CN100595077C - 一种环保耐用黑板及制造方法 - Google Patents

一种环保耐用黑板及制造方法 Download PDF

Info

Publication number
CN100595077C
CN100595077C CN200610126035A CN200610126035A CN100595077C CN 100595077 C CN100595077 C CN 100595077C CN 200610126035 A CN200610126035 A CN 200610126035A CN 200610126035 A CN200610126035 A CN 200610126035A CN 100595077 C CN100595077 C CN 100595077C
Authority
CN
China
Prior art keywords
blackboard
fiberglass
glass epoxy
foamed plastic
face
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200610126035A
Other languages
English (en)
Other versions
CN1958305A (zh
Inventor
刘德安
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200610126035A priority Critical patent/CN100595077C/zh
Publication of CN1958305A publication Critical patent/CN1958305A/zh
Application granted granted Critical
Publication of CN100595077C publication Critical patent/CN100595077C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明一种玻璃钢黑板及其生产方法,属于用玻璃钢制作黑板技术领域。它所要解决的技术问题是提供一种玻璃钢环保耐用黑板及其生产方法;本发明的黑板不用黑板漆、书写面的表面粗糙度用不去除材料的方法在模具粗糙面上直接形成,因此可有效控制黑板书写面的表面质量,本发明造价低廉、经久耐用、使用安全,主要用于学校、企事业单位,深受广大师生等欢迎。

Description

一种环保耐用黑板及制造方法
技术领域
本发明是一种玻璃钢黑板及其生产方法,属于黑板制造技术领域,特别涉及用玻璃钢制造黑板的技术领域。
背景技术
目前使用的黑板有水泥黑板、金属黑板、玻璃黑板,有的经过一段时间使用后,表面受空气、阳光侵蚀,氧化、变质,有的存在表面粗糙、粉笔尘较多,他们一方面影响学生视力,另一方面影响师生身体健康。金属黑板易变形。而现有的玻璃黑板,表面太粗糙,凹凸明显,粉笔灰较多粉笔灰易藏在凹处,且不易檫干净,黑板不黑,呈白灰色,板书困难,字迹不清晰。国家知识产权局2000年3月22日公开了“一种吸磁性树脂复合板材及其无尘黑板的制作方法”,它公开的板材具有强度高、不锈蚀、不变形、坚固耐用的优点,其黑板具有书写流利、粉尘极低、字迹清晰、易擦易洗的优点;但生产过程中需要将板材毛坯放入水中浸泡5~10小时,浸泡前按其浸泡水量加入2%~10%的氢氧化纳于水中,将浸泡好的板材毛坯取出用清水冲洗干净后将其晒干,然后在板材面上刮一层铁粉和石膏粉后进行打磨,将打磨好的板材涂上树脂胶即得吸磁性树脂复合板材成品;生产工艺复杂,生产成本高,而且在打磨过程中回产生大量粉尘,容易对环境造成污染。
发明内容
本发明的目的在于公开一种强度高、重量轻、不锈蚀、耐磨性好、不需要打磨、使用的复合树脂少因而成本低廉的环保耐用黑板及制造方法。
本发明的技术方案为:
一种环保耐用黑板,由玻璃钢板面、衬板和边框构成,玻璃钢板面在平板模具上一次成型。平板模具由玻璃钢制成,模具形状大小与黑板的形状大小相当,模具工作面用160~200微米基本粒度的磨料充分打磨形成黑板书写面所需的粗糙面;玻璃钢板面的制作工艺为:先在模具工作表面涂上一层脱模剂,再把用树脂、颜料、填料三者搅拌混合的原料涂覆在脱模剂上,在混合的原料上放置一层玻璃纤维布,然后再在玻璃纤维布上涂覆混合的原料,玻璃钢总厚度为1~4毫米,经固化干燥后从模具上取出玻璃钢黑板板面;玻璃钢黑板板面直接在模具粗糙面上形成自然书写面,其表面粗糙度轮廓算数平均偏差为6.3~12.5微米,玻璃钢板面的书写面的颜色由颜料决定,不涂黑板漆,把制成的玻璃钢黑板板面与衬板粘接一起,与衬板一起镶嵌在边框中。
本发明与现有技术相比,由于采用了上述技术方案,黑板所用树脂少,产品成本低、强度高,重量轻、不锈蚀,不开裂,黑板书写面表面粗糙度容易控制在最佳状态。由于书写面的表面粗糙度用不去除材料的方法获得,省去了烦琐的打磨过程,因而简化生产工艺,产品质量容易掌握,在书写时书写流利、字迹清晰、易擦易洗,书写表面不会因粉笔灰堆积而呈灰白色、反光柔和不怕日晒雨淋,可用于室内外任何场所。
本发明的实施例:
一种环保耐用黑板,由玻璃钢板面、衬板和边框构成,玻璃钢板面在平板模具上一次成型。平板模具由玻璃钢制成,模具形状大小与黑板的形状大小相当,模具工作面用160~200微米基本粒度的磨料充分打磨形成粗糙面;玻璃钢板面的制作工艺为:先在模具工作表面涂上一层脱模剂,再把用树脂、颜料、填料三者搅拌混合的原料涂覆在脱模剂上,在混合的原料上放置一层玻璃纤维布,然后再在玻璃纤维布上涂覆混合的原料,经固化干燥后从模具上取出玻璃钢黑板板面;玻璃钢黑板板面直接在模具粗糙面上形成自然书写面,其表面粗糙度轮廓算数平均偏差为6.3~12.5微米,玻璃钢板面的书写面的颜色由颜料决定,不涂黑板漆,把制成的玻璃钢黑板板面与衬板粘接一起,衬板用木板和发泡塑料板粘接而成,发泡塑料板在黑板板面与木板之间起填充作用;将黑板板面的背面与起填充作用的发泡塑料正面粘接,发泡塑料的背面与起支撑作用的木板粘接,配上黑板边框形成完整的黑板。

Claims (2)

1、一种环保耐用黑板,由玻璃钢板面、衬板和边框构成,其特征在于:玻璃钢板面在平板模具上一次成型,平板模具由玻璃钢制成,模具形状大小与黑板的形状大小相当,模具工作面用160~200微米基本粒度的磨料充分打磨形成黑板书写面所需的粗糙面;玻璃钢板面的制作工艺为:先在模具工作表面涂上一层脱模剂,再把用树脂、颜料、填料三者搅拌混合的原料涂覆在脱模剂上,在混合的原料上放置一层玻璃纤维布,然后再在玻璃纤维布上涂覆混合的原料,玻璃钢总厚度为1~4毫米,经固化干燥后从模具上取出玻璃钢黑板板面;玻璃钢黑板板面直接在模具粗糙面上形成自然书写面,其表面粗糙度轮廓算数平均偏差为6.3~12.5微米,玻璃钢板面的书写面的颜色由颜料决定,不涂黑板漆,把制成的玻璃钢黑板板面与衬板粘接一起,与衬板一起镶嵌在边框中。
2、权利要求1所述的环保耐用黑板,其特征在于:衬板用木板和发泡塑料板粘接而成,发泡塑料板在黑板板面与木板之间起填充作用;将黑板板面的背面与起填充作用的发泡塑料正面粘接,发泡塑料的背面与起支撑作用的木板粘接。
CN200610126035A 2006-08-28 2006-08-28 一种环保耐用黑板及制造方法 Expired - Fee Related CN100595077C (zh)