200克H-2固化剂搅拌均匀即为底层涂料,面层为501-3聚氨酯清漆,铝合金试片用有机溶液除油,用200目刚玉粉吹砂,表面均匀喷涂底层后,放入循环热风炉,加热至100℃,保温2小时,取出空冷;再喷涂一层底层涂料,用同样方法固化并冷却后喷涂一层面层,放入循环热风炉,加热至150℃,保温1小时。
CNA2006100150822A 2006-08-01 2006-08-01 金属表面防腐蚀涂料的制备方法 Withdrawn CN101117513A (zh)