CN101087496A - Side wall printing method of porcelain block - Google Patents
Side wall printing method of porcelain block Download PDFInfo
- Publication number
- CN101087496A CN101087496A CN 200710011924 CN200710011924A CN101087496A CN 101087496 A CN101087496 A CN 101087496A CN 200710011924 CN200710011924 CN 200710011924 CN 200710011924 A CN200710011924 A CN 200710011924A CN 101087496 A CN101087496 A CN 101087496A
- Authority
- CN
- China
- Prior art keywords
- block
- ceram
- printed
- ceramic
- ceramic block
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a printing method on the side-wall of ceram block in photoelectric module, which includes following step: a. four ceram backing plates are folded together, the metal plasm is printed on the top surface of top layer or the lower surface of lower layer; b. the printed four ceram backing plate are compressed; c. the said compressed sheet material is hot cut into rectangle, the metal plasm is printed on the opposite side-face of rectangle; d. the sheet material is hot cut into upper ceram block(1) and lower ceram block(2) along the direction vertical with the side-face of metal plasm; e. upper ceram block(1) and lower ceram block(2) are compressed to form the ceram block. Comparing with present technique, because it changes the present method that the print is done after the compression, it is to say, the single ceram print is changed into several cerams printed together to improve the work efficiency, good print quality, and it can not effect other printed faces, and reduce the cost at the same time.
Description
Technical field
The present invention relates to the side wall printing method of the ceramic block in a kind of optical-electric module.
Background technology
Optical-electric module utilizes the aluminium oxide ceramics piece to make carrier, prints out circuit on the surface with particulate metal slurry, inside and outside the conduction module shell.External signal enters enclosure by the circuit that prints on the ceramic block, after internal structure is handled signal, transfers out shell again.Aluminium oxide ceramics is through lamination with after cutting into ceramic block, need be fixed in the square groove that machining goes out on the side wall of outer shell, as shown in Figure 1: the end face of the last ceramic block 1 in the ceramic block, down the bottom surface and the side faces at both ends 3 of ceramic block 2 all need the type metal slurry, be used for and shell between welding fix.At present to the end face of last ceramic block 1, the bottom surface of ceramic block 2 and the method for side faces at both ends 3 type metal slurries are down:, go forward to print ceramic block being soldered to shell earlier to the ceramic substrate lamination with earnestly form the ceramic block of strip.Because the ceramic block size is little, length is generally about 20mm, and very soft before the ceramic post sintering, easy deformation.Simultaneously,,, be coated onto easily on other the face, cause short circuit during use easily, influence quality, inefficiency, production cost height so the side wall printing efficiency is on the low side because four need printing surface areas are all very little.
Summary of the invention
The side wall printing that the purpose of this invention is to provide a kind of ceramic block evenly, with shell welding fixation, good airproof performance, efficient height, side wall printing method of porcelain block that cost is low, overcome the deficiencies in the prior art.
Side wall printing method of porcelain block of the present invention comprises the steps:
A, four layers of ceramic substrate are superimposed together before, at the end face of the superiors' ceramic substrate or the bottom surface type metal slurry of orlop ceramic substrate;
B, four layers of ceramic substrate after the last step printing are carried out lamination;
C, the sheet material that will go up behind the step lamination earnestly form rectangle, type metal slurry on wherein one group of relative side of rectangle;
D, perpendicular in the step on the side surface direction of type metal slurry earnestly sheet material form ceramic block 1 and following ceramic block 2;
E, last ceramic block 1 and following ceramic block 2 are carried out lamination form ceramic block.
Side wall printing method of porcelain block of the present invention, since changed lamination in the prior art and earnestly after the mode of printing, be about to former single ceramic bar printing change into fervent one-tenth a plurality of before integral body print together, improved operating efficiency, printing quality is good, can not have influence on other does not need the face that prints, has reduced production cost simultaneously.
Description of drawings
Fig. 1 is the perspective view of ceramic block;
Fig. 2 utilizes ceramic substrate earnestly to become to go up the schematic diagram of ceramic block 1;
Fig. 3 utilizes ceramic substrate earnestly to become the schematic diagram of ceramic block 2 down.
Embodiment
As shown in the figure: operation as follows:
A, four layers of ceramic substrate are superimposed together before, utilize the end face type metal slurry of screen printing mode at the superiors' ceramic substrate, in the same way at the bottom surface type metal slurry of orlop ceramic substrate of the ceramic substrate of four layers of another groups, promptly adopt the mode that individual ceramic substrate is printed, and then with four stacked lumping together.
B, four layers of ceramic substrate after adopting common lamination to last step printing carry out lamination, make it into as a whole.
C, the sheet material that will go up behind the step lamination earnestly remove the corner, form rectangle, length and width size according to ceramic substrate, the wide A that determines rectangle is consistent with the length of ceramic block, the long B of rectangle is the integral multiple (referring to Fig. 2) of the width of last ceramic block 1, or the long B of rectangle is the integral multiple (referring to Fig. 3) of following ceramic block 2 width.
Select side, the two ends type metal slurry of rectangle Width.
D, perpendicular in the step on the side surface direction of type metal slurry earnestly sheet material form ceramic block 1 and following ceramic block 2.
E, last ceramic block 1 and following ceramic block 2 are carried out lamination form ceramic block (referring to Fig. 1).
Claims (1)
1, a kind of side wall printing method of porcelain block is characterized in that: comprise the steps:
A, four layers of ceramic substrate are superimposed together before, at the end face of the superiors' ceramic substrate or the bottom surface type metal slurry of orlop ceramic substrate;
B, four layers of ceramic substrate after the last step printing are carried out lamination;
C, the sheet material that will go up behind the step lamination earnestly form rectangle, type metal slurry on wherein one group of relative side of rectangle;
D, perpendicular in the step on the side surface direction of type metal slurry earnestly sheet material form ceramic block (1) and following ceramic block (2);
E, last ceramic block (1) and following ceramic block (2) are carried out lamination form ceramic block.